Trends of Recycling Technologies in Utilization of Coal Combustion Byproducts for Manufacturing Geopolymers through Patent and Literature Analysis (특허와 논문으로 본 석탄 연소부산물의 지오폴리머 원료화 기술 동향)

  • Lee, Sujeong;Cho, Young-Ju;Cho, Bong-Gyoo
    • Resources Recycling
    • /
    • v.23 no.2
    • /
    • pp.81-89
    • /
    • 2014
  • Approximately 8.5 million tons of fly ash and 740,000 tons of briquette ash were produced in 2010. Inefficient recycling of coal ash has been a heavy economic and environmental burden and economical coal ash utilization technologies are required to turn coal ash into valuable resources. In this study the patents and literature were analyzed to understand the present situation of coal ash recycling technologies and to promote utilization of coal ash for producing a non-sintering green cement, geopolymer. The survey was based on the open patents of USA, European Union, Japan and Korea, and the papers in SCI - indexed journals published between 1979 and 2013. Technical key words were used for data collection and noise filtering. Trends of recycling technologies in utilization of coal ash for producing geopolymers were discussed in terms of time periods, countries, companies and various forms of technologies.

Efficient repair of damaged FRP-reinforced geopolymeric columns using carbon fiber reinforced polymers

  • Mohamed Hechmi El Ouni;Ali Raza;Khawar Ali
    • Structural Engineering and Mechanics
    • /
    • v.87 no.6
    • /
    • pp.585-599
    • /
    • 2023
  • Geopolymer concrete (GC) can be competently utilized as a practical replacement for cement to prevent a high carbon footprint and to give a direction toward sustainable concrete construction. Moreover, previous studies mostly focused on the axial response of glass fiber reinforced polymer (glass-FRP) concrete compressive elements without determining the effectiveness of repairing them after their partial damage. The goal of this study is to assess the structural effectiveness of partially damaged GC columns that have been restored using carbon fiber reinforced polymer (carbon-FRP). Bars made of glass-FRP and helix made of glass-FRP are used to reinforce these columns. For comparative study, six of the twelve circular specimens-each measuring 300 mm×1200 mm-are reinforced with steel bars, while the other four are axially strengthened using glass-FRP bars (referred to as GSG columns). The broken columns are repaired and strengthened using carbon-FRP sheets after the specimens have been subjected to concentric and eccentric compression until a 30% loss in axial strength is attained in the post-peak phase. The study investigates the effects of various variables on important response metrics like axial strength, axial deflection, load-deflection response, stiffness index, strength index, ductility index, and damage response. These variables include concentric and eccentric compression, helix pitch, steel bars, carbon-FRP wrapping, and glass-FRP bars. Both before and after the quick repair process, these metrics are evaluated. The results of the investigation show that the axial strengths of the reconstructed SSG and GSG columns are, respectively, 15.3% and 20.9% higher than those of their original counterparts. In addition, compared to their SSG counterparts, the repaired GSG samples exhibit an improvement in average ductility indices of 2.92% and a drop in average stiffness indices of 3.2%.

Synchrotron X-ray diffraction study on alkali-activated slag cement and fly ash-based geopolymers (플라이 애시 지오폴리머와 활성 슬래그 시멘트 생성물의 방사광 X선 회절 실험 연구)

  • Oh, Jae-Eun;Jun, Ssang-Sun;Choi, Se-Jin;Paulo, J.M-Monteiro
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.319-320
    • /
    • 2009
  • The alkali activation products of slag, fly ash C and fly ash F were investigated using compressive strength test and synchrotron x-ray diffraction. We propose that the predominantly amorphous geopolymer formed under ambient conditions is a disordered form of one of the ABC-6 group of zeolites, which includes poly-types such as hydroxycancrinite, hydroxysodalite, chabazite, levyne or fransinite.

