Room Temperature Strength and Crack Healing Morphology of Si3N4 Composite Ceramics with SiO2 Colloidal (SiO2 콜로이달에 의한 Si3N4 복합 세라믹스의 상온굽힘강도 및 균열치유 현상)

  • Nam, K.W.;Kim, J.S.;Lee, H.B.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.7
    • /
    • pp.652-657
    • /
    • 2009
  • Strength characteristics of $Si_3N_4$ composite ceramics has been studied as functions of heat-treatment temperature and additive $SiO_2$. $SiO_2$ colloidal could significantly increase the bending strength. Crack healing temperature decreased 300 K by additive $TiO_2$. Bending strength of specimen added $SiO_2$ is higher than that of non-added $SiO_2$. Moreover, bending strength of specimen with $SiO_2$ colloidal coating is much higher that of non-coated specimen. In in-situ observation, crack-healed specimen at 1,573 K shows phenomenon like a fog on the surface. By SPM, both crack-healed specimen, non-coating and coating of $SiO_2$ colloidal, at 1,273 K were healed completely but both of 1,573 K exist crack. This was made by evaporation of $SiO_2$ at high temperature. Crack-healing materials of $Si_3N_4$ composite ceramics is crystallized $Y_2Si_2O_7$, $Y_2Ti_2O_7$ and $SiO_2$. A large amount of Si and O, and little C were detected by EPMA. Si and O increase but C decreases according to heat treatment temperature. Specimens with additive $SiO_2$ were more detected Si and O than that of non-additive $SiO_2$. Specimen with $SiO_2$ colloidal coatings were much more detected O.

Effects of Healing Agent on Crack Propagation Behavior in Thermal Barrier Coatings

  • Jeon, Soo-Hyeok;Jung, Sung-Hoon;Jung, Yeon-Gil
    • Journal of the Korean Ceramic Society
    • /
    • v.54 no.6
    • /
    • pp.492-498
    • /
    • 2017
  • A thermal barrier coating (TBC) with self-healing property for cracks was proposed to improve reliability during gas turbine operation, including structural design. Effect of healing agent on crack propagation behavior in TBCs with and without buffer layer was investigated through furnace cyclic test (FCT). Molybdenum disilicide ($MoSi_2$) was used as the healing agent; it was encapsulated using a mixture of tetraethyl orthosilicate and sodium methoxide. Buffer layers with composition ratios of 90 : 10 and 80 : 20 wt%, using yttria stabilized zirconia and $MoSi_2$, respectively, were prepared by air plasma spray process. After generating artificial cracks in TBC samples by using Vickers indentation, FCTs were conducted at $1100^{\circ}C$ for a dwell time of 40 min., followed by natural air cooling for 20 min. at room temperature. The cracks were healed in the buffer layer with the healing agent of $MoSi_2$, and it was found that the thermal reliability of TBC can be enhanced by introducing the buffer layer with healing agent in the top coat.

Evaluation of Healing Properties of Asphalt Mixtures (아스팔트 혼합물의 손상회복 특성 평가)

  • Kim, Boo-Il
    • International Journal of Highway Engineering
    • /
    • v.7 no.2 s.24
    • /
    • pp.69-76
    • /
    • 2005
  • While the repeated traffic loading accumulates the damage of asphalt pavement, the damage has being healed during rest periods. And then, this healing enhances the fatigue life of asphalt pavement. A method was developed to determine the healing rate of asphalt mixture in terms of recovered dissipated creep strain energy (DCSE) per unit time, and the healing properties of four different asphalt mixtures were evaluated. The test procedure consists of repeated loading test and periodical resilient modulus tests. A normalized healing rate in terms of $DCSE/DCSE_{applied}$ was defined to evaluate the healing properties independently of the amount of damage incurred in the mixture. From the test results, it was concluded that the healing rates of asphalt mixtures were increased exponentially as the temperature was increased and more affected by the structural characteristics of mixture such as asphalt content than the binder characteristics such as the polymer modification.

  • PDF

Analysis of Electroencephalogram and Electrocardiogram Changes in Adults in National Healing Forests Environment

