• 제목/요약/키워드: molten steel

검색결과 240건 처리시간 0.032초

DEVELOPMENT OF IMMERSION TYPE MOLTER STREEL LEVELMETER

  • Morii, Michio;Azuma, Makoto;Kobayashi, Kazuo;Tezuka, Masao
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 1990년도 한국자동제어학술회의논문집(국제학술편); KOEX, Seoul; 26-27 Oct. 1990
    • /
    • pp.1316-1321
    • /
    • 1990
  • Molten steel level information of ladle is very important for process control in steelmaking process. At secondary refining process, measuring lance and snokel have to keep constant thier depth from molten steel surfaces. But, there is much slag on the molten steel surface. Besides, not only the thickness of slag is varied with refining condition, but also molten steel level is largely affected by firebrick errosion. Then, optical measuring method and/or by human eyes cannot detect true molten steel surface, but slag surface. This slag thickness is 300mm at maximum, then huge diameter eddy current sensor will be needed if that type sensor is applied. In addition to, cooling system is necessary because the molten steel and slag temperature is high. This is not practically. To solve this problem, immersion type levelmeter is developed. This sensor is made up from primary and secondary cylindrical coils. High frequency current is applied to primary coil. Electro-motive force from secondary coil is measured, which is varied with molten steel level. This complete set is installed within stainless steel long capsule and attached to top of lance. This sensor is immersed into molten steel bath of ladle or tundish with protection of expendable paper sleeve.

  • PDF

Ladle내 잔류(殘留) 용융(熔融)슬래그의 LF 공정(工程)으로 재활용(再活用)에 관한 연구(硏究) (A Study on the Recycling of Molten Ladle Slag Residue into LF Process)

  • 김영환;유정민;김동식;임종훈;양성호
    • 자원리싸이클링
    • /
    • 제22권1호
    • /
    • pp.36-41
    • /
    • 2013
  • 전기로 제강공정 중 LF 공정에서 슬래그는 전기로(EAF)에서 이월된 슬래그와 출강 중에 조재제인 생석회, 돌로마이트 등이 용강 중에 투입되어 생성된다. LF 조업이 끝나면 ladle은 연속주조 공정(CCM)으로 이송되며, ladle 하부의 노즐을 통해 tundish로 용강을 내보내어 연속 주조조업을 하게 된다. 일반적으로 연속 주조공정 후 ladle에 남는 슬래그와 잔강(殘鋼)은 슬래그 포트(Pot)에 받아 슬래그 야적장으로 이송되어 파쇄 후 처리된다. 본 연구에서는 연속 주조공정 후 ladle에 잔류한 용융슬래그(잔강(殘鋼) 포함)를 전기로 출강 후에 ladle 상부에 직접 투입하여 LF 공정 초기의 슬래그를 형성하는데 활용하고자 하였다. 그 결과 LF 공정 중에 사용되는 생석회의 원단위는 2.2 ~ 3.2 kg/steel-ton 저감되었으며, 용강의 생산회수율은 0.3 ~ 0.5% 증가되었다.

연주 탕면레벨 안정화를 위한 하이브리드형 퍼지제어기 설계 (Design of hybrid-type fuzzy controller for stabilizing molten steel level in high speed continuous casting)

  • 이덕만;권영섭;이상호
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 2000년도 제15차 학술회의논문집
    • /
    • pp.67-67
    • /
    • 2000
  • In this paper, a hybrid type fuzzy controller is proposed to maintain molten steel level stable and reliable manner in high speed continuous casting regardless of various disturbances such as casting speed change, tundish weight variation, 치ogging/undoning of SEN(Submerged Entry Nozzle), periodic bulgings, etc. To accomplish this purpose, hardware filter and software filer are carefully designed to eliminate high frequency noise and to smooth input signals from harsh environments. In order to minimize the molten steel level variations from various disturbances the controller uses hybrid type control term: fuzzy logic term, proportional term, differential term and nonlinear feedback compensation tenn. The proposed controller is applied tn commercial mini-mill plant and shows considerable improvement in minimizing the molten steel variation.

  • PDF

A Numerical Analysis of Molten Steel Flow Under Applied Magnetic Fields in Continuous Casting

  • Yoon, Teuk-Myo;Kim, Chang-Nyung
    • Journal of Mechanical Science and Technology
    • /
    • 제17권12호
    • /
    • pp.2010-2018
    • /
    • 2003
  • Although continuous casting process has highly developed, there still remain many problems to be considered. Specifically, two vortex flows resulting from impingement against narrow walls make a flow field unstable in a mold, and it is directly related to internal and external defects of steel products. To cope with this instability, EMBR (Electromagnetic Brake Ruler) technique has been lately studied for the stability of molten steel flow, and it is revealed that molten steel flow in a mold can be controlled with applied magnetic field. However, it is still difficult to clarify flow pattern in an EMBR caster due to complex correlations among variables such as geometric factors, casting conditions, and the place and the intensity of charged magnetic field. In the present study, flow field in a mold is focused with different conditions of electromagnetic effect. To accurately analyze the case, three dimensional low Reynolds turbulent model and appropriate boundary conditions are chosen. To evaluate the electromagnetic effect in molten steel flow, dimensionless numbers are employed. The results show that the location and the intensity of the applied magnetic field significantly influence the flow pattern. Both impingement and internal flow pattern are changed remarkably with the change of the location of applied magnetic field. It turns out that an insufficient magnetic force yields adverse effect like channeling, and rather lowers the quality of steel product.

