• Title/Summary/Keyword: interface microstructure

Search Result 447, Processing Time 0.023 seconds

Microstructure modification and electrochemical properties of steel corrosion in the blended cement systems containing internal chlorides (고농도 염화물을 함유하는 혼합시멘트 계에서 철근부식에 따른 미세구조의 변화와 전기화학적 특성)

  • 나종윤;이승헌;김창은
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.131-134
    • /
    • 1999
  • Microstructure modification and electrochemical properties are investigate to estimate the effects of internal chlorides on the steel corrosion in the blended cement systems. According to the test results, slag cement system showed high chloride binding capacity and low corrosion rate. The impedance data showed three distince arcs from lowest(mHz) frequency to highest (MHz) frequency due to product layer, interfacial reaction and bulk matrix. Through the microstructural investigation, fine steel-matrix interface of slag cement system was observed but rough steel-matrix interface of OPC system was observed. Friedel's salt was thought that the substantial material contributed to the chloride binding of slag cement system.

  • PDF

The TEM Characterization of the Interfacial Microstructure between In Solder and Au/Ni/Ti Thin Films during Reflow Process (리플로 공정 후에 형성된 In과 Au/Ni/Ti 다층 박막의 계면 구조의 TEM 분석)

  • 조원구;김영호;김창경
    • Journal of the Korean institute of surface engineering
    • /
    • v.32 no.4
    • /
    • pp.503-512
    • /
    • 1999
  • The crystal structure and the microstructure of the intermetallic compounds formed in the interface between In solder and Au/Ni/Ti thin films have been investigated by XRD, SEM, and TEM. Indium solder was deposited on the Au/Ni/Ti thin films/Si substrate by evaporation. The heat treatments simulated the flip chip solder joining were performed in RTA system or in furnace. $Auln_2$ phase is formed in all specimens.$ In_{27}$ $Ni_{10}$ and/or $In_{X}$ $Ni_{Y}$ phase are formed in the interface between $Auln_2$ and Ni depending the heat treatment conditions.

  • PDF

Review of interface engineering for high-performance all-solid-state batteries (계면 제어를 기반으로 한 고성능 전고체 전지 연구)

  • Insu, Hwang;Hyeon Jeong, Lee
    • Journal of Industrial Technology
    • /
    • v.42 no.1
    • /
    • pp.19-27
    • /
    • 2022
  • This review will discuss the effort to understand the interfacial reactions at the anode and cathode sides of all-solid-state batteries. Antiperovskite solid electrolytes have received increasing attention due to their low melting points and anion tunability which allow controlling microstructure and crystallographic structures of this material system. Antiperovskite solid electrolytes pave the way for the understanding relationship between critical current density and mechanical properties of solid electrolytes. Microstructure engineering of cathode materials has been introduced to mitigate the volume change of cathode materials in solid-state batteries. The hollow microstructure coupled with a robust outer oxide layer effectively mitigates both volume change and stress level of cathode materials induced by lithium insertion and extraction, thus improving the structural stability of the cathode and outer oxide layer, which results in stable cycling performance of all-solid-state batteries.

Analysis and Propagation Behavior of Dissimilar Friction Welded Materials for Fatigue Crack in around Interface (이종마찰압접 계면근방에서의 피로균열의 전파거동 및 해석)

  • 오환섭
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1998.10a
    • /
    • pp.140-145
    • /
    • 1998
  • In this study, analysis for fatigue crack propagation behavior of interface and aroud interface under rotary bending stress. Though K values are nearly the same in around interface by BEM 2-D, fatigue crack propagated H.A.Z. Around Interface crack propagation speed is m=0.678 in H.A.Z by Paris' law. In this case(friction welded materials: STS304, SM15C), fatigue crack growth is considered SM15C metal microstructure and elastic flow from this result. Result is more metal microstructute dependence than stress dependence by analysis (BEM 3-D, BEM 2-D) and fatigue crack propagation

  • PDF

Evaluation of Microstructure and Mechanical Properties of Friction Stir Lap Jointed Inconel 600/SS 400 (겹치기 마찰교반접합된 Inconel 600/SS 400 합금의 미세조직과 기계적 특성 평가)

  • Song, Kuk-Hyun;Nakata, Kazuhiro
    • Korean Journal of Materials Research
    • /
    • v.22 no.3
    • /
    • pp.123-129
    • /
    • 2012
  • The microstructures and mechanical properties of friction stir welded lap joints of Inconel 600 and SS 400 were evaluated; friction stir welding was carried out at a tool rotation speed of 200 rpm and welding speed of 100 mm/min. Electron back-scattering diffraction and transmission electron microscopy were introduced to analyze the grain boundary characteristics and the precipitates, respectively. Application of friction stir welding was notably effective at reducing the grain size of the stir zone. As a result, the reduced average grain size of Inconel 600 ranged from $20{\mu}m$ in the base material to $8.5{\mu}m$ in the stir zone. The joint interface between Inconel 600 and SS 400 showed a sound weld without voids and cracks, and MC carbides with a size of around 50 nm were partially formed at the Inconel 600 area of lap joint interface. However, the intermetallic compounds that lead to mechanical property degradation of the welds were not formed at the joint interface. Also, a hook, along the Inconel 600 alloy from SS 400, was formed at the advancing side, which directly brought about an increase in the peel strength. In this study, we systematically discussed the evolution of microstructures and mechanical properties of the friction stir lap joint between Inconel 600 and SS 400.

Microstructure and Processing of Bioactive Ceramic Composites as Dental Implants (치과 임플란트용 bioactive 세라믹 복합재료의 제조와 미세조직)

  • Kim, Bu-Sob
    • Journal of Technologic Dentistry
    • /
    • v.25 no.1
    • /
    • pp.21-28
    • /
    • 2003
  • The purpose of this study was to process bio-active glass ceramic composite, reinforced with sapphire fibers, by hot press. Also to study the interface of the matrix and the sapphire fiber, and the mechanical properties. Glass raw materials melted in Pt crucible at 1300$^{\circ}C$ during 3.5 hours. The melt was crushed in ball mill and then crushed material, ground and sieved to $<40{\beta}{\mu}m$. Sapphire fibers cut (30mm) and aligned. Powder and fibers hot pressed. The micrographs show good bonding between the matrix and the fiber and no porosity in the glass matrix. This means ideal fracture phenomena. Glass is fractured before the fiber. This is indication of good fracture strength. EDXS showing aluminum rich phase and crystalline phase. Bright field image of the matrix showing crystalline phase. Also diffraction pattern of TEM showing the crystalline phase and more than one phase. Strength of the samples was determined by 3 point bend testing. Strength of the 10vol% sample was approximately 69MPa, while strength of the control sample is 35MPa. Conclusions through this study as follow: 1. Micrographs show no porosity in the glass matrix and the interface. 2. The interface between the fiber and the glass matrix show no gaps. 3. Fracture of the glass indicates characteristic fiber-matrix separation. 4. Presence of crystalline phase at high processing temperature. 5. Sapphire is compatible with bioactive glass.

  • PDF