  • Hong, Jae-Yoon;Lee, Jeong-Hee
    • Journal of People, Plants, and Environment
    • /
    • v.21 no.6
    • /
    • pp.575-589
    • /
    • 2018
  • This study analyzed the changes in Electroencephalogram(EEG) and Electrocardiogram(ECG) depending on the healing environment in order to find a way to improve the forest healing program based on the healing environment in response to the demand for qualitative improvement of the program since the program is a charged service. This study selected eight sites running forest healing programs at four national healing forests (i.e., Saneum, Cheongtaesan, Daegwanryeng, and Jangseong) - two routes per national healing forest - considering forest environments. This study chose NUMBER standard sampling plots ($20{\times}20m$) and measured three atmospheric environment items, seven physical environment items, two soil environment items, and eight vegetation environment items including forest sound and anion at each plot to evaluate physiological changes in it. EEG and ECG, which have been widely used in forest healing evaluation, were utilized as criteria. Seventy three subjects were selected with taking the age, drug, caffeine, smoking, and the time of last meal into consideration. As a result, EEG changes were correlated with three atmospheric environment items, six physical environment items, one soil environment item, and two vegetation environment items. ECG changes were significantly correlated with two atmospheric environment items, six physical environment items, two soil environment items, and two vegetation environment items (p<.05). It is expected that 11 environmental factors such as temperature, density, and altitude affecting EEG (e.g., alpha balance and gamma balance) and ECG (e.g., HRV mean) could be used as effective tools in developing more differentiated programs for improving healing effects.

Characteristics of Crack Healing and High Temperature Strength of High Strength Sialon (고강도 사이알론의 균열치유와 고온강도 특성)

  • Nam, Ki-Woo;Park, Sang-Hyun;Park, Seung-Won;Moon, Suk-Jae
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.9
    • /
    • pp.957-962
    • /
    • 2009
  • Sialon was produced by hot-pressing the mixtures of $Si_3N_4$, AlN and $Y_2O_3$ powders. All fracture tests were performed on a three-point loading system with a 30 mm bending span. Fracture toughness and Vickers hardness of smooth specimen were average 7.05 $MPa{\cdot}m^{0.5}$ and Hv = 1580, respectively. Density of three kinds of specimens, smooth specimen, smooth and healed specimen, smooth with $SiO_2$ colloidal coating and healed specimen, had beyond 99 % of theoretical density. Bending strength of smooth healed specimens had high strength more than 1 GPa. Crack healed specimens recovered as strength as smooth specimen. That is, cracked specimen with $SiO_2$ colloidal coating on cracked part recovered strength by heat treatment, completely. Crack healing of $Si_3N_4$ composite ceramics had contributed glassy $SiO_2$ to strength recovery. Limiting high temperature for bending strength of heat treated smooth specimen for bending strength was about 1273 K.

Application of Thermography in Thoroughbred Horses (말에서 체열찰영술의 적용에 관한 연구)

  • 양영진;조길재;손원근;남치주
    • Journal of Veterinary Clinics
    • /
    • v.19 no.2
    • /
    • pp.139-146
    • /
    • 2002
  • The purpose of this study was to construct fundamental information for the usefulness and effects of thermography in Thoroughbred horses. total 10 horses were examined to determine a normal thermal pattern before and after sedation in lower limbs and ophthalmic area, and to investigate the effects of thermography during 42 days after induced wound and arthritis. In normal horses, the range of temperature difference(${\Delta}T$) of symmetry site in lower limbs was 0.20 to $0.68^{\circ}C$ on pre-sedation, which was simillar to that of post sedation, 0.17 to $0.74^{\circ}C$, and eyeball area was 0.34 to $0.68^{\circ}C$. Thermographically, the warmest area in normal limbs were coronary band of frontal view and the region between heel bulbs of back view. And temperature difference(${\Delta}T$) after clipping in left forelimb was increased 1 to $3^{\circ}C$ more than before clipping. However, there was no significant change of the temperature difference and degree of clinical signs by the process of inflammation healing during the experiment period in the all groups. These results suggest that the thermography was especially helpful in following clinical course of a disease because the thermal pattern will return to normal with declining clinical signs and healing of the lesion.

A study on Crack Healing of Various Glassy Polymers (part I) -theoretical modeling- (유리질 중합체의 균열 Healing에 관한 연구 (제1보) -이론 모델링-)

  • Lee, Ouk-Sub
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.3 no.1
    • /
    • pp.40-49
    • /
    • 1986
  • Crack, craze and void are common defects which may be found in the bulk of polymeric materials such as either themoplastics or thermosets. The healing phenomena, autohesion, of these defects are known to be a intrinsic material property of various polymeric materials. However, only a few experimental and theoretical investigations on crack, void and craze healing phenomena for various polymeric materials have been reported up to date [1, 2, 3]. This may be partly due to the complications of healing processes and lacking of appropriate theoretical developments. Recently, some investigators have been urged to study the healing phenomena of various polymenic materials since the significance of the use of polymer based alloys or composites has been raised in terms of specific strength and energy saving. In the earlier published reports [1, 2, 3, 4], the crack and void healing velocity, healing toughness and some other healing mechanical and physical properties were measured experimentally and compared with predicted values by utilizing a simple model such as the reptation model under some resonable assumptions. It seems, however, that the general acceptance of the proposed modeling analyses is yet open question. The crack healing processes seem to be complicate and highly dependent on the state of virgin material in terms of mechanical and physical properties. Furthermore, it is also strongly dependent on the histories of crack, craze and void development including fracture suface morphology, the shape of void and the degree of disentanglement of fibril in the craze. The rate of crack healing may be a function of environmental factors such as healing temperature, time and pressure which gives different contact configurations between two separated surfaces. It seems to be reasonable to assume that the crack healing processes may be divided in several distinguished steps like stress relaxation with molecular chain arrangement, surface contact (wetting), inter- diffusion process and com;oete healing (to obtain the original strength). In this context, it is likely that we no longer have to accept the limitation of cumulative damage theories and fatigue life if it is probable to remove the defects such as crack, craze and void and to restore the original strength of polymers or polymer based compowites by suitable choice of healing histories and methods. In this paper, we wish to present a very simple and intuitive theoretical model for the prediction of healed fracture toughness of cracked or defective polymeric components. The central idea of this investigation, thus, may be the modeling of behavior of chain molecules under healing conditions including the effects of chain scission on the healing processes. The validity of this proposed model will be studied by making comparisons between theoretically predicted values and experimentally determined results in near future and will be reported elsewhere.

