• 제목/요약/키워드: high-manganese steel

검색결과 83건 처리시간 0.022초

변형률 속도에 따른 Fe-24.5Mn-4Cr-0.45C 합금의 인장 특성과 동적 변형시효 (Influence of Strain Rate on Tensile Properties and Dynamic Strain Aging of an Fe-24.5Mn-4Cr-0.45C Alloy)

  • 이승용;황병철
    • 한국재료학회지
    • /
    • 제26권5호
    • /
    • pp.281-286
    • /
    • 2016
  • In the present study, the tensile properties and dynamic strain aging of an Fe-24.5Mn-4Cr-0.45C alloy were investigated in terms of strain rate. During tensile testing at room temperature, all the stress-strain curves exhibited serrated plastic flows related to dynamic strain aging, regardless of the strain rate. Serration appeared right after yield stress at lower strain rates, while it was hardly observed at high strain rates. On the other hand, strain-rate sensitivity, indicating a general relationship between flow stress and strain rate at constant strain and temperature, changed from positive to negative as the strain increased. The negative strain-rate sensitivity can be explained by the Portevin Le Chatelier effect, which is associated with dynamic strain aging and is dependent on the strain rate because it is very likely that the dynamic strain aging phenomenon in high-manganese steels is involved in the interaction between moving dislocations and point-defect complexes.

Fe-Cr-Ni-Mn 2 상 스테인레스강의 인장성질에 미치는 변형온도 및 Mn 함량변화의 영향 (Effect of Deformation Temperature and Manganese Contents on the Tensile Properties of Fe-Cr-Ni-Mn Duplex Stainless Steel)

  • 강창룡;성장현
    • 열처리공학회지
    • /
    • 제4권4호
    • /
    • pp.44-52
    • /
    • 1991
  • The effect of deformation temperature and manganes contents on the tensile properties of duplex stainless steels with the structure of both ferrite and austenite were investigate. For this investigation, Fe-19% Cr-5% Ni-4~8% Mn alloys were prepared. The result obtained from this experiment are summerized as follows. With decreasing deformation temperature, tensile strengths of duplex stainless steel increased. Elongation showd to be increased and then decreased after representing the highest value at specific temperature. Tensile properties of duplex stainless steel were controlled by TRIP behavior in this experimental range of austenite contents. Tensile strengths decreased with increasing Mn contents. With increasing Mn contents, elongation decreased in the high temperature region, but increased in the low temperature region. The peak temperature representing the maximum elongation were changed to low temperature and the width of peak appeared to be broaden with increasing Mn contents.

  • PDF

고 Mn계 TWIP 강의 미세조직과 기계적 성질 (Microstructure and Mechanical Properties of High Mn TWIP Steels)

  • 정종구;이오연;박영구;김동은;진광근;김성규;송기홍
    • 대한금속재료학회지
    • /
    • 제46권10호
    • /
    • pp.627-633
    • /
    • 2008
  • The austenitic Fe-Mn alloys have received considerable attention as a possible candidate for the automotive structural materials due to their high strength and high formability with high elongation. This research investigates the effect of alloying elements on the phase transformation, deformation behavior and mechanical properties in high Mn steels for the development of a high strength high ductility steel. The mechanical stability of austenitic phases is very important for high ductility and it depends largely on the composition of carbon, manganese and aluminum. The dominant deformation mode shifts from TRIP to TWIP mode as the amount of C, Mn and Al is increased. Especially, even a small amount of Al addition facilitates significantly TWIP deformation due to the increase of stacking fault energy in Fe-Mn alloys, this leads to increase the ductility and also decrease the crack sensitivity.

Al 첨가 TWIP강에서의 지연파괴에 대한 변형유기 마르텐사이트 변태의 영향 (Effects of the Strain Induced Martensite Transformation on the Delayed Fracture for Al-added TWIP Steel)

