• Title/Summary/Keyword: high early strength concrete

Search Result 461, Processing Time 0.026 seconds

Surface Curing Method of Hot weather Concreting with the Combination of Surface Curing sheets (표면 양생시트 조합에 의한 서중콘크리트용 표면 양생공법)

  • Lee, Ju-Suck;Kim, Jong-Back;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.785-788
    • /
    • 2006
  • This paper investigates the temperature history of slab mock-up specimens with various surface curing sheets, in order to determine a favorable surface curing method in hot weather condition. Test showed that insulating double bubble sheets+aluminum foil simultaneously on the upper section of a specimen prevented an increase of sudden temperature and a decrease of vaporization when placed during the hot weather condition. It also secured the high strength in early age. Therefore it is found that using the double bubble sheets+aluminum foil on concrete surface declined the plastic and drying shrinkage and inclined the early strength, thus improving the concrete quality.

  • PDF

Development and Application of Concrete using Ground Granulated Blast Slag in Winter Season (동절기 슬래그 혼입 콘크리트의 실용화기술개발)

  • Yoo, Jo-Hyeong;Kim, Woo-Jae;Hong, Seok-Beom
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.05a
    • /
    • pp.256-257
    • /
    • 2014
  • Concrete made with ground granulated blast-furnace slag(GGBS) has many advantage, including improved durability, workability and economic benefits. GGBS concrete is that its strength development is considerably slower under standard 20℃ curing conditions than that of portland cement concrete, although the ultimate strength is higher for same water-binder ratio. GGBS is not therefore used in application where high early age strength is required. However, hydration of GGBS is much more sensitive to temperatures, the strength development of GGBS concrete is significantly enhanced.

  • PDF

Development of High Performance Shotcrete for Permanent Shotcrete Tunnel Linings (III) (Field Test of Wet-mixed Shotcrete with Powder Types Cement Mineral Accelerator) (Permanent Shotcrete Tunnel Linings 구축을 위한 고성능 숏크리트 개발(III)(시멘트 광물계 분말형 급결제를 사용한 습식숏크리트 현장시험시공))

  • 박해균;이명섭;김재권;김용하
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.609-617
    • /
    • 2003
  • The use of Shotcrete(Sprayed concrete) for the support of underground excavations was pioneered by the Civil engineering industry. Permanent shotcrete tunnel linings such as Single-shell, NMT(Norwegian Method of Tunnelling) have been constructed in many countries for reducing construction time and lowering construction costs instead of conventional in-situ concrete linings. Among essential technologies for successful application of Permanent Shotcrete Linings, high performance shotcrete having high strength, high durability, better pumpability has to be developed in advance. This paper presents the ideas and the first field test results of wet-mixed Steel Fiber Reinforced Shotcrete(SFRS) with powder types cement mineral accelerator. From the results, wet-mix SFRS with powdered accelerator exhibited good early strength improvement and less rebound ratio compared to the ordinary accelerator.

  • PDF

Effect of Powder Hardening Accelerator on the Physical Properties of Precast Concrete (분말형 경화촉진제를 혼입한 PC부재용 콘크리트의 기초특성에 관한 실험적 연구)

  • Jun, Woo-Chul;Seo, Hwi-Wan;Bae, Yeoun-Ki;Park, Hee-Gon;Min, Tae-Beom;Kwon, Yeong-Ho
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.3
    • /
    • pp.265-271
    • /
    • 2015
  • This study is intended to produce a PC (Precast Concrete) member without a steam curing process in developing the high early strength concrete satisfying the condition of 10MPa in compressive strength at the age of 6 hours, and is intended to ensure economic feasibility by increasing the turnover rate of concrete form. Hence, high early strength cement with high $C_3S$ content and the hardening accelerator of powder type accelerating the hydration of $C_3S$ was used. And the properties of concrete were evaluated according to the hardening accelerator mixing ratio (0, 1.2, 1.6, 2.0). No big difference was found from the tests of both slump and air content. When 1.6 % or higher amounts of the hardening accelerator were mixed, the compressive strength of 10MPa was achieved at the age of 6 hours. From the test results of autogenous (drying) shrinkage and plastic shrinkage, it can be seen that there was a difference according to hydration reaction rate due to the addition of the hardening accelerator. However, it was shown that no problem arose with crack and durability. And it was shown that resistance to freezing-thawing, carbonation, and penetration were excellent.

