An Experimental Study on the Characteristics of Strength in Mortar under High Temperature conditions in an Early Age (모르터 압축강도 특성에 영향을 미치는 고온이력에 관한 실험적 연구)

  • Kim Young Joo;Gong Min Ho;Song In Myung;Yang Dong Il;Paik Min Su;Jung Sang Jin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.11a
    • /
    • pp.703-706
    • /
    • 2004
  • This study is basic experiment for estimating influence of strength by curing temperature of concrete's heat of hydration and estimate relationship of compressive strength development by initial curing temperature factor, and then asume temperature factor which influence compressive strength development and for showing basic document of quality control. According to the result of cement mortar by the curing temperature factor high-curing temperature shows high strength on 3 day compare with low curing-temperature, shows higher strength than the piece of high curing temperature.

  • PDF

Temperature History of Concrete at Cold Weather Depending on the Kinds of Insulating Sheet (단열양생시트 종류 변화에 따른 한중콘크리트의 온도이력)

  • Jeon, Chung-Keun;Kim, Jong;Shin, Dong-An;Oh, Seon-Kyo;Han, Cheon-Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05a
    • /
    • pp.618-621
    • /
    • 2006
  • This paper is to investigate temperature history of cold weather concrete depending on insulation curing sheet kinds. Insulating effect according to curing sheet is shown in order of 5 layer bubble sheet, combination of PE form and 3 layer bubble sheet and 3 layer bubble sheet. It maintained above $10^{\circ}C$ of minimum temperature until the completion of initial curing period when bubble curing sheet was supplied regardless of curing sheet kinds. Five layer bubble curing sheet secure higher curing temperature than any other curing sheet applied in this experiment by as much as $2{\sim}3^{\circ}C$, which performed remarkable insulation effect. Concrete applied with curing sheet secured above $65^{\circ}D{\cdot}D$ of maturity, at which concrete had 5MPa of compressive strength at 3 days.

  • PDF

Temperature Properties of Vertical Reinforcements in Wall Structures in Relation to the Different Methods of Bubble Sheet Installation in Winter (겨울철 버블시트 포설방법 변화에 따른 벽식구조 수직철근의 온도 특성)

  • Kim, Tae-Woo;Lee, Jea-Hyeon;Kyung, Yeong-Hyeok;Lee, Jong-Gyo;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.05a
    • /
    • pp.11-12
    • /
    • 2017
  • This study aims to analyze the properties of the temperature change in vertical reinforcements in outdoor wall structures in winter in relation to the different methods of bubble sheet installation, and to subsequently determine the possibility of initial frost damage to the concrete as a result of low temperature. As for the experimental variables, double bubble sheets were used as curing materials, and the curing method was to model the part where the slab and the wall intersect and the rebar is exposed, and to measure the change of temperature around the exposed rebar in accordance with the change of the coating curing. It was found that by employing curing method B, which is to install the bubble sheet between the vertical reinforcements, the most vulnerable area, which is 50mm below(④) the surface of the concrete, would be lowered to sub-zero temperature 20 hours later than when using curing method A, and that therefore it is more effective to install the bubble sheet between the vertical reinforcements for the prevention of initial frost damage.

  • PDF

Study on Initial Scattering State as a Function of Curing Temperature for Polymer Dispersed Liquid Crystal Cells with Different Mixing Ratio (고분자 분산형 액정 셀에서 혼합물의 비율에 따라 노광 온도가 초기 산란도에 미치는 영향)

  • 김미숙;서영현;이명훈;이종문;이택수;이승희
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.1
    • /
    • pp.59-64
    • /
    • 2004
  • We have fabricated the polymer dispersed liquid crystal (PDLC) cell where a control of phase separation is very important. The factors to influence the phase separation are mixing ratio of LC and polymer, curing temperature and UV intensity. In this paper, we inspected the change of a phase separation as a function of curing temperature for the mixture of E7 and. NOA65 with different ratios. When the LC concentration is less than polymer such as LC:NOA65 = 40:60wt%, the PDLC cell is influenced strongly by the curing temperature. However, when the LC concentration is much less than polymer such as LC:NOA65 = 80:20wt%, it is influenced slightly by the curing temperature. The reason is because the mixture shows upper critical solution temperature behavior and therefore it is important to know the behavior of phase separation as a function of curing temperature of the mixture.