  • PDF

An Analysis of the Air Void Volume Image Analysis of Porous Cement Mortar Composites (Image analysis를 통한 다공성 시멘트 모르타르 복합체 내 공극량 산출)

  • Son, Dasom;Yi, Chong ku
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.211-212
    • /
    • 2021
  • This study was conducted to derive quantitative air void volume calculation techniques in various complexes with porosity. Calculation of voids in a complex is an essential factor in improving mechanical properties, and quantitative measurement techniques are needed because the environment is not constant to apply the currently used ASTM criteria. Using the analysis technique obtained through 2D image analysis, it is believed that meaningful results can be derived through Micro CT analysis results and cross-check later.

  • PDF

Strength Development of Alkali-Activated Fly Ash Exposed to a Carbon Dioxide-Rich Environment at an Early Age

  • Park, Sol-Moi;Jang, Jeong-Gook;Kim, Gwang-Mok;Lee, Haeng-Ki
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.1
    • /
    • pp.18-23
    • /
    • 2016
  • The development of a binder system with a lower carbon footprint as an alternative to Portland cement has been intensely researched. In the present study, alkali-activated fly ash exposed to carbon dioxide at an early age was characterized in compressive strength tests and by MIP, XRD and FT-IR analyses. The compressive strength of carbonated specimens experienced a dramatic increase in comparison to uncarbonated specimens. The microstructural densification of the carbonated specimens was evidenced by MIP. The XRD pattern showed peaks assigned to nahcolite, indicating that the pH was lower in the carbonated specimens. Under the carbon dioxide-rich environment, the aluminosilicate gel reached a more Si-rich state, which improved the mechanical properties of the alkali-activated fly ash.

Preparation and Characterization of the Mine Residue-based Geopolymeric Ceramics (광미를 이용한 지오폴리머 세라믹제조 및 물성)

  • Son, Se-Gu;Lee, Woo-Keun;Kim, Young-Do;Kim, Kyung-Nam
    • Korean Journal of Materials Research
    • /
    • v.21 no.9
    • /
    • pp.502-508
    • /
    • 2011
  • The goal of the present work was to investigate the development of a geopolymeric ceramic material from a mixture of mine residue, coal fly ash, blast furnace slag, and alkali activator solution by the geopolymer technique. The results showed that the higher compressive strength of geopolymeric ceramic material increased with an increase in active filler (blast furnace slag + coal fly ash) contents and with a reduction of mine residue contents. The geopolymeric ceramic had very high early age strength. The compressive strength of the geopolymeric ceramic depended on the added active filler content. The maximum compressive strength of the geopolymeric ceramic containing 20 wt.% mine residue was 141.2 MPa. The compressive strength of geopolymeric ceramic manufactured by adding mine residue was higher than that of portland cement mortar, which is 60 MPa, when cured for 28 days. SEM observation showed the possibility of having amorphous aluminosilicate gel within geopolymeric ceramic. XRD patterns indicate that the geopolymeric ceramic was composed of amorphous aluminosilicate, calcite, quartz, and muscovite. The Korea Standard Leaching Test (KSLT) was used to determine the leaching potential of the geopolymeric ceramic. The amounts of heavy metals were noticeably reduced after the solidification of mine residue with active filler.

Effect of the Heating Temperature on the Alkali-activation Reaction of Calcined Kaolin Powder (열처리 카올린 분말의 알칼리활성화 반응에 미치는 가열온도의 영향)

  • Kim, Sung Gon;Song, Tae Woong
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.6
    • /
    • pp.601-607
    • /
    • 2012
  • The alkali-activation reaction of two types of typical kaolin calcined at various lower temperatures was investigated at room temperature and at elevated temperatures. For the assessment of the reactivity, the temperature increase and the setting time of pastes prepared with calcined kaolin and sodium/potassium hydroxide solution were measured. Unlike raw kaolin, calcined kaolin samples prepared at various temperature showed an alkali-activation reaction according to the different aspects of the changes in the mineral phases. The reactivity with alkaline solutions was exceedingly activated in the samples calcined at $600-650^{\circ}C$, but the reactivity gradually decreased as the temperature increased in a higher temperature range, most likely due to the changes in the crystal structure of the dehydrated kaolin. The activation effect of the calcination treatment was achieved at reaction temperatures that exceeded $60^{\circ}C$ and was enhanced as the temperature increased. The reactivity of the calcined kaolin with an alkaline solution was more enhanced with the solution of a higher concentration and with a solution prepared from sodium hydroxide rather than potassium hydroxide.

