• Title/Summary/Keyword: microstructure hardness

Search Result 1,339, Processing Time 0.033 seconds

Mechanical and Forming Characteristics of High-Strength Boron-Alloyed Steel with Hot Forming (핫 포밍을 이용한 고강도 보론 첨가 강의 기계적 및 성형 특성 평가)

  • Chae, M.S.;Lee, G.D.;Suh, Y.S.;Lee, K.H.;Kim, Y.S.
    • Transactions of Materials Processing
    • /
    • v.18 no.3
    • /
    • pp.236-244
    • /
    • 2009
  • In response to growing environmental and collision-safety concerns, the automotive industry has gradually used high-strength and ultla-high-strength steels to reduce the weight of automobiles. In order to overcome inherent process disadvantages of these materials such as poor formability and high springback at room temperature, hot forming has recently been developed and adopted to produce some important structural parts in automobiles. This method enables manufacturing of components with complex geometric shapes with minimal springback. In addition, a quenching process may enhance the material strength by more than two times. This paper investigates mechanical and forming characteristics of high-strength boron-alloyed steel with hot forming, in terms of hardness, microstructure, residual stress, and springback. In order to compare with experimental results, a finite element analysis of hot forming process coupled with phase transformation and heat transfer was carried out using DEFORM-3D V6.1 and also, to predict high temperature mechanical properties and flow curves for different phases, a material properties modeler, JMatPro was used.

Fabrication of WC-Ni-Si-B4C Composite and Diffusion Bonding with Stainless Steel (WC-Ni-Si-B4C계 초경합금 제조 및 스테인레스 스틸과의 확산접합)

  • Won, Jong-Wun
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.24 no.6
    • /
    • pp.594-598
    • /
    • 2015
  • The effects of Ni on the mechanical properties of WC-Xwt.%Ni-1.5wt.%Si-1.1wt.%$B_4C$ composite (X = 21.6, 23.6, 25.6 and 27.6 wt.%) were investigated in order to replace Co with Ni as the binder metal for hard materials based on WC-Co system. Using X-ray diffraction, optical microscopy, field-emission scanning electron microscopy results, the microstructure, pore distribution and grain size of the composites sintered at $1,150^{\circ}C$ were examined with different fraction (X = 21.6, 23.6, 25.6 and 27.6 wt.%) of binder metal Ni. The average WC grain size of the $WC-Ni-Si-B_4C$ composites was about $1{\mu}m$. The Rockwell hardness : A (HRA) and transverse rupture strength were about 88HRA and $110kgf/mm^2$, respectively. The obtained sample was bonded with SM45C at a temperature of $1,050^{\circ}C$. The thickness and mechanical properties of the bonded area were investigated with different dwell time at a bonding temperature of $1,050^{\circ}C$.

The Influence of Microstructures on the Change of Monotonic Tensile Fracture Mode in Al-Li-Cu-Zr Alloy with Ageing (Al-Li-Cu-Zr합금의 시효에 따른 인장파괴모드변화에 미치는 미세조직의 영향)

  • Chung, D.S.;Lee, S.J.;Cho, H.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.9 no.3
    • /
    • pp.212-218
    • /
    • 1996
  • To clarify the influence of precipitation microstructure and inclusion on the monotonic tensile fracture behaviors in 2090 alloy aged at $180^{\circ}C$, the detailed measurement of hardness, tensile strength, elongation and the observation of scanning electron micrography, transmision electron micrography have been carried out. The transgranular shear ductile fracture has been observed in specimen quenched after solution treatment at $500^{\circ}C$ for 45min. While the under-aged specimen was fractured in both transgranular shear ductile and intergranular fracture mode, the fracture mode of peak-aged and over-aged alloy was predominantly intergranular fracture. The fracture behavior of each ageing condition was influenced by the change of precipitation microstructural features. In the case of peak-aged and over-aged alloys, the coarse and heterogeneous slip band caused by both shearable nature of the ${\delta}^{\prime}(Al_3Li)$ precipitates and PFZ along the high angle grain boundary aid the localization of deformation, resulting in low energy intergranular fracture. It was also estimated that the fractured T-type intermetallic phases (inclusion) and the equilibrium ${\delta}$(AlLi) phases which were formed at grain boundaries palyed an important role in promoting intergranular fracture mode.

