• 제목/요약/키워드: fracture strength marginal gap

검색결과 5건 처리시간 0.018초

Marginal accuracy and fracture strength of Targis/Vectris Crowns prepared with different preparation designs

  • Song, Ho-Yong;Cho, Lee-Ra
    • 대한치과보철학회지
    • /
    • 제38권6호
    • /
    • pp.791-799
    • /
    • 2000
  • Statement of problem. Targis/Vectris restorations provide excellent esthetics. Marginal accuracy is significantly influenced by the preparation design. There were no studies to examine the effect of preparation design on the marginal discrepancy and fracture strength of Targis / Vectris crowns. Purpose. This study evaluated the marginal accuracy before and after cementation, and the fracture strength of FRC/Ceromer(Targis / Vectris) crowns according to different preparation design. Material and method. Three metal dies with different convergence angles($6^{\circ},\;10^{\circ},\;15^{\circ}$) were prepared. Total 30 (10 for each angle) Targis/Vectris crowns were made. The restorations were evaluated for adaptation of the margin before and after cementation, then were compressively loaded to failure. Fracture surfaces of the crowns were examined using a SEM. Results. The mean marginal gap was $49{\yen}m\;for6^{\circ},\;55{\S}>for\;10^{\circ}\;and\;70{\S}>for\;15^{\circ}$ and in clinically acceptable level. The mean marginal gap increased significantly after cementation. The increasing amount during cementation was the largest in the $6^{\circ}$ group. The crowns on 60 convergence angle had a significantly higher fracture strength than the crowns on $15^{\circ}$ angle. Mean fracture strength of total crowns regardless of convergence angle was 1390 N, which was higher than all-ceramic crowns. SEM observation showed two-mode fracture pattern. Conclusion. From the results of this study, all of the FRC/Ceromer crowns had clinically acceptable marginal accuracy and could withstand the bite force. Moreover, less convergent angle than all-ceramic crown might be recommended for preparation procedure.

  • PDF

MARGINAL FIDELITY AND FRACTURE STRENGTH OF IPS EMPRESS $2^{(R)}$ CERAMIC CROWNS ACCORDING TO DIFFERENT CEMENT TYPES

  • Cho Hyun-Ok;Kang Dong-Wan
    • 대한치과보철학회지
    • /
    • 제40권6호
    • /
    • pp.545-559
    • /
    • 2002
  • There has been increasing use of IPS Empress $2^{(R)}$ owing to easy fabrication method, high esthetics similar to natural teeth, good marginal accuracy, and sufficient fracture strength. However, in clinical application, although a luting agent and the tooth cementation bonding procedure influence the marginal accuracy and fracture strength restoration, there has been a controversy in the selection of proper luting agent. This study was to measure the marginal fidelites and fracture strength of IPS Empress crowns according to three cement types, Protec $cem^{(R)}$, Variolink $II^{(R)}$ and Panavia $21^{(R)}$. After construction of 12 experimental dies for each group, IPS Empress $2^{(R)}$ crowns were fabricated and luted the metal master die prepartion of the maxillary right premolar. Marginal gaps before cementation and after cementation were measured. Buccal incline on the functional cusp of specimens were loaded until the catastrophic failure and fracture strength was measured. The results of this study were as follows: 1. The range of gap was $34.04{\pm}4.84{\mu}m$ before cementation and $37.88{\pm}5.00{\mu}m$ after cementation, which showed significant difference by paired t-test (p<0.05). The difference in the results from marginal accuracy according to measuring point proved to be not statistically significant by two-way ANOVA test (p>0.05). 2. The difference in the results from marginal accuracy according to three cement types Proved that The Variolink $II^{(R)}$ cement group had the least gap, $35.43{\pm}5.03{\mu}m$, and showed superior marginal accuracy while there existed statistic significance in Protec $cem^{(R)}$ cement group, $39.06{\pm}4.41{\mu}m$ or Panavia $21^{(R)}$ cement group, $39.16{\pm}4.39{\mu}m$ by two-way ANOVA test & multiple range test (p<0.05). 3. The difference in the results from fractures strength testing according to three cement type groups proved to be statistically significant (p<0.05). The Variolink $II^{(R)}$ cement group shows highest fracture strength of $1257.33{\pm}226.77N$, Panavia $21^{(R)}$ cement group has $1098.08{\pm}138.45N$, and Protec $cem^{(R)}$ cement group represents the lowest fracture strength of $926.75{\pm}115.75N$. 4. Three different cement groups of different components showed acceptable marginal fidelity and fracture strength. It is concluded that IPS Empress $2^{(R)}$ crowns luted using Variolink $II^{(R)}$ cement group had stronger fracture strength and smaller marginal gap than the other cement groups. Although Variolink $II^{(R)}$ resin cement seemed acceptable to clinical applications in IPS Empress $2^{(R)}$ system, the IPS Empress $2^{(R)}$ system still requires long-term research due to the lack of data in clinical applications.

