• Title/Summary/Keyword: nano crystalline

Search Result 424, Processing Time 0.039 seconds

Development of Nano Crystal Embedded Polymorphous Silicon Thin Film by Neutral Beam Assisted CVD Process at Room Temperature

  • Jang, Jin-Nyoung;Lee, Dong-Hyeok;So, Hyun-Wook;Yoo, Suk-Jae;Lee, Bon-Ju;Hong, Mun-Pyo
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.171-171
    • /
    • 2012
  • Neutral beam assisted chemical vapor deposition (NBa-CVD) process has been developed as a nove,l room temperature deposition process for the light-soaking free nano-crystalline silicon (nc-Si) thin films including intrinsic and n-type doped thin film. During formation of nc-Si thin films by the NBa-CVD process with silicon reflector at room temperature, the energetic particles enhance doping efficiency and crystalline phase in nc-Si thin films without additional heating at substrate. The effects of incident NB energy controlled by the reflector bias have been confirmed by Raman spectra analysis. Additionally, TEM images show uniform nc-Si grains which imbedded amorphous phase without incubation layer. The nc-Si films by the NBa-CVD are hardly degenerated by light soaking; the degradations of photoconductivity were just a few percents before and after light irradiation.

  • PDF

The Relation of Crystallite Size and Ni2+ Content to Ferromagnetic Resonance Properties of Nano Nickel Ferrites

  • Lafta, Sadeq H.
    • Journal of Magnetics
    • /
    • v.22 no.2
    • /
    • pp.188-195
    • /
    • 2017
  • The ferromagnetic resonance and other magnetic properties dependence on $Ni^{2+}/Fe^{3+}$ ratio and crystallite size were investigated for nano nickel ferrite ($NiFe_2O_4$). The crystallite size was controlled by controlling the nickel content in the starting material solution. The XRD and TEM were utilized to measure the crystallite size through Scherrer formula and particle size respectively. The most frequent particle sizes were lower than crystallite size, which ranged from 16.5 to 44.65 nm. The general behavior of M-H loop shapes and parameters showed superparamagnetic one. The saturation magnetization had a maximum value at $Ni^{2+}/Fe^{3+}$ molar ratio equal to 0.186. The FMR signals showed, generally, broad linewidths, where the maximum width and minimum resonance field were for the sample of the lowest crystalline size. Furthermore, FMR resonance field shows linear dependence on crystalline size. The fitting relation was estimated to express this linear dependency on the base of behavior coincidence between particle size and the inverse of saturation magnetization. The given interpretations to understand the intercept and the slope meanings of the fitted relation were based on Larmor equation, and inhomogeneous in the anisotropy constant.

Dielectric properties of bismuth magnesium niobate thin films deposited by sputtering using two main phase target in the system (두 메인 상의 타겟을 사용하여 스퍼터링으로 증착한 bismuth magnesium niobate 박막의 유전특성)

  • Ahn, Jun-Ku;Kim, Hae-Won;Yoon, Soon-Gil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.264-264
    • /
    • 2007
  • $B_2Mg_{2/3}/Nb_{4/3}O_7\;(B_2MN)$ thin films and $Bi_{3/2}MgNb_{3/2}O_7\;(B_{1.5}MN)$ thin films were deposited as a function of various deposition temperatures on Pt/$TiO_2/SiO_2$/Si substrates by radio frequency magnetron sputtering system. Both of their thin films are shown to crystalline phase at $500^{\circ}C$, deposition temperature, using 100W RF power. The composition of them and structural micro properties are investigated by RBS spectrum and SEM, AFM. 200 nm-thick $B_2MN$ thin films were deposited at room temperature had capacitance density of $151nF/cm^2$ at 100kHz, dissipation factor of 0.003 and had capacitance density of $584nF/cm^2$ at 100kHz, dissipation factor of 0.0045 at $500^{\circ}C$ deposition temperature. Both of their dielectric constant deposited at room temperature and at $500^{\circ}C$ were each approximately 40 and 100.

  • PDF

Synthesis of TiO2 nanoparticles using Water-in-oil microemulsion method (유중수형(油中水型) 마이크로에멀젼법을 이용한 타이타니아 나노입자의 제조)

  • So Min Jin;Hyeon Jin;Seong Ju Kim;Yu Na Kim;Dae-Won Lee
    • Journal of Industrial Technology
    • /
    • v.43 no.1
    • /
    • pp.1-6
    • /
    • 2023
  • TiO2 is a versatile metal oxide material that is frequently used as a photo-catalyst for organic pollutant oxidation and a functional material for ultraviolet-ray protection. To improve its chemical/physical properties and widen the range of industrial application, it is demanded to control the crystalline feature and morphology precisely by applying advanced nano-synthesis methods. In this study, we prepared TiO2 nanoparticles using the water-in-oil (W/O) microemulsion method and compared them with the particles synthesized by the conventional precipitation method. Also, we tried to find the optimum conditions for obtaining nano-sized, anatase-rich TiO2 particles by the W/O microemulsion method. We analyzed the crystalline feature and particle size of the prepared samples using X-ray diffraction (XRD) and Transmission electron microscopy (TEM). In summary, we found the W/O microemulsion is more effective than precipitation in obtaining nano-sized TiO2. The best result was derived when the microemulsion was formed using AOT surfactant, hydrolysis was performed under basic condition and the sample was calcined at 200℃.

Characterization of Photoelectron Behavior of Working Electrodes with the Titanium Dioxide Window Layer in Dye-sensitized Solar Cells

  • Gong, Jaeseok;Choi, Yoonsoo;Lim, Yeongjin;Choi, Hyonkwang;Jeon, Minhyon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.346.1-346.1
    • /
    • 2014
  • Porous nano crystalline $TiO_2$ is currently used as a working electrode in a dye-sensitized solar cell (DSSC). The conventional working electrode is comprised of absorption layer (particle size:~20 nm) and scattering layer (particle size:~300 nm). We inserted window layer with 10 nm particle size in order to increase transmittance and specific surface area of $TiO_2$. The electrochemical impedance spectroscope analysis was conducted to analysis characterization of the electronic behavior. The Bode phase plot and Nyquist plot were interpreted to confirm the internal resistance caused by the insertion of window layer and carrier lifetime. The photocurrent that occurred in working electrode, which is caused by rise in specific surface area, increased. Accordingly, it was found that insertion of window layer in the working electrode lead to not only effectively transmitting the light, but also increasing of specific surface area. Therefore, it was concluded that insertion of window layer contributes to high conversion efficiency of DSSCs.