• Title/Summary/Keyword: low porosity

Search Result 526, Processing Time 0.031 seconds

A Study on the Mechanical Properties of Interfacial Transition Zone (ITZ) of Lightweight High Strength Concrete Via Nanoindentation (나노 인덴테이션을 통한 경량 고강도 콘크리트 Interfacial Transition Zone (ITZ)의 역학적 특성에 관한 연구)

  • Im, Su-Min;Bae, Sung-Chul
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.4
    • /
    • pp.537-544
    • /
    • 2020
  • The interfacial transition zone(ITZ) which is the boundary layer between cement composites and aggregates is considered to be the region of gradual transition, heterogeneous, and the weakest part of concrete. For the development of lightweight high strength concrete, it is essential to evaluate the mechanical properties of ITZ between high strength concrete with low water-binder ratio and lightweight aggregates. However, the mechanical properties of ITZ are not well established due to its high porosity and complex structure. Furthermore, the properties of ITZ in concrete using lightweight aggregates are dominated by more various variations (e.g. water-binder ratio, water absorption capacity of aggregate, curing conditions) than normal-weight aggregate concrete. This study aims to elucidate the mechanical properties of ITZ in lightweight high-strength cement composites according to the types of aggregates and the aggregate sizes. Nanoindentation analysis was used to evaluate the elastic modulus of ITZ between high strength cement composites with the water-binder ratio of 0.2 and normal sand, lightweight aggregate with different aggregate siz es of 2mm and 5mm in this study.

Hydrophilic/Hydrophobic Dual Surface Coatings for Membrane Distillation Desalination (막증류 담수화를 위한 친수성/소수성 이중 표면 코팅)

  • Kim, Hye-Won;Lee, Seungheon;Jeong, Seongpil;Byun, Jeehye
    • Journal of Korean Society on Water Environment
    • /
    • v.38 no.3
    • /
    • pp.143-149
    • /
    • 2022
  • Membrane distillation (MD) has emerged as a sustainable desalination technology to solve the water and energy problems faced by the modern society. In particular, the surface wetting properties of the membrane have been recognized as a key parameter to determine the performance of the MD system. In this study, a novel surface modification technique was developed to induce a Janus-type hydrophilic/hydrophobic layer on the membrane surface. The hydrophilic layer was created on a porous PVDF membrane by vapor phase polymerization of the pyrrole monomer, forming a thin coating of polypyrrole on the membrane walls. A rigid polymeric coating layer was created without compromising the membrane porosity. The hydrophilic coating was then followed by the in-situ growth of siloxane nanoparticles, where the condensation of organosilane provided quick loading of hydrophobic layers on the membrane surface. The composite layers of dual coatings allowed systematic control of the surface wettability of porous membranes. By the virtue of the photothermal property of the hydrophilic polypyrrole layer, the desalination performance of the coated membrane was tested in a solar MD system. The wetting properties of the dual-layer were further evaluated in a direct-contact MD module, exploring the potential of the Janus membrane structure for effective and low-energy desalination.

Tafoni Patterns on Tuff Slopes in Gogulsa Temple, Gyeongju and Its Microstructural Properties (경주 골굴사 응회암 사면의 타포니 분포 특성과 미세구조)

  • Choo, Chang-Oh;Lee, Jin-Kook
    • The Journal of Engineering Geology
    • /
    • v.32 no.3
    • /
    • pp.339-350
    • /
    • 2022
  • There are a variety of types in tafoni formed in Miocene tuff from Golgulsa, Gyeongju. Tuff bearing tafoni was quite weathered, composed of quartz, feldspars, micas, vermiculite, chlorite, smectite, and analcite. In the early stage of the tafoni development, tafoni preferentially formed from cavities where volcanic breccias were removed or from microcavities where microcrystals were chemically altered. Small tafoni grew into large one by merging each other. The orientation of tafoni is inversely arranged to slopes, with slight inclination toward the inner cavity. Height, width, and depth of tafoni are closely interrelated: the correlation coefficients are 0.839 (width-height), 0.900 (width-depth), and 0.856 (height-depth), respectively. Removal of walls between tafoni resulted in lenticular or crescent forms, and small tafoni laterally combined to large tafoni. Large tafoni is weak because of high porosity and low strength compared to normal slope. Therefore, systematic monitoring for slope strength, pore proportion and volume, and growth of cavity needs to secure the slope stability where tafoni in Golgulsa is widespread.