Basic Creep Model by Considering Autogenous Shrinkage

  • Lee, Yun;Kim, Jin-Keun;Kim, Min-Su
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.1071-1076
    • /
    • 2003
  • Basic creep of concrete during very early ages is an important factor on the behavior of young concrete and a great deal of research has been executed. However, in recent studies, it was revealed that the basic creep measured by sealed concrete was inaccurate, especially for high strength concrete because of autogenous shrinkage at early age. This paper presents the results from experimental study that investigate to explore the effect of autogenous shrinkage in basic creep. More specifically, four different mix proportions were casted and the primary variables were water-cement ratios. Through this research, it was found that the differences between apparent specific creep and real specific creep were remarkable in low water-cement ratio at early age. Therefore, it is recommended to modify existing creep model by considering autogenous shrinkage

  • PDF

Compressive and Flexural Strength Development Characteristics of Polymer Concrete (폴리머 콘크리트의 압축 및 휨강도 발현 특성)

  • Jin, Nan Ji;Yeon, Kyu-Seok
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.60 no.1
    • /
    • pp.101-110
    • /
    • 2018
  • This study experimentally investigated the compressive and flexyral strength development characteristics of polymer concrete using four different type polymeric resins such as unsaturated polyester, vinyl ester, epoxy, and PMMA (polymethyl methacrylate) as binders. The test results show that the average compressive strength of those four different polymer concretes was 88.70 MPa, the average flexural strength was 20.30 MPa. Those test results show that compressive and flexural strengths of polymer concrete were much stronger than compressive and flexural strengths of ordinary Portland cement concrete. In addition, the relative gains of the compressive strength development at the age of 24 hrs compared to the age of 168 hrs were 68.6~88.3 %. Also, the relative gains of the flexural strength development at the age of 24 hrs compared to the age of 168 hrs were 73.8~93.4 %. These test results show that compressive and flexural strengths of each polymer concrete tested in this study were developed at the early age. Moreover, the prediction equations of compressive and flexural strength developments regarding the age were determined. The determined prediction equations could be applied to forecast the compressive and flexural strength developments of polymer concrete investigated in this study because those prediction equations have the high coefficients of correlation. Last, the relations between the compressive strength and the flexural strength of polymer concrete were determined and the flexural/compressive strength ratios were from 1/4 to 1/5. These results show that polymer concretes investigated in this study were appropriate as a flexural member of a concrete structure because the flexural/compressive strength ratios of polymer concrete were much higher than the flexural/compressive strength ratios of Portland cement concrete.

Strength and durability of concrete in hot spring environments

  • Chen, How-Ji;Yang, Tsung-Yueh;Tang, Chao-Wei
    • Computers and Concrete
    • /
    • v.6 no.4
    • /
    • pp.269-280
    • /
    • 2009
  • In this paper an experimental study of the influence of hot springs curing upon concrete properties was carried out. The primary variables of the investigation include water-to-binder ratio (W/B), pozzolanic material content and curing condition. Three types of hot springs, in the range $40-90^{\circ}C$, derived from different regions in Taiwan were adopted for laboratory testing of concrete curing. In addition, to compare with the laboratory results, compressive strength and durability of practical concrete were conducted in a tunnel construction site. The experimental results indicate that when concrete comprising pozzolanic materials was cured by a hot spring with high temperature, its compressive strength increased rapidly in the early ages due to high temperature and chloride ions. In the later ages, the trend of strength development decreased obviously and the strength was even lower than that of the standard cured one. The results of durability test show that concrete containing 30-40% Portland cement replacement by pozzolanic materials and with W/B lower than 0.5 was cured in a hot spring environment, then it had sufficient durability to prevent steel corrosion. Similar to the laboratory results, the cast-inplace concrete in a hot spring had a compressive strength growing rapidly at the earlier age and slowly at the later age. The results of electric resistance and permeability tests also show that concrete in a hot spring had higher durability than those cured in air. In addition, there was no neutralization reaction being observed after the 360-day neutralization test. This study demonstrates that the concrete with enough compressive strength and durability is suitable for the cast-in-place structure being used in hot spring areas.

