KCN 첨가에 따른 (K,Na)$NbO_3$ 세라믹스의 압전특성 (Piezoelectric Properties of (K,Na)$NbO_3$ ceramics with the amount of KCN addition)

  • 서병호;성금현;이상호;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.188-189
    • /
    • 2009
  • In this study, in order to develop excellent lead-free composition ceramics for piezoelectric transformer, $(K_4CuNb_8O_{23})$ added $(K_{0.5}Na_{0.5})(Nb_{0.96}Sb_{0.04})O_3$ ceramics were fabricated using conventional mixed oxide method and their piezoelectric and dielectric properties were investigated as a function of the amount of KCN addition. With increasing the amount of KCN addition, density and mechanical quality factor(Qm), electromechanical coupling factor (Kp) were increased up to 1.2mol% and then decreased. At the 1.2mol% KCN added specimen, mechanical quality factor (Qm), electromechanical coupling factor (Kp), density and dielectric constant (${\varepsilon}r$) showed the optimal values of 781, 0.445, $4.42g/cm^3$ and 443, respectively, for piezoelectric transformer application.

  • PDF

CuO첨가에 따른 $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$세라믹스의 유전 및 압전 특성 (Dielectric and piezoelectric properties of CuO added $(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3$ ceramics)

  • 이유형;박민호;노정래;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2009년도 하계학술대회 논문집
    • /
    • pp.160-161
    • /
    • 2009
  • In this study, in order to develop the lead free piezoelectric ceramics with excellent piezoelectric properties, (Na,K)$NbO_3$ ceramics according to the amount CuO addition were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated. At the 0.8mol% CuO added composition, density, electromechanical coupling factor(kp), echanical quality factor(Qm), dielectric constant$(\varepsilon_r$) and piezoelectric constant($d_{33}$) showed the optimum value of $4.459g/cm^3$, 0.469, 540, 410, 69.57pC/N, respectively.

  • PDF

마그네틱 파우더 브레이크를 이용한 소형 진자형 충격시험기 개발 (Development of a Miniature Pendular Type Impact Testing Machine Using a Magnetic Powder Brake)

  • 유인동;이만석;김호경
    • Tribology and Lubricants
    • /
    • 제27권3호
    • /
    • pp.140-146
    • /
    • 2011
  • A miniature pendular type impact testing machine was designed and developed, adopting a magnetic powder brake in order to investigate tensile and shear behavior of a small solder ball at high speed. In this testing system, the potential energy of the pendulum is transferred into the impact energy during its drop. Then, the impact energy is transmitted through the striker which is connected to the push rods to push the specimen for tensile loading. The tensile behavior of lead-free solder ball in diameter of 760 ${\mu}m$ was successfully investigated in a speed range of 0.15 m/s~1.25 m/s using this designed device. The maximum tensile strength of the solder joint decreases with the loading speed in the testing condition. The maximum tensile strength of the joint was 56 MPa in the low speed region.

조성비에 따른 (1-x)(Na,K)$NbO_3$-xBa(Zr,Ti)$O_3$ 세라믹스의 압전 특성 (Piezoelectric properties of (1-x)(Na,K)$NbO_3$-xBa(Zr,Ti)$O_3$ ceramics with composition)

  • 이영희;이동현;배선기;이상철;최달해
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2011년도 제42회 하계학술대회
    • /
    • pp.1436-1437
    • /
    • 2011
  • (1-x)(Na,K)$NbO_3$-xBa(Zr,Ti)$O_3$ lead free piezoelectric ceramics were synthesized to enhance the piezoelectric properties of (Na,K)$NbO_3$. The synthesis and sintering method were the conventional solid state reaction method and general sintering method in air atmosphere. We report the improved piezoelectric properties in the perovskite structure composed of the NKN and BZT ceramics. We investigated the effects of NKN, BZT on the structural and electrical properties of the NKN-BZT ceramics. The NKN-BZT ceramics show good performance with piezoelectric constant $d_{33}$=155pC/N. The results reveal that (1-x)(Na,K)$NbO_3$-xBa(Zr,Ti)$O_3$ ceramics are promising candidate materials for lead-free piezoelectric application.

  • PDF

K4CuNb8O23 첨가에 따른 (K,Na)NbO3 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of (K,Na)NbO3 Ceramics with the amount of K4CuNb8O23 Addition)

  • 서병호;류주현;마석범;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제22권11호
    • /
    • pp.930-934
    • /
    • 2009
  • In this study, in order to develop excellent lead-free composition ceramics for piezoelectric transformer, ($K_4CuNb_8O_{23}$) added $(K_{0.5}Na_{0.5})(Nb_{0.96}Sb_{0.04})O_3$ ceramics were fabricated using conventional mixed oxide method and their piezoelectric and dielectric properties were investigated as a fu+EY50nction of the amount of KCN addition. With increasing the amount of KCN addition, density and mechanical quality factor(Qm), electromechanical coupling factor (Kp) were increased up to 1.2 mol% and then decreased. At the 1.2 mol% KCN added specimen, mechanical quality factor (Qm), electromechanical coupling factor (Kp), density and dielectric constant (${\varepsilon}r$) showed the optimal values of 781, 0.445, $4.42\;g/cm^3$ and 443, respectively, for piezoelectric transformer application.

