Tunisian phosphogypsum tailings: Assessment of leaching behavior for an integrated management approach

  • Zmemla, Raja;Sdiri, Ali;Naifar, Ikram;Benjdidia, Mounir;Elleuch, Boubaker
    • Environmental Engineering Research
    • /
    • v.25 no.3
    • /
    • pp.345-355
    • /
    • 2020
  • This study has been carried out to evaluate the leaching behavior of Tunisian phosphogypsum (PG) tailings in Skhira city (southern Tunisia). Two PG samples, including old and freshly deposited samples, were characterized in terms of physical, geotechnical, mechanical, chemical and mineralogical properties. Special attention was paid to their leaching behavior when subjected to standard leaching tests. Our results indicated that both samples are mainly composed of more than 31.85% CaO and 31.4% SO3, indicating the predominance of gypsum. This was further confirmed by XRD patterns that revealed the presence of characteristic reflections of gypsum, brushite, quartz and Maladrite. Compressive strength after 90 d exceeded 769 kPa, but still lower than that of natural sand (1,800 kPa). Leaching test was proposed as an appropriate method to determine the released contaminants from PG. The obtained results showed that Fluorine and Phosphorus are the most released elements from PG with 40 and 30%, respectively. The released Se, Cd, and Zn were the only trace elements that exceeded the threshold limits. It seemed that leached element concentrations were independent aging or particle size of the PG. Based on the assessment of leaching behavior, an integrated management approach of the PG deposits was proposed.

Leachability of lead, cadmium, and antimony in cement solidified waste in a silo-type radioactive waste disposal facility environment

  • Yulim Lee;Hyeongjin Byeon;Jaeyeong Park
    • Nuclear Engineering and Technology
    • /
    • v.55 no.8
    • /
    • pp.2889-2896
    • /
    • 2023
  • The waste acceptance criteria for heavy metals in mixed waste should be developed by reflecting the leaching behaviors that could highly depend on the repository design and environment surrounding the waste. The current standards widely used to evaluate the leaching characteristics of heavy metals would not be appropriate for the silo-type repository since they are developed for landfills, which are more common than a silo-type repository. This research aimed to explore the leaching behaviors of cementitious waste with Pb, Cd, and Sb metallic and oxide powders in an environment simulating a silo-type radioactive waste repository. The Toxicity Characteristic Leaching Procedure (TCLP) and the ANS 16.1 standard were employed with standard and two modified solutions: concrete-saturated deionized and underground water. The compositions and elemental distribution of leachates and specimens were analyzed using an inductively coupled plasma optical emission spectrometer (ICP-OES) and energy-dispersive X-ray spectroscopy combined with scanning electron microscopy (SEM-EDS). Lead and antimony demonstrated high leaching levels in the modified leaching solutions, while cadmium exhibited minimal leaching behavior and remained mainly within the cement matrix. The results emphasize the significance of understanding heavy metals' leaching behavior in the repository's geochemical environment, which could accelerate or mitigate the reaction.

Soldering characteristics of Ag-Pd electrodes in relationship to differing particle size of LTCC substrate (LTCC 기판의 Particle Size 에 따른 Ag-Pd 전극의 Soldering 특성 변화)

  • 조현민;유명재;박종철
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2002.05a
    • /
    • pp.130-133
    • /
    • 2002
  • Solder leaching resistance of the metal electrode is an important factor with regard to adhesion properties of ceramic substrate. In the Low Temperature Co-fired Ceramics (LTCC), Ag-Pd or Ag-Pt pastes are used instead of pure Ag paste to prevent leaching. Solder leaching behavior of the Ag-Pd paste in relation to LTCC raw material powder size was investigated. First fabrication of LTCC green tape with different particle size was done. LTCC substrates with Ag-Pd electrode were prepared using conventional multilayer ceramic process. Dipping test was performed to test solder leaching behavior of the electrode. Ag-Pd electrode on LTCC substrate with smaller particle size achieved higher solder leaching resistance.

