Evaluation of 1Cr-1Mo-0.25V Steel Degradation Using Magnetic Barkhausen Noise (Magnetic Barkhausen Noise를 이용한 1Cr-1Mo-0.25V강의 열화도 평가)

  • Lee, J.M.;Ahn, B.Y.;Nam, Y.H.;Nahm, S.H.;Lee, S.S.;Lee, O.S.
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.250-255
    • /
    • 2001
  • It is inevitable to evaluate the life of turbine rotor because the operating periods of power plants need to be extended. The magnetic methods utilizing Magnetic Barkhausen noise curve were applied to detect the degradation caused by thermal aging. The Magnetic property of material depends on the domain dynamics and it is affected by the microstructure of material. Therefore the magnetic property is very sensitive to the microstructure change of the material. It is, thus, very useful to detect the state of degradation of varying materials. The test specimen made of 1Cr-1Mo-0.25V steel was used widely for turbine rotor material, and seven kinds of specimens with different degradation levels were prepared by the isothermal heat treatment at $630^{\circ}C$. With the increase of degradation, BHN was decreased. The result was compared with coercive force and vickers hardness.

  • PDF

Evaluation of 1Cr-1Mo-0.25V Steel Degradation Using Magnetic Barkhausen Noise (Barkhausen noise를 이용한 1Cr-1Mo-0.25V강의 열화도 평가)

  • Lee, Jong-Min;Ahn, Bong-Young;Nahm, Seung-Hoon;Lee, Seung-Seok;Lee, Ouk-Sub;Nam, Young-Hyun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.7
    • /
    • pp.1262-1269
    • /
    • 2002
  • It is inevitable to evaluate the life of turbine rotor because the operating periods of power plants need to be extended. For the test, seven kinds of specimens with different degradation levels were prepared by the isothermal heat treatment at $630^{\circ}C$. Magnetic methods utilizing Barkhausen noise coercive force($BN_c$) were applied to detect the degradation caused by thermal aging. Magnetic property of material is related with domain dynamics and that is affected by the microstructure of material. Therefore $BN_c$ is very sensitive to the microstructure change of the material. With the increase of degradation, $BN_c$ was decreased and this phenomenon is considered due to precipitations and grain size. The result was compared with Vickers hardness($H_v$) and coercive force($H_c$) to detect the relative variation, and was related with $H_v$ and YS to estimate the change of the mechanical properties with the degradation.

Basic Study of Degradation Test for Magnetic Contactors and Reliability Centered Maintenance

  • Ryu, Haeng-Soo;Han, Gyu-Hwan;Yoon, Nam-Sik
    • Journal of Electrical Engineering and Technology
    • /
    • v.2 no.4
    • /
    • pp.441-444
    • /
    • 2007
  • The mechanical endurance is the critical characteristic of Magnetic contactors (MCs), which are widely used in such industrial equipments as elevators, cranes, and factory control rooms in order to close and open the control circuit. Testing time, however, is so long in most cases that some method of reducing the testing period is required. Therefore, the degradation test by the detected vibration of MCs is developed to reduce the testing time in this work. The degradation test data are analyzed and the prediction model is provided. Also, the possibility of this technology for Reliability Centered Maintenance (RCM) will be shown. This will reduce the period of the product development and raise the reliability of the equipment in power distribution.

Design of a Reflector for Infrared Camera (열화상 카메라용 반사경 설계)

  • Bae, Young-Chul
    • The Journal of the Korea institute of electronic communication sciences
    • /
    • v.9 no.1
    • /
    • pp.97-104
    • /
    • 2014
  • Recently infrared cameras have been widely used to diagnosis degradation status of the power substitution system. At the place of high magnetic field, however, electronic parts of infrared camera take a place problem that is not reasonable working due to high magnetic field. In this paper, technique of design for reflector is proposed to perform degradation diagnosis without damage of infrared camera in a power substation system including the rectifier that is able to impact to the infrared camera by high magnetic field.

A practical approach to handling protein samples under degradation

  • Jeong-Yong, Suh;Sung Hyun, Hong
    • Journal of the Korean Magnetic Resonance Society
    • /
    • v.26 no.4
    • /
    • pp.66-70
    • /
    • 2022
  • Protein structure determination using NMR spectroscopy requires a suite of heteronuclear 3-D NMR experiments that can take a couple of weeks for completion. During the experiments, protein samples may suffer from slow degradation due to co-purifying proteases, which complicates and slows down the assignment procedure. Here we describe a practical protocol to avoid unwanted proteolysis during the experiment.

Degradation of Soft Magnetic Properties of Fe-Hf-N/Cr/SiO2 Thin Films Reacted with Bonding Glass (접합유리와 반응된 Fe-Hf-N/Cr/SiO2 박막의 연자기 특성 열화)

  • Je Hae-June;Kim Byung-Kook
    • Korean Journal of Materials Research
    • /
    • v.14 no.11
    • /
    • pp.780-785
    • /
    • 2004
  • The degradation mechanism of soft magnetic properties of $Fe-Hf-N/Cr/SiO_2$ thin films reacted with a bonding glass was investigated. When $Fe-Hf-N/Cr/SiO_2$ films were annealed under $600^{\circ}C$ without the bonding glass, the compositions and the soft magnetic properties of Fe-Hf-N layers were not changed. However, after reaction with the bonding glass at $550^{\circ}C$, the soft magnetic properties of the film were degraded. At $600^{\circ}C$, the saturation magnetization of the reacted film decreased to 13.5 kG, and its coercivity increased to 4 Oe, and its effective permeability decreased to 700. It was founded that O diffused from the glass into the Fe-Hf-N layers during the reaction and generated $HfO_2$ phases. It was considered that the soft magnetic properties of the $Fe-Hf-N/Cr/SiO_2$ films reacted with the bonding glass were primarily degraded by the formation of the Fe-Hf-O-N layer of which the Fe content was below 60 $at\%$, and secondarily degraded by the Fe-Hf-O-N layer above 70 $at\%$.

