Timber from plantation forests has inferior physical and mechanical properties compared to timber from natural forest because it is mostly from fast-growing tree species that are cut at a young age. Filling cell voids with methyl methacrylate (MMA) can improve the wood properties. The purpose of this study was to determine the physical and mechanical properties of MMA-impregnated wood from three fast-growing wood species, namely jabon (Anthocephalus cadamba (Roxb.) Miq.), mangium (Acacia mangium Willd) and pine (Pinus merkusii Jungh. & de Vriese). Wood samples were either immersed in MMA monomer or impregnated with it and then heated to induce the polymerization process. Jabon, which was the lowest density wood, had the highest polymer loading, followed by pine and mangium. The physical and mechanical properties of samples were affected by wood species and the presence of MMA, with higher-density wood having better properties than wood with a lower density. Physical and mechanical properties of MMA wood were enhanced compared to untreated wood. Furthermore, the impregnation process was better than immersion process resulting the physical and mechanical properties. Based on MOR values, the MMA woods were one strength class higher compared to untreated wood with regard to Strength Classification of Indonesian Wood.
Wood cell-wall modification with acetic anhydride, lumen filled with styren monomer and methyl methacrylate, and a combination of these two treatments were studied for their effectiveness for dimensional stability. Compared to those of untreated Pinus densiflora Sieb. et Zucc and sole acetylated red pine, The combination of acetylation and impregnation with methy methacrylate greatly reduced water absorption, increased ASE to the best and gave better bending strength and compression strength.
Hadi, Yusuf Sudo;Massijaya, Muh. Yusram;Zaini, Lukmanul Hakim;Abdillah, Imam Busyra;Arsyad, Wa Ode Muliastuty
Journal of the Korean Wood Science and Technology
/
제46권6호
/
pp.748-755
/
2018
Timber from fast-growing tree species is susceptible to by biodeterioration attack, particularly subterranean termites. Impregnation with methyl methacrylate (MMA) potentially increases wood resistance to subterranean termite attack. Four wood species, namely sengon (Falcataria moluccana), jabon (Anthocephalus cadamba), mangium (Acacia mangium), and pine (Pinus merkusii), were impregnated with MMA, and samples of untreated and imidacloprid-preserved wood were prepared for comparison purposes. Small stakes, sized 0.8 cm by 2 cm in cross section by 20 cm in the longitudinal direction, were inserted into the ground for 3 months, and the weight loss of each specimen was determined at the end of the test period. A factorial $4{\times}3$ completely randomized design was used for data analysis; the first factor was wood species, and the second factor was treatment. The results showed that MMA polymer loadings were 27.88%, 24.91%, 14.14%, and 17.81% for sengon, jabon, mangium, and pine, respectively, and amounts of imidacloprid retention were $7.56kg/m^3$, $5.98kg/m^3$, $5.34kg/m^3$, and $9.53kg/m^3$, respectively. According to an analysis of variance, wood species, treatment, and interaction of both factors significantly affected the weight loss of wood specimens. Mangium had the smallest weight loss, followed by pine, sengon, and jabon. MMA impregnation into the wood increased the resistance of wood samples to subterranean termite attack during in-ground testing, but the resistance level was lower than that of imidacloprid-preserved wood. Except for mangium wood, the MMA treatment did not significantly affect resistance.
This study was conducted to analyze the application of boron compounds, methyl methacrylate (MMA), and heat treatment (HT) on changes in the density, moisture content, and flexural properties of samama (Anthocephalus macrophyllus) wood. Samama wood was impregnated with borax (BX) and boric acid (BA) using a pressure method at 5 atm for 4 h. Afterwards, the wood was impregnated with MMA at the same pressure and duration. Finally, the samama wood was given HT at 90 ℃ and 180 ℃. The results indicate that there was a weight gain of 93.4% in the wood impregnated using BA and MMA monomer and HT at 90 ℃. Consequently, the wood's density increased by 82.3%. Increased MOE and MOR percentages of 32.2% and 29.4%, respectively, were also found. HT at 180 ℃ degraded the wood components and MMA, and consequently, the density, MOE, and MOR also decreased. The wood impregnated by BX, BA, and MMA, and subjected to HT also had decreased moisture content (MC). This research recommends that the application of boron (BX, BA) should be combined with an MMA monomer and HT at 90 ℃ as an alternative method to improve samama wood quality. If darker color is preferable, HT should be conducted at 180 ℃.