수명을 향상시키기 위해 Al 메탈 코팅과 양극산화처리된 Steel 도가니의 파괴 거동 (Fracture Behavior of Fe Crucible in Molten Aluminum Coated with Al and Anodized Al)

  • 차태민;신병현;황명원;김도형;정원섭
    • 한국표면공학회지
    • /
    • 제51권1호
    • /
    • pp.34-39
    • /
    • 2018
  • Steel crucible used for molten Al has a problem of very limited lifetime because of the interaction between Fe and molten Al. This study was performed to improve the lifetime of steel crucible for molten Al by coating metallic Al and by further anodizing treatment to form thick and uniform anodic oxide films. The lifetime of the steel crucible was improved slightly by Al coating from 30 to 40 hours by metallic Al coating and largely to 120 hours by coating the surface with anodic oxide film. The improved lifetime was attributed to blocking of the reaction between Fe and molten Al with the help of anodic oxide layer with more than 20 um thickness on the crucible surface. The failure of the steel crucible arises from the formation of intermetallic compounds and pores at the steel/Al interface.

쌍롤 연속 주조에서의 난류 유동, 온도 및 응고 예측을 위한 연구 (A Numerical Study of Turbulent Flow, Heat Transfer, and Solidification in Twin-Roil Continuous Casting)

  • 하만영;최봉석
    • 대한기계학회논문집B
    • /
    • 제23권1호
    • /
    • pp.12-24
    • /
    • 1999
  • A computer program has been developed for analyzing the two-dimensional, unsteady conservation equations for transport phenomena in the molten region of twin-roll continuous casting in order to predict the turbulent velocity, temperature fields, and solidification process of the molten steel. The energy equation of the cooling roll is solved simultaneously with the conservation equations of molten steel in order to consider heat transfer through the cooling roll. The results show the velocity, temperature and solidification pattern in the molten region with roll temperature as a function of time. The results for velocity and temperature fields with solidification are compared with those without solidification, giving different thermofluid characteristics in the molten region. We also investigated the effects of revolutional speed of roll, superheat and nozzle geometry on the turbulent flow, temperature and solidification in the molten steel and temperature fields in the cooling roll.

턴디쉬용 코팅재에 의한 강중 개재물 저감효과 (The Removal of Inclusions in Molten Steel by Coating Materials for Tundish)

  • 조문규;이석근
    • 한국세라믹학회지
    • /
    • 제35권1호
    • /
    • pp.33-40
    • /
    • 1998
  • A MgO-CaO-based coating material for ferrous melt refining is applied to the tundish operation for mol-ten steel having low carbon. The changes in the total oxygen content insoluble aluminum content and the content of inclusions in molten steel during tundish operation were measured at the pouring part strand of tundish and mold. On the basis of the experimental results the interfacial reaction occurring between the coating materials and the molten steel in tundish was discussed and compared with the theoretical con-sideration. It is concluded that interfacial reaction is not active at the strand part of tundish but is active at the pouring part because of the turbulent flow in the molten steel.

  • PDF

연속 주조의 용강 높이 제어를 위한 퍼지-PI 제어기 (Fuzzy-PI controller for molten steel level of continuous casting process)

  • 주문갑;김도응;김호경;김종민
    • 한국지능시스템학회논문지
    • /
    • 제18권4호
    • /
    • pp.488-493
    • /
    • 2008
  • 본 논문은 연속 주조 공정에서의 용강 높이에 대한 수학적인 비선형모델을 유도하는데, 여기에는 용강 높이, 몰드내의 입출력 유량, 스토퍼의 위치와 입력유량의 관계 등이 고려되었다. 비선형 모델은 MATLAB을 사용하여 구현되었으며 실제 데이터와 비교하여 수학적 모델이 유효함을 확인하였다. 구현된 비선형 모델을 사용하여, 퍼지 시스템에 의하여 변화하는 $K_p$값을 가지는 퍼지 PI 제어기를 사용하여, 기존에 사용되던 PI 제어기보다 나은 제어 성능 및 외란에의 강인성을 가짐을 시뮬레이션으로 보였다.

필터댐에 의한 강중 개재물 저감효과 (Removal of Inclusions in molten Steel by Filter Dam)

  • 조문규;이석근;정두화;남수희;이재우
    • 한국세라믹학회지
    • /
    • 제35권2호
    • /
    • pp.201-207
    • /
    • 1998
  • A tube-type filter dam(or baffle with holes) for ferrous melt refining is applied to the tundish operation for molten steel having low carbon and ultra-low carbon. The changes in the total oxygen content insoluble aluminum content and the distribution of inclusion size in molten steel during tundish operation were in-vestigated at the pouring part strand and mold of tundish. Removal mechanism of inclusions is considered to be caused by buoyancy action of the filter dam better than filtration action and the size range of in-clusions filtrated by the filter dam was for 30-50$\mu\textrm{m}$. Decrease in deviation of inclusion content in molten steel was confirmed for appling the filter dam in comparison with using conventional dam and weir. Also the filter dam had the advantage of baffle with holes at lower part in the efficiency of inclusions removal.

  • PDF

사파이어 광섬유를 이용한 용선 온도측정 (Measurement of the Molten Steel Temperature Using the Sapphire Fiber)

  • Kim, Hasul;Homun Bae
    • 한국광학회:학술대회논문집
    • /
    • 한국광학회 2000년도 제11회 정기총회 및 00년 동계학술발표회 논문집
    • /
    • pp.240-241
    • /
    • 2000
  • Sapphire fiber has been used to provide an optical path for the total radiation pyrometry. In measuring the temperature, we use the two-color detector, which consists of a high-performance Silicon detector mounted in a "sandwich" configuration over a Germanium detector. Sapphire fiber can withstand high temperature in the molten steel for two and a half hours. The maximum value of the error is the $\pm$2.5$^{\circ}C$ in the range of 152$0^{\circ}C$~1$600^{\circ}C$. This paper presents the simple scheme for measuring the molten steel temperature in the blast furnace of the iron & steel making process.g process.

  • PDF