• Title/Summary/Keyword: lattice oxygen

Search Result 223, Processing Time 0.042 seconds

Interaction of Oxygen and $CH_4$ with Molybdenum Oxide Catalysts

  • Kim, C. M.
    • Bulletin of the Korean Chemical Society
    • /
    • v.18 no.10
    • /
    • pp.1082-1085
    • /
    • 1997
  • The Near-Edge X-ray Absorption Fine Structure (NEXAFS) technique and Differential Scanning Calorimetry (DSC) were utilized to investigate the reaction of CH4 and O2 on the MoO3/SiO2 catalyst. The NEXAFS results showed that the stoichiometry of the molybdenum oxide catalyst supported on silica was MoO3. MoO3 was reduced to MoO2 when the catalyst was exposed to CH4 at 773 K. NEXAFS results confirm that lattice oxygen is directly related to the process of CH4 oxidation which takes place on the surface of MoO3/SiO2 catalysts. DSC results show that the structure of MoO3 changes around 573 K and this structural change seems to improve the migration of oxygen in the lattice.

X-ray Photoelectron Spectroscopy Study of LaFeO3 Powders Synthesized by Solution Combustion (용액연소법으로 제조한 LaFeO3의 XPS 특성)

  • Hwang, Yeon;Kang, Dae-Sik;Park, Mi-Hye;Cho, Sung-Baek
    • Korean Journal of Materials Research
    • /
    • v.18 no.6
    • /
    • pp.313-317
    • /
    • 2008
  • [ $LaFeO_3$ ] powders were synthesized using a method involving solution combustion, and the surface properties of these powders were examined by x-ray photoelectron spectroscopy. As the amount of fuel increased during the synthesis, the $LaFeO_3$ powders became amorphous with a large plate-like shape. It was found that the O 1s spectra were composed of two types of photoelectrons by deconvolutioning the spectra. Photoelectrons with higher binding energy come from adsorbed oxygen ($O^-$) whereas those with lower energy come from lattice oxygen ($O^{2-}$). The ratio of adsorbed and lattice oxygen increased as the ratio of the fuel and nitrate (${\Phi}$) increased. The binding energy of both types of oxygen increased as ${\Phi}$ increased due to the formation of carbonates.

Finding interstitial oxygen in an Si substrate during low temperature plasma oxidation

  • Kim, Bo-Hyun;Ahn, Jin-Hyung;Ahn, Byung-Tae
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2003.07a
    • /
    • pp.690-693
    • /
    • 2003
  • An Si substrate (100) was oxidized at $400^{\circ}C$ in inductively coupled oxygen plasma. Interstitial oxygen was found in the Si substrate at the initial stage of oxidation by IR measurements. An x-ray rocking curve of Si substrates showed a lower peak intensity due to lattice distortion by the interstitial oxygen. The refractive index of thin oxides, below which interstitial oxygen existed in the Si substrate, was smaller than the refractive index of thick oxides, below which no interstitial oxygen existed. The interstitial oxygen was found by plasma oxidation using $O_{2}$ gas and $N_{2}O$ gas. The inductively coupled plasma oxidation using $N_{2}O$ gas was performed by atomic oxygen, not by molecular oxygen, indicating that atomic oxygen in plasma is responsible for the incorporation of interstitial oxygen.

  • PDF

Effect of Annealing on c-axis Orientation of $PbTiO_3$ Thin Films by D.C magnetron Reactive Sputtering (D.C Magnetron Reactive Sputtering 법으로 증착한 $PbTiO_3$ 박막의 열처리에 따른 c-축 배향성의 변화)

  • 이승현;권순용;최한메;최시경
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.7
    • /
    • pp.802-808
    • /
    • 1996
  • PbTiO3 thin films were fabricated onto MgO(100) single crystal substrate by reactive D. C magnetron sput-tering of Pb and Ti metal in an oxygen and argon gas mixture. The annealing of the thin films resulted in the decrease of both the c-axis orientation ratio and the lattice parameter. It is well known that the c-axis lattice parameter of thin film is dependent on the Pb/(Pb+Ti)ratio and the residual stress in the film The PbTiO3 thin films with a Pb/(Pb+T) ratio ranging from 0.45 to 0.57 were fabricated and annealed. The structure of the film the c-axis orientation ratio and the lattice parameter were not dependent on the Pb/(Pb+Ti) ratio before and after annealing. These experimental results proved that the decrease of the c-axis lattice parameter under the annealing conditions was due to the relaxation of the intrinsic stress in the film. This relaxation of the intrinsic stress caused the decrease of the c-axis orientation ratio and this phenomenon can be explained by c-axis growth lattice model.

  • PDF

Effect of Ce0.9Gd0.1O1.95 as a promoter upon the oxygen transfer properties of MgMnO3-δ-Ce0.9Gd0.1O1.95 composite oxygen carrier materials for chemical looping combustion

  • Hwang, Jong Ha;Lee, Ki-Tae
    • Journal of Ceramic Processing Research
    • /
    • v.20 no.1
    • /
    • pp.18-23
    • /
    • 2019
  • Chemical looping combustion (CLC) is a promising carbon capture and storage (CCS) technology whose efficiency and cost primarily relies on the oxygen carrier materials used. In this paper, gadolinium-doped ceria (GDC, Ce0.9Gd0.1O1.95) was added as a promoter to improve the oxygen transfer rate of MgMnO3-δ oxygen carrier materials. Increasing GDC content significantly increased the oxygen transfer rate of MgMnO3-δ-GDC composites for the reduction reaction due to an increase in the surface adsorption of CH4 via oxygen vacancies formed on the surface of the GDC. On the other hand, the oxygen transfer rate for the oxidation reaction decreased linearly with increasing GDC content due to the oxygen storage ability of GDC. Adsorbed oxygen molecules preferentially insert themselves into oxygen vacancies of the GDC lattice rather than reacting with (Mg,Mn)O to form MgMnO3-δ during the oxidation reaction.