  • PDF

Hydrochloric Acid Leaching Behavior of Mechanically Activated Black Dross (기계적 활성화처리한 블랙드로스의 염산 침출)

  • Nguyen, Thi Hong;Nguyen, Thi Thuy Nhi;Lee, Man Seung
    • Resources Recycling
    • /
    • v.27 no.3
    • /
    • pp.78-85
    • /
    • 2018
  • Effect of ball milling treatment on the hydrochloric acid leaching performance of black dross was investigated to recover alumina. Ball milling time and speed showed limited effect on the leaching behavior of the alumina in the mechanically dross. Under the optimum mechanical activation condition (for 1h at 700 rpm), the leaching of alumina in hydrochloric acid solution was significantly affected by leaching time and reaction temperature. MgO was completely dissolved in most of the leaching conditions, while a small amount of Ca, Fe, Si and Ti oxides was dissolved. Although 80% of alumina was dissolved, the dissolved minor components such as Ca, Fe, Mg, Si and Ti oxides should be separated to recover pure alumina solution.

An Experimental Study on Characteristics of Flexural Behavior in RC Member with Mineral Admixture under Calcium Leaching Degradation (칼슘용출 열화 조건에서 광물질 혼화재를 사용한 RC부재의 휨 거동에 관한 실험적 연구)

  • Lee, Gyung-Jong;Choi, So-Yeong;Choi, Yoon-Suk;Yang, Eun-Ik
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.2
    • /
    • pp.16-25
    • /
    • 2018
  • Concrete is a suitable construction material for long-term structure, however, it is needed to understand the calcium leaching damage caused by exposure to underground pure water for a long time. In this paper, it is experimentally investigated that the characteristics of flexural behavior in RC member damaged by calcium leaching degradation. From the test results, when calcium leaching is happened, yielding load and flexural rigidity is reduced, neutral axis depth and displacement is increased. That is, calcium leaching degradation adversely affects RC member performance. And, when the mineral admixture is used in the calcium leaching environment, it is considered that the optimal replacement ratio should be prepared according to the type of mineral admixture.

Recovery of Lithium and Leaching Behavior of NCM Powder by Hydrogen Reductive Treatment from NCM System Li-ion Battery Scraps (NCM계(係) 리튬이온전지(電池) 공정(工程)스크랩의 수소환원처리(水素還元處理)에 의한 리튬회수(回收) 및 NCM 분말(粉末)의 침출거동(浸出擧動))

  • Kim, Dae Weon;Jang, Seong Tae;Baek, Kyung Min
    • Resources Recycling
    • /
    • v.22 no.3
    • /
    • pp.43-49
    • /
    • 2013
  • A study on the recovery of lithium and leaching behavior of NCM powder by hydrogen reduction for NCM system Li-ion battery scraps was investigated. The reductive rate was about 93% at $800^{\circ}C$ by hydrogen treatment. The lithium carbonate with 99% purity was manufactured by using $CO_2$ gas and washing method with water for NCM powder after hydrogen reduction. As a result of comparing the powders before and after the hydrogen reduction treatment for acid leaching behavior we obtained 32% enhanced leaching rate of cobalt, 45% enhanced leaching rate of nickel and the 90% leaching effect for manganese by hydrogen reduction at 2M $H_2SO_4$ concentration condition.

Leaching behavior of rhenium and molybdenum from molybdenite roasting dust in NaOH solutions (휘수연석(輝水鉛石)의 배소(焙燒) 중 발생한 분경(粉慶)으로부터 NaOH에 의한 Rhenium과 Molybdenum의 침출(浸出))

  • Kim, Young-Uk;Kang, Jin-Gu;Sohn, Jeong-Soo;Cho, Bong-Gyu;Shin, Shun-Myung
    • Resources Recycling
    • /
    • v.18 no.5
    • /
    • pp.37-43
    • /
    • 2009
  • The demand for rhenium has considerably increased recently owing to the large-scale consumption in industries and the price of rhenium has increased owing to the lack of supply and its availability. The dust from the roasting of molybdenite was employed to investigate the leaching behavior of rhenium and molybdenum. Leaching experiments were done by varying optimum parameters, such as reaction time, NaOH concentration and leaching temperature. The optimum leaching condition was found to be $4\;mol{\cdot}L^{-1}$ NaOH, 2 hours leaching time, $100\;g{\cdot}L^{-1}$ solid/liquid ratio, $80^{\circ}C$ temperature, and 250 rpm. At this condition, leaching percentage of rhenium and molybdenum was 86.1% and 88.6%, respectively.

