Behavior of Shear Strength of Coarse Grained Materials Based on Large Scale Direct Shear Test (I) (대형직접전단시험을 이용한 조립재료의 전단거동 특성 (I))

  • Lee Dae-Soo;Kim Kyoung-Yul;Hong Sung-Yun;Jo Hwa-Kyung;Whang Sung-Chun
    • Journal of the Korean Geotechnical Society
    • /
    • v.21 no.6
    • /
    • pp.81-91
    • /
    • 2005
  • 'Coarse grained material' refers to crushed stones or gravels, and the behaviour of soil containing coarse grained material is not easily defined using the conventional soil mechanics theory due to the influences of large particles, therefore large scale test is essential to investigate their effects. Previous studies have identified the major factors affecting the properties of coarse grained materials by using large scale shear testing apparatus, such as maximum particle size, water content, density and uniformity coefficients. In this paper, the effect of variation of maximum particle size and water content on shear strength was analyzed from the results of large scale shear test. In addition, the fiction coefficient at critical state per vertical load was estimated using the equation proposed by Wood (1998). The sample for the test was obtained from the local quarry sites. Tests results show that the shear strength for 50.8 m maximum particle size is relatively larger than that of 76.3 m and air-dry sample has larger shear strength than saturated sample. In the meantime, the friction coefficient at critical state shows $1.0\sim1.6$ according to the test conditions.

Effect of Board Thickness and Ring Angle on Press - drying for Heartwood and Sapwood of Quercus acutissima C. (상수리나무 심재(心材)와 변재판재(邊材板材)의 두께와 연륜각도(年輪角度)가 열판건조(熱板乾燥)에 미치는 영향(影響))

  • Lee, Nam-Ho;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.15 no.2
    • /
    • pp.67-78
    • /
    • 1987
  • This study was designed to investigate the effect of board thickness and ring angle on the characteristics including internal check. ring failure, surface check, end check, collapse, thickness shrinkage and width shrinkage of press-drying. The exprimental materials of 6mm-. 9mm- and 12mm-thick board were taken from heartwood and sapwood of oak (Quercus acutissima Carr.) respectively. And boards were numbered according to position in the log(No. 1 to No. 4 for heartwood :md No. 9 for sapwood). Press-drying was at $145^{\circ}C$ platen temperature and 3.5kg/$Cm^2$ platen pressure. The results of this study were summarized as follows. 1. Drying rates for sapwood materials were greater than those for heartwood materials. And drying rates for thinner materials were greater than those for thicker materials. 2. The thinner boards were. the severer surface checking developed in the heartwood materials, and surface checking for heartwood materials had no tendency in board position for the same thickness. Sapwood materials were completely free from surface checking. 3. End checking for heartwood materials had no tendency in board position. The greater deviation of ring angle from perfectly edge-grained was, the severer and checking developed in the sapwood materials. But end checking did not occur in 6mm-thick sapwood materials. 4. The greater deviation of ring angle from perfectly edge-grained was, the severer end checking developed for heartwood and sapwood materials. As board thickness increased, maternal checking developed more severely for heartwood and sapweed materials. 5. For heartwood materials, ring failure, reduced with increasing deviation of ring angle from perfectly edge-grained except 12mm-thick material and showed no significant difference attributable to board thickness. Sapwood materials were completely free from ring failure. 6. For heartwood and sapwood materials, collapse was slight and showed no significant differences attributable to both board thickness and board position. 7. As deviation of ring angle from perfectly edge-grained increased, shrinkage of board thickness decreased for heartwood and sapwood materials. 8. Shrinkage of board width showed no significant differences attributable to both board thickness and board position for heartwood and sapweed materials.

  • PDF

Characteristic of Shear Behavior of Coarse Grained Materials Based on Large Scale Direct Shear Test (II) (대형직접전단시험을 이용한 조립재료의 전단거동 특성 (II))

  • Lee Dae-Soo;Kim Kyoung-Yul;Hong Sung-Yun;Hwang Sung-Chun
    • Journal of the Korean Geotechnical Society
    • /
    • v.22 no.4
    • /
    • pp.51-59
    • /
    • 2006
  • In this paper, the effect of variation of density and uniformity coefficient on shear strength was analyzed from the results of large scale shear test. In addition, the friction coefficient at critical state per vertical load was estimated using the equation proposed by Wood (1998). The test sample fur the test was obtained from the local quarry sites. Tests results show that the shear strength of $2.10g/cm^3$ is relatively larger than that of $1.85g/cm^3$ and uniformity coefficient (5.0) has larger shear strength than that in 10.0. In the meantime, the friction coefficient at critical state shows $1.0{\sim}1.6$ according to the test conditions.