  • PDF

Abrasive Wear Characteristics of Materials for Diesel Engine Cylinder Liner and Piston Ring (디젤엔진 실린더 라이너-피스톤 링 소재의 연삭 마멸 특성)

  • Jang, Jeong-Hwan;Kim, Jung-Hoon;Kim, Chang-Hee;Moon, Young-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.20 no.2
    • /
    • pp.72-77
    • /
    • 2007
  • Abrasive wear between piston ring face and cylinder liner is an extremely unpredictable and hard-to-reproduce phenomenon that significantly decreases engine performance. Wear by abrasion are forms of wear caused by contact between a particle and solid material. Abrasive wear is the loss of material by the passage of hard particles over a surface. From the pin-on-disk test, particle dent test and scuffing test, abrasive wear characteristics of diesel engine cylinder liner-piston ring have been investigated. Pin-on-disk test results indicate that abrasive wear resistance is not simply related to the hardness of materials, but is influenced also by the microstructure, temperature, lubricity and micro- fracture properties. In particle dent test, dent resistance stress decreases with increasing temperature. From the scuffing test by using pin-on-disk tester, scuffing mechanisms for the soft coating and hard coating were proposed and experimentally confirmed.

Cr - Mo鋼 熔接 後熱處理材 의 勞破壞 에 關한 硏究

  • 박재규;김석원;김연식
    • Journal of Welding and Joining
    • /
    • v.3 no.2
    • /
    • pp.16-26
    • /
    • 1985
  • Post weld heat treatment(PWHT), at more than 600.deg. C, is essential to remove residual stress and hydrogen in weld HAZ and improve fatigue characteristics. However, residual stress during PWHT is responsible for PWHT embitterment and it promotes precipitation of impurities to grain boundary. In this paper, the effect of stress simulated residual stress on fatigue failure was evaluated by fatigue test, microhardness test and fractograph. The obtained results are summarized as follows; (1) The fatigue crack growth rate(da/dN) of parent and heat treated parent was affected by microstructure due to heat treatment and it depended on stress intensity factor (.DELTA.k). (2) The fatigue strength of weld HAZ was dependent on applied stress during PWHT and da/dN after PWHT was slower than as-weld. (3) Softening amount of weld HAZ was bigger than any other due to PWHT. Hardness value of weld HAZ was affected by heat treatment under the applied stress of 10 $kgf/mm^2$, but beyond 20 $kgf/mm^2$ it was increased by the applied stress rather than heat treatment. (4) Beyond the applied stress of 20 $kgf/mm^2$ during PWHT, intergranular fracture surface was observed and its amount was increased with applied stress during PWHT. (5) Effect of applied stress during PWHT on aspect of fracture surface was larger rather than that on fatigue crack growth behavior.

  • PDF

Evaluation of the Reactivity of Bulk Nano Ni/Al Powder Manufactured by Shock Compaction Process (충격압분공정으로 제조된 나노 니켈/알루미늄 혼합분말재의 특성 평가)

  • Kim, W.;Ahn, D.H.;Park, L.J.;Kim, H.S.
    • Transactions of Materials Processing
    • /
    • v.26 no.4
    • /
    • pp.216-221
    • /
    • 2017
  • Recently, interest in multifunctional energetic structural materials (MESMs) has grown due to their multifunctional potential, especially in military applications. However, there are few studies about extrinsic factors that govern the reactivity of MESMs. In this paper, a shock compaction process was performed on the nano Ni/Al-mixed powder to investigate the effect of particle size on the shock reaction condition. Additionally, heating the statically compacted specimen was also performed to compare the mechanical properties and microstructure between reacted and unreacted material. The results show that the agglomerated structure of nanopowders interrupts the reaction by reducing the elemental boundary. X-ray diffraction analysis shows that the NiAl and $Ni_3Al$ intermetallics are formed on the reacted specimen. The microhardness results show that the $Ni_3Al$ phase has a higher hardness than NiAl, but the portion of $Ni_3Al$ in the reacted specimen is minor. In conclusion, using Ni/Al composites as a reactive material should focus on energetic use.

