Patterning Barrier Ribs of PDP by Transparent Soft Mold

  • Paek, Sin-Hye;Choi, Hyung-Suk;Park, Lee-Soon
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2002년도 International Meeting on Information Display
    • /
    • pp.639-642
    • /
    • 2002
  • A new PDP barrier rib formation technique was investigated utilizing transparent soft maid made of silicon resin. Transparent soft mold was fabricated by pouring a silicone resin into the base mold made with photosensitive glass. The photosensitive barrier rib paste was coated on the glass substrate and dried in a 90 $^{\circ}C$ convection oven for 20min. The transparent soft mold was pressed on top of the semi-dry barrier rib layer and then irradiated with a UV lamp to a total dose of $900{\sim}1000mJ/cm^2$ The soft maid was then removed from the pressed barrier rib by winding up and fine pattern of barrier rib was obtained. The photosensitive barrier rib paste makes the demolding easy due to reduced interfacial forces and shrinking of paste materials.

  • PDF

AC PDP의 addressing time과 유전체 및 Barrier Rib 높이와의 상관관계 (The relationship between addressing time and dielectric layer, barrier rib hight)

  • 박정태;박차수;송기동;박정후;조정수
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2000년도 하계학술대회 논문집 C
    • /
    • pp.1824-1826
    • /
    • 2000
  • Up to date, the dual scanning method has been adopted to decrease address-ing period in AC PDP. In this case, addressing period can be reduced, but the driving circuit cost should be increased. In this study, to increase addressing speed we have studied the relationship between addressing speed and cell structure. That is to say, we varied the thickness of dielectric layer on the front glass, the thickness of white back and the height of barrier rib on the rear glass. So, we found that the addressing time was decreased 4% with decreasing 5um thickness of dielectric layer on the front glass and 2um thickness of white back on the rear glass. Also in case of decreasing the height of barrier rib, addressing time was decreased about 4% per 10um.

  • PDF

레이저빔에 의한 PDP 격벽 재료의 식각 (Etching of the PDP barrier rib material using laser beam)

  • 안민영;이경철;이홍규;이상돈;이천
    • 한국전기전자재료학회논문지
    • /
    • 제13권6호
    • /
    • pp.526-532
    • /
    • 2000
  • The paste on the glass or fabrication of the PDP(Plasma Display Panel) barrier rib was selectively etched using focused A $r_{+}$ laser(λ=514 nm) and Nd:YAG(λ=532, 266 nm) laser irradiation. The depth of the etched grooves increase with increasing a laser fluence and decreasing a laser beam scan speed. Using second harmonic of Nd:YAG laser(532 nm) the etching threshold laser fluence was 6.5 mJ/c $m^2$ for the sample of PDP barrier rib. The thickness of 180 ${\mu}{\textrm}{m}$ of the sample on the glass was clearly removed without any damage on the glass substrate by fluence of 19.5J/c $m^2$beam scan speed of 20${\mu}{\textrm}{m}$ /s. In order to increase the etch rate of the barrier rib material barrier rib samples heated by a resistive heater during laser irradiation. The heated sample has many defects and becomes to be fragile. This imperfection of the structure compared to the sample without heat treatment allows the effective etching by the focused laser beam. The etch rates were 65${\mu}{\textrm}{m}$/s and 270 ${\mu}{\textrm}{m}$/s at room temperature and 20$0^{\circ}C$, respectively.y.

  • PDF

플라즈마 디스플레이 패널을 위한 레이저 직접 패터닝 (Laser-Direct Patterning for Plasma Display Panel)

  • 안민영;이경철;이홍규;이천
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.99-102
    • /
    • 1999
  • A mixture which was made from organic gel, glass powder and ceramic powder was masklessly etched for fabrication of barrier rib of PDP(Plasma Display Panel) by focused Ar$^{+}$ laser( λ =514 nm) and Nd:YAG(λ =532, 266 nm) laser irradiation at the atmosphere. The depth of the etched grooves increases with increasing a laser fluence and decreasing a scan speed. Using second harmonic of Nd:YAG laser, the threshold laser fluence was 6.5 mJ/$\textrm{cm}^2$ for the sample of PDP barrier rib softened at 12$0^{\circ}C$. The thickness of 130 ${\mu}{\textrm}{m}$ of the sample on the glass was clearly removed without any damage on the glass substrate by fluence of 19.5 J/$\textrm{cm}^2$....