접착재의 종류에 따른 In-Ceram 도재관의 변연적합도와 파절강도에 관한 연구 (MARGINAL FIDELITY AND FRACTURE STRENGTH OF IN-CERAM CROWNS ACCORDING TO VARIOUS RESIN CEMENTS)

  • 임주환
    • 대한치과보철학회지
    • /
    • 제36권6호
    • /
    • pp.888-899
    • /
    • 1998
  • In-Ceram system is one of contemporary esthetic all ceramic restorations and has relatively high flexural strength. The purpose of this study was to evaluate the marginal fidelity according to type of resin cement and measuring position, and to evaluate fracture strength according to type of resin cement. In this study, twenty seven In-Ceram crowns were fabricated on the metal master die of prepared maxillary right central incisor and devided into three groups. All specimens were cemented with Panavia 21 (group PV), Super-bond (group SB) and Lute-it (group LI) on the metal master die. After cementation, specimens were measured marginal gap between the margin of the In-Ceram crown and the finishing line of metal master die by using a stereomicroscope (SZ-ST, Olympus, Japan). Marginal gaps were recorded at the labial, lingual, mesial and distal measuring points on the metal master die. For the mesurement of fracture strength, lingual surfaces of cemented specimens were loaded at a distance of 1mm from incisal edge by using the Autograph S-2000 (Shimadzu, Japan). The results of marginal fidelity and fracture strength were statistically analyzed with the SPSS version 8.0 programs. The results of this study were as follows: 1. In comparison of marginal fidelity according to the measuring points, there was no significant difference. 2. The marginal fidelity according to the type of resin cement was decreased in order of group $LI\;(63.75{\mu}m),\;SB\;(77.78{\mu}m),\;PV\;(86.53{\mu}m)$, and there was significant difference between group LI and PV (p<0.05). 3. The fracture strength according to the type of resin cement was showed descending order of group $LI\;(60.00kg/cm^2),\;SB\;(56.80kg/cm^2),\;PV\;(56.11kg/m^2)$, but there was no significant difference.

  • PDF

OPTIMAL PRESSABLE CERAMIC 금관의 변연형태에 따른 변연적합도와 파절강도에 관한 연구 (Marginal Fidelity and Fracture Strength of OPTIMAL PRESSABLE CERAMIC Crown according to Margin Types)

  • 이주석;김기석
    • 구강회복응용과학지
    • /
    • 제16권1호
    • /
    • pp.13-25
    • /
    • 2000
  • Optimal Pressable Ceramic is one of the all-ceramic restorations with a shaded translucent pressed core and layering porcelains. The purpose of this study was to evaluate the marginal fidelity according to margin types and measurement sites, and to evaluate fracture strength according to margin types. Twenty seven OPC crowns made according to 3 types of cervical finishing lines were used in this study. Marginal gaps were measured before and after cementation. A Steromicroscope(SZ-ST(R), Olympus, Japan) was used to measure the space between the margin of OPC crown and the finishing line of metal model. Marginal gaps were measured at the labial, mesial, lingual and distal site, which were demonstrated in advance. Fracture strength testing was carried out using an Instron(Model M100EC, Mecmesin, England) at a cross head speed of 5 mm/min. All crowns were loaded until catastrophic failures occurred. The result were as follow: 1. In comparison according to variable margin before cementation, the marginal gap were increased in chamfer margin($47.50{\pm}18.39{\mu}m$), $120^{\circ}$shoulder margin ($55.21{\pm}14.4{\mu}m$) and $90^{\circ}$shoulder margin($71.18{\pm}13.30{\mu}m$) in ascending order, and there were significant differences between chamfer margin and $90^{\circ}$shoulder margin, $120^{\circ}$shoulder margin and between $120^{\circ}$shoulder margin and $90^{\circ}$shoulder margin respectively(p<0.05). 2. In comparison according to variable margin after cementation, the gap discrepancies were increased in chamfer margin($60.78{\pm}30.37{\mu}m$), $120^{\circ}$shoulder margin($66.67{\pm}11.18{\mu}m$) and $90^{\circ}$shoulder margin($85.78{\pm}17.23{\mu}m$) in ascending order, but there was significant difference only between chamfer margin and $90^{\circ}$shoulder margin(p<0.05). 3. Labio-lingual points showed a better marginal fidelity than that of proximal point(p<0.05). 4. Chamfer margin($48.76{\pm}8.45kgf$) showed higher fracture strength than $120^{\circ}$ shoulder margin($40.57{\pm}7.90kgf$) and $90^{\circ}$ shoulder margin(32.7.90kgf) (p<0.05), but there was significant difference only between chamfer margin and $90^{\circ}$ shoulder margin(p<0.05).

  • PDF

A new manufacturing method of all ceramic restoration using alumina tape and presentation of clinical cases

  • Oh, Nam-Sik;Kim, Eui-Seong;Lee, Keun-Woo;Han, Jung-Suk;Kim, Dae-Joon;Lee, Myung-Hyun
    • 대한치과보철학회지
    • /
    • 제38권6호
    • /
    • pp.800-805
    • /
    • 2000
  • In an effort to facilitate fabrication procedure of all ceramic crowns, a novel preparation method for all ceramic crown using alumina tape was developed. The alumina tape having a uniform thickness was cast by using Doctor blade method. The physical properties of newly introduced alumina tape has biaxial flexure strength of $500\sim600MPa$. The value of toughness is $3.18\sim3,28MPa.m^{1/2}$ which corelates with fracture and the linear shrinkage rate of the alumina tape is 0.44% during core production. The marginal fitness of the alumina tape all-ceramic restoration with $90{!`}$shoulder margin had average marginal discrepancy at $78.3{\S}$ > and average marginal gap at $44.4{\S}$ >. At the marginal preparation of $135{!`}$deep chamfer, the average marginal discrepancy at $82.1{\S}$ > and the average marginal gap at $40.2{\S}$ > had been reported. This fabrication procedure of all ceramic crowns with alumina tapes is easier and less technical sensitive for dental technicians. After restoration with new all ceramic crowns we followed the patients 2 years later, there were no complications as porcelain fractures or periodontal disease. We had good esthetic clinical results with new all ceramic crowns.

  • PDF