Effect of Organic Photosensitizers on the Antimicrobial Property of Polyurethane coated Leather

  • Oh, Kyung Wha;Lim, Ki Sub
    • 한국의류산업학회지
    • /
    • 제15권4호
    • /
    • pp.630-634
    • /
    • 2013
  • Cow leather coated with polyurethane film that contains various organic photosensitizers was investigated to demonstrate the antimicrobial properties in the application of the material to protective clothing and home appliances. To prepare the antimicrobial coating on leather surfaces with high potency against microbes, photoactive agents, such as benzophenone (BP), 4,4'-bis(dimethylamino) benzophenone (MK), 4,4'-dihydroxybenzophenone (DHBP) and methylene blue (MB), were incorporated into polyurethane-based coating solutions. The photoactive antimicrobial agent treated leather samples were characterized by SEM, color appearance, color fastness against abrasion, and antimicrobial tests. The optical properties of organic photosensitizers indicated that active UV absorbance ranges were different: BP (around 250 nm), MK (around 360 nm), DHBP (around 305 nm) and MB (around 295 nm &570 nm-685 nm). The intensity of the UV absorbance curve at the UVA light wavelength for the antimicrobial test showed the highest value with MK; subsequently, this was followed by MB, DHBP and BP in decreasing order. The treated-leather samples demonstrated excellent antibacterial activity under UVA light. The antimicrobial effects for the Staphylococcus aureus were superior to Escherichia coli. Moreover, the polyurethane finishing showed an effective durability to abrasion. The overall results indicated that DHBP is the most suitable PU coating additive to provide antimicrobial properties to leather as well as color and surface appearance than MK, MB, and BP.

실리콘의 특성 이해와 합성피혁 코팅제로서의 적합성 (Properties of Silicone and its Suitability as a Synthetic Leather Coating Agent)

  • 김수홍;백두현
    • 한국염색가공학회지
    • /
    • 제35권1호
    • /
    • pp.42-65
    • /
    • 2023
  • Leather is widely used in human lives and many industries, and the market size continues to grow. In terms of quality and durability, natural leather is still being used as the most luxurious product. And synthetic leather, made of polyvinyl chloride (PVC) and polyurethane (PU), were developed and being widely have been used as alternative materials for natural leather. Processes, properties and issues of these leather were reviewed. Then silicone leather was reviewed why they can be good candidates for leather. Properties of general silicone polymers and silicone rubber coating agents were reviewed such as eco-friendliness, human-friendliness, stain resistances, resistance to uv light and ozone, heat stability and so on. Papers and patents related to silicone leather were studied to understand current status of development and commercialization of silicone leather. Finally direction of development was described how to improve deficient performances of current silicone leather, such as formulation of silicone, combination with organic materials and manufacturing processes.

Marbling 기법을 응용한 천연가죽의 디자인 연구 (I) (Design Research of the Natural Leather using a Marbling Technique (I))

  • 이상철;신은철;김원주;박수민
    • 한국염색가공학회지
    • /
    • 제20권1호
    • /
    • pp.1-7
    • /
    • 2008
  • The study has attempted to introduce a new coating than the conventional standardized method of spray, padding and roll coating. The study has focused on finding condition for separating water and organic layer in marble bath and surface effects according to kind of raw hide. It was found that dyestuff-free was to be used in water layer and the input amount of initial insoluble pigment to be added in marble bath should be adjusted following the change of surface area of the marble bath in order to get efficient marble effect while preventing coagulation of water and organic layers. Eventually, amorphous high value-added leather could be obtained treated in process other than the conventional standardized method. Even raw hides of low grades($C{\sim}E$ grades) could be processed into amorphous marble effect that could conceal or shield surface scratches by the colorant, which eventually eliminated necessity of using excessive amount of chemicals in the coating process leading to achieving high quality marble leather of natural look.

Enhancement of antimicrobial properties of shoe lining leather using chitosan in leather finishing

  • Mahmud, Yead;Uddin, Nizam;Acter, Thamina;Uddin, Md. Minhaz;Chowdhury, A.M. Sarwaruddin;Bari, Md. Latiful;Mustafa, Ahmad Ismail;Shamsuddin, Sayed Md.
    • Advances in materials Research
    • /
    • 제9권3호
    • /
    • pp.233-250
    • /
    • 2020
  • In this study, a chitosan based coating method was developed and applied on the shoe lining leather surface for evaluating its inhibition to bacterial and fungal attacks. At first, chitosan was prepared from raw prawn shells and then the prepared chitosan solution was applied onto the leather surface. Secondly, the characterization of the prepared chitosan and chitosan treated leather was performed by solubility test, ATR-FTIR, XRD pattern, SEM and TGA. Evaluation of antimicrobial efficacy of chitosan was assessed against two gram positive, two gram negative bacteria and a reputed fungi by agar diffusion test. The results of this study demonstrated that chitosan took place in both the surface of collagen fibres and inside the collagen matrix of crust leather. The chitosan showed strong antimicrobial activities against all the tested microorganisms and the inhibition increased with increasing percentage of chitosan. Therefore, the prepared chitosan in this study can be an environment friendly biocide, which functions simultaneously against different spoilage bacteria and fungi on the finished leather surface. Thus by using the prepared chitosan in shoe lining leather, the possibility of microbial attack during shoe wearing can be minimized which is one of the important hygienic requirements of footwear.