Strength Development of High-Strength Concrete in Structure

  • Msuda, Yochihiro
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10a
    • /
    • pp.31-45
    • /
    • 2000
  • Because of the high unit cement content in the concrete mix, major concrete temperature rises are observed in the initial stages of hardening in structural members with large cross-sections made of high-strength concrete. While this temperature rise in the initial stages of hardening contributes to the initial development of the concrete strength, it also causes thermal cracking and obstructs medium to long-term increases of the concrete strength. In the study reports below, investigations were made on the effects of the concrete temperature rise in the initial stages of hardening on the medium to long-term development of the strength of structural concrete between the ages of 28 and 91 days. In the study, comparisons were made, for example, between the compressive strength of a control specimen subjected to standard curing at 28 days and the compressive strength of core specimens taken from structural members, and observations were made on the methods of evaluating the concrete strength in structure, defined here as the compressive strength of core specimens at 91 days. The results obtained indicate that, when the maximum temperature of the concrete is the structure does not exceed $60^{\circ}C$, the concrete strength in structure at the age of long-term will generally be greater than the compressive strength of the standard-curing specimens at 28 days, allowing one to evaluate the strength of the structural concrete in terms of the compressive strength of the 28-days standard-curing specimens. When, on the other hand, the maximum temperature of the concrete in the structure exceeds $60^{\circ}C$, the strength in concrete structure may be smaller than the compressive strength of the 28-days standard-curing specimens, creating risks in the evaluation of the concrete strength in structure by latter.

  • PDF

A Study on the Curing of Positive Plate and Grid to Improve the Capacity of the Lead-Acid Batteries (납축전지의 성능 향상을 위한 양극판의 숙성과 그리드에 관한 연구)

  • Ku, Bon-Keun;Jeong, Soon-Wook
    • Journal of the Korean Applied Science and Technology
    • /
    • v.25 no.1
    • /
    • pp.41-47
    • /
    • 2008
  • This study was conducted to made a grid alloy (Pb-Ca-Sn-Al) which has a temporary composition ratio in order to improve the efficiency of lead acid batteries. The positive activity material made a 3BS(tri-basic lead sulfate; $3PbO{\cdot}PbSO_4{\cdot}H_2O$) by a low temperature curing and it evaluates the plate efficiency through the life cycle testing. The initial current capacity of low temperature curing plate was excellent but the life cycle was not good (S1). As for the S2 plate, however, the initial current capacity and the life cycle were superior.

The Experimental Study on Early Strength Properties of High Volume Fly-Ash Concrete (플라이애쉬를 다량 치환한 콘크리트의 초기강도성상에 관한 실험적 연구)

  • 이동하;김상미;강태경;백민수;이영도;정상진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.281-286
    • /
    • 2002
  • To study of binder and fine aggregate a lot of replacement fly-ash concrete, initial characteristics, standard environment of curing temperature $20^{\circ}C$, hot-weather environment of curing temperature $35^{\circ}C$, . Flesh concrete tested slump. air contest and Hardening concrete valuated setting period of form, day of age 1, 3, 5. 7, 10, 28 compression strength in sealing curing. Purpose of study is consultation materials in field that variety of fly-ash replacement concrete mix proportion comparison and valuation. (1) Experiment result age 28day compression strength more higher plan concrete then standard environment in curing temperature $20^{\circ}C$, , most strength F43 is hot-weather environment in curing temperature $35^{\circ}C$, replacement binder 25%, fine aggregate 15%. (2) Hot-weather environment replacement a mount of fly-ash is a same of plan concrete setting period of form. Age 28day compression strength replacement a mount of fly-ash more hot-weather concrete then plan concrete.

