수중불분리성콘크리트의 고품질화 연구 (A Study on high Quality of Antiwashout Underwater Concrete)

  • 문한영;김성수;전중규;송용규
    • 콘크리트학회논문집
    • /
    • 제12권5호
    • /
    • pp.111-120
    • /
    • 2000
  • In case of constructing concrete structure under water, generally concrete mixed with antiwashout admixture, high range water reducer, or AE-water reducing agent etc has been manufactured to ensure the quality of antiwashout underwater concrete because of being difficulty in ascertaining construction situation by the naked eye. The properties of high quality antiwashout underwater concrete that were aimed at affluent fluidity, workability and the compressive strength of 450 kgf/$\textrm{cm}^2$ at 28 ages using two types of blended cements are following as;(1) Setting time of antiwashout underwater concretes using blended cements was more greatly delayed than that of control concrete, however, was satisfied with criteria value of "Quality standard specification of antiwashout admixture for concrete".(2) As a test results of slump flow, efflux time and box elevation of head, it was found that workability of high quality antiwashout underwater concrete was improved. (3) Heat evolution amount of OPC was 1.5 times as high as that of two types of bended cements in 72 hours. (4) Suspended solids of antiwashout underwater concrete using blended cements was more than that of control concrete, also compressive strength of high quality antiwashout underwater concrete was very low in early age, but was better than that of control concrete as to increasing ages.

수중불분리성 콘크리트의 염화물이온 침투저항성에 대한 고찰 (Diffusion of Chloride Ion in Antiwashout Underwater Concrete)

  • 김성수;김진철;김홍삼;김종필;김동현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.451-454
    • /
    • 2000
  • Recently, the antiwashout underwater concrete has been increasingly used for underwater structure such as high strength massive concrete structures. However, Concrete has poor quality ad durability due to dilution with separating cementitious material. In this study, specimens were made with antiwashout underwater concrete replaced with mineral admixtures to improve their properties and were placed in air, water, and salt water. To estimation the chloride ion permeation in concrete, ASTM C 1202 Test was performed. The experimental results demonstrate that the increase of the admixtures improved the properties of antiwashout underwater concrete.

  • PDF

고로슬래그 미분말 치환율에 따른 수중불분리성 콘크리트의 압축강도 발현에 관한 실험적 연구 (An Experimental Study on the Compressive Strength Development of antiwashout underwater Concrete with Blended Ratio of Finely Ground Granulated Blast Furnace Slag)

  • 김명식;이환우;양영인;정해동
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.57-61
    • /
    • 2000
  • This experimental study was carried out to estmate the effects of mixing dosage rate and blain on the compressive strength properties of antiwashout underwater concrete admixed with finely ground granulated blast furnace slag. The experimental parameters are slag contents(0, 20, 30, 40, 50, 60%). As a result the compressive strength have a high correlation with slag blended ratio. Thus, it is possible to calculate the modulus of modified age using compressive strength of antiwashout underwater concrete blended with slag.

  • PDF

In-Situ Application of High-Strength Antiwashout Underwater Concrete

  • 문한영;송용규
    • 콘크리트학회논문집
    • /
    • 제16권2호
    • /
    • pp.283-291
    • /
    • 2004
  • Recently, the construction of underwater structures has been gradually increased, but underwater concrete got some problems of quality deterioration and water contamination around cast-in-situ of construction. In addition, massive underwater structures such as LNG tank, underwater concrete structures of large and continuous high- strength subterranean wall under water are being demanded lower heat of hydration. In this paper, the mechanical properties of high-strength antiwashout underwater concrete (HAWC) containing with two kinds of mineral admixtures respectively were investigated. On the basis of these results, the pH value and suspended solids of HAWC manufactured in the mock-up test were 10.0$\Box$11.0 and 51 mg/${\iota}$ at 30 minutes later, respectively, initial and final setting time were about 30,37 hours, and the slump flow was 530$\pm$20Tm. In the placement at a speed of $27 m^3/hr$, there was no large difference in flowing velocity with or without reinforcing bar, and flowing slope was maintained at horizontal level. Compressive strength and elastic modulus of the cored specimen somewhat decreased as flowing distance was far; however, those of central area showed the highest value.

Fundamental Properties of Antiwashout Underwater Concrete Mixed with Mineral Admixtures

  • Han-Young, Moon;Kook-Jae, Shin;Yong-Kyu, Song
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.457-460
    • /
    • 2003
  • This paper discusses laboratory evaluations to assess the physical properties of antiwashout underwater concrete (AWC) containing pozzolanic materials such as fly ash (FA), blast furnace slag (SG) and metakaolin(MK). For the experiments, pH value, suspended solids, slump flow, efflux time and compressive strength were tested. According to the results from compressive strength test, MK10 showed the very high compressive strength characteristic during the entire curing days, but the rate of strength development was decreased as time goes by.