Structure of laser ablated $Ba_{0.8}Sr_{0.2}TiO_3$ thin films grown on MgO (레이저 증착법으로 MgO 기판에 성장한 $Ba_{0.8}Sr_{0.2}TiO_3$ 박막의 구조 연구)

  • Kim, Won-Jeong;Kim, Sang-Su;Hahn, Chang-Hee;Song, Tae-Kwon;Moon, Seung-Eon;Kwak, Min-Hwan;Kim, Young-Tae;Ryu, Han-Cheol;Lee, Su-Jae;Kang, Kwang-Yong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.04b
    • /
    • pp.157-160
    • /
    • 2004
  • Ferroelectric $(Ba_xSr_{1-x})TiO_3$ (BST) thin films have been deposited on (001) MgO single crystals by a pulsed laser deposition (PLD) method. The structure of deposited BST thin films were investigated by an x-ray diffractometer. Calculated c-axis lattice parameters of the BST films exhibit a strong lattice distortion, which was not observed in ceramic BST at room temperature. This lattice distortion of BST has been attributed to strains caused by lattice constant difference between film and substrate, oxygen vacancies in BST film, and thermal expansion difference between film and substrate. Ferroelectric properties at 10 GHz have been measured using a HP 8510C vector network analyzer. Dielectric properties, capacitance tunability and quality factor, of the interdigitaed capacitors fabricated on BST films were calculated from the measured s-parameters. Two distinct behaviors in structural, opitical, and microwave properties of BST films were observed; below and above 200 mTorr of oxygen pressure in the deposition chmber.

  • PDF

Ambient Oxygen Effects on the Growth of ZnO Thin Films by Pulsed Laser Deposition

  • Park, Jae-Young;Kim, Sang-Sub
    • Korean Journal of Materials Research
    • /
    • v.17 no.6
    • /
    • pp.303-307
    • /
    • 2007
  • ZnO thin films were prepared by pulsed laser deposition on amorphous fused silica substrates at different ambient $O_2$ pressures varying from 0.5 to 500 mTorr, to observe the effect of ambient gas on their crystalline structure, morphology and optical properties. Results of X-ray diffraction, scanning electron microscopy, atomic force microscopy and photoluminescence studies showed that crystallinity, surface features and optical properties of the films significantly depended on the oxygen background pressure during growth. A low oxygen pressure (0.5 mTorr) seems to be suitable for the growth of highly c-axis oriented and smoother films possessing a superior luminescent property. The films grown at the higher $O_2$ pressures (50-500 mTorr) were found to have many defects probably due to an excessive incorporation of oxygen into ZnO lattice. We speculate that the film crystallinity could be affected by the kinetics of atomic arrangement during deposition at the higher oxygen pressures.

Ferroelectric Characteristics of Pb-containing Perovskite-Pyrochlore Composites (Pb계 Perovskite-Pyrochlore 복합체의 강유전특성)

  • 조진우;손정호;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.5
    • /
    • pp.500-504
    • /
    • 1997
  • Perovskite Pb0.7Ba0.3Zn1/3Nb2/3O3 substituted with 0.3 mole fraction for Pb-site in PbZn1/3Nb2/3O3 relaxor and pyrochlore Pb1.83Ba0.29Zn1.71Nb2/3O6.39 were mixed and dielectric characteristics of this composites were investigated. Percolation limit of perovskite phase, which was determined by microstructural observation in the composite as an isolation of perovskite phase from pyrochlore matrix, was 28.9-47.5 vol%. Ferroelectric phase transition below percolation limit depends on a parameter which affects the propagation of lattice vibration between isolated perovskite phase and pyrochlore matrix. Therefore, it is believed that ferroelectric lattice vibration of isolated perovskite phase could be transfered to pyrochlore matrix when the oxygen octahedra are linked in 3-dimension and highly polarizable Pb2+ ions are contained in both phases.

  • PDF

The Luminescence Property of Ba-Mg-Al-O:$Eu^2+$ Blue Phosphors (Ba-Mg-Al-O:$Eu^2+$ 청색형광체의 발광특성)

  • 김광복;천희곤;조동율;구경완
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.157-161
    • /
    • 2000
  • Blue phosphor of Ba-Mg-Al-O:Eu$^{2+}$ phase was fabricated by conventional firing techniques under reducing atmosphere and its photoluminescence properties are studied with varying Eu concentration and phost-annealing temperature under air atmosphere. This phosphors were well crystallized with particle size in the range of 3~5um and emitted a blue light at a dominent wavelength 450nm for 254nm UV irradiation. The concentration quenching wit Eu$^{2+}$ was that with increasing Eu concentration the energy transfer between the activator ions steadily improves, so that the excitation energy is transported over larger distances through the lattice before luminescence can occur. Thermal quenching also occurred in this phosphor means that in a host lattice with the $\beta$-alumina structure the bond of an Eu$^{2+}$ ion with the nearest-neighbour oxygen ion is much stronger than in a lattice with the magnetoplumbite structure.cture.

  • PDF