  • 김영우;강남현;박영도;최일동;김교성;김성규;조경목
    • 대한금속재료학회지
    • /
    • 제46권12호
    • /
    • pp.780-787
    • /
    • 2008
  • For the advanced high strength steels (AHSS), high-manganese TWIP (twinning induced plasticity) steels exhibit high tensile strength (800-1000 MPa) and high elongation (50-60%). However, the TWIP steels need to be understood of delayed fracture following the cup drawing test. Among the factors to cause delayed fracture, i.e, martensite transformation, hydrogen embrittlement and residual stress, the effects of martensite transformation (${\gamma}{\rightarrow}{\varepsilon}$ or ${\gamma}{\rightarrow}{\alpha}^{\prime}$) were investigated on the delayed fracture phenomenon. Microstructural phase analysis was conducted for cold rolled (20, 60, 80% reduction ratio) steels and tensile deformed (20, 40, 60% strain) steels. For the Al-added TWIP steels, no martensite phase was found in the cold rolled and tensile deformed specimen. But, the TWIP steels with no Al addition indicated the martensite transformation. The cup drawing specimens showed the martensite transformation irrespective of the Al-addition to the TWIP steel. However, the TWIP steel with no Al exhibited the larger amount of martensite than the case of the TWIP steel with Al addition. For the reason, it was possible to conclude that the Al addition suppressed the martensite transformation in TWIP steels, therefore preventing the delayed fracture effectively. However, it was interesting to note that the mechanism of delayed fracture should be incorporated with hydrogen embrittlement and/or residual stress as well as the martensite transformation.

A Brief Review of κ-Carbide in Fe-Mn-Al-C Model Alloys

  • Seol, Jae Bok
    • Applied Microscopy
    • /
    • 제48권4호
    • /
    • pp.117-121
    • /
    • 2018
  • The multiple length scale analysis of previously designed Fe-Mn-Al-C based low-density model alloys reveals the difference in ordered ${\kappa}-carbide$, $(Fe,Mn)_3AlC_x$, between Fe-25Mn-16Al-5.2C (at%) alloy and Fe-3Mn-10Al-1.2C (at%) alloy. For the former alloy composition consisting of fully austenite grains, ${\kappa}-carbide$ showed majorly cuboidal and minorly pancake morphology and its chemical composition was not changed through aging for 24 h and 168 h at $600^{\circ}C$. Meanwhile, for the isothermally annealed ferritic alloy system for 1 hr at 500 and $600^{\circ}C$, the dramatic change in the chemical composition of needle-shape ${\kappa}-carbide$, $(Fe,Mn)_3(Fe,Al)C_x$, was found. Here we address that the compositional fluctuations in the vicinity of the carbides are significantly controlled by abutting phase, either austenite or ferrite. Namely, the cooperative ordering of carbon and Al is an important factor contributing to carbide formation in the high-Mn and high-Al alloyed austenitic steel, while the carbon and Mn for the low-Mn and high Al alloyed ferritic steel.

용접흄 충 금속함량 변화에 관한 연구 (A Study on the Content Variation of Metals in Welding Fumes)

  • 윤충식;박동욱;박두용
    • 한국환경보건학회지
    • /
    • 제28권2호
    • /
    • pp.117-129
    • /
    • 2002
  • Concentration of welding fumes and their components is known to be hazardous to welder and adjacent worker. To determine the generation rates of metals in fumes, $CO_2$ flux cored arc welding on stainless steel was performed in well designed fume collection chamber. Variables were different products of flux cored wire(2 domestic products and 4 foreign products) and input energy(low-, optimal- , high input energy). Mass of welding fumes was determined by gravimetric method(NIOSH 0500 method), and 17 metals were analysed by inductively coupled plasm-atomic emission spectroscopy(NIOSH 7300 method). Flux cored wire tube and flux were analysed by scanning electron microscopy to determine their metal composition. 17 metals were classified by their generation rates. Generation rates of iron, manganese, potassium and sodium were all above 50mg/min at optimal input energy level. Generation rates of chromium and amorphous silica were 25~50mg/min. At 1~25mg/min level, nickel, titanium, molybdenum, and aluminum were included. Copper, zinc, calcium, lead, magnesium, lithium, and cobalt were generated below 1 mg/min. Generation rates of metal components in fumes were influenced by input energy, types of flux cored wire. Flux cored wire was consisted of outer shell tube and inner flux. Iron, chromium, and nickel were the major components of outer tube. Flux contained iron, chromium, nickel, potassium, sodium, silica, and manganese. The use of flux cored wire can increase the hazards by increasing the amounts of fumes formed relative to that of solid wire. The reason might be the direct transfer of elements from the flux, since the flux is fine power. Ratio of metals to the fume of flux cored wire was lower than that of solid wire because non-metal components of flux were transferred. Total metal content of fumes in flux cored arc welding was 47.4(24.3~57.2) percent that is much lower than that of solid wire, 75.9 percent. We found that generation rates of iron, manganese, chromium and nickel, all well known to cause work related disease to welder, increased more rapidly with increasing input energy than those of fumes. To reduce worker exposure to fumes and hazardous component at source, further research is needed to develop new welding filler materials that decrease both the amount of fumes and hazardous components.

