• 제목/요약/키워드: ion deposition

검색결과 1,000건 처리시간 0.027초

Solid State Cesium Ion Beam Sputter Deposition

  • Baik, Hong-Koo
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 1996년도 The 9th KACG Technical Annual Meeting and the 3rd Korea-Japan EMGS (Electronic Materials Growth Symposium)
    • /
    • pp.5-18
    • /
    • 1996
  • The solid state cesium ion source os alumino-silicate based zeolite which contains cerium. The material is an ionic conductor. Cesiums are stably stored in the material and one can extract the cesiums by applying electric field across the electrolyte. Cesium ion bombardment has the unique property of producing high negative ion yield. This ion source is used as the primary source for the production of a negative ion without any gas discharge or the need for a carrier gas. The deposition of materials as an ionic species in the energy range of 1.0 to 300eV is recently recognized as a very promising new thin film technique. This energetic non-thermal equilibrium deposition process produces films by “Kinetic Bonding / Energetic Condensation" mechansim not governed by the common place thermo-mechanical reaction. Under these highly non-equilibrium conditions meta-stable materials are realized and the negative ion is considered to be an optimum paeticle or tool for the purpose. This process differs fundamentally from the conventional ion beam assisted deposition (IBAD) technique such that the ion beam energy transfer to the deposition process is directly coupled the process. Since cesium ion beam sputter deposition process is forming materials with high kinetic energy of metal ion beams, the process provider following unique advantages:(1) to synthesize non thermal-equilibrium materials, (2) to form materials at lower processing temperature than used for conventional chemical of physical vapor deposition, (3) to deposit very uniform, dense, and good adhesive films (4) to make higher doposition rate, (5) to control the ion flux and ion energy independently. Solid state cesium ion beam sputter deposition system has been developed. This source is capable of producing variety of metal ion beams such as C, Si, W, Ta, Mo, Al, Au, Ag, Cr etc. Using this deposition system, several researches have been performed. (1) To produce superior quality amorphous diamond films (2) to produce carbon nitirde hard coatings(Carbon nitride is a new material whose hardness is comparable to the diamond and also has a very high thermal stability.) (3) to produce cesiated amorphous diamond thin film coated Si surface exhibiting negative electron affinity characteristics. In this presentation, the principles of solid state cesium ion beam sputter deposition and several applications of negative metal ion source will be introduced.

  • PDF

Nucleation, Growth and Properties of $sp^3$ Carbon Films Prepared by Direct $C^-$ Ion Beam Deposition

  • Kim, Seong I.
    • The Korean Journal of Ceramics
    • /
    • 제3권3호
    • /
    • pp.173-176
    • /
    • 1997
  • Direct metal ion beam deposition is considered to be a whole new thin film deposition technique. Unlike other conventional thin film deposition processes, the individual deposition particles carry its own ion beam energies which are directly coupled for the formation of this films. Due to the nature of ion beams, the energies can be controlled precisely and eventually can be tuned for optimizing the process. SKION's negative C- ion beam source is used to investigate the initial nucleation mechanism and growth. Strong C- ion beam energy dependence has been observed. Complete phase control of sp3 and sp3, control of the C/SiC/Si interface layer, control of crystalline and amorphous mode growth, and optimization of the physical properties for corresponding applications can be achieved.

  • PDF

Development of High Flux Metal Ion Plasma Source for the Ion Implantation and Deposition

  • Kim, Do-Yun;Lee, Eui-Wan
    • Journal of Korean Vacuum Science & Technology
    • /
    • 제7권2호
    • /
    • pp.45-56
    • /
    • 2003
  • A high flux metal plasma pulse ion source, which can simultaneously perform ion implantation and deposition, was developed and tested to evaluate its performance using the prototype. Flux of ion source was measured to be 5 A and bi-polar pulse power supply with a peak voltage of 250 V, repetition of 20 Hz and width of 100 ${\mu}\textrm{s}$ has an output current of 2 kA and average power of 2 kW. Trigger power supply is a high voltage pulse generator producing a peak voltage of 12 kV, peak current of 50 A and repetition rate of 20 Hz. The acceleration column for providing target energy up to ion implantation is carefully designed and compatible with UHV (ultra high vacuum) application. Prototype systems including various ion sources are fabricated for the performance test in the vacuum and evaluated to be more competitive than the existing equipments through repeated deposition experiments.