  • PDF

The Study on the Strength Properties of High Volume Fly-Ash Concrete (플라이애시를 다량 사용한 콘크리트의 강도특성에 관한 연구)

  • Paik, Min-Su;Lee, Young-Do;Jung, Sang-Jin
    • Journal of the Korea Institute of Building Construction
    • /
    • v.2 no.4
    • /
    • pp.169-176
    • /
    • 2002
  • To study of binder and fine aggregate a lot of replacement fly-ash concrete, initial characteristics, standard environment of curing temperature $20^{\circ}C$, hot-weather environment, cold weather environment of curing temperature $5^{\circ}C$. Flash concrete tested slump, air contest, setting and Hardening concrete valuated setting period of form, day of age 3, 7, 28 compression strength in sealing curing. Underwater curing specimen compression strength of age 3. 7, 28day used strength change accordingly fly-ash concrete curing temperature. Purpose of study is consultation materials in field that variety of fly-ash replacement concrete mix proportion comparison and valuation. (1) Setting test result, fly-ash ratio of replacement higher delay totting time. Same volume of fly-ash ratio of replacement is lower fly-ash ratio of replacement fine aggregate delay setting time. Setting test in curing temperature $35^{\circ}C$ over twice fast setting in curing temperature $20^{\circ}C$ and all specimen setting delay in curing temperature $5^{\circ}C$. F40 specimen end of setting about 30 time. (2) Experiment result age 28day compression strength more fisher plan concrete then standard environment in curing temperature $20^{\circ}C$, cold weather environment in curing temperature $5^{\circ}C$, most strength F43 is hot-weather environment in curing temperature $35^{\circ}C$ replacement binder 25%, fine aggregate 15%. (3) Hot-weather environment replacement a mount of fly-ash is a same of plan concrete setting period of form. Age 28day compression strength replacement a mount of fly-ash more hot-weather concrete then plan concrete.

Comparison of Standard Specification for the Curing of Cold Weather between Korea and China (한국과 중국의 한중 콘크리트 표준시방서의 보온양생 규정 비교)

  • Hu, Yun-Yao;Jeong, Jun-Taek;Lim, Gun-Su;Han, Jun-Hui;Kim, Jong;Han, Min-Cheol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.11a
    • /
    • pp.131-132
    • /
    • 2023
  • In this paper, standard specification of heat curing section of cold weather concrete between Korea and China were compared. First, Korea concrete specification (KCS 14 20 40) stipulates that the application period is less than 4℃ per day or less than 0℃ per day right after pouring, but in China, the outdoor daily average temperature is less than 5℃ for five consecutive days. This is believed to be due to the difference in temperatures between Korea and China in winter. Next, in the case of Korea, KCS do not show that the concrete temperature in curing should be 5℃ or higher to prevent early frost damage and obtain the minimum required compressive strength. On the other hand, in the case of China, the specificaion does not show that the curing method is selected based on the concrete surface coefficient after considering the outdoor temperature. In addition, in Korea and China regulation, the temperature of the space during thermal curing was shown to be similar.

  • PDF

Effect of temperature on the behavior of self-compacting concretes and their durability

  • Salhi, M.;Li, A.;Ghrici, M.;Bliard, C.
    • Advances in concrete construction
    • /
    • v.7 no.4
    • /
    • pp.277-288
    • /
    • 2019
  • The formulation of self-compacting concretes (SCC) and the study of their properties at the laboratory level were currently well mastered. The aim of this work is to characterize SCC under hot climatic conditions and their effects on the properties of fresh and hardened SCC. Particularly, the effect of the initial wet curing time on the mechanical behavior such as the compressive strength and the durability of the SCCs (acid and sulfate attack) as well as the microstructure of SCCs mixtures. In this study, we used two types of cement, Portland cement and slag cement, three water/binder (W/B) ratio (0.32, 0.38 and 0.44) and five curing modes. The obtained results shows that the compressive strength is strongly influenced by the curing methods, 7-days of curing in the water and then followed by a maturing in a hot climate was the optimal duration for the development of a better compressive strength, regardless of the type of binder and the W/B ratio.