• 제목/요약/키워드: heat resistance molding condition

검색결과 6건 처리시간 0.017초

자동차 플라스틱 부품의 내열변형 예측에 관한 연구 (A study on the warpage and post-deformation in heat resistance test of automotive plastic components)

  • Kim, H.Y.;Kim, J.J.;Kim, J.S.
    • 한국정밀공학회지
    • /
    • 제13권5호
    • /
    • pp.44-52
    • /
    • 1996
  • A procedure predicting warpage and post-deformation due to heat resistance test is presented. The procedure is applied to the injection molding processes of automotive plastic components, which are the door trim and the instrument pannel. The warpage of products is obtained from the residual stress after filling, packing and cooling process, and the post deformation due to the heat resistance test is calculated in the structural analysis of the product at the ejection temperature with the initial condition of residual stress, the boundary conditions and heat resistance conditions. The analyses give some useful guide lines in the design of automotive plastic parts which should satisfy heat resistance regulation.

  • PDF

Examination of heat resistant tensile properties and molding conditions of green composites composed of kenaf fibers and PLA resin

  • Ben, Goichi;Kihara, Yuichi;Nakamori, Keita;Aoki, Yoshio
    • Advanced Composite Materials
    • /
    • 제16권4호
    • /
    • pp.361-376
    • /
    • 2007
  • Disposing of conventional fiber-reinforced polymers (FRPs) poses an environmentally challenging problem. Disposal of FRPs by combustion discharges carbon dioxide in the air because the resin of FRPs is made of fossil fuel. When they are disposed of in the ground, FRPs remain semipermanently without decomposing. In response to these problems, green composites are now being developed and are extensively studied as a material that produces a lower environmental burden. In this paper, green composites using kenaf fiber yarn bundles and PLA (poly(lactic acid)) are fabricated and their tensile properties are evaluated in the experiment. The tensile Young's modulus of all of the laminations is larger than that of PLA alone and the tensile strength of some laminations is larger than that of PLA alone. In particular, the value of UD composite of $0^{\circ$ shows double the tensile strength of PLA alone. Furthermore, the molding conditions for fabricating with a hot press are investigated and the heat resistant tensile properties of green composites are also reported.

PET 병용 프리폼 사출성형에서 잔류응력과 수축 최소화를 위한 성형조건의 연구 (Investigation of the Molding Conditions to Minimize Residual Stress and Shrinkage in Injection Molded Preform of PET Bottle)

  • 조성환;홍진수;류민영
    • 폴리머
    • /
    • 제35권5호
    • /
    • pp.467-471
    • /
    • 2011
  • PET병은 프리폼(preform)을 사출성형한 후 이를 블로우 성형기에 이송시켜 블로잉하여 성형된다. 내열을 요구하는 병 즉, 주스나 곡류음료용 PET병은 목 부분(neck 또는 thread 부분)에 내열성을 부여하기 위해 프리폼 성형 후 블로잉하기 전에 목 부분을 결정화시킨다. 그러나 사출성형품에 존재하는 잔류응력이 결정화를 방해하기 때문에 프리폼 목 부분의 충분한 결정화를 위해 사출 후 프리폼을 열처리(annealing)한다. 이 열처리는 잔류응력을 해소시키기 위해서 수행하는데 사출 시 성형조건의 최적화를 통하여 잔류응력을 최소화한다면 열처리 시간을 단축시킬 수 있다. 본 논문에서는 사출 시 프리폼에 형성되는 잔류응력을 최소화하고 치수정밀도를 유지하기 위한 연구로 CAE 해석을 통하여 최적 사출조건을 제시하였다. 성형조건별 잔류응력 및 수축률의 변화를 관찰하고 이를 최소화시키는 성형조건을 찾기 위해 실험계획법을 적용하였다. 사출온도, 보압크기, 그리고 사출시간을 인자로 하여 최적의 성형조건을 결정하였다. 잔류응력에 영향을 주는 인자는 사출온도와 사출시간 순으로 나타났고 수축률에 영향을 주는 인자는 사출온도로 나타났다. 본 연구에서 결정한 최적 조건에서 최대 잔류응력, 잔류응력의 분포, 그리고 수축률이 기존 조건에 비해 각각 22%, 40%, 그리고 25% 감소하였다.