Prediction on the Wear Resistance of Contact Tips for GMA Welding (GMA용접에서 콘택트팁의 내마모성에 대한 예측)

  • 김남훈;김희진;유회수;고진현
    • Journal of Welding and Joining
    • /
    • v.22 no.4
    • /
    • pp.35-42
    • /
    • 2004
  • Contact tips are required to have a higher resistance to wear and thus to have an extended life time under the advanced GMAW welding process. Several requirements have been specified and employed by domestic industries for selecting their tips for such a purpose. However no attempt has been made to justify their requirements based on the experimental data of wear resistance or life time of contact tips. In this study, five different contact tips with three different compositions were employed for actual GMA welding up to 4 hours and were evaluated their wear resistance by measuring in every one hour the area of enlarged hole at the exit side. Experimental results clearly showed that the Cr-containing tips strengthened by precipitation hardening have much better resistance to wear than those made by work hardening. It was further noticed that Cr is an excellent alloying element for improving the wear resistance of contact tips only when it is in an properly aged condition. Initial hardness may play some role in the early stage of wear but not in the later stage of welding because the microstructure of tip changes significantly by the prolonged exposure to welding arc heat. Based on these results, critical review has been made on the current requirements employed by domestic industries. Of importance is that a new guideline has been confirmed to be more reasonable.

Effects of Amorphous Phase Fraction on the Scratch Response of NiTiZrSiSn Bulk Meatllic Glass in the Kinetic Spraying Process (저온분사공정을 통한 NiTiZrSiSn 벌크 비정질 코팅의 비정질 분율에 따른 스크래치 반응)

  • Yoon, Sang-Hoon;Kim, Soo-Ki;Lee, Chang-Hee
    • Journal of Welding and Joining
    • /
    • v.25 no.3
    • /
    • pp.28-36
    • /
    • 2007
  • A bulk amorphous NiTiZrSiSn powder produced using an inert gas atomization was sprayed by kinetic spraying process that is basically a solid-state deposition process onto a mild steel substrate. They were successfully overlaid onto the mild steel substrate. In order to evaluate the tribological behavior of the kinetic sprayed NiTiZrSiSn BMG (Bulk Metallic Glass) coatings, a partially crystallized coating and a fully crystallized coating were prepared by the isothermal heat treatments. Tribological behaviors were investigated in view of friction coefficient, hardness and amorphous phase fraction of coating layer. Surface morphologies and depth in the wear tracks were observed and measured by scanning electron microscope and alpha-step. From the examination of the scratch wear track microstructure, transition from the ductile like deformation (micro cutting) to the brittle deformation (micro fracturing) in the scratch groove was observed with the increase of the crystallinity.

Characterization of electron beam (EB) welds for SUS310S

  • Kim, Hyun-Suk;Castro, Edward Joseph D.;Lee, Choong-Hun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.02a
    • /
    • pp.360-360
    • /
    • 2011
  • In this work, SUS310S used for valve plate assembly was electron beam (EB) welded to determine the influence of the parametric conditions on the characteristics of the weld and to minimize porosity and micro-fissures among others. The evolution in the weld geometry and microstructure was examined as a function of the process conditions such as beam current and focusing current under a constant welding speed and accelerating voltage. The integrity of the EB welds in SUS310S was examined for defects (e.g. cracking, porosity, etc.), adequate penetration depth, and tolerable weld width deviation for the various welding conditions. Optical microscopy (OM), x-ray photoelectron spectroscopy analysis (XPS), scanning electron microscopy (SEM) and 3D micro-computed tomography (Micro-CT) for the cross section analysis of the electron beam welded SUS310S were utilized. The tensile strength and hardness were analyzed for the mechanical properties of the EB weld. At the 6 kV accelerating voltage, it was determined that a satisfactory penetration depth and desirable weld width deviation requires a beam current of 30 mA and a focusing current of 0.687 A at the welding speed of 25 mm/sec.

  • PDF

The Effect of Long Term Thermal Aging on High Temperature Mechanical Properties in STS316 (장시간 시효처리가 316 스트인리스 강의 고온 기계적 성질에 미치는 영향)

  • 임지우;정찬서;임병수
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.10 no.2
    • /
    • pp.110-116
    • /
    • 2002
  • At elevated temperature, very complex precipitations occur in STS316. To investigate the effect of the precipitation on mechanical properties in SIS316, tensile tests and fatigue crack growth tests were carried out at $650^{\circ}C$ using artificially degraded materials. The material degradation was simulated by aging for up to 20000 hrs. at $750^{\circ}C$, which is equal to 179000hrs (about 20yrs) of service life at $650^{\circ}C$, after conducting solution treatment for 20 min. at $11300^{\circ}C$. The result of the hardness test and the tensile test showed that both properties are closely related to the mean free distance of carbides. Also, from the results of fracture tests at $650^{\circ}C$, ${\triangle}K_{th}$, after values were found to decrease as aging time and microstructure, as the volume fraction of $\sigma$ phase increased.