  • PDF

SOLID STATE CESIUM ION BEAM SPUTTER DEPOSITION

  • Baik, Bong-Koo;Choi, Dong-Jun;Han, Dong-Won;Kim, Yong-Hwan;Kim, Seong-In
    • 한국표면공학회지
    • /
    • 제29권5호
    • /
    • pp.474-477
    • /
    • 1996
  • The solid state cesium ion beam sputter deposition system has been developed for negative carbon ion beam deposition. The negative carbon ion beams are effectively produced by cesium ion bombardment. The C-ion beam current and deposition energy can be independently controlled for the deposition of a-D films. This system is very compact, reliable and high flux without any gas discharge or plasma and has been successfully used in the studies of the ion beam deposited amorphous diamond(a-D)

  • PDF

익산지역 대기에어로졸 중 수용성 이온성분의 계절별 침적 특성 (Seasonal Deposition Characteristics of Water-soluble Ion Species in Ambient Aerosol in Iksan City)

  • 강공언
    • 한국환경보건학회지
    • /
    • 제39권1호
    • /
    • pp.56-70
    • /
    • 2013
  • Objectives: This paper aims to investigate the seasonal deposition characteristics of water-soluble ion species by comparing the deposition amount of two samples taken according to different sampling methods of deposition for ambient aerosol such as gases and particulate matters. Methods: Deposition samples were collected using two deposition gauges in the downtown area of Iksan City over approximately two weeks of each season in 2004. The type of deposition gauges consisted of two different sampling methods known as dry gauge and a wet gauge. The dry gauge was empty and used a dry PE bottle with an inlet diameter of 9.6 cm. Before the beginning of each deposition sampling, a volume of 30-50 ml distilled ionized water was added to the wet gauge to wet the bottom during the sampling period. Deposition samples were measured twice per day and analyzed for inorganic water-soluble ion species using ion chromatography. Results: The daily deposition amounts of all measured ions in the dry gauge and the wet gauge showed a significant increase when precipitation occurred, having no difference of deposition amount between in the wet gauge and in the dry gauge. By excluding two samples from rainy days during the sampling period, the mean daily deposition of all ions in dry gauge and wet gauge were $6.58mg/m^2/day$ and $18.16mg/m^2/day$, respectively. The mean deposition amounts of each ion species were higher in the wet gauge than in the dry gauge because of the surface difference of the sampling gauge, especially for $NH_4{^+}$ and ${SO_4}^{2-}$. The mean deposition amounts of $NH_4{^+}$ and ${SO_4}^{2-}$ in the wet gauge were found to be about 15.4 times and 5.2 times higher than that in dry gauge, with a pronounced difference between spring and summer, while the remaining ion species were 1.1-2.0 times higher in the wet gauge than in the dry gauge. Dominant species in the dry gauge were $Ca^{2+}$ and $NO_3{^-}$, accounting for 36.4% and 18.1% of the total ion deposition, whereas those in the wet gauge were $NH_4{^+}$ and ${SO_4}^{2-}$, accounting for 32.5% and 25.0% of the total ion deposition, respectively. Conclusion: The seasonal differences in deposition amounts of water-soluble ion species in ambient aerosol depending on the two types of different sampling methods were identified. This suggests that the removal of ambient aerosol is strongly influenced by the weather conditions of each season as well as the condition of earth's surface, such as dry ground and water.

