• 제목/요약/키워드: grain growth behavior

검색결과 284건 처리시간 0.026초

Co를 첨가한 $ZnO-Bi_2O_3-Sb_2O_3$ 바리스터의 소결 및 전기적 특성 (Sintering and the Electrical Properties of Co-doped $ZnO-Bi_2O_3-Sb_2O_3$ Varistor System)

  • 김철홍;김진호
    • 한국세라믹학회지
    • /
    • 제37권2호
    • /
    • pp.186-193
    • /
    • 2000
  • Effects of 1.0 mol% CoO addition on sintering and the electrical properties of ZnO-Bi2O3-Sb2O3(ZBS) varistor system with 3.0 mol% co-addition of Sb2O3 and Bi2O3 at various Sb/Bi ratio (0.5, 1.0, and 2.0) were investigated. Cobalt had little influence on the liquid-phase formation and the pyrochlore decomposition temepratures of ZBS, while densification was mainly dependent on Sb/Bi ratio: when Sb/Bi=0.5, excess Bi2O3 irrelevant to the formation of pyrochore(Zn2Sb3Bi3O14) forms eutectic liquid at ~75$0^{\circ}C$ which promotes densification and grain growth; with Sb/Bi=2.0, the second phase Zn7Sb2O12 formed by excess Sb2O3 irrelevant to the formation of the pyrochlore retards densification up to ~100$0^{\circ}C$. These phases caused the coarsening and uneven distribution of the second phase particles on the grain boundaries of ZnO above the pyrochlore decomposition temperature(~105$0^{\circ}C$), which led to broad size dist-ribution of ZnO; the specimen with Sb/Bi=1.0 showed homogeneous microstructure compared with the others, which enabled improved varistor characteristics. Doping of Co increased the nonlinearity and the potential barrier height of ZBS, which is thought to stem from improved sintering behavior such as homogenized microstructure due to size reduction and even distribution of the second phase and suppressed volatility of Bi2O3, as well as the improvement in the potential barrier structure via increased donor and interface electron trap densities.

  • PDF

급속 소결 공정에 의한 초미립 WC-10Co와 WC-10Fe 초경재료 제조와 기계적 성질 (Mechanical Properties and Consolidation of Ultra-Fine WC-10Co and WC-10Fe Hard Materials by Rapid Sintering Process)

  • 정인균;박정환;도정만;김기열;우기도;고인용;손인진
    • 대한금속재료학회지
    • /
    • 제46권4호
    • /
    • pp.223-226
    • /
    • 2008
  • The comparison of sintering behavior and mechanical properties of ultra-fine WC-10wt.%Co and WC-10wt.%Fe hard materials produced by high-frequency induction heated sintering (HFIHS) was accomplished using ultra fine powder of WC and binders(Co, Fe). The advantage of this process allows very quick densification to near theoretical density and prohibition of grain growth in nano-structured materials. Highly dense WC-10Co and WC-10Fe with a relative density of up to 99% could be obtained with simultaneous application of 60 MPa pressure and induced current within 1 minute without significant change in grain size. The hardness and fracture toughness of the dense WC-10Co and WC-10Fe composites produced by HFIHS were investigated.

수도(水稻)의 직파(直播) 및 이식재배(移植栽培) 조건하(條件下)의 인산(燐酸) 소장(消長)에 대(對)하여 (Studies on the Behavior of Phosphorus under the Conditions of Transplanting and Direct-sowing Culture in Rice Plants)

  • 안학수
    • Applied Biological Chemistry
    • /
    • 제11권
    • /
    • pp.185-188
    • /
    • 1969
  • 본실험(本實驗)은 수도(水稻)에 있어서의 직파재배(直播栽培)와 이앙재배(移秧栽培) 시(時) 수도체내(水稻體內)의 인산(燐酸)에 대(對)한 소장상(消長相), 생육(生育)및 수량(收量)등을 시기별(時期別)로 비교(比較)하여 본 결과(結果) 다음과 같은 사실을 알수 있있다, 1. 인산(燐酸) 함량(含量)은 직파재배구(直播栽培區)보다 이앙재배구(移秧栽培區)가 많았으나 활착기(活着期) 및 분얼초기(分蘖初期)까지는 직파재배구(直播栽培區)가 더 많았다. 이는 직파재배(直播栽培)는 인산(燐酸) 공급(供給)및 소비(消費)가 초기생육과정(初期生育過程)에서 일어났고 이앙재배(移秧栽培)에서는 후기(後期) 내지 중기(中期) 이후(以後)에 이루어진다는 것을 나타내고 있다고 볼수있다. 2. 수도체내(水稻體內)의 수분함량(水分含量)은 활착기(活着期) 및 분얼초기(分蘖初期)에 직파재배구(直播栽培區)가 많았으나 그 후(後)는 이앙재배구(移秧栽培區)가 더 많은 수분함량(水分含量)을 보였고 초장(草長)에 있어서는 분얼초기(分蘖初期) 까지 직파구(直播區)가 더 켰으나 그후 계속하여 이앙구(移秧區)가 앞섰다. 3. 건물중(乾物重)은 분얼초기(分蘖初期)까지는 직파재배구(直播栽培區)가 많았으나 그후는 이앙구(移秧區)가 많았다. 그리고 수확량(收穫量)을 백분율(百分率)로 표시(表示)할때 이앙재배구(移秧栽培區)가 직파재배구(直播栽培區)에 비(比)하여 약(約) 15% 내외(內外)의 증수(增收)를 가져왔다.