Effect of Y2O3 Additive Amount on Densification of Reaction Bonded Silicon Carbides Prepared by Si Melt Infiltration into All Carbon Preform (완전 탄소 프리폼으로부터 Si 용융 침투에 의해 제조한 반응 소결 탄화규소의 치밀화에 미치는 Y2O3 첨가량의 영향)

  • Cho, Kyeong-Sik;Jang, Min-Ho
    • Korean Journal of Materials Research
    • /
    • v.31 no.5
    • /
    • pp.301-311
    • /
    • 2021
  • The conversion of all carbon preforms to dense SiC by liquid infiltration can become a low-cost and reliable method to form SiC-Si composites of complex shape and high density. Reactive sintered silicon carbide (RBSC) is prepared by covering Si powder on top of 0.5-5.0 wt% Y2O3-added carbon preforms at 1,450 and 1,500℃ for 2 hours; samples are analyzed to determine densification. Reactive sintering from the Y2O3-free carbon preform causes Si to be pushed to one side and cracking defects occur. However, when prepared from the Y2O3-added carbon preform, an SiC-Si composite in which Si is homogeneously distributed in the SiC matrix without cracking can be produced. Using the Si + C = SiC reaction, 3C and 6H of SiC, crystalline Si, and Y2O3 phases are detected by XRD analysis without the appearance of graphite. As the content of Y2O3 in the carbon preform increases, the prepared RBSC accelerates the SiC conversion reaction, increasing the density and decreasing the pores, resulting in densification. The dense RBSC obtained by reaction sintering at 1,500 ℃ for 2 hours from a carbon preform with 2.0 wt% Y2O3 added has 0.20 % apparent porosity and 96.9 % relative density.

Effectiveness study of a cement mortar coating based on dune sand on the carbonation of concrete

  • Korichi, Youssef;Merah, Ahmed;Khenfer, Med Mouldi;Krobba, Benharzallah
    • Advances in concrete construction
    • /
    • v.13 no.4
    • /
    • pp.315-325
    • /
    • 2022
  • Reinforced concrete structures are exposed throughout their lifetime to the phenomenon of carbonation, which considerably influences their durability by causing corrosion of the reinforcements. The fight against this phenomenon is usually ensured by anti-carbonation coatings which have the possibility of limiting the permeability to carbon dioxide or with coatings which absorb the CO2 present in the air. A coating with good crack-bridging (sealing) capacity will prevent water from entering through existing cracks in concrete. Despite the beneficial effect of these coatings, their durability decreases considerably over time with temperature and humidity. In order to use coatings made from local materials, not presenting any danger, available in abundance in our country, very economical and easy to operate is the main objective of this work. This paper aim is to contribute to the formulation of a corrected dune sand-based mortar as an anti-carbonation coating for concrete. The results obtained show that the cement mortar based on dune sand formulated has a very satisfactory compressive strength, a very low water porosity compared to ordinary cement mortar and that this mortar allows an improvement in the protection of the concrete against the carbonation of 60% compared to ordinary cement mortar based on alluvial sand. Moreover, the formulated cement mortars based on dune sand have good adhesion to the concrete support, their adhesion strengths are greater than 1.5MPa recommended by the standards.

Micro-computed tomography for assessing the internal and external voids of bulk-fill composite restorations: A technical report