주요 침 활엽수재에 대하여 methyl methacrylate를 이용하여 만든 목재-polymer복합체에 대하여 polymer의 분포와 존재상태등을 목재의 조직학적인 면에서 조사하였으며 그것을 요약하면 다음과 같다. 1. polymer의 침투성은 수종에 따라 다르며 수종고유의 특성에 따라 다르다. 낙엽송은 침투성이 대단히 나쁘며 활엽수재에 있어서는 환공재가 산공재보다 침투성이 양호 하였다. 2. 횡단면에서 침투성이 가장 양호하며 방사단면과 접선단면에서의 주입은 저하되고 양자의 차이는 거의 없었다. 3. 동일 수종에서는 변재가 섬재보다 침투성이 양호 하였다. 수종에 따라 변심재간에 침투성이 다른 것은 심재화에 의한 tyloses의 형성 또는 도관중의 침착물에 의한 것으로 생각되고 있다. 4. 환공성 수종에서는 조재부가 만재부보다 polymer의 침투성이 양호 하였으며 산공재에서는 반대로 만재부가 조재부보다 침투성이 양호하였다. 5. 도관의 크기와 침투성과의 사이에는 명확한 상관이 없는 것으로 생각된다. 도관의 직경이외에도 도관의 비율, tyloses의 발달, 내용물의 충진 혹은 천공판등이 관계하는 것으로 생각되고 있다. 6. 침엽수재 방사조직에 있어서는 방사유세포보다 방사가도관의 침투성이 양호하였으며 활엽수재의 방사조직은 구성비율이 높음에도 불구하고 단량체의 방사방향에 미치는 영향은 침엽수재보다 적었다. 7. 비중과 연륜폭은 모두 polymer의 침투성과 거의 관계가 없었다.
Boron compound had many advantages as wood preservative, but it was prone to leaching. Improving boron preservation was required to extend the service life of fast growing and low durability red jabon (Antochephalus macrophyllus) hardwood. This study aimed to evaluate the dimensional stability, color change and durability of modified red jabon wood by double impregnation with boron and methyl methacrylate (MMA) and heat treatment. Impregnation I used boric acid or borax, and impregnation II used MMA, while heat treatment used temperatures of 90 ℃ or 180 ℃ for 4 hours. The dimensional stability, leachability, water absorption, color change and decay resistance of modified red jabon wood were tested. The results showed that MMA impregnation increased the dimensional stability of red jabon wood, while the leaching and water absorption in the wood significantly reduced. Heating at 180 ℃ caused less water absorption and higher dimensional stability of the wood than that of heating at 90 ℃. Impregnation with boric acid and MMA followed by heating at 90 ℃ resulted in the highest wood ASE, 89.9%. The color change (∆E*) of wood increased significantly after MMA impregnation and heating at 180 ℃. Boric acid impregnation caused more resistant wood than borax impregnation against decay fungi and termites. Impregnation with boric acid and MMA followed with heating at 180 ℃ increased significantly the wood resistance against decay fungi and termites.
Moon, Seok Kyu;Kim, Eun-jin;Kwon, Yong Rok;Kim, Jung Soo;Kim, Hae Chan;Park, Han Soo;Kim, Dong Hyun
Elastomers and Composites
/
제57권3호
/
pp.100-106
/
2022
Waterborne polyurethane-acrylate(WPUA) dispersions were prepared by surfactant-free emulsion polymerization in a two-step process. In the first step, polytetrahydrofuran, isophorone diisocyanate, dimethylol proponic acid, and 2-hydroxyethyl methacrylate were used to synthesize a vinyl-terminated polyurethane prepolymer. In the second step, styrene, methyl methacrylate, butyl acrylate, and different multi-functional crosslinkers were copolymerized. 1,6-hexanediol diacrylate, trimethylolpropane triacrylate, and pentaerythritol tetraacrylate were used as the crosslinkers, and their effect on the mechanical and thermal properties of WPUA was investigated. Overall, as the number of functional groups of the cross-linker increased, the gel fraction improved to 79.26%, the particle size increased from 75.9 nm to 148.7 nm, and the tensile strength was improved from 5.86 MPa to 12.40 MPa. In thermal properties, the glass transition temperature and decomposition temperature increased by 9.9℃ and 18℃, respectively. The chemical structures of the WPUA dispersions were characterized by Fourier-transform infrared spectroscopy. The synthesized WPUA has high potential for applications such as coatings, leather coatings, adhesives, and wood finishing.
육송 미송 포플라 등 국산 연질 목재에 단량체 또는 단량체 혼합물을 촉매와 함께 침투시키고 열중합함에 있어서 시간에 따르는 중합율을 구하고 이것을 방사선 중합으로 WPC를 제조할 때 얻은 간과 비교 검토하여 다음과 같은 결론을 얻었다. (1) 중합율로 보아서는 육송, 미송이 포플라보다 좋으며 M.M.A.가 다른 단량체보다 효과적이다. (2) 비닐아세테이트는 일반적으로 열중합에 의한 중합율이 저조한 편이며 특히 포플라에 침투된 경우 매우 낮아 W.P.C.를 만들기 곤란하다. 그러나 비닐아세테이트와 M.M.A.를 같이 침투시키면 나무종류나 중합방법에 별 관계없이 매우 빨리 중합하여 가장 효과적이다. (3) 나무에 침투된 단량체나 단량체 혼합물의 중합의 경향은 나무가 많은량의 수지를 함유하지 않는다면 중합방법에 관계없이 단량체나 단량체 혼합물 자체만일때의 중합의 경향과 같다.
