• Title/Summary/Keyword: freezing and thawing of concrete

Search Result 352, Processing Time 0.028 seconds

Status and Prospect of Test Methods of Quality Silicone Water Repellent for Protecting Reinforced Concrete

  • Sun, H.Y.;Yuan, Z.Y.;Yang, Z.;Shan, G.L.;Shen, M.X.
    • Corrosion Science and Technology
    • /
    • v.16 no.3
    • /
    • pp.141-150
    • /
    • 2017
  • Impregnating with quality silicone water repellent on the concrete surface is an effective method of protecting concrete. Quality silicone water repellent has been widely used in the engineering profession because of its desirable properties such as hydrophobicity, keeping concrete breathable and preserving the original appearance of the concrete. The companies in China that produce silicone water repellent are listed. Test methods in the specifications or standards about silicone water repellent in China are summed. The test methods relative to durability of concrete impregnated with silicone water repellent (such as resistant to chloride ion penetration, resistant to alkali, resistance to freezing and thawing and weatherability etc.) and the constructive quality (such as water absorption rate, impregnating depth and the dry velocity coefficient etc.) are compared and analyzed. The results indicate that there are differences among test methods relative to different specifications with the same index and therefore, confusion has ensued when selecting test methods. All test methods with the exception of the method of water absorption rate by using a Karsten flask are not non-destructive methods or conducted in a laboratory. Finally, further research on silicone water repellent during application is proposed.

Finite element analysis of CFRP laminate repairs on damaged end regions of prestressed concrete bridge girders

  • Shaw, Ian D.;Andrawes, Bassem
    • Advances in Computational Design
    • /
    • v.2 no.2
    • /
    • pp.147-168
    • /
    • 2017
  • Over the past couple decades, externally bonded fiber reinforced polymer (FRP) composites have emerged as a repair and strengthening material for many concrete infrastructure applications. This paper presents an analytical investigation of the use of carbon FRP (CFRP) for a specific problem that occurs in concrete bridge girders wherein the girder ends are damaged by excessive exposure to deicing salts and numerous freezing/thawing cycles. A 3D finite element (FE) model of a full scale prestressed concrete (PC) I-girder is used to investigate the effect of damage to the cover concrete and stirrups in the end region of the girder. Parametric studies are performed using externally bonded CFRP shear laminates to determine the most effective repair schemes for the damaged end region under a short shear span-to-depth ratio. Experimental results on shear pull off tests of CFRP laminates that have undergone accelerated aging are used to calibrate a bond stress-slip model for the interface between the FRP and concrete substrate and approximate the reduced bond stress-slip properties associated with exposure to the environment that causes this type of end region damage. The results of these analyses indicate that this particular application of this material can be effective in recovering the original strength of PC bridge girders with damaged end regions, even after environmental aging.

Mechanical Properties of Permeable Polymer Concrete for Permeability Pavement with Recycled Aggregate and Fiber Volume Fraction (재생골재 및 섬유 혼입률에 따른 포장용 투수성 폴리머 콘크리트의 역학적 특성)

  • Sung, Chan-Yong;Kim, Young-Ik
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.52 no.1
    • /
    • pp.69-77
    • /
    • 2010
  • Research on permeable pavement like asphalt and concrete pavement with porous structure has been increasing due to environmental and functional need such as reduction of run off and flood, and increase and purification of underwater resource. This study was performed to evaluate permeability, strengths and durability of permeable polymer concrete (PPC) using recycled aggregate that is obtained from waste concrete. Also, 6mm length of polypropylene fiber was used to increase toughness and interlocking between aggregate and aggregate surrounded by binder. In the test results, regardless of kinds of aggregates and fiber contents, the compressive strength and permeability coefficient of all types of PPC showed the higher than the criterion of porous concrete that is used in permeable pavement in Korea. Also, strengths of PPC with increase polypropylene fiber volume fraction showed slightly increased tendency due to increase binder with increase of fiber volume fraction. The weight reduction ratios for PPC after 300 cycles of freezing and thawing were in the range of 1.6~3.8 % and 2.2~5.6 %, respectively. The weight change ratio was very low regardless of the fiber volume fraction and aggregates. The weight reduction ratios of PPC with fiber and aggregate were in the range of 1.3~2.7 % and 2.2~3.2 % after 13 weeks and was very low regardless of the fiber volume fraction and aggregates.