  • PDF

Self-Healing Properties of Fiber-Reinforced Cement Composite (FRCC) Depending on Various Curing Conditions (양생조건에 따른 섬유보강 시멘트계 복합재료(FRCC)의 균열 자기치유 특성)

  • Choi, Heesup;Choi, Hyeonggil
    • Journal of the Korea Institute of Building Construction
    • /
    • v.16 no.4
    • /
    • pp.289-296
    • /
    • 2016
  • In this study, the self-healing effect of a fiber-reinforced cement composite (FRCC) was examined using a drying-wetting test and an outdoor exposure test. The influence of various curing conditions on the self-healing effect of the FRCC was also investigated. The effect of self-healing was evaluated using a permeability coefficient and by investigating the cracks using a optical microscope. The results confirmed that the FRCC was capable of self-healing under a long wetting time and a low drying temperature. In addition, watertight performance by self-healing was shown to have a significant influence on wetting time. Meanwhile, this self-healing effect was enhanced by hydration as a result of rainfall when the FRCC was put under actual environmental conditions. Moreover, it was determined that cracking self-healing can be improved by using the appropriate admixture materials.

Effect of Ca Implantation on the Sintering and Crack Healing Behavior of High Purity Al2O3 Using Micro-lithographic Technique - I. Formation of Crack-like Pore and Its Morphological Evolution (Ion Implantation으로 Ca를 첨가한 단결정 Al2O3의 Crack-like Pore의 Healing 거동 - I. Crack-like Pore의 형성과 Morphological Evolution)

  • 김배연
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.8
    • /
    • pp.834-842
    • /
    • 1997
  • Controlled Ca impurity implanted inner crack-like pore in the high purity alumina single crystal, sapphire, had been created by micro-fabrication technique, which includes ion implantation, photo-lithography, Ar ion milling, and hot press technique. The morphological change and the healing of cracklike pore in Ca doped high purity single crystal alumina, sapphire, during high temperature heat treatment in vacuum were observed using optical microscopy. The dot-like surface roughening was developed and hexagon like crystal appeared on inner surface of crack-like pore after heat treatment. Bar type crystals, probably CaO.6Al2O3, were observed on the inner surface after 1 hour heat treatment at 1, 50$0^{\circ}C$, but this bar type crystal disappeared after 1 hour heat treatment at 1, $600^{\circ}C$. This disappearance means that there should be a little increase of Ca solubility limit to alumina at this temperatures.

  • PDF

Crack-healing Behavior and Corrosion Characteristics of SiC Ceramics (SiC 세라믹스의 균열치유거동 및 부식특성)

  • Hwang, Jin Ryang;Kim, Dae Woong;Nam, Ki Woo
    • Journal of Ocean Engineering and Technology
    • /
    • v.27 no.5
    • /
    • pp.10-15
    • /
    • 2013
  • The crack-healing behavior and corrosion resistance of SiC ceramics were investigated. Heat treatments were carried out from $900^{\circ}C$ to $1300^{\circ}C$. A corrosion test of SiC was carried out in acid and alkaline solutions under KSL1607. The results showed that heat treatment in air could significantly increase the strength. The heat-treatment temperature has a profound influence on the extent of crack healing and the degree of strength recovery. The optimum heat-treatment temperature was $1100^{\circ}C$ for one hour at an atmospheric level. In the two kinds of solutions, the cracks in a specimen were reduced with increasing time, and the surface of the crack healed specimen had a greater number of black and white spots. The strength of the corroded cracked specimen was similar to that of the cracked specimen. The strength of the corroded crack healed specimen decreased 47% and 75% compared to that of the crack healed specimen in the acid and alkaline solutions, respectively. Therefore, the corrosion of SiC ceramics is faster in an alkaline solution than in an acid solution.