  • PDF

Feasibility of BaO-ZnO-$B_2O_3$ based Glass as a Host to Employ Various Ceramic Fillers to be applied to Barrier Ribs in Plasma Display Panels

  • Kim, Sang-Gon;Shin, Hyun-Ho;Park, Jong-Sung;Hong, Kug-Sun;Kim, Hyung-Sun
    • Journal of Information Display
    • /
    • 제5권3호
    • /
    • pp.25-29
    • /
    • 2004
  • Effects of additing various types of ceramic fillers to the BZB-based glass on the thermo-chemical stability, optical reflectance, and mechanical properties were investigated. The glass system demonstrated the feasibility to host various types of ceramic fillers to form micro-composites at the processing temperature suitable for PDP systems. The optical reflectance and mechanical strength of the filler-glass composites were improved as compared to the glass itself. These results demonstrate the feasibility of applying the Pb-free BZB-based glass system as a matrix for employing various types of crystalline ceramic fillers to be used as barrier rib materials in plasma display panels.

Photolithographic Method of Patterning Barrier Ribs for PDP by Green Sheet

  • Park, Lee-Soon;Jang, Dong-Gyu;Hur, Young-June;Lee, Sung-Ho;Kim, Duck-Gon;Kwon, Young-Hwan
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.1225-1228
    • /
    • 2005
  • Barrier ribs in the plasma display panel(PDP) function to maintain the discharge space between the glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, and barrier rib powder of which surface was treated with fumed silica particles. Study on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation and photolithographic process, it was found that photolithographic patterning of barrier ribs with photosensitive barrier rib green sheet could be used in the fabrication of high resolution PDP.

  • PDF

Barrier Rib Patterning Technology for Cost Effective High Resolution PDP

  • Park, Lee-Soon;Paek, Sin-Hye;Yun, Sang-Won;Choi, Hyung-Suk
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2002년도 International Meeting on Information Display
    • /
    • pp.989-993
    • /
    • 2002
  • Barrier ribs in the color plasma display panel(PDP) function to maintain the discharge space between to glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, mid barrier rib powder. Study on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation, both photolithographic and transparent soft molding method resulted in fine pattern of barrier ribs with high aspect ratio.

  • PDF

Photosensitive Barrier Rib Paste and Materials and Process

  • Park, Lee-Soon;Kim, Soon-Hak;Jang, Dong-Gyu;Kim, Duck-Gon;Hur, Young-June;Tawfik, Ayman
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.823-827
    • /
    • 2005
  • Barrier ribs in the plasma display panel (PDP) function to maintain the discharge space between the glass plates as well as to prevent optical crosstalk. Patterning of barrier ribs is one of unique processes for making PDP. Barrier ribs could be formed by screen-printing, sand blasting, etching, and photolithographic process. In this work photosensitive barrier rib pastes were prepared by incorporating binder polymer, solvent, functional monomers photoinitiator, and barrier rib powder of which surface was treated with fumed silica particles. Studies on the function of materials for the barrier rib paste were undertaken. After optimization of paste formulation and photolithographic process, it was applied to the photosensitive barrier rib green sheet and was found that photolithographic patterning of barrier ribs could be formed with good resolution up to $110{\mu}m$ height and $60{\mu}m$ width after sintering.

  • PDF

($TruNano^{TM}$ processing of dielectric layers and barrier-rib on soda-lime glass substrate for PDP panel

  • Lee, Michael M.S.;Kim, Nam-Hoon;Cheon, Chae-Il;Cho, Guang-Sup;Kim, Jeong-Seog
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2006년도 6th International Meeting on Information Display
    • /
    • pp.125-125
    • /
    • 2006
  • We present a low temperature thermal process for the transparent dielectric layer, barrier rib, and white back dielectric layer on the soda-lime glass substrate of the PDP by the $TruNano^{TM}$ processor in combination with a compositional modification to the conventional dielectric pastes. By this method the firing temperature can be lowered by more than $100^{\circ}C$.

  • PDF

실리콘고무형과 전자기파에 의한 PDP격벽의 성형에 관한 연구 (A Study on Plasma Display Panel Barrier Rib Fabrication by Silicone Rubber Tooling and electromagnetic Wave)

  • 정해도;손재혁;조인호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.20-23
    • /
    • 2001
  • Plasma Display Panel(PDP) is a type of flat panel display utilizing the light emission produced by gas discharge. Barrier Ribs of PDP separating each sub-pixel prevents optical and electrical crosstalks from adjacent sub-pixels. The mold for forming the barrier ribs has been newly researched to overcome the disadvantages of conventional manufacturing processes such as screen printing, sand-blasting and photosensitive glass methods. The mold for PDP barrier ribs have stripes of micro grooves transferring glass-material wall. In this paper, Stripes of grooves of which width 48${\mu}{\textrm}{m}$, depth 124$\mu\textrm{m}$ , pitch 274$\mu\textrm{m}$ was acquired by machining of single crystal silicon with dicing saw blade. Maximum roughness of the bottom of the grooves was 59.6nm Ra in grooving Si. Barrier ribs were formed with silicone rubber mold, which is transferred from grooved Si forming hard mold. Silicone rubber mold has the elasticity, which enable to accommodate the waveness of lower glass plate of PDP. The methods assisted by the microwave and UV was adopted for reducing the forming time of glass paste.