  • PDF

고강도 수중불분리성콘크리트의 기초물성에 대한 연구 (Fundamental Properties High-Strength Antiwashout Underwater Concrete)

  • 문한영;김성수;송용규;전중규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.195-198
    • /
    • 2000
  • Recently, the anriwashout underwater concrete has been increasingly used for underwater structures such as vary high diaphrame walls of high strength massive concrete structures. In this study, experiments were made on the fundamental properties of antiwashout underwater concrete replaced with Fly Ash from 10% to 30% to improve its properties. Resultant to the test, we got the results as follows; the value of slump flow wasi ncreased, the setting, time was very delayed, and the heat evolution amount decreased, whereas the amount of suspended solids became high, and pH value became low as to increasing the replacement ratio of Fly Ash. Also the ratios of compressive strength (in water compared to in air) at 28day were obtained over 90%, and these values were satisfied with 70% of a criterion.

  • PDF

수중불분리성 콘크리트 중의 철근부식 평가 (Estimation on Corrosion of Reinforcing bar in Antiwashout Underwater Concrete)

  • 문한영;김성수;김홍삼;김종필
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.447-450
    • /
    • 2000
  • Recently, antiwashout underwater concrete has used for underwater structure such as high strength massive concrete structures. When, concrete is placed in seawater the quality and durability of concrete could be doubt to especcially because the amount of cement placed in the concrete can be diminished by flowing seawater. In this study, antiwashout underwater concrete mixed with mineral admixtures for improvement of properties was placed in air, water, and salt water. Half-cell potential and current density was of specimens which made under different conditions measured for estimating corrosion degree. The experimental results demostrate that corrosion resistantce in saltwater was little and mineral admixtures improved properties of concrete.

  • PDF

Fundamental Properties of Antiwashout Underwater Concrete Mixed with High Reactivity Metakaloin

  • Moon, Han Young;Shin, Kook Jae;Song, Yong Kyu
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.1077-1080
    • /
    • 2003
  • High reactivity metakaolin (HRM) is a manufactured pozzolan produced by thermal processing of purified kaolinitic clay. Field performance and laboratory research of concrete containing HRM have demonstrated its value for bridge decks, bridge deck overlays, high-strength concrete and masonry products. This paper discusses laboratory evaluations to assess the physical properties of antiwashout underwater concrete (AWC) containing HRM, such as pH value, suspended solids, slump flow, and compressive strength. There were not much variations of pH value with the changing HRM contents, but suspended solid test showed that the amount of suspended solids of AWC with 10 and 20% of HRM were reduced in comparison with plain. Due to the fast hydration and reaction property of HRM, slump flow was decreased with increasing HRM contents. According to the results of compressive strength test, AWC with 10 and 20% of HRM showed higher strength characteristic than plain at all curing ages.

  • PDF

고로슬래그 미분말을 사용한 고유동 수중불분리성 콘크리트의 최적배합비 도출 (Optimum Mix Proportions of High Fluidity Antiwashout Underwater Concrete Using Ground Granulated Blast Furnace Slag)

  • 김성욱;박정준;배수호;박재임
    • 한국산학기술학회논문지
    • /
    • 제13권8호
    • /
    • pp.3704-3712
    • /
    • 2012
  • 최근, 장대교량의 해상기초 구조물에 수중불분리성 콘크리트의 사용이 증가되고 있다. 그러나, 해상기초 구조물에 사용되는 수중불분리성 콘크리트의 공사기간을 단축시키기 위해서는 이전의 수중불분리성 콘크리트보다 유동성을 크게 개선시키는 고유동 수중불분리성 콘크리트의 제조가 필요하다. 따라서 본 연구의 목적은 해상기초 구조물에 사용되는 고유동 수중불분리성 콘크리트의 최적배합비를 도출하는 것이다. 이를 위하여 단위결합재량 550, 600kg/$m^3$ 각각에 대해서 수중불분리성 혼화제 첨가량별로 고로슬래그 미분말을 혼입한 콘크리트를 제작하였다. 제작된 콘크리트의 슬럼프 플로, 응결시간, 수중분리저항성 및 압축강도 비와 같은 품질성능을 관련 규격에 따라 평가하였다. 결국, 고로슬래그 미분말을 혼입한 고유동 수중불분리성 콘크리트는 관련 규격을 만족시키는 수중불분리성 혼화제의 최소 첨가량이 필요한 것으로 나타났다.

고로슬래그 미분말을 혼합한 고강도 수중불분리성 콘크리트 (High-strength Antiwashout Underwater Concrete Containing the GGBF Slag)

  • 문한영;송용규;전중규;김태욱
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1999년도 학회창립 10주년 기념 1999년도 가을 학술발표회 논문집
    • /
    • pp.199-202
    • /
    • 1999
  • Recently, the antiwahout underwater concrete with an natiwashout admixture has been increasingly used for underwater structures. However, the credibility of antiwahout underwater concrete was brought up as problems because it was seldom applied to fields. In this study, experiments were made on the basic properties of antiwashout underwater concrete replaced with GGBF Slag from 40% to 60% to improve its properties. Resultant to the test, we got the results as follows; the difference of U-type heght was decreased, and the slump flow was increased. Whereas the amount of suspended solids became high as to increasing the replacement ratio of GGBF Slag, pH value became low. Beacause the ratio of compressive strengths (in water compared to in air) at 28days was obtained over 90%, its value is satisfied with 70% of a criterion.

  • PDF