Bending of Korea red pine (Pinus densiflora) by Microwave Irradiation (마이크로파 가열에 의한 소나무재의 곡가공)

  • Jung, Sung-Soo;Lee, Weon-Hee
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.3
    • /
    • pp.17-22
    • /
    • 1999
  • The effect of microwave irradiation on wood bending was investigated in this study. The specimens irradiated with microwave were bent around a form by using pedestal-steel and clamps. The specimens, korea red pine (Pinus densiflora), for this test were water-soaked for 78 hours. Saturated specimens were boiled in water for an hour. The size of specimens was 350mm(L) by 20mm(R) by 10mm(T). These specimens were heated by microwave of 2,450MHz. The most suitable time for microwave irradiation seems to range from 60 to 90 seconds. Wood moisture content decreased remarkably with the increase of irradiation time. When a softened wood piece is bent, its convex side was stretched while the concave side was compressed. It can be compressed considerably, but stretched very little. Therefore the failure will be governed by the tensile breaking strain and occur mainly on the convex face. So we obtained results from three different bending process methods as follows : 1) When bending with a pedestal-steel, convex face had not tensile breakings, but concave face had compression fails. 2) When bending with a clamp, bending time increased more than pedestal-steel and occurred tensile breaking. 3) Bending with a pedestal-steel and a clamp was found to be the most excellent operation method in this study.

  • PDF

Teak (Tectona grandis Linn. f.): A Renowned Commercial Timber Species

  • Palanisamy, K.;Hegde, Maheshwar;Yi, Jae-Seon
    • Journal of Forest and Environmental Science
    • /
    • v.25 no.1
    • /
    • pp.1-24
    • /
    • 2009
  • Teak (Tectona grandis) is one of the most valuable timber yielding species in the world, with predominant distribution in tropical or sub-tropical countries. However, natural teak available only in few countries like India, Myanmar, Laos People's Democratic Republic and Thailand. Teak grows well in deep, well-drained alluvial soils, fairly moist, warm, tropical climate with pH ranges from 6.5-7.5. Teak is cultivated in many Asian, African and South American countries for timber production. The global teak plantations are estimated to be three million hectare with major share in India (44%) followed by Indonesia (33%). India is considered as richest genetic resources of teak with large areas of natural teak bearing forests (8.9 million ha), plantations (1.5 million ha), clonal seed orchards (1000 ha) and seed production areas (5000 ha). The studies on diversity of teak populations showed that teak is an out crossing species with major portion of diversity present within the populations. The productivity and quality of teak timber varies depending upon the site and environmental conditions. Teak wood is moderately heavy, strong and tough,straight grained, coarse textured and ring porous with specific gravity varies from 0.55 to 0.70. The sapwood is white to pale yellow in colour and clearly demarcated while heartwood is dark brown or dark golden yellow in colour. Teak is one of the most durable timbers in the world, practically, impervious to fungus and white ant attack and resistant to decay. Teak wood is used in ship and boat constructions, furnitures and aesthetic needs. Genetic improvement programmes have been undertaken in countries like Thailand, India, Malaysia and Indonesia. The programme includes provenance identification and testing, plus tree selection and clonal multiplication, establishment of seed orchards and controlled hybridization. Several aspects like phenology, reproductive biology, fruit characteristics, silvicultural practices for cultivation, pest and diseases problems, production of improved planting stock, harvesting and marketing, wood properties and future tree improvement strategy to enhance productivity have been discussed in this paper.

  • PDF

Metallurgical Analysis of Forged Iron Axe Excavated from the Wood-framed Tomb at the Hwangseongdong, Gyeongju, Korea (경주 황성동 목곽묘에서 출토된 단조 철부의 금속학적 특성 분석)

  • Lee, Chan-Hee;Lee, Myeong-Seong;Kim, Jeong-Hun;Yi, Ki-Wook
    • 한국문화재보존과학회:학술대회논문집
    • /
    • 2004.10a
    • /
    • pp.33-42
    • /
    • 2004
  • The forged iron axe found in the No. 2 wood-framed tomb (the middle 3rd century) of Hwangseongdong, Gyeongju is rectangular on the plane level. It shows an obtuse angle in the edge part, while the joint part has the both sides folded up and shows the traces of wood. Under the reflected light, the Iron axe shines in metal luster, which is bright light gray or light creamy colors. The result of x-ray diffraction analysis shows that the axe consists of magnetite and geothite, which can explain why the composition and structure of the original ore has been kept intact. The microtexture of the axe has the irregular network of ferrite and pearlite, and tile cementite of tiny amount in the ferrite background. The overall treatment of the texture seems to be thermal with a high ratio of carbon. There are fine-grained magnetite, wolframite, quartz, calcite, mica, hornblende and pyroxene inside the axe. Those must be the impurities that they failed to remove in the refining process. The normal ferrite is composed of pure iron whose $Fe_2O_3$ proportion is from 99.16 to $99.84\;wt.\%$. Other than them, the ferrite parts usually contain $Al_2O_3\;and\;SiO_2$. The irregular network of pearlite also contains Impurities including $Al_2O_3\;and\;SiO_2$ and shows highly diverse patterns of carbon content. It's because the axe was carburized after the material was made to resemble pure iron. The decarbonization work didn't go well along the process marks. It's estimated that the original ore was bloom produced in low-temperature reduction and formed around in $727^{\circ}C$, which is eutetic temperature.