  • PDF

Residual Stress on Concentric Laminated Fibrous Al2O3-ZrO2 Composites on Prolonged High Temperature Exposure

  • Sarkar, Swapan Kumar;Lee, Byong Taek
    • 한국재료학회지
    • /
    • 제23권9호
    • /
    • pp.531-536
    • /
    • 2013
  • This paper investigates the effect of prolonged high temperature exposure on concentric laminated $Al_2O_3-ZrO_2$ composites. An ultrafine scale microstructure with a cellular 7 layer concentric lamination with unidirectional alignment was fabricated by a multi-pass extrusion method. Each laminate in the microstructure was $2-3{\mu}m$ thick. An alternate lamina was composed of 75%$Al_2O_3$-(25%m-$ZrO_2$) and t-$ZrO_2$ ceramics. The composite was sintered at $1500^{\circ}C$ and subjected to $1450^{\circ}C$ temperature for 24 hours to 72 hours. We investigated the effect of long time high temperature exposure on the generation of residual stress and grain growth and their effect on the overall stability of the composites. The residual stress development and its subsequent effect on the microstructure with the edge cracking behavior mechanism were investigated. The residual stress in the concentric laminated microstructure causes extensive micro cracks in the t-$ZrO_2$ layer, despite the very thin laminate thickness. The material properties like Vickers hardness and fracture toughness were measured and evaluated along with the microstructure of the composites with prolonged high temperature exposure.

극저온 압연으로 제조된 5052 Al Alloy의 기계적 성질 (Mechanical Properties of Ultrafine Grained 5052 Al Alloy produced by Cryogenic Rolling Process)

  • 이영범;남원종
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.233-239
    • /
    • 2004
  • The effect of annealing temperature on microstructures and mechanical properties of the sheets received $88\%$ reduction at cryogenic temperature was investigated for the annealing temperature of $150\~300^{\circ}C$, in comparison with those at room temperature. The presence of equiaxed grains, whose size is about 200nm in a diameter, was observed in 5052 Al alloy deformed $88\%$ and annealed $200^{\circ}C$ for an hour. When compared with the deformation at room temperature, the deformation at cryogenic temperature showed the higher strengths and equivalent elongation after annealing at the annealing temperature below $200^{\circ}C$. However, for annealing above $250^{\circ}C$ materials deformed at cryogenic temperature showed the lower strength than those deformed at room temperature. This behavior might be attributed to the higher rate of recrystallization and growth in materials deformed at cryogenic temperature during annealing, due to the lager density of dislocations accumulated during the deformation.

  • PDF

Cu 첨가에 따른 Al-Y-Ni의 나노결정화 거동 (Nanocrystallization Behavior of Al-Y-Ni with Cu Additions)

  • 홍순직;천병선;강세선;이임렬
    • 한국분말재료학회지
    • /
    • 제9권1호
    • /
    • pp.19-24
    • /
    • 2002
  • This paper reports the results of an investigation into the effect of Cu additions upon the nano-crystallization behaviour of an Al-Y-Ni alloy. 1 at.% Cu was added to a base alloy of Al/sub 88/Y₄Ni/sub 8/ either by substitution for Al to form Al/sub 87/Y₄Ni/sub 8/Cu₁, or by substitution for Ni to form Al/sub 88/Y₄Ni/sub 7/Cu₁. Consistent with previous findings in the literature, the substitution of Cu for Al was found to increase the thermal stability of the amorphous phase whereas the substitution of Cu for Ni was found to decrease its thermal stability. Comparing the microstructures of these alloys after heat treatment to produce equivalent volume fractions of Al nanocrystals showed average grain sizes of 14 nm, 12 nm and 9 nm for the alloys Al/sub 88/Y₄Ni/sub 8/, Al/sub 87/Y₄Ni/sub 8/Cu₁respectively. The effect of Cu in refining the size of the nanocrystals was attributed to enhanced nucleation increasing the number density of the nanocrystals, rather than diffusion limited or interface limited growth.