Critical Current Degradation Analysis in HTS Pancake Coil due to Self Field Effects

  • Nah, Wan-Soo;Joo, Jin-Ho;Yoo, Jai-Moo
    • Progress in Superconductivity
    • /
    • v.1 no.1
    • /
    • pp.68-72
    • /
    • 1999
  • Since the discovery of high Tc superconductors, great efforts have been focused to develop high performance HTS magnets for the ultimate applications to power system devices. Magnet designers, however, have had difficulties in the estimation of the maximum operating current of the designed magnet from the tested short sample data, due to the degradation of the critical current density in the magnet. Similar story applies to the HTS electrical bus bar. It has been found that the critical current of Bi-2223 stacked tapes is much less than the total summation of critical currents of each tape, which is mainly attributed to the self magnetic fields. Furthermore, since the critical current degradation of Bi-2223 tape is greater in the normal magnetic field (to the tape surface) than in the parallel one, detailed magnetic field configurations are required to reduce the self field effects. In this paper, we calculate the self field effects of a stacked conductor, defining self field factors of normal and parallel magnetic fields to the tape surface. Finally, the critical current degradations in the HTS magnet are explained by the introduced self field factors of the stacked conductor.

  • PDF

Evaluation of degradation in aged 2.25CrMo steel by electrical resistivity, magnetic Barkhausen noise and carbide analysis (전기비저항, 바크하우젠노이즈 및 탄화물 분석법을 이용한 2.25Cr-1Mo 강의 열화도 평가)

  • Byeon, Jai-Won;Pyo, S.W.;Kwun, S.I.
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.210-215
    • /
    • 2001
  • The ferritic 2.25CrMo steel has been used for high temperature structure applications such as turbine rotors, boilers and pressure vessels in fossil plant and petroleum chemical facilities. However, this steel is known to result in aging degradation due to temper embrittlement, carbide induced brittleness and softening of matrix after long time exposure to high temperature. This research investigated the microstructural and mechanical changes after artificial degradation treatment and evaluated the degree of degradation by several nondestructive methods. The decrease of electrical resistivity and increase of magnetic Barkhausen noise(RMS voltage) with increasing aging time were observed. The change of electrical resistivity and Barkhausen noise showed a good correlation with the ductile-brittle transition temperature.

  • PDF

Magnetic Susceptibility depending on the Thermal Degradation of HK-40 Steel (HK-40강의 열화도에 따른 자화율의 변화)

  • Kim, Jeong-Min;Son, De-Rac;Park, Jong-Seo;Nahm, Seung-Hoon;Kim, Dong-Gyun;Han, Sang-In;Choi, Song-Chun;Ryu, Dae-Hyun
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.24 no.1
    • /
    • pp.22-28
    • /
    • 2004
  • Since the used materials of furnace heater tube with different kinds of thermal degradation were not commonly available, the HK-40 steel specimens were heat-treated isothermally at elevated temperature to simulate the microstructure at the service temperature. HK-40 steel specimens with five different aging time were prepared by isothermal heat treatment at $1050^{\circ}C$. The characteristics of the magnetic susceptibility have been investigated for the degradation evaluation of HK-40 steel. The magnetic susceptibility at room temperature increases as the extent of degradation of the materials increases. The variation of magnetic susceptibility was compared with the variation of tensile properties and Vickers hardness. To investigate the effect of the microsturctural change on the characteristics of tensile properties, hardness and magnetic susceptibility, the microstructures were examined by a scanning electron microscope(SEM) and the chemical compositions were analyzed by a energy spectrometer of SEM. As a result, the magnetic susceptibility method can be suggested as one of the nondestructive evaluation methods for the degradation of the HK-40 steel.

Changes of Carbide Characteristics and Magnetic Properties in Artificially Aging Heat Treated 2.25CrMo Steel (경년열화 열처리된 2.25CrMo 강에서의 탄화물 특성 및 자기적 성질의 변화)

  • Byeon, Jal Won;Kwun, S.I.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.14 no.6
    • /
    • pp.323-329
    • /
    • 2001
  • Artificial aging was performed to simulate the microstructural degradation in 2.25CrMo steel arising from long time exposure at $540^{\circ}C$. The carbide morphologies were classified as acicular, pipe and globular type, and the number of carbides per unit area was measured for each type of carbides. The fine acicular carbides were found to diminish drastically in the initial stage of aging. An attempt was made to evaluate the microstructural degradation in artificially aging heat treated 2.25CrMo steel by the magnetic property measurements such as saturation magnetization, coercivity and remanence. The saturation magnetization showed no distinct trend with aging time. However, the coercivity and remanence were observed to decrease rapidly in initial 920 hours of aging time and then decrease slowly afterwards.