PDP 격벽 재료의 인장 물성 측정 방법 (Measurement Method for Tensile Properties of PDP's Barrier Rib Materials)

  • 오충석;배종성;홍병규
    • 한국정밀공학회지
    • /
    • 제26권7호
    • /
    • pp.91-98
    • /
    • 2009
  • A reliable tensile test technique for PDP's barrier rib materials was introduced. A tensile specimen was prepared by punching out of green sheet, curing the specimen in a high temperature furnace, attaching sand paper tabs on each grip ends, and then attaching two strain gages for the strain monitoring and specimen alignment. Preliminary tensile tests were successfully done with the specimens made from ZnO-based lead-free green sheet. The specimens cured at 3 different maximum curing temperatures were tested to demonstrate the applicability of the test method. The Young's modulus was 88 ${\pm}$ 4 GPa regardless of the maximum curing temperature. The ultimate tensile strength was decreased with increasing the temperature. The tensile test method proposed in this study was proven to be reliable, useful and easy to estimate the bulk mechanical properties of barrier rib materials.

마이크로 압입 크리프 시험기 개발 및 성능평가 (Development and its Performance Evaluation of a Micro-Impression Creep Machine)

  • 양경탁;김현준;김호경
    • Tribology and Lubricants
    • /
    • 제24권1호
    • /
    • pp.27-33
    • /
    • 2008
  • A micro-impression creep machine was designed and developed, adopting a small punch in diameter of 150 um, displacement gage with an accuracy of sub-${\mu}m$ scale, and load-cell with an accuracy of mN scale in order to investigate creep behavior of small solder ball in diameter of less than 1 mm. Creep behavior of lead-free solder ball(Sn-3.0Ag-0.5Cu) in diameter of $760\;{\mu}m$ was investigated in the stress range of $8{\sim}60\;MPa$ and at $303\;K{\sim}393\;K$. The applied load became decreased slightly and continuously in the creep rate of $10^{-4}/s$ range during the current experiments. Also, the machine frame was so sensitive to the environmental temperature that nm scaled displacement recording was unstable according to the change in environmental temperature.

Sr 치환에 따른 $Bi_{0.5}(Na_{0.84}K_{0.16})_{0.5}TiO_3$ 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of $Bi_{0.5}(Na_{0.84}K_{0.16})_{0.5}TiO_3$ Ceramics with the variations of Sr Substitution)

  • 오동언;류주현;박창엽;윤현상;정영호;정문영
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.660-663
    • /
    • 2003
  • In this Study, lead-free $Bi_{0.5}(Na_{0.84}K_{0.16})_{0.5}TiO_3$ system ceramics were fabricated with the variations of Sr substitution and their dielectric and piezoelectric characteristics were investigated. With the increase of Sr substitution, dielectric constant increased linearly and Curie temperature decreased slightly. Also, the temperature dependence curve of dielectric constant was moved to left-ward. At 4mol% Sr substitution, Tc of 292, kp of 34.03%, kt of 45.32% and ${\epsilon}r$ of 868 were shown, respectively.

  • PDF

소결시간변화에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Characteristics of (Na,K)NbO3 Ceramics System According to Sintering Time)

  • 김도형;류주현;김인성;송재성
    • 한국전기전자재료학회논문지
    • /
    • 제21권10호
    • /
    • pp.901-905
    • /
    • 2008
  • In this study, $0.95(K_{0.5}Na_{0.5})NbO_{3}-0.05Li(Sb_{0.8}Nb_{0.2})O_{3}+0.2\;wt%Ag_{2}O$ were investigated as a variations of sintering times in order to improve dielectric and piezoelectric properties of lead-free piezoelectric ceramics. $Ag_{2}O$ were used as sintering aids and the specimens were sintered during 3, 5, 7, 9 and 11 hours, respectively. At the specimen sintered during 7 hour, Electromechanical coupling factor ($k_p$), density, dielectric constant (${\epsilon}_{\gamma}$), piezoelectric constant ($d_{33}$) and curie temperature ($T_c$) of composition ceramics showed the optimal value of 0.450, 4.274 $[g/cm^3]$, 1007, 257 [pC/N] and $396^{\circ}C$, respectively.

K5.4Cu1.3Ta10O29 첨가에 따른 (Na,K)NbO3계 세라믹스의 압전특성 (Piezoelectric Properties of (Na,K)NbO3 Ceramics as a Function of K5.4Cu1.3Ta10O29 Addition)

  • 노정래;류주현;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제23권5호
    • /
    • pp.379-382
    • /
    • 2010
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $(K_{0.5}Na_{0.5})(Nb_{0.97}Sb_{0.03})O_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition. $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition enhanced density, electromechanical coupling factor($k_p$) piezoelectric constant $d_{33}$ and mechanical quality factor($Q_m$). At the 0.9 mol% $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum values of 0.46, 471, and 148 pC/N, respectively.