Development of Strength and Durability Properties of Latex-Modified Concrete with Rapid-Setting Cement (초속경 시멘트를 사용한 라텍스 개질 콘크리트의 강도발현 및 내구특성)

  • 최성욱;홍창우;김동호;최상릉;장홍균
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.1029-1034
    • /
    • 2001
  • The purpose of this research is to develop rapid setting cement latex modified concrete (RSLMC) which will be used to overlay bridge deck for maintaining and repairing. The main experimental variables were the types of rapid setting cement and variation of latex and antifoam agent contents were selected as admixture factor, then the properties of workability and strength development and durability properties were investigated. The results of this study show that latex content give increment of a slump due to surface tension in polymer particles and reduce unit weight of water for preservation of workability. In addition, When no and 1.6~3.2% antifoam agent were mixed, 8%, 2.0~3.8% were respectively obtained. An increasing the amount of latex produced concrete with increased flexural strength, but with slightly lower compressive strength. Rapid chloride permeability and freezing-thawing test carried out. As a results, according to increment of containing ratio antifoamer, strength of RSLMC increase, permeability showed lower value than ignorable 100 coulombs. Also, in the case of more than antifoamer 1.6%, the relativity dynamic modulus is mantained more than 90%, but in case of 0, 5%, it decrease. In consequence, with the view of strength and workability of RSLMC, it is considered that appropriate content ratio of antifoam agent and latex solid are respectively 1.6% by latex weight, 15% by cement weight.

  • PDF

Influence of Admixtures on Strengths and Freezing and Thawing Resistance of Cement Mortar for Precast Products (혼화재료가 공장제품용 시멘트 모르타르의 강도 및 동결융해 저항성에 미치는 영향)

  • 한천구;신병철;김기철;이상태
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.3
    • /
    • pp.11-19
    • /
    • 2000
  • It has been reported that few manufacturers of cement mortar for precast products use chemical and mineral admixture due to the absense of restrictions related to the application of admixture and the poor manufacturing facilities. Therefore, this paper is intended to contribute to the improvement of quality by investigating the properties of cement mortar for precast products using fly ash, blast furnace slag and AE water reducing agent. According to the test results. it was found that the cement mortar products using fly ash and AE water-reducing agent had better qualities than those of ordinary portland cement.

Flexural and Cracking Characteristics of Concrete Beams Exposed to Freeze-Thaw Cycles after Patch-Repaired with SHCC (SHCC로 단면 복구후 동결융해에 노출된 콘크리트 보의 휨 및 균열특성)

  • Yun, Hyun-Do;Kim, Sun-Woo;Jeon, Ester;Lee, Young-Oh;Jang, Kwang-Soo;Park, Whan-Shin
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.21-22
    • /
    • 2009
  • This paper presents the results of an experimental study on flexural behavior and cracking process of concrete beams subjected to cycles of freezing and thawing after patch-repaired with strain-hardening cement composites (SHCCs). The SHCCs were reinforced with hybrid 0.75% PVA and 0.75% PE fibers. Experimental testing of concrete beams patch-repaired with SHCCs revealed that the SHCC patch-repair system without freeze thaw (FT) exposure showed average 3.31 times increased load carrying capacity and for beams exposed to 300 FT cycles, load carrying capacity increased up to 2.42 times. Cracking damage of SHCC patch-repaired beams mitigated compared to plain concrete beams but this trend decreased under FT exposure.