  • PDF

Effect of Tension, Compression Lamination and Number of Lamination on the Flexural Properties of Platanus occidentalis L. Laminated Beam (인장(引張) 및 압축부재(壓縮部材)와 적층수(積層數)가 플라타너스 집성재(集成材)의 휨성질(性質)에 미치는 영향(影響))

  • Oh, Se-Chang;Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.14 no.2
    • /
    • pp.3-12
    • /
    • 1986
  • The aim of this study is to determine the flexural properties(Modulus of Rupture, Modulus of Elasticity) of Platanus occidentalis L. laminated beams fabricated with 1, 3, 5, 8, 15 lamination and Tension, Compression lamination. The results were as follows: 1. MOR increased with increasing number of lamination in 3, 5, 8, 15-beam and Tension lamination beam. MOR of Compression lamination beam was lower than that of 3-beam, MOR of vertical beam not having Tension or compression lamination was lower than that of horizontal beam, but MOR of vertical beam with tension or compression lamination was same or slightly higher than that of horizontal beam. 2. The allowable working stress showed the same tendency. This stress increased with increasing number of lamination. This value of Tension lamination beam was higher than that of compression lamination beam. 3. MOE of all laminated beams was higher than that of solid beam and Tension lamination beam was higher than that of 3-beam. MOE of Tension lamination beam was higher than that of Compression lamination beam. MOE of all vertical beam was higher than that of horizontal beam except for T-2, T-5, C-3. 4. Most beam failures appeared to begin in tension. These tension failures were classified into Splintering tension, Cross-grained tension, Simple tension, Brittle tension. All test beam failures could be classified into three categories. 1) Tension failure 2) Compression failure 3) Horizontal shear failure.

  • PDF

Metallic Mineralogical Characteristics of Forged Iron Axe from the Wood-framed Tomb at the Hwangseongdong, Gyeongju, Korea (경주 황성동 목곽묘 출토 단조 철부의 금속광물학적 특성)

  • Kim, Jeong-Hun;Yi, Ki-Wook;Lee, Chan-Hee
    • Journal of the Mineralogical Society of Korea
    • /
    • v.20 no.4
    • /
    • pp.231-245
    • /
    • 2007
  • The forged iron axe of the middle 3rd Century found in the No. 2 wood-framed tomb from the Hwangseongdong site, Gyeongju is rectangular on the plane level. The iron axe shines in met-allic luster, which is light grey with pale creamy tint. The result of X-ray diffraction analysis shows that the axe consists of magnetite and geothite, which can explain why the composition and texture of the original ore has been kept intact. There are fine-grained quartz, calcite, mica, magnetite, amphibole, unknown tungsten minerals, pyroxene and olivine inside the axe. Those must be the impurities that they failed to remove in the thermal treatment process. Generally, the iron axe consists mainly of pearlite texture coexisting ferrite and cementite, and show high carbon contents with homogeneous distribution. It can be interpreted the axe was carburized after the material was made to resemble pure iron. The decarbonization work didn't go well along the process marks. Crude ores of the iron axe are possible utilized by magnetite from the Ulsan mine on the basis of the occurrences and inclusions. It's estimated that the original ore was bloom produced in low-temperature reduction and formed around in $727^{\circ}C$, which is eutetic temperature.

Oxygen Index for Wood in Burning Test by the Up and Down Method (Up and Down법(法)에 의(依)한 목재(木材) 연소시험(燃燒試驗)에 있어서의 산소지수(酸素指數))

  • Eom, Young Geun;Lee, Phil Woo;Kim, Hyun Joong
    • Journal of Korean Society of Forest Science
    • /
    • v.79 no.3
    • /
    • pp.255-259
    • /
    • 1990
  • To investigate relative flammability in flaming combustion among 10 softwoods and 10 hardwoods, oxygen indices were determined for flat-grained sapwoods through Up and Down method following oxygen index test of ASTM D 2863-77. Oxygen index ranged from 21.0 for Pinus strobus to 28.2 for Larix gmelinii var. principis-ruprechtii in softwoods and from 20.7 for Populus davidiana to 27.6 for Quercus acntissima in hardwoods, which indicates Larix gmelinii var. principis-ruprechtii and Quercus acutissima being ranked first in inflammability and Pinus strobus and Populus davidiana being the least in fire resistance by softwood and hardwood because highly flammable materials are likely to have a low oxygen index.

  • PDF

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.