Leaching behavior of Ga and In from MOCVD dust (MOCVD 더스트로부터 Ga과 In의 침출 거동)

  • Park, Kyung-Soo;Swain, Basudev;Kang, Lee Seung;Lee, Chan Gi;Hong, Hyun Seon;Shim, Jong-Gil;Park, Jeung-Jin
    • Journal of Powder Materials
    • /
    • v.21 no.3
    • /
    • pp.202-206
    • /
    • 2014
  • Leaching of MOCVD dust in the LED industry is an essential stage for hydro-metallurgical recovery of pure Ga and In. To recover Ga and In, the leaching behavior of MOCVD scrap of an LED, which contains significant amounts of Ga, In, Al and Fe in various phases, has been investigated. The leaching process must be performed effectively to maximize recovery of Ga and In metals using the most efficient lixiviant. Crystalline structure and metallic composition of the raw MOCVD dust were analyzed prior to digestion. Subsequently, various mineral acids were tested to comprehensively study and optimize the leaching parameters such as acidity, pulp density, temperature and time. The most effective leaching of Ga and In was observed for a boiling 4 M HCl solution vigorously stirred at 400 rpm. Phase transformation of GaN into gallium oxide by heat treatment also improved the leaching efficiency of Ga. Subsequently high purity Ga and In can be recovered by series of hydro processes.

Ammoniacal Leaching for Recovery of Valuable Metals from Spent Lithium-ion Battery Materials (폐리튬이온전지로부터 유가금속을 회수하기 위한 암모니아 침출법)

  • Ku, Heesuk;Jung, Yeojin;Kang, Ga-hee;Kim, Songlee;Kim, Sookyung;Yang, Donghyo;Rhee, Kangin;Sohn, Jeongsoo;Kwon, Kyungjung
    • Resources Recycling
    • /
    • v.24 no.3
    • /
    • pp.44-50
    • /
    • 2015
  • Recycling technologies would be required in consideration of increasing demand in lithium ion batteries (LIBs). In this study, the leaching behavior of Ni, Co and Mn is investigated with ammoniacal medium for spent cathode active materials, which are separated from a commercial LIB pack in hybrid electric vehicles. The leaching behavior of each metal is analyzed in the presence of reducing agent and pH buffering agent. The existence of reducing agent is necessary to increase the leaching efficiency of Ni and Co. The leaching of Mn is insignificant even with the existence of reducing agent in contrast to Ni and Co. The most conspicuous difference between acid and ammoniacal leaching would be the selective leaching behavior between Ni/Co and Mn. The ammoniacal leaching can reduce the cost of basic reagent that makes the pH of leachate higher for the precipitation of leached metals in the acid leaching.

Potential Environmental Influences in Soil by Accidental Fluorine (F) Leakage, Using Leaching Test (용출시험을 통한 불산 누출사고지역의 토양 내 불소(F)의 거동특성)

  • Kim, Doyoung;Lee, Junseok;Kwon, Eunhye;Lee, Hyun A;Yoon, Hye-On;Lee, Sanghoon
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.37 no.4
    • /
    • pp.234-239
    • /
    • 2015
  • Various leaching tests were applied to the soil affected by accidental leakage of HF in an industrial area in Korea. Three different leaching methods including pH-stat, continuous batch leaching, and column tests were adopted to assess leaching characteristics and mobility of fluorine(F) in soil and the potential risks to ecosystem. Both natural and spiked samples were used for the leaching tests. F concentrations in the batch tests increased by leaching rapidly in the early stage of leaching and then maintained rather constant levels. Column leaching test also show similar result to that of the batch test. pH also controlled the leaching behavior of the soil. With increasing pH, more F was released in the pH-stat test. This is mainly due to the competition and exchange with hydroxyl ions, as pH increase to the alkaline range. Most of the F released by the accident seem to have removed in the very early stage of leaching, whereas some natural proportion from soil minerals are thought to have been released very slowly. Therefore, little F released during the accident remained, based on the results of this study on the samples after two years of the accident. We could conclude that soil contaminated by external effects such as chemical accidents should be managed immediately, especially with F.