Buffalo Leather 코팅에 대한 수분산 폴리우레탄의 합성 및 3가 알콜 첨가에 의한 물성변화 연구 (A Study on the Property Changes by Trihydric Alcohol Addition Reaction and Polyurethane Dispersion Synthesis for Buffalo Leather Coatings)

  • 이주엽
    • 한국응용과학기술학회지
    • /
    • 제32권4호
    • /
    • pp.623-630
    • /
    • 2015
  • Buffalo leather 표면 코팅에 사용된 폴리우레탄 수지에 glycerol의 함유를 mole % 비로 달리하면서 첨가 하였다. 합성된 폴리우레탄 수지의 기계적 특성은 SEM, FT-IR, UTM 등을 이용하여 측정하였다. 친환경적인 고분자 수지의 관심이 고조됨에 따라 용제의 사용을 최소화한 buffalo leather 코팅에 사용되는 수분산 수지를 합성하였다. 지방족 3가 알콜인 glycerol의 mole % 비가 증가함에 따라 내마모도, 인장강도가 감소함을 알 수 있었다. 반대로 연신율, 내굴곡 물성은 증가함을 알 수 있었다. Toluene을 이용한 내용제성 물성측정 결과에는 glycerol의 mole % 증가에 따른 물성 증감 효과는 없었다.

Vegetable Leather 표면코팅에 대한 Glycerol을 이용한 수분산 폴리우레탄의 합성 및 기계적 특성 (Mechanical Properties and Synthesis of Polyurethane Dispersion by Glycerol for Vegetable Leather Surface Coatings)

  • 이주엽
    • 한국응용과학기술학회지
    • /
    • 제32권1호
    • /
    • pp.100-107
    • /
    • 2015
  • Vegetable leather 표면 코팅에 사용된 폴리우레탄 수지는 glycerol의 함유를 mole % 비로 달리하면서 합성하였다. 합성된 폴리우레탄 수지의 기계적 특성은 SEM, FT-IR, UTM 등을 이용하여 측정하였다. 친환경적인 고분자 수지의 관심이 고조됨에 따라 용제의 사용을 최소화한 vegetable leather 코팅에 사용되는 수분산 수지를 합성하였다. 지방족 3가 알콜인 glycerol의 mole % 비가 증가함에 따라 내마모도, 인장강도가 증가함을 알 수 있었다. 반대로 연신율, 내굴곡 물성은 감소함을 알 수 있었다. Toluene을 이용한 내용제성 물성측정 결과에는 glycerol의 mole % 증가에 따른 물성 증감 효과는 없었다.

Inkjet Printing on the Grain Leather: Evaluation of Line Image Quality on the Grain Leather

  • Park, Heung-Sup;Park, Soo-Min
    • 한국염색가공학회지
    • /
    • 제19권2호
    • /
    • pp.24-31
    • /
    • 2007
  • This paper addresses factors of line image quality on grain leather printed via inkjet printer. Lines were printed onto coated leather media, and line width, edge blurriness, and edge raggedness were evaluated for line image quality. Various factors influenced to wetting and capillary wicking were studied and found out that wicking through capillary between fibers causes significant feathering on leather surface similar with pulp capillary in copy Paper. Polyurethane and acrylic resin coating resulted good image qualify by reducing capillary wicking. The mixture of polyurethane and acrylic resin applied on grain leather satisfied with both image quality and surface hand. $AllWrite^{TM}$ ink brought best results of image quality, comparing with $VeraPrint^{TM}$ ink and $JetWrite^{TM}$ ink.

Synthesis and Properties of Polyurethane-Acrylate Top-Coating Agent

  • Son, Young-Joon;Lee, Dong Jin;Bae, Jong Woo;Lee, Jung Hee
    • Elastomers and Composites
    • /
    • 제50권2호
    • /
    • pp.98-102
    • /
    • 2015
  • A series of polyurethane-acrylate hybrids were synthesized by 2-step emulsion polymerization of a variety of acrylate monomers such as 2-hydroxy ethyl methacrylate (HEMA), methyl methacrylate (MMA). Experiment was performed to improve stability and emulsibility of surface treatment agent, and it was found that the polyurethane-acrylate hybrids having an optimum composition (MMA : 20%, LA(EO)3-S : 3% and TDA-7 : 5%) was shown to be quite surface active in the solid contents. These results suggests that the optimal polyurethane-acrylate hybrids in this study have high potential as top coating agent, which may have high gloss and excellent properties.

피혁가공용 수용성 아크릴-폴리우레탄 Hybrid Resin의 합성 및 기계적 특성에 관한 연구 (Study on Mechanical Properties of Waterborne Polyurethane-Acrylic Hybrid Resin for Leather Coationgs)

  • 이주엽;김기준
    • 한국응용과학기술학회지
    • /
    • 제27권2호
    • /
    • pp.188-195
    • /
    • 2010
  • In this study, we experimented that how to synthesis waterborne urethane-acrylic hybrid resin for leather coatings. First of all, We had analyzed data by FT-IR, SEM and TGA for the machanical properties. By TGA analysis polymers showed heat distortion temperature. and by FT-IR measurement we confirmed that synthesis of urethane and acrylic. In the experiment, solvent resistance, polyurethane and acrylic grades 4-5 showed both a high. Tensile strength measured in the waterborne polyurethane > Acrylic emulsion showed strength in the order. Films were obtained by coating the water born resin on leveled surfaces and allowing them to dry at room temperature for 72hrs. After demolding, the films were kept in a desiccator to avoid moisture contant at $25^{\circ}C$ for 45hrs before the measurements. In this result, the mechanical propersies of waterborne polyurethane-acrylic hybrid resin showed that how effect to resin in leather coating between polyurethane content and acrylic content. Therefore, acrylic emulsion had most high solvent resistance glade and waterborne polyurethane had good result in abrasion test and tensile strength.