TiN증착 조건에 따른 박막의 특성에 대한 실험적 연구 (A study on an experimental basis a special quality character of thin film use in order to TiN a conditioned immersion)

  • 박일수
    • 한국산학기술학회논문지
    • /
    • 제12권11호
    • /
    • pp.4711-4717
    • /
    • 2011
  • PVD방식에 의한 TiN박막의 형성은 DC와 RF sputtering deposition 방식을 적용할 수 있지만, 플라즈마 생성을 위해 주입된 가스의 이온화율이 떨어져 박막성형 속도가 느려지며, 박막과의 접착력을 높이는 것에도 한계성을 가지고 있다. 이를 개선하기 위해 증착과 동시에 이온빔을 조사하는 이온빔 진공증착 IBAD(Ion beam assisted deposition)를 이용 하게 되면, 코팅 전에 소재 표면을 Ion beam으로 조사하기 때문에 표면cleaning의 효과가 크고, 접착력이 높은 박막을 얻을 수 있다. 또한 고 진공과 낮은 온도에서도 균일한 두께의 고순도의 박막을 얻을 수 있는 이점이 있다.

Filtered Plasma Deposition and MEVVA Ion Implantation

  • Liu, A.D.;Zhang, H.X.;Zhang, T.H.
    • 한국진공학회지
    • /
    • 제12권S1호
    • /
    • pp.46-48
    • /
    • 2003
  • The modification of metal surface by ion implantation with MEVVA ion implanter and thin film deposition with filtered vacuum arc plasma device is introduced in this paper. The combination of ion implantation and thin film deposition is proved as a better method to improve properties of metal surface.

나노 패터닝을 위한 이온빔-고체 상호작용 분석 (Analysis of Ion Beam-Solid Interactions for Nano Fabrication)

  • 김흥배
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.581-584
    • /
    • 2005
  • Ion beam processing is one of the key technologies to realize mastless and resistless sub 50nm nano fabrication. Unwanted effects, however, may occur since an energetic ion can interact with a target surface in various ways. Depending on the ion energy, the interaction can be swelling, deposition, sputtering, re-deposition, implantation, damage, backscattering and nuclear reaction. Sputtering is the fundamental mechanisms in ion beam induced direct patterning. Re-deposition and backscattering are unwanted mechanisms to avoid. Therefore understanding of ion beam-solid interaction should be advanced for further ion beam related research. In this paper we simulate some important interaction mechanisms between energetic incident ions and solid surfaces and the results are compared with experimental data. The simulation results are agreed well with experimental data.

  • PDF

XRD Patterns and Bismuth Sticking Coefficient in $Bi_2Sr_2Ca_nCu_{n+1}O_y(n\geq0)$ Thin Films Fabricated by Ion Beam Sputtering Method

  • Yang, Seung-Ho;Park, Yong-Pil
    • Journal of information and communication convergence engineering
    • /
    • 제4권4호
    • /
    • pp.158-161
    • /
    • 2006
  • [ $Bi_2Sr_2Ca_nCu_{n+1}O_y(n{\geq}0)$ ] thin film is fabricatedvia two different processes using an ion beam sputtering method i.e. co-deposition and layer-by-layer deposition. A single phase of Bi2212 can be fabricated via the co-deposition process. While it cannot be obtained by the layer-by-layer process. Ultra-low growth rate in our ion beam sputtering system brings out the difference in Bi element adsorption between the two processes and results in only 30% adsorption against total incident Bi amount by layer-by-layer deposition, in contrast to enough Bi adsorption by co-deposition.

Linear Ion Beam Applications for Roll-to-Roll Metal Thin Film Coatings on PET Substrates

  • Lee, Seunghun;Kim, Do-Geun
    • Applied Science and Convergence Technology
    • /
    • 제24권5호
    • /
    • pp.162-166
    • /
    • 2015
  • Linear ion beams have been introduced for the ion beam treatments of flexible substrates in roll-to-roll web coating systems. Anode layer linear ion sources (300 mm width) were used to make the linear ion beams. Oxygen ion beams having an ion energy from 200 eV to 800 eV used for the adhesion improvement of Cu thin films on PET substrates. The Cu thin films deposited by a conventional magnetron sputtering on the oxygen ion beam treated PET substrates showed Class 5 adhesion defined by ASTM D3359-97 (tape test). Argon ion beams with 1~3 keV used for the ion beam sputtering deposition process, which aims to control the initial layer before the magnetron sputtering deposition. When the discharge power of the linear ion source is 1.2 kW, static deposition rate of Cu and Ni were 7.4 and $3.5{\AA}/sec$, respectively.