Crack-healing Behavior and Corrosion Characteristics of SiC Ceramics  

Hwang, Jin Ryang (Interdisciplinary Program of Mechanical Engineering Graduate School, Pukyon Nat'l Univ.)
Kim, Dae Woong (Interdisciplinary Program of Mechanical Engineering Graduate School, Pukyon Nat'l Univ.)
Nam, Ki Woo (Department of Materials Science and Engineering, Pukyon Nat'l Univ.)
Publication Information
Journal of Ocean Engineering and Technology / v.27, no.5, 2013 , pp. 10-15 More about this Journal
Abstract
The crack-healing behavior and corrosion resistance of SiC ceramics were investigated. Heat treatments were carried out from $900^{\circ}C$ to $1300^{\circ}C$. A corrosion test of SiC was carried out in acid and alkaline solutions under KSL1607. The results showed that heat treatment in air could significantly increase the strength. The heat-treatment temperature has a profound influence on the extent of crack healing and the degree of strength recovery. The optimum heat-treatment temperature was $1100^{\circ}C$ for one hour at an atmospheric level. In the two kinds of solutions, the cracks in a specimen were reduced with increasing time, and the surface of the crack healed specimen had a greater number of black and white spots. The strength of the corroded cracked specimen was similar to that of the cracked specimen. The strength of the corroded crack healed specimen decreased 47% and 75% compared to that of the crack healed specimen in the acid and alkaline solutions, respectively. Therefore, the corrosion of SiC ceramics is faster in an alkaline solution than in an acid solution.
Keywords
Crack-healing; Strength; Optimum heat-treatment temperature; Corrosion resistance; Sulphuric acid solution; Sodium hydroxide solution;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Lee, S.K., Ishida, W., Lee, S.Y., Nam, K.W., Ando, K., 2005. Crackhealing Behavior and Resultant Strength Poperties of Silicon Carbide Ceramic. Journal of the European Ceramic Society, 25, 569-576.   DOI   ScienceOn
2 Nam, K.W., Lee, K.C., Kohyama, A., 2009. A Feasibility Study on the Application of Ultrasonic Method for Surface Crack Detection of SiC/SiC Composite Ceramics. KSNT, 29, 479-484.
3 Nam, K.W. and Kim, J.S., 2010a. Critical Crack Size of Healing Possibility of SiC Ceramics. Materials Science and Engineering A, 527, 3236-3239.   DOI   ScienceOn
4 Nam, K.W., Kim, J.S., Park, S.W. 2010b. The High Temperature Strength of SiC Ceramics Based on $SiO_{2}$ Nanocolloidal Employed. Materials Science and Engineering A, 527, 5400-5404.   DOI   ScienceOn
5 Nam, K.W., Kim, J.S., Park, S.W., 2010c. Crack-Healing Behavior and Bending Strength Properties of SiC Ceramics Based on the Type of Additive $SiO_{2}$ Employed, International Journal of Modern Physics B, 24, 2869-2874.   DOI   ScienceOn
6 Nam, K.W., Kim, J.W., Hinoki, T., Kohyama, A., Murai, J., Murakami, T. 2011a. Application of Untrasonic Inspection to Characterization of Advanced SiC/SiC Composites. Journal of Nuclear Materials, 417, 353-355.   DOI   ScienceOn
7 Nam, K.W., Moon, C.K. Seo, I.S., 2011b. A Fundamental Study for the Crack Healing of SiC Ceramics and SiCf/ SiC Composite Ceramics. Journal of Ceramic Processing Research, 12, 646-649.
8 Raffray, A.R., Jones, R., Aeill, G., Billone, C., Giancarli, L., Golfer, H., Hasegawa, A., Katoh, Y., Kohyama, A., Nishio, S., Riccardi, B., Tillack, M.S., 2001. Design and Material Issues for High Performance SiCf/SiC-based Fusion Cower Cores. Fusion Eng. Des., 55, 55-95.   DOI   ScienceOn
9 Saddow, S.E., Agarwal, A., 2004. Advances in Silicon Carbide Processing and Applications. Artech House, Inc., Boston.
10 Sembokuya, H., Kubouchi, M., Oshida, Y., Tsuda, K., 2002. Corrosion Behavior of Alumina or Silicon Carbide Filled Epoxy Resin Immersed in Alkaline Solution", Journal of Network Polymer (Japan), 23, 72-80.
11 Snead, L.L., Jones, R.H., Kohyama, A., Fenici, P., 1996. Status of Silicon Carbide Composites for fFsion. J. Nucl. Mater., 233-237, 26-36.   DOI   ScienceOn
12 Sydow, U., Schneider, M., Herrmann, M., Kleebe, H.J., Michaelis, A., 2010. Electrochemical Corrosion of Silicon Carbide Ceramics. Pt.1: Electrochemical Investigation of Sintered Silicon Carbide (SSiC). Materials and Corrosion, 61, S.657-664.
13 Ando, K., Ikeda, T., Sato, S., Yao, F. and Kobayasi. A., 1998. A Preliminary Study on Crack Healing Behavior of $Si_{3}N_{4}$/ SiC Composite Cermiacs. Fatigue & Fracture of Engineering Materials & Structures, 21, 119-122.
14 Giancarli, L., Bonal, J.P., Caso, A., Marois, G. Le., Morley, N.B., Salavy, J.F., 1998. Design Requirements for SiC:SiC Composites Structural Material in Fusion Power Reactor Blankets. Fusion Engineering and Design, 41, 65-171.
15 Takahashi, K., Uchiide, K., Kimura, Y., Nakao, W., Ando, K., 2007. Threshold Stress for Crack Healing of Mullite Reinforced by SiC Whiskers and SiC Particles and Resultant Fatigue Strength at the Healing Temperature. J. Am. Ceram. Soc., 90, 2159-2164.   DOI   ScienceOn