• Title/Summary/Keyword: flexure strength

Search Result 304, Processing Time 0.028 seconds

The Improvement of Biaxial Flexure Test (BFT) Method for Determination of the Biaxial Flexure Tensile Strength of Concrete (콘크리트 이방향 휨인장강도 결정을 위한 이방향 휨인장강도 시험법 개선)

  • Kim, Jihwan;Zi, Goangseup;Oh, Hongseob
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.31 no.5A
    • /
    • pp.389-397
    • /
    • 2011
  • In this study, an experiment for the biaxial behavior of specimens was carried out to identify whether the isotropic flexure tensile stress of concrete in the BFT method is feasible. Another experiment for the improvement of the BFT method was conducted to ensure the isotropic flexure tensile stress of BFT specimens during the test. In addition, the biaxial flexure strength of concrete given by the improved BFT method was compared to the uniaxial flexure strength by the four-point bending test. Test results show that the isotropic flexure tensile stress of concrete using the BFT method was highly influenced by the surface conditions and warping of the specimens. Using improved BFT method, we could obtained the isotropic flexure tensile stress of concretes. The biaxial flexure strength of BFT was about 32% greater than the uniaxial flexure strength of the four-point bending test. In the experiment, with the smaller scatter, the improved BFT method gave a reliable biaxial flexure strength like the four-point bending test.

Flexure Strength of Glass-infiltrated Zirconia Complex (유리침투 지르코니아 복합체의 굴곡 강도)

  • Kim, Sa-Hak
    • Journal of Technologic Dentistry
    • /
    • v.31 no.2
    • /
    • pp.9-14
    • /
    • 2009
  • In this study, to improve the flexure strength of Zirconia, on the Zirconia pellet surface measure the flexure strength to melt or permeate the Alumina (Vita Zahnfabrik, Bad Sachkingen, Germany) of private used In-Cream and observe by Scanning election microscope. In the control group(3Y-TZP group), the average of flexure strength was 1623.7MPa, and in the experimental group(Glass-infiltrated 3Y-TZP group) was 1800.2MPa. As a result of observing the interface between glass and zirconia with a scanning election microscope, it was showed that the glass dissolves to permeate into the surface of zirconia, so filled the zirconia with particles.

  • PDF

Manufacture and Structural Test of the Small-scaled Composite Hingeless Hub Part for Helicopter (헬리콥터용 축소 복합재료 힌지없는 허브 부품 제작 및 구조 시험)

  • Kim, Deog-Kwan;Hong, Dan-Bi;Kee, Young-Jung;Rhee, Wook;Lee, Myeong-Kyu
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2003.10a
    • /
    • pp.119-122
    • /
    • 2003
  • This report describes the procedure of detailed design and structural test for the composite flexure which is a part of the hingeless hub system. First, stacking sequence design for composite flexure was done, and structural analysis by using NASTRAN was made to verify structural stability and safety. Using FPS installed at KIMM, composite flexure was laid up and cured using a autoclave. Before rotor ground test, the basic structural tests such as a bench test, tensile strength test and shear strength test, for flexure, were accomplished. Through replacing existing metal hub part with new fabricated composite flexure, improvement of aeroelastic stability and weight reduction were achieved. This result will be applied to composite rotor system design fur helicopter.

  • PDF

Flexure Strength of Various Colored and Uncolored Zirconia Ceramics for All-Ceramic Restoration (전부도재수복물을 위한 유색 및 무색 지르코니아 세라믹의 굴곡강도)

  • Oh, Sang-Chun;Lee, Hae-Hyoung;Shin, Mee-Ran;Lee, Il-Kwon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.23 no.2
    • /
    • pp.119-130
    • /
    • 2007
  • Purpose: This investigation was designed to estimate the flexure strength, density, and microstructure of the colored and uncolored zirconia oxide ceramics for fixed partial denture. Material and Methods: LAVATM All Ceramic(3M-ESPE, USA), Cercon Smart Ceramic(Dentsply, USA), and Z-match Ceramic(DentAim, Korea) were used for this study. All specimen was fabricated by ASTM C1161. After preparing $25{\times}2{\times}1.5mm$ of rectangular column and sitting rectangular column on universal test machine (UTM), external supporting point distance is 20.0 mm, internal supporting point distance is 10.0 mm. Specimen was loaded with 0.2 mm/min of cross head speed until fracture and at the time of broken of specimen, measuring loading value with PC software. Results: The results were obtained as follows: 1. Flexure strength of uncolored zirconia was higher than that of colored zirconia. 2. In uncolored zirconia, flexure strength of LAVATM Ceramic was more higher than the other ceramics, and it showed statistical difference between LAVATM Ceramic and Cercon Smart Ceramic (P<0.05). 3. In colored zirconia, flexure strength of LAVATM Ceramic was more higher than the other ceramics too, but they did not show statistical difference (p>0.05). 4. In Weibull analysis, Characterastic strength was showed highest value to uncolored LAVATM Ceramic and lowest value to Z-match ceramic, and Weibull modulus(m) of uncolored zirconia was higher than that of colored zirconia. 5. In XRD analysis, all group except Z-match showed high peak of t-ZrO2 but they did not show m-ZrO2. Colored zirconia group showed lower peak of t-ZrO2 than that of uncolored zirconia group.