One of the disadvantages of. wood and wood products is their hydroscopicity or dimensional instability. This is responsible for the loss of green volume of lumber as seasoning degrade. Dimensional stabilization is needed to substantially reduce seasoning defects and degrades and for increasing the serviceability of wood products. Recently, considerable world-wide attention has been drawn to the so-called Wood-Plastic Composites by irradiation-and heat-catalyst-polymerization methods and many research and developmental works have been reported. Wood-Plastic Composites are the new products having the superior mechanical and physical properties and the combinated characteristics of wood and plastic. The purpose of this experiment was to obtain the basic data for the improvement of wooden materials by manufacturing WPC. The species examined were Mulpurae-Namoo (Fraxinus, rhynchophylla), Sea-Namoo (Carpinus laxiflora), Cheungcheung-Namoo (Cornus controversa), Gorosae-Namoo (Acermono), Karae-Namoo(Juglans mandshurica) and Sanbud-Namoo (Prunus sargentii), used as blocks of type A ($3{\times}3{\times}40cm$) and type B ($5{\times}5{\times}60cm$), and were conditioned to about 10~11% moisture content before impregnation in materials humidity control room. Methyl methacrylate (MMA) as monomer and benzoyl peroxide (BPO) as initiator are used. The monomer containing BPO was impregnated into wood pieces in the vacuum system. After impregnation, the treated samples were polymerized with heat-catalyst methods. The immersed weights of monomer in woods are directly proportionated to the impregnation times. Monomer impregnation properties of Cheungcheung-Namoo, Mulpurae-Namoo and Seo-Namoo are relatively good, but in Karae-Namoo, it is very difficult to impregnate the monomer MMA. Fig. 3 shows the linear relation between polymer retentions in wood and polymerization times; that is, the polymer loadings are increasing with polymerization times. Furthermore species, moisture content, specific gravity and anatomical or conductible structure of wood, bulking solvents and monomers etc have effects on both of impregnation of monomer and polymer retention. Physical properties of treated materials are shown in table 3. Increasing rates of specific gravity are ranged 3 to 24% and volume swelling 3 to 10%. ASE is 20 to 46%, AE 14 to 50% and RWA 18 to 40%. Especially, the ASE in relation to absorption of liquid water increases approximately with increase of polymer content, although the bulking effect of the polymerization of monomer may also be influential. WPCs from Mulpurae-Namoo and Cheungcheung-Namoo have high dimensional stability, while its of Karae-Namoo and Seo-Namoo are-very low. Table 4 shows the mechanical properties of WPCs from 6 species. With its specific gravity and polymer loading increase, all mechanical properties are on the increase. Increasing rate of bending strength is 10 to 40%, compression strength 25 to 70%, ;impact bending absorbed energy 4 to 74% and tensile strength 18 to 56%. Mulpurae-Namoo and Cheungcheung-Namoo with high polymer content have considerable high increasing rate of strengths. But incase of Karae-Namoo with inferior monomer impregnation it is very low. Polymer retention in cell wall is 0.32 to 0.70%. Most of the polymer is accumulated in cell lumen. Effective. of polymer retention is 58.59% for Mulpurae-Namoo, 26.27% for Seo-Namoo, 47.98% for Cheungcheung-Namoo, 25.64% for Korosae-Namoo, 9.96% for Karae-Namoo and 25.84% for Sanbud-Namoo.
5-methylthioninhydrin (5-MTN) is an amino acid sensitive reagent used for the development of latent fingermarks deposited on porous surfaces such as paper and wood. The present study demonstrates that the 5-MTN can be used as a latent footwear impression enhancement reagent, by reacting with trace multivalent metal ions, which are the main components of the latent footwear impression. 5-MTN and L-alanine complex (MTN-ALA) used for the latent footwear impression development was prepared, by mixing $4.5{\times}10^{-3}M$ 5-MTN (in methanol) and $4.5{\times}10^{-3}M$ L-alanine (in methanol) in 1:1 ratio, and keeping undisturbed at room temperature for 24 h. The latent footwear impressions were deposited on white and black non-porous surfaces (glass plate, polyethylene panel, polypropylene panel, acryl panel, polyvinyl chloride (PVC) panel, poly(methyl methacrylate) (PMMA) panel, acrylonitrile-butadiene-styrene (ABS) panel, tile), and a semi-porous surfaces (painted wood). The latent footwear impressions on these surfaces were treated with MTN-ALA complex by spraying. The fluorescence of footwear impressions (occurred due to the reaction between MTN-ALA and metal complexes) was observed under a 505 nm forensic light source and an orange barrier filter. The enhancement of latent footwear impression was achieved from black surfaces without any blurring. However, the fluorescence (enhancement) of footwear impression was not observed on the white PVC, PMMA, and ABS surfaces, because the incident light interfered and reflected on the surface. The sensitivity of MTN-ALA was superior to 2,2'-dipyridil, which is a representative non-fluorescing footwear impression enhancement reagent, and similar to 8-hydroxyquinoline, which is a representative fluorescing footwear impression enhancement reagent.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.