열처리에 따른 미세구조 변화가 Ti 판재의 부식특성에 미치는 영향 (The Effect of Microstructural Evolution on Corrosion Property of Ti Plate with Heat Treatment)

  • 김민규;이찬수;김태규;김혜성
    • 열처리공학회지
    • /
    • 제31권1호
    • /
    • pp.12-17
    • /
    • 2018
  • We investigated the corrosion behavior of commercially pure cold working processed (CP)-Ti with coarse-grained (CG) microstructure heat-treated at $400^{\circ}C$ and $600^{\circ}C$, respectively. It is observed that corrosion resistance of as-received CP-Ti heat-treated at $400^{\circ}C$, at which recrystallization proceeds, is largely improved. Interestingly, the mechanical property of CP-Ti sample at $400^{\circ}C$ was scarcely deteriorated. It is attributed to the decrease of the defects such as strain variance and dislocation density. On the other hand, the annealing treatment at $600^{\circ}C$ of CP-Ti plate causes to grain growth with the noticeable reduction of mechanical property. Hence, it is considered that defect density such as strain and dislocation density is important microstructural parameter for the improvement of corrosion resistance. The introduction of proper annealing treatment can help to improve corrosion resistance without scarifying mechanical property of CP-Ti.

Temperature Dependence of the Deposition Behavior of Yttria-stabilized Zirconia CVD Films: Approach by Charged Cluster Model

  • Hwang, Nong-Moon;Jeon, In-Deok;Latifa Gueroudji;Kim, Doh-Yeon
    • 한국세라믹학회지
    • /
    • 제38권3호
    • /
    • pp.218-224
    • /
    • 2001
  • Yttria-stabilized zirconia (YSZ) films were deposited with varying temperatures of ZrCl$_4$between 250~55$0^{\circ}C$ with YCl$_3$and the substrate at 100$0^{\circ}C$. Nanoamperes per square centimeter of the electric current were measured in the reactor during deposition and the current increased with increasing evaporation temperature of ZrCl$_4$. The zirconia nanometer size clusters were captured on the grid membrane near the substrate during the CVD process and observed by transmission electron microscopy (TEM). The deposition rate decreased with increasing evaporation temperature of ZrCl$_4$. A cauliflower-shaped structure was developed at 25$0^{\circ}C$ then gradually changed to a faceted-grain structure above 35$0^{\circ}C$. Dependence of the growth rate and the morphological evolution on the evaporation temperature of ZrCl$_4$was approached by the charged cluster model.

  • PDF

DC 스퍼터법과 비대칭 양극성 펄스 스퍼터법으로 제작된 고분자 전해질 연료전지 금속분리판용 CrN 코팅막의 특성 연구 (A Comparative Study of CrN Coatings Deposited by DC and Pulsed DC Asymmetric Bipolar Sputtering for a Polymer Electrolyte Membrane Fuel Cell (PEMFC) Metallic Bipolar Plate)

  • 박상원;전성용
    • 한국세라믹학회지
    • /
    • 제50권6호
    • /
    • pp.390-395
    • /
    • 2013
  • Nanocrystalline CrN films were deposited on Si (100) substrates by means of asymmetric pulsed DC reactive magnetron sputtering. We investigated the growth behavior, corrosion resistance and mechanical properties of CrN films with a change in the duty cycle and pulse frequency. The grain size of the CrN films decreased from 25.4 nm to 11.2 nm upon a decrease in the duty cycle. The corrosion potentials for the CrN films by DC sputtering was approximately - 0.6 V, and it increased to - 0.3 V in the CrN films which underwent pulsed sputtering. The nanoindentation hardness of the CrN films also increased with a decrease in the duty cycle. This enhancement of the corrosion resistance and mechanical properties of pulsed sputtered CrN films could be attributed to the densification and surface smoothness of the microstructure of the films.

Development of Alkali Metal Thermal-to-Electric Converter Unit Cells Using Mo/TiN Electrode

  • Seog, Seung-won;Choi, Hyun-Jong;Kim, Sun-Dong;Lee, Wook-Hyun;Woo, Sang-Kuk;Han, Moon-Hee
    • 한국세라믹학회지
    • /
    • 제54권3호
    • /
    • pp.200-204
    • /
    • 2017
  • Molybdenum (Mo), an electrode material of alkali metal thermal-to-electric converters (AMTEC), facilitates grain growth behavior and forms Mo-Na-O compounds at high operating temperatures, resulting in reduced performance and shortened lifetime of the cell. Mo/TiN composite materials have been developed to provide a solution for such issues. Mo is a metal that possesses excellent electrical properties, and TiN is a ceramic compound with high-temperature durability and catalytic activity. In this study, a dip-coating process with an organic solvent-based slurry was used as an optimal coating method to achieve homogeneity and stability of the electrodes. Cell performance was evaluated under various conditions such as the number of coatings, ranging from 1 to 3 times, and heat treatment temperatures of $800-1100^{\circ}C$. The results confirmed that the cell yielded a maximum power of 9.99 W for the sample coated 3 times and heat-treated at $900^{\circ}C$.