EFFECTS OF AGING AND THERMAL CYCLING ON THE BIAXIAL FLEXURE STRENGTH OF VENEERING RESIN COMPOSITES FOR CROWN (시효처리와 thermal cycling이 치관전장용 복합레진의 2축굽힘강도에 미치는 영향)

  • Jeong, Gwan-Ho;Ha, Il-Soo;Song, Kwang-Yeob
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.5
    • /
    • pp.597-606
    • /
    • 1999
  • This study was performed to evaluate the effect of aging and thermal cycling on the biaxial flexure strength of low commercially available veneering resin composites for crown(Dentacolor : DC, Artglass : AG, Esternia : ET and Targis : TG). Disc specimens were fabricated in a teflon mold giving 12mm in diameter and 1mm in thickness. All samples were divided into 4 groups. Group 1 was dried in a dessicator at $25^{\circ}C$ for 30 days. Group 2 was immersed in distilled water at $37^{\circ}C$ for 30 days. Group 3 was immersed in distilled water at $65^{\circ}C$ for 30 days. Group 4 was subjected to 10,000 thermal cycles between $5^{\circ}C\;and\;55^{\circ}C$, and the immersion time in each bath was 15 seconds per cycle. Biaxial flexure test was conducted using the ball-on-three-ball method at the cross head speed of 0.5mm/min and fracture surfaces were observed with scanning electoron microscope. The results obtained were summarized as follows; 1. Weibull modulus values, except for the AG group, decreased after thermal cycling treatment. 2. Biaxial flexure strength values of aging group at $37^{\circ}C$ were the lowest in all sample groups. Except for the DC group, strength values were significantly decreased for the drying group. 3. After thermal cycling test, the highest value of biaxial flexure strength of 188.8 MPa was observed in the ET group and the lowest value of 73.2 MPa was observed in the DC group. The strength values showed the significant differences in each group (p<0.05). 4. Observation of surfaces after thermal cycling test revealed the ditching in the part of surrounding large fillers.

  • PDF

FLEXURE STRENGTH AND COLOR CHANGE OF REUSED IPS EMPRESS 2 (반복 사용된 IPS Empress 2의 굽힘강도와 색변화에 관한 연구)

  • Song Young-Kuk;Kim Yu-Lee;Kim Sung-Hoon;Ahn Hee-Young;Jin Tai-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.1
    • /
    • pp.71-80
    • /
    • 2003
  • Development of new ceramic and esthetic need of patient increased the use of ceramic restorations. The purpose of this study was to confirm the possibility of recycling for IPS Empress2 which has a lot of advantages in esthetics. 1st, 2nd and 3rd pressed disc-shaped($10{\times}1.5mm$) IPS Empress 2 specimens were made with IPS Empress ingot(shade 200, Ivoclar, Liechtenstein) and pressing furnace(IPS Empress EP 500, Ivoclar, Liechtenstein). Flexure strength was measured with universal testing machine(Zwick 145641, Zwick, Germany), and color change and staining resistance of specimens were evaluated with colorimeter (Model TC-6FX, Tokyo Denshoku Co., Japan). The followings were drawn from this study : 1. Flexure strength of the 1st, the 2nd, and the 3rd pressed specimens showed 236.78 MPa. 247.16MPa, and 220.72MPa, respectively. Flexure strength of the 2nd pressed specimens was higher than others, but there's no statistical difference between them. 2. The color difference between the 1st and the 2nd pressed specimens was 3.25, and that between the 1st and the 3rd pressed specimens was 3.63(P<0.05). 3. The color change after staining of the 1st, the 2nd. and the 3rd pressed specimens were 1.43, 2.64, and 1.45, respectively. In this study, reused IPS Empress 2 specimens showed insignificant change of flexure strength and stain resistance, but they showed some color change according to reuse. From this results, the limited possibility of reuse for IPS Empress 2 could be considered.

THE COMPARISON OF RELATIVE RELIABILITY ON BIAXIAL AND THREE POINT FLEXURAL STRENGTH TESTING METHODS OF LIGHT CURING COMPOSITE RESIN (광중합형 레진의 3점 굴곡 강도와 이축 굴곡 강도 측정 방법에 대한 상대적 신뢰도의 비교)

