INFLUENCE OF LIGHT IRRADIATION OVER SELF-PRIMING ADHESIVE ON DENTIN BONDING (상아질접착제에 대한 광조사가 접착에 미치는 영향)

  • 류현욱;김기옥;김성교
    • Restorative Dentistry and Endodontics
    • /
    • v.26 no.5
    • /
    • pp.409-417
    • /
    • 2001
  • The purpose of this study was to investigate the influence of light irradiation over self-priming adhesive on dentin bonding. After acid etching the exposed dentin, a self-priming adhesive (Prime&Bond$^{\circledR}$NT dental adhesive system Dentsply DeTrey, GmbH, Konstanz, Germany) was applied and light irradiation was done for 20 sec with regular intensity (600 mW/$\textrm{cm}^2$) in group I and for 3 sec with ultra-high intensity (1930 mW/$\textrm{cm}^2$) in group III. No light irradiation was done over self-priming adhesive in groups II and IV. Composite resin was added on the self-priming adhesive and irradiated for 40 sec with regular intensity (600 mW/$\textrm{cm}^2$) in groups I and II and for 3 sec with ultra-high intensity (1930 mW/$\textrm{cm}^2$) in groups III and IV. To see the effect of light curing time on dentin bonding, another 3 group specimens were prepared. Without light-irradiation over self-priming adhesive, added composite resin was irradiated for 3, 6, or 12 sec with ultra-high intensity light. After bonded specimens were stored in 37$^{\circ}C$ distilled water for 24 hours, shear bond strength were measured using a universal testing machine (4202, Instron, Instron Co., U.S.A.) and fractured surfaces were examined under a stereomicroscope (SZ-PT Olympus, Japan). Statistical analysis were done with one-way, two-way ANOVA and chi-square test. The results were as follows : 1. The shear bond strengths from the groups irradiated over self-priming adhesive were significantly higher than those from the groups without irradiation (p<0.05). 2. There was no significant shear bond strength difference between regular intensity light irradiation groups and ultra-high intensity ones (p>0.05). 3. There was no significant shear bond strength difference among various irradiation time groups with ultra-high intensity ones (p>0.05). 4. In stereomicroscopic examination of fractured surfaces, adhesive-cohesive mixed failure mode was mostly seen in all groups, and there was no significant difference in failure mode among groups (p>0.05).

  • PDF