Effects of the Knife-Incising and Longitudinal Kerfing Treatment on High-Temperature Drying Characteristics of Red Pine Square Timber (배할 및 자상-인사이징 처리가 소나무 정각재의 고온건조 특성에 미치는 영향)

  • Lee, Chang-Jin;Lee, Nam-Ho;Oh, Seung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.5
    • /
    • pp.677-684
    • /
    • 2016
  • This study was carried out to confirm the effects of the knife-incising and longitudinal kerfing treatment on high-temperature drying characteristics of red pine square timber with dimensions of thickness 15 cm. The range of final moisture content was investigated 5.6% to 7.5% after drying. The differences did not exist in the moisture content and distribution according to the pretreatment condition. In the case of longitudinal kerfing treatment, the surface check occurrence was reduced than the control. In addition, the twist had a tendency to decrease due to the longitudinal kerfing treatment. The knife-incising and longitudinal kerfing treatment were investigated to be ineffective on internal checks and drying shrinkage.

Effects of The Knife-incising and Kerfing Pretreatment on Moisture Content and Surface Check Occurrence of Douglas-fir Heavy Timber (배할 및 자상-인사이징 전처리가 Douglas-fir 중목구조부재의 함수율과 재면할렬 발생에 미치는 영향)

  • Lee, Chang-Jin;Lee, Nam-Ho;Oh, Seung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.3
    • /
    • pp.302-314
    • /
    • 2016
  • This study was carried out to confirm the effects of the knife-incising and kerfing pretreatment on the moisture content and surface check occurrence of Douglas-fir heavy timber. In the case of moisture content, the moisture gradient that formed in the inner part of the specimen was observed in all specimens. In addition, the moisture gradient was formed differently from the surface layer to 72 mm depending on the pretreatment conditions, and it was formed gradually in the kerfing than the knife-incising. In addition, it was found that the solid volume should be considered when measuring the average moisture content. In the case of surface check, the surface check occurrence was reduced in the knife-incising, kerfing, and the combination of knife-incising and kerfing than the control. In particular, the kerfing treatment was shown that the expansion of surface check width was effectively suppressed. In the case of knife-incising treatment, although the surface check was less than the control, the preventive effect on the surface check occurrence did not reach the level of the kerfing treatment.

Effect of Kerfing and Incising Pretreatments on High-Temperature Drying Characteristics of Cedar and Larch Boxed-Heart Timbers with Less than 150 mm in Cross Section Size (배할 및 인사이징 전처리가 횡단면 크기 150 mm 이하 삼나무와 낙엽송 수심재의 고온건조특성에 미치는 영향)

  • LEE, Chang-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.3
    • /
    • pp.345-363
    • /
    • 2020
  • This study was conducted to identify the effect of kerfing and incising pretreatments on high-temperature drying characteristics of cedar and larch boxed-heart timbers with a cross section of less than 150 mm. The result showed that the pretreatments have made a significant difference regarding surface check and shrinkage. Although the kerfing was suitable as a pretreatment to reduce the occurrence of surface check, the incising was not suitable as a pretreatment since the knives of timber joined together, causing the conversion to the surface checks. The shrinkage showed a significant result that the final moisture content was reduced in the order of incising, kerfing, and kerfing-incising after the drying process based on the pretreatment condition. Twist was more affected by the grain angle than the anisotropy of the juvenile wood, and there was no effect of pretreatments.