A Study on Characteristic of Autogenous Shrinkage of High Strength Concrete (고강도 콘크리트의 자기수축 특성에 관한 연구)

  • Lee, Young-Jae
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.16 no.1
    • /
    • pp.1-8
    • /
    • 2013
  • In case that W/B is 20%, 30%, 40% respectively, the effects of additive and shrinkage reducing agent on the autogenous shrinkage for high strengthen concrete through the substitution of FA and SF analysis were obtained as following conclusions. When the ratio of FA increased, the compressive strength of high strengthen concrete is decreased in the early times. As the ratio of SF increase, the compressive strength also increased. Comparing with PC(Portland Cement) for 7 days curing, the strength is 13.8% of FA10 + SR0.5 and 19.2% of FA15 + SR0.5 decreased when W/B is 20%, and 6.1% of SF7.5 + SR0.5, 4.8% of SF15 + SR0.5, the strength are increased. In case that W/B is 30%, 13.1% of FA10 + SR0.5 19.1% of FA15 + SR0.5 the strength is decreased and 4.1% of SF 7.5 + SR0.5, 7.2% of SF15 + SR0.5 the strength are increased. In case of W/B 40%, 4.3% of FA10 + SR0.5, and 8.7% of FA15 + SR0.5, the strength is decreased and 3.3% of SF7.5 + SR0.5, 6.3% SF15 + SR0.5 the strength is increased. When the ratio of SR is 0.5%, autogenous shrinkage strain of OPC concrete appeared $-417{\times}10-6$ in 56days curing, the shrinkage strain is decreased 23.7%. The reducing effects of autogenous shrinkage when the mineral and shrinkage agent are used are the same as ones when only shrinkage agent used.

An Experimental Research on the Material Properties of Super Flowing Concrete (초유동 콘크리트의 재료특성에 관한 실험적 연구)

  • 김진근;한상훈;박연동;노재호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.10a
    • /
    • pp.56-62
    • /
    • 1995
  • In this study, the properties of super flowing cocrete containing gly ash were experimentally investigated and compared with those of ordinary concrete. Tests were carried out on five types of super flowing concrete mixes containing fly ash and three types of ordinary concrete mixes without fly ash. Flow test, O-funnel test, box test, Ltype thest and slump test were carried out to obtain the properties for the workability of fresh concrete. Compressime strength, splitting tensile strength, modulus of elasticity. creep and shrinkage test were also obtained as the mechanical properties of hardened concrete. In fresh concrete, it was found that super flowing concrete had excellent workability and flowability compared with ordinary concrete, and the volume ratio of coarse aggregate to concrete volume greatly influenced flowability. Super flowing concrete also had good mechanical properties at both early and late ages with compressive strengths reaching as high as 40 MPa at 28 days. The creep deformation of super flowing concrete investigated were relatively lower than that of ordinary concrete.

  • PDF

Expansion Model of Cement Paste using Expansive Additive (팽창재를 혼입한 시멘트 경화체의 팽창모델)

  • Park, Sun-Gyu;Takahumi, Noguchi;Kim, Moo-Han
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.11a
    • /
    • pp.789-792
    • /
    • 2005
  • Development of high-strength concrete and improved durability has brought new opportunities to the construction industry. However, some attention was given to characteristics of such concrete, in particular with respect to their cracking sensitivity. It has been argued and demonstrated experimentally that a low water/cement ratio concrete undergoes shrinkage due to self-desiccation. This so-called autogenous shrinkage cracking is a major concern for concrete durability. One possible method to reduce cracking due to autogenous shrinkage is the addition of expansive additive. Tests conducted by many researches have shown the beneficial effects of addition of expansive for reducing the risk of shrinkage-introduced cracking. This paper aimed at forecasting deformation of high strength cement paste with expansive additive for early age.

  • PDF