  • Tosco, Vincenzo;Monterubbianesi, Riccardo;Furlani, Michele;Giuliani, Alessandra;Putignano, Angelo;Orsini, Giovanna
    • Imaging Science in Dentistry
    • /
    • v.52 no.3
    • /
    • pp.303-308
    • /
    • 2022
  • Purpose: This technical report aims to describe and detail the use of micro-computed tomography for a reliable evaluation of the bulk-fill composite/tooth interface. Materials and Methods: Bulk-fill composite restorations in tooth cavities were scanned using micro-computed tomography to obtain qualitatively and quantitatively valuable information. Two-dimensional information was processed using specific algorithms, and ultimately a 3-dimensional (3D) specimen reconstruction was generated. The 3D rendering allowed the visualization of voids inside bulk-fill composite materials and provided quantitative measurements. The 3D analysis software VG Studio MAX was used to perform image analysis and assess gap formation within the tooth-restoration interface. In particular, to evaluate internal adaptation, the Defect Analysis addon module of VG Studio Max was used. Results: The data, obtained with the processing software, highlighted the presence and the shape of gaps in different colours, representing the volume of porosity within a chromatic scale in which each colour quantitatively represents a well-defined volume. Conclusion: Micro-computed tomography makes it possible to obtain several quantitative parameters, providing fundamental information on defect shape and complexity. However, this technique has the limit of not discriminating materials without radiopacity and with low or no filler content, such as dental adhesives, and hence, they are difficult to visualise through software reconstruction.

Direct Microwave Sintering of Poorly Coupled Ceramics in Electrochemical Devices

  • Amiri, Taghi;Etsell, Thomas H.;Sarkar, Partha
    • Journal of Electrochemical Science and Technology
    • /
    • v.13 no.3
    • /
    • pp.390-397
    • /
    • 2022
  • The use of microwaves as the energy source for synthesis and sintering of ceramics offers substantial advantages compared to conventional gas-fired and electric resistance furnaces. Benefits include much shorter processing times and reaching the sintering temperature more quickly, resulting in superior final product quality. Most oxide ceramics poorly interact with microwave irradiation at low temperatures; thus, a more complex setup including a susceptor is needed, which makes the whole process very complicated. This investigation pursued a new approach, which enabled us to use microwave irradiation directly in poorly coupled oxides. In many solid-state electrochemical devices, the support is either metal or can be reduced to metal. Metal powders in the support can act as an internal susceptor and heat the entire cell. Then sufficient interaction of microwave irradiation and ceramic material can occur as the sample temperature increases. This microwave heating and exothermic reaction of oxidation of the support can sinter the ceramic very efficiently without any external susceptor. In this study, yttria stabilized zirconia (YSZ) and a Ni-YSZ cermet support were used as an example. The cermet was used as the support, and a YSZ electrolyte was coated and sintered directly using microwave irradiation without the use of any susceptor. The results were compared to a similar cell prepared using a conventional electric furnace. The leakage test and full cell power measurement results revealed a fully leak-free electrolyte. Scanning electron microscopy and density measurements show that microwave sintered samples have lower open porosity in the electrode support than conventional heat treatment. This technique offers an efficient way to directly use microwave irradiation to sinter thin film ceramics without a susceptor.

Stewartia pseudocamellia and Torilis japonica Extracts Inhibit RANKL-induced Osteoclastogenesis in RAW 264.7 Cells

  • Anh-Thu Nguyen;Chun Soo Na;Ki-Young Kim
    • Journal of the Korean Chemical Society
    • /
    • v.67 no.2
    • /
    • pp.120-128
    • /
    • 2023
  • Osteoporosis is a disease that causes the weakening of bone by increasing porosity, which often results in fractures. Osteoporosis treatment measures include the use of Bisphosphonates and estrogen. However, these treatments cannot be used in the long term as these treatments have adverse side effects. Therefore, there is a need to identify better and safer treatment options. For this, 63 plant extracts were screened and among them, six extracts showed high anti-osteoclastic activity with low cytotoxicity. Of these six extracts, three extracts, Cudrania tricuspidata (P371), Ulmus davidiana var. japonica (P401), and Torilis japonica (P411), showed more than 50 percent osteoclast inhibition. While the remaining, Stewartia pseudocamellia extracts I and II (P370, P397) and Cuscuta chinensis (P418), showed moderate or between 40-50 percent osteoclast inhibition. Among all the extracts, Torilis japonica (P411) showed the highest inhibitory action against osteoclast development. Torilis japonica (P411) primary components include Kaempferol, Quercetin, and Luteolin, all proven to inhibit osteoclastogenesis. Stewartia pseudocamellia extracts I and II (P370 and P397) showed moderate or 44% osteoclast inhibition. Stewartia pseudocamellia extract II (P397) enhanced the growth of RAW 264.7 cells by 19%. Torilis japonica (P411) and Stewartia pseudocamellia extract II (P397) suppressed the expression of osteoclast-specific genes in RANKL-induced osteoclastogenesis in RAW 246.7 cells. Torilis japonica (P411) extracts even increased osteoblast-specific RUNX2 gene expression. This results provide that six extracts could be used as a potential treatment option for osteoporosis disease with the extracts of Torilis japonica (P411) and Stewartia pseudocamellia (P397) as an ideal candidates. However, the combination of the extract with higher osteoclastic inhibition and less toxic effects with further analysis should be recommended.