오스테나이트계 고질소 스테인레스 강의 열간 및 냉간 압연특성 (Hot and Cold Rolling Characteristic with High-Nitrogen Steel of Austenitic Stainless (HNS))

  • 이명열;이종욱;김동수;김병구;김동권;김영득;차도진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 추계학술대회 논문집
    • /
    • pp.99-101
    • /
    • 2008
  • At 21st century, material development concepts were changed to fulfill the environmental friendly demands. This study is to study the effect of pressurized nitrogen gas and manganese in high nitrogen austenitic stainless steel(HNS) in which N and Mn elements substitute the nickel element. 100kg HNS ingots were made by Pressurized Vacuum Induction Melting(P-VIM) and were forged according to free forging process. As forged HNS were hot and cold rolled by pilot scale rolling machine. Depending on the rolling condition, the mechanical properties of HNS were changed. The roll thrust and sheet folding showed asymmetry condition between work and drive side during cold and hot rolling. The purpose of this study are to improve workability the hot and cold rolling machine and to set the conditions for establishing the rolling process.

  • PDF

대구경-후판 압력용기용 저 합금강(Mn-Mo)의 용접특성 (A Welding Characteristics of Large Caliber-Thick Plate Pressure Vessel Low Alloy Steel (Mn-Mo))

  • 안종석;박진근;윤재연
    • Journal of Welding and Joining
    • /
    • 제30권6호
    • /
    • pp.10-14
    • /
    • 2012
  • Recently the low alloy steel plate made with manganese-molybdenum is used widely in steam drum and separator of the new coal-fired power plant boiler. This material is suitable for the vapor storage of high pressure and high temperature. The high temperature creep strength of Mn-Mo alloy is higher than the carbon plate(SA516) that used in the subcritical pressure boiler. It reduces the thickness of the pressure vessel and makes the lightweight possible. Recently in the power plant boiler operation and production process, the damage has happened frequently in the heat affected zone and base material according to the hydrogen crack and delayed crack. This paper describes the research result about the damage case experienced in the boiler steam drum production process and present the optimum manufacture method for the similar damage prevention of recurrence.

Manganese Distribution in Brains of Sprague Dawley Rats after 60 Days of Stainless Steel Welding-Fume Exposure

  • Yu, Il-Je;Park, Jung-Duck;Park, Eon-Sub;Song, Kyung-Seuk;Han, Kuy-Tae;Han, Jeong-Hee;Chung, Yong-Hyun;Park, Byung-Sun;Chung, Kyu-Hyuck
    • 한국독성학회:학술대회논문집
    • /
    • 한국독성학회 2003년도 추계학술대회
    • /
    • pp.68-83
    • /
    • 2003
  • Welders working in a confined space, like in the shipbuilding industry, are at risk of being exposed to high concentrations of welding fumes and developing pneumoconiosis or other welding-fume exposure related diseases. Among such diseases, manganism resulting from welding-fume exposure remains a controversial issue, as the movement of manganese into specific brain regions has not been clearly established.(omitted)

  • PDF

Manganese Distribution in Brains of Sprague Dawley Rats after 60 Days of Stainless Steel Welding-Fume Exposure

  • Yu, Il-Je;Park, Jung-Duck;Park, Eon-Sub;Song, Kyung-Seuk;Han, Kuy-Tae;Han, Jeong-Hee;Chung, Yong-Hyun;Park, Byung-Sun;Chung, Kyu-Hyuck
    • 대한약학회:학술대회논문집
    • /
    • 대한약학회 2003년도 Proceedings of the Convention of the Pharmaceutical Society of Korea Vol.2-1
    • /
    • pp.72-72
    • /
    • 2003
  • Welders working in a the confined space, like in the shipbuilding industry, are have at risk of being exposed toing a high concentrations of welding fumes and of developing pneumoconiosis or other welding- fume exposure related diseases. Among such diseasesthem, manganism resulting fromcaused by welding- fume exposure remains ais still controversial issue, as the movement ofnd no clear demonstration of manganese movement into the specific brain regions has not been clearly established. (omitted)

  • PDF