A new geopolymeric grout blended completely weathered granite with blast-furnace slag

  • Zhang, Jian;Li, Shucai;Li, Zhaofeng;Li, Hengtian;Du, Junqi;Gao, Yifan;Liu, Chao;Qi, Yanhai;Wang, Wenlong
    • Advances in concrete construction
    • /
    • v.9 no.6
    • /
    • pp.537-545
    • /
    • 2020
  • In order to reduce the usage of cement slurry in grouting engineering and consume the tunnel excavation waste soil, a new geopolymeric grouting material (GGM) was prepared by combine completely weathered granite (CWG) and blast-furnace slag (BFS), which can be applied to in-situ grouting treatment of completely weathered granite strata. The results showed CWG could participate in the geopolymerization process, and GGM slurry has the characteristics of short setting time, high flowability, low viscosity, high stone rate and high mechanical strength, and a design method of grouting pressure based on viscosity evolution was proposed. By adjusted the content of completely weathered granite and alkali activator concentration, the setting time of GGM were ranged from 5 to 30 minutes, the flowability was more than 23.5 cm, the stone rate was higher than 90%, the compressive strength of 28 days were 7.8-16.9 MPa, the porosity were below 30%. This provides a novel grouting treatment and utilizing excavated soil of tunnels in the similar strata.

Analysis of Mechanical Properties and Micro structure of Fly Ash Based Alkali-activated Mortar (플라이애쉬 기반(基盤) 알칼리 활성(活性) 모르타르의 역학적(力學的) 특성(特性) 및 미세구조(微細構造) 분석(分析))

  • Ryu, Gum-Sung;Koh, Kyung-Taek;Chung, Young-Soo
    • Resources Recycling
    • /
    • v.21 no.3
    • /
    • pp.28-38
    • /
    • 2012
  • The purpose of this paper is to develop the alkali-activated concrete which uses 100% fly ash as a binder without any cement. The compressive strength of the mortar was examined depending on the chemical change in alkali-activator through SEM and SEM/EDS observations and the XRD analysis. It was found from the test that the higher molar concentration induced the greater effect on the initial strength, and that $Si^{4+}$ and $Al^{3+}$ were eluted relative to the compressive strength of mortar. In addition, it was confirmed that Al and Si were determined to be most influential ingredients on the microstructural development of the mortar, and that the different ingredient of the activator was almost no change in solidity from the XRD analysis.

Effect of Foaming Agent Content on the Apparent Density and Compressive Strength of Lightweight Geopolymers (발포제 함량에 따른 경량 다공성 지오폴리머의 밀도와 강도 특성)

  • Lee, Sujeong;An, Eung-Mo;Cho, Young-Hoon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.4
    • /
    • pp.363-370
    • /
    • 2016
  • Lightweight geopolymers are more readily produced and give higher fire resistant performance than foam cement concrete. Lowering the density of solid geopolymers can be achieved by inducing chemical reactions that entrain gases to foam the geopolymer structure. This paper reports on the effects of adding different concentrations of aluminum powder on the properties of cellular structured geopolymers. The apparent density of lightweight geopolymers has a range from 0.7 to $1.2g/m^3$ with 0.025, 0.05 and 0.10 wt% of a foaming agent concentration, which corresponds to about 37~60 % of the apparent density, $1.96g/cm^3$, of solid geopolymers. The compressive strength of cellular structured geopolymers decreased to 6~18 % of the compressive strength, 45 MPa of solid geopolymers. The microstructure of geopolymers gel was equivalent for both solid and cellular structured geopolymers. The workability of geopolymers with polyprophylene fibers needs to be improved as in fiber-reinforced cement concrete. The lightweight geopolymers could be used as indoor wall tile or board due to fire resistance and incombustibility of geopolymers.