순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(IV) - 겹치기 용접 및 실물 열교환기로의 적용 - (A Study of Weldability for Pure Titanium by Nd:YAG Laser(IV) - Lap Welding and Application for Heat Exchanger -)

  • 김종도;곽명섭;이창제;길병래
    • Journal of Welding and Joining
    • /
    • 제28권1호
    • /
    • pp.66-71
    • /
    • 2010
  • With large specific strength and outstanding corrosion resistance and erosion resistance in sea water, titanium and titanium alloy are widely used in heat exchanger production. In particular, pure titanium demonstrates outstanding molding performance and may be considered optimal for production of heat exchanger. Since titanium is very vulnerable to oxidation and embrittlement during welding, processes with less heat input are widely used, and laser welding is widely applied by considering production performance and shield etc in atmosphere. So far, 1st report and 2nd report compared and analyzed embrittlement degrees by bead colors of weldment through oxygen and nitrogen quantitative analysis and hardness measurement, and evaluated welding performance and mechanical properties of butt welding. This study evaluated field applicability of lap welding to heat exchange plate of LPG re-liquefaction device for ships through tensile stress test, hardness test and internal pressure test etc after deducing optimal weding condition and applying to actual heat exchange plate. In bead overlap area, the experiment produced sound welds with no porosity or defect by increasing and decreasing laser power, and tensile-shear test results indicated virtually the same tension and yield strength as base metal. As a result of measuring hardness at lateral cross section and bead overlap zone of actual heat exchanger welds, hardness difference within 20Hv was produced at base metal, HAZ and weldment, and as a result of pneumatic and hydraulic pressure test, no leakage occurred.

금형재료용 주철의 다이오드 레이저 표면경화처리에 관한 연구(III) - 경화부의 미세조직 특성 - (A Study on the Diode Laser Surface Hardening Treatment of Cast Iron for Die Material(III) - Characteristics of Microstructures in Hardened Zone -)

  • 김종도;송무근;황현태
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제36권1호
    • /
    • pp.78-84
    • /
    • 2012
  • 금형의 공정 과정에서 금형과 성형품 사이에서 발생하는 마찰로 인해 발생하는 금형의 마모가공차로 작용하여 성형 품질을 저하시킬 수 있다. 따라서 금형의 내마모성을 향상시키기 위해 질화나 침탄처리, 화염 및 고주파 표면처리 등의 방법들이 적용되어 왔다. 하지만 형상의 제한이나 제품의 변형 등과 같은 문제점을 수반하고 있기 때문에, 이러한 문제점을 해결할 수 있는 표면처리 방법으로써 레이저 표면처리 기술이 검토되고 있다. 따라서 본 연구에서는 고출력 다이오드 레이저를 이용, 금형재료용 주철의 표면처리를 시도하였다. 앞서 제1보와 제2보의 논문에서는 금형의 재료 및 형상의 차이에 따른 열처리 특성을 비교하였다면, 본 논문에서는 열처리 후 생성되는 경화부, 경계부위 및 모재의 조직적 차이를 분석하기 위해 광학 현미경 및 전자 현미경을 이용하여 미세조직을 관찰하고, EDS를 통해 조직의 상태를 파악하였다. 미세조직 관찰 결과, 경화부는 침상의 마르텐사이트 조직이 형성되어 있었다.

전기저항 평가법 및 접촉각을 이용한 CF/PP 복합재료 사출성형품 섬유 배열성 평가 (Evaluation of Fiber Arrangement Condition of CF/PP Composites Using Electrical Resistance Measurement and Wettability)

  • 권동준;신평수;김종현;박종만
    • 접착 및 계면
    • /
    • 제17권1호
    • /
    • pp.15-20
    • /
    • 2016
  • 열가소성 섬유강화 복합재료를 위해 사출성형법이 사용되며, 사출품 내부의 섬유 배열이 열가소성 복합재료의 기계적 물성에 영향을 미친다. 본 연구에서는 탄소섬유/폴리프로필렌(CF/PP, carbon fiber/polypropylene) 복합재료를 사출성형할 때, 금형에 구리선을 붙여 사출품의 상태에 따라 확인되는 전기저항 변화도를 감지하여 사출품 내부의 섬유 배열 상태를 분석하였다. 사출될 때 발생되는 전기저항 변화도를 3가지의 종류로 구분할 수 있었다. 사출될 때 발생되는 금형의 전기저항 변화도 크기가 클수록 인장강도가 높은 CF/PP 성형품을 제조할 수 있었다. 이러한 이유는 CF/PP 성형품 내부의 섬유 배열에 의한 영향임을 접촉각 평가 및 시편의 표면 분석, 인장시편의 파단면 관찰 결과로 확인하였다. 균일한 섬유 배열을 가질 경우 사출 용융액 내부의 섬유가 열을 고르게 가지고 있으며, 금형에 일정한 열을 사출기간 동안 전달하게 되어 금형의 전기저항 변화도가 증가됨을 감지할 수 있었다. 궁극적으로 전기저항 평가방법을 이용하여 CF/PP 복합재료 성형품의 상태를 예측할 수 있었다.