  • PDF

Evaluation on Compressive Strength of Mortar and Concrete at Early Age Using Variable Cement and Self-heating Binder (시멘트 산지 및 자기발열분체 사용에 따른 모르타르 및 콘크리트의 저온에서의 압축강도성능 평가)

  • Hong, Seok-Beom;Kim, Woo-Jae;Yoo, Jo-Hyeong
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.152-153
    • /
    • 2016
  • In this research, we evaluate the performance for preventing frost damage at early age of mortar using variable cement and self-heating binder. Purpose of final research is preventing freezing and thawing by making the compressive strength 5MPa in 3days below zero temperature without heat curing. We compare the compressive strength of mortar and concrete using variable cements and self-heating binder in low temperature.

  • PDF

Enhanced Durability Performance of Polymer Modified Cement Composites for Concrete Repair Under Combined Aging Conditions (복합열화 환경을 받는 콘크리트 시설물을 위한 보수용 폴리머 시멘트 복합체의 내구성능 향상에 관한 연구)

  • Won, Jong-Pil;Park, Chan-Gi
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.47 no.6
    • /
    • pp.27-34
    • /
    • 2005
  • The purpose of this study is to improve the durability performance of polymer modified cement composites for repair of concrete under combined aging conditions. The experimental procedure was divided into three parts. First, the replacement level of mineral admixtures in polymer modified cement composites were determined in an experimental study based on a Box Behnken design. Second, the flow value, compressive strength and chloride permeability test of sixteen types of mixtures were conducted. Test results show that the polymer modified cement composites were effected on the improvement of the compressive strength and permeability performance. Third, the effects on the replacement level of silica fume mixture was evaluated by the compressive strength, chloride permeability, chemical resistance and repeated freezing and thawing cycles test. They demonstrated that the polymer modified cement composites using mixture of silica fume, fly ash, and blast furnace slag improved the durability performance.

A Experimental Study on The Durability and Mechanical of Permanent Form Mortar (비탈형영구 거푸집용 모르터의 내구성 및 역학적 특성에 관한 실험적 연구)

  • 김우재;표순주;임남기;김형남;김성식;이영도;정상진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.04b
    • /
    • pp.731-736
    • /
    • 1998
  • The dynamics and Durability of Permanent Form Mortar were observed. The results were as the followings. To construct New permanent form, this study constructed permanent form with fiber mortar. In this course glass fiber and polymer, fine aggregate were substituted with river sand and crush sand. To understand material quality effect, flexible mortar and inflexible mortar were tested. According to the microstructure of polymermatrix test by SEM, higher density by Co-matrix effect from polymer addiction was observed. This is considered to increase acid-resistanc, impact proof strenght. In the test of durability of freezing and thawing, polymer mortar was proved to be water proof. It seems to be improved in its characteristics in proportion to increasing W/C ratio. When the W/C ratio is 30%, it is most effective.

  • PDF

A Study on the Freeze-Thaw Resistance of Water-permeable Concretes (투수성 콘크리트의 동결융해 저항성에 관한 연구)

  • 은재기;김완기;소양섭
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10a
    • /
    • pp.433-438
    • /
    • 2000
  • The purpose of this study is to examine the resistance of water-permeable concretes to freezing and thawing action. The water-permeable concretes with cement-aggregate ratio of 1:5.5(by weight) and two kinds of admixture content [SP : superplasticizer(0, 1.0%), HPAE : high performance air entraining agent(0.5, 1%)] used OPC(ordinary portland cement) as binder were prepared, and then tested for relative dynamic modulus of elasiticity, mass change, length change and durablity factor. It's been concluded from the test results that the superior relative dynamic modulus of elasiticity and durability factor of water-permeable concretes were obtained at superplaciticizer 1.0% after 300 cycles. The water-permeable concretes used superplasiticizer 1.0% having relative durability factor of 88% after 300 cycles.

  • PDF