Li4SiO4 slurry conditions and sintering temperature for fabricating Li4SiO4 pebbles as tritium breeders for nuclear-fusion reactors

  • Young Ah Park;Ji Won Yoo;Yi-Hyun Park;Young Soo Yoon
    • Nuclear Engineering and Technology
    • /
    • v.55 no.8
    • /
    • pp.2966-2976
    • /
    • 2023
  • A tritium breeder is a lithium-based material capable of producing tritium. Many researchers designing nuclear-fusion energy are studying tritium production using pebbles, which are solid-type breeders. The sphericity and size of the pebbles are critical in obtaining pebbles with good tritium-breeding efficiency. Furthermore, tritium-release efficiency can be increased by using pebbles with appropriate porosities. Promising raw materials for tritium-breeding materials include Li4SiO4 and Li2TiO3. Li4SiO4 has a higher lithium density than Li2TiO3 and exhibits excellent tritium-breeding efficiency. However, it has the disadvantage of being easily decomposed during the Li4SiO4-green-pebble sintering process because of its low structural stability at high temperatures and high lithium density. In this study, we attempted to determine the optimal conditions for manufacturing Li4SiO4 pebbles using the droplet-freeze-drying method. The optimal Li4SiO4 slurry conditions and sintering temperatures were determined. The optimal Li4SiO4 slurry-fabrication conditions were 3 wt% polyvinyl alcohol and 75 wt% Li4SiO4 based on the deionized-water weight content. The sintering temperature at which Li4SiO4 did not decompose and exhibited the optimum porosity of 10.8% was 900 ℃.

Study of Hydrated Asteroids via Polarimetry: Correlation between Polarimetric Properties and the Degree of Aqueous Alteration of Hydrated asteroids (편광을 통한 수화한 소행성 연구)

  • Geem, Jooyeon;Ishiguro, Masateru;Naito, Hiroyuki;Kuroda, Daisuke;Takahashi, Koki;Sekiguchi, Tomohiko;Takagi, Seiko;Ono, Tatsuharu;Kuramoto, Kiyoshi;Nakamura, Tomoki
    • The Bulletin of The Korean Astronomical Society
    • /
    • v.46 no.1
    • /
    • pp.46.1-46.1
    • /
    • 2021
  • Hydrated asteroids get widespread attention for the evolution of water in the Solar System, especially thanks to the recent successes of the Hayabusa2 and OSIRIS-REx space missions. The target asteroids of these missions are believed to be fragments that have experienced aqueous alteration in their parent bodies [3]. Although hydrated asteroids have been studied well via spectroscopy, focusing on the 0.7 um or the 2.7 um absorption bands [2, 3, 4], polarimetric properties of these asteroids have rarely been investigated. In this study, we conducted a polarimetric observation of 18 C-complex main-belt asteroids with the 1.6-m Pirka telescope at the Nayoro Observatory of Hokkaido University, Japan. We used a polarimetric imaging mode of the Multi-Spectral Imager (MSI) with the standard Rc-band filter (the central wavelength at 0.64 um) [5]. As a result, we found that all of these hydrated asteroids indicate deep negative branches of their polarimetric profiles. Accordingly, the hydrated asteroids have the polarization minima (Pmin), whose values are significantly lower than any other taxonomic types of asteroids (including C-group asteroids). Because Pmin depends on albedo, particle size, and porosity of the surface materials [1], we suspect that hydrated asteroids are distinctive from other asteroids in terms of these physical properties. In this presentation, we introduce our polarimetric observation and findings. We discuss why hydrated asteroids indicate such low Pmin values, comparing Pmin with spectral features at 0.7 um and 2.7 um based on the observation results.

  • PDF