  • Seo, Deog-Gyu;Roh, Byoung-Duck
    • Restorative Dentistry and Endodontics
    • /
    • v.31 no.1
    • /
    • pp.58-65
    • /
    • 2006
  • The possibility of applying a hi-axial flexure strength test on composite resin was examined using three point and hi-axial flexure strength tests to measure the strength of the light-cured resin and to compare the relative reliability using the Weibull modulus. The materials used in this study were light-curing restorative materials, $MICRONEW^{TM},\;RENEW^{(R)}$ (Bisco, Schaumburg, USA). The hi-axial flexure strength measurements used the piston-on-3-ball test according to the regulations of the International Organization for Standardization (ISO) 6872 and were divided into 6 groups, where the radius of the specimens were 12mm (radius connecting the 3-balls: 3.75mm), 16 mm(radius connecting the 3-balls: 5mm), and the thickness were 0.5mm, 1mm, 2mn for each radius. The hi-axial flexure strength of the $MICRONEW^{TM}\;and\;RENEW^{(R)}$ were higher than the three point flexure strength and the Weibull modulus value were also higher in all of the bi-axial flexure strength groups, indicating that the hi-axial strength test is relatively less affected by experimental error. In addition, the 2 mm thick specimens had the highest Weibull modulus values in the hi-axial flexure strength test, and the $MICRONEW^{TM}$ group showed no significant statistical difference (p>0.05). Besides the 2mm $MICRONEW^{TM}$ group, each group showed significant statistical differences (p<0.05) according to the thickness of the specimen and the radius connecting the 3-balls. The results indicate that for the 2mm group, the hi-axial flexure strength test is a more reliable testing method than the three point flexure strength test.

Simplified design formula of slender concrete filled steel tubular beam-columns

  • Chung, Jinan;Matsui, Chiaki;Tsuda, Keigo
    • Structural Engineering and Mechanics
    • /
    • v.12 no.1
    • /
    • pp.71-84
    • /
    • 2001
  • The objective of this paper is to develop a simplified method that could predict the strength of concrete filled steel tube (CFT) columns applicable to high strength material under combined axial compression and flexure. The simplified method for determining the strength of CFT columns is based on the interaction curve of the section approached by a polygonal connection of the points. These points are determined by using symmetrical properties of the CFT section. For each point, a simple equation is proposed to determine the strength of the slender columns under compression and flexure. The simple equation was adjusted with results of elasto-plastic analysis results. Validation of the simplified method is undertaken by comparison with data from the test conducted at Kyushu University. These results confirm the fact that the simplified method could accurately and reliably predict the strength of CFT columns under combined axial compression and flexure.

Mechanical Properties of Zirconia Reinforced Glass-Ceramic (지르코니아 강화형 Glass-Ceramic의 기계적 성질)

  • Park, Eun-Eui;Dong, Jin-Keun;Lee, Hae-Hyoung;Song, Ki-Chang;Oh, Sang-Chun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.17 no.3
    • /
    • pp.199-204
    • /
    • 2001
  • This study was to investigate the reused possibility of zirconia reinforced glass-ceramic(IPS Empress Cosmo ceramic) with sprue button in the flexure strength and fracture toughness. 40 disk-shaped ceramic specimens (20 specimens: as-pressed material; 20 specimens: reused material) with approximately 1.7 mm thickness and 15 mm diameter were prepared by "lost wax" technique. The remnants(sprue buttons) were used for repressing. The surface treatments for the discs were gradually abraded with 320, 800, 1200, and 2000 grit SiC sandpaper. The specimens were evaluated their flexure strength with the biaxial flexure jig(ball-on-three balls) and their fracture toughness with Vickers Indentation-microfracture test. The Weibull moduli were calculated for biaxial flexural strength. The mean flexure strength and fracture toughness of each group were $122.2{\pm}18.3MPa$, $1.00{\pm}0.09MPa{\cdot}m^{0.5}$ (as-pressed ceramics), and $122.2{\pm}20.3MPa$, $1.01{\pm}0.10MPa{\cdot}m^{0.5}$ (reused ceramics). There were no significant differences in the strength and the fracture toughness between the as-pressed and the reused IPS Empress Cosmo ceramic (P>0.05). This implied zirconia reinforced glass-ceramic(IPS Empress Cosmo ceramic) could be used one more time by reusing of sprue button in the flexure strength and fracture toughness.

  • PDF

Evaluation of Residual Strength in Damaged Brittle Materials (취성재의 손상후 잔류강도 평가)

  • Oh, Sang-Yeob;Shin, Hyung-Seop;Suh, Chang-Min
    • Proceedings of the KSME Conference
    • /
    • 2001.11a
    • /
    • pp.137-142
    • /
    • 2001
  • In structural applications, brittle materials such as soda-lime glasses and ceramics are often subjected to multiaxial stress. Brittle materials with crack or damaged by foreign object impacts are abruptly fractured from cracks, because of their properities of very high strength and low fracture toughness. But in most cases, the residual strength has been derived from tests under uniaxial stress such as a 4-point bend test. The strengths under multiaxial stresses might be different from the strength. In comparable tests, the residual strength under biaxial stress state by the ball-on-ring test was greater than that under the uniaxial one by the 4-point bend test. In the case that crack having 90deg. to loading direction, the ratio of biaxial to uniaxial flexure strength was 1.12. At a different crack angle to loading direction when it was evaluated by the 4-point bend test, the residual strength was different and the ratio of 45deg. to 90deg. was 1.16.

  • PDF