  • Portland cement concrete is made with coarse aggregate, fine aggregate, portland cement, water and, in some cases, selected chemical admixture such as air-entraining agents, water reducer, superplasticizer, and so on, and mineral admixture such as fly ash, silica fume, slags, etc. Typically, in the concrete, the coarse aggregate and fine aggregate will occupy approximately 80 percent of the total volume of the finished mixture. Therefore, the coarse and fine aggregates affect to the properties of the portland cement concrete. As the deposits of natural sands have slowly been depleted, it has become necessary and economical to produce crushed sand(manufactured fine aggregate). It is reported that crushed sand differs from natural sands in gradation, particle shape and texture, and that the content of micro fines in the crushed sand affect to the quality of the portland cement concrete. Therefore, the purpose of this paper is to investigate the characteristics of fresh and hardened concrete with higher micro fines. This study provides a firm data to apply crushed sand with higher micro fines.

  • PDF

균열주입재로서 초미립자 시멘트의 이용 (Use of Ultra Fine Cement Particles as Crack Repair Materials)

  • 이종열;정연식;이웅종;양승규;채재홍
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회 논문집(II)
    • /
    • pp.1205-1210
    • /
    • 2000
  • In this research we made the mean cement particle size 4 $\mu\textrm{m}$ which can penetrate even minor cracks based on the theory of J.K. Michel who reported particles can penetrate the crack of width up to 3 times of maximum particle size. The cement slurries were produced by adding super plasticizer. The slurries were tested with slurry characterization methods and its rheological properties were characterized. The early hydrated phenomena of ultra fine cement were observed by SEM, XRD and DSC during 24 hours. Mechanical properties of hardened slurry with JIS molds were also tested in 3, 7 and 28 days. The cracked specimens which were repaired with slurries produced various conditions were tested after 3, 7 and 28 days curing in the air and adhesion properties were characterized.

입도분급 미분 시멘트를 이용한 조강형 콘크리트의 현장실용화에 관한 연구 (A study on the Practical Application of High Early Strength Type Concrete Using Fine Particle Classifying Cement)

  • 최성용;노동현;김기훈;김경민;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2008년도 춘계 학술논문 발표대회
    • /
    • pp.117-121
    • /
    • 2008
  • This study investigates practical application of high early strength type concrete using fine particle classifying cement, and the results are summarized as following. The replacement use of FC 30% did not great influence on concrete mix, therefore mixing without additional SP and AE was available using equal mix with OPC. The ratio of increasing temperature by heat of hydration was similar with OPC, and the compressive strength was over then 5MPa at -28℃ outside temperature on 2nd day. Therefore, it is considering that the first purpose, the effect of shortening terms of work by early demolding, will be available. The rebound rate of type "P" schumidt hammer was relative with compressive strength, and the rebound rate for verifying 5MPa of compressive strength was estimated about 55 considering rate of safety. Therefore, assuming demolding date is available efficiently.

  • PDF

Laboratory tests for studying the performance of grouted micro-fine cement

  • Aflaki, Esmael;Moodi, Faramarz
    • Computers and Concrete
    • /
    • 제20권2호
    • /
    • pp.145-154
    • /
    • 2017
  • In geological engineering, grouting with Portland cement is a common technique for ground improvement, during which micro-fine cement is applied as a slurry, such that it intrudes into soil voids and decreases soil porosity. To determine the utility and behavior of cements with different Blaine values (index of cement particle fineness) for stabilization of fine sand, non-destructive and destructive tests were employed, such as laser-ray determination of grain size distribution, and sedimentation, permeability, and compressive strength tests. The results of the experimental study demonstrated a suitable mix design for the upper and lower regions of the cement-grading curve that are important for grouting and stabilization. Increasing the fineness of the cement decreased the permeability and increased the compressive strength of grouted sand samples considerably after two weeks. Moreover, relative to finer (higher Blaine value) or coarser (lower Blaine value) cements, cement with a Blaine value of $5,100cm^2/g$ was optimal for void reduction in a grouted soil mass. Overall, study results indicate that cement with an optimum Blaine value can be used to satisfy the designed geotechnical criteria.

미분의 효과적인 이용에 관한 연구 (Effective Use of Micro Fines)

  • 백신원
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.73-78
    • /
    • 2001
  • Portland cement concrete is made with coarse aggregate, fine aggregate, portland cement, water and, in some cases, selected chemical admixtures such as air-entraining agents, water reducer, superplasticizer, and so on, and mineral admixtures such as fly ash, silica fume, slags, etc. Typically, in the concrete, the coarse aggregate and fine aggregate will occupy approximately 80 percent of the total volume of the final mix. Therefore, the coarse and fine aggregates affect to the properties of the portland cement concrete. As the natural sands are drained, it is necessary and economical to utilize crushed sands(manufactured fine aggregate). It is reported that crushed sands differ from natural sands in gradation, particle shape and texture, and the micro fines in the crushed sands affect to the quality of the portland cement concrete. Therefore, the purpose of this paper is to investigate the characteristics of fresh and hardened concrete with high content of micro fines. This study provides firm data for the use of crushed sands with higher micro fines.

  • PDF

잔골재 종류변화가 시멘트 모르터의 기초적 특성에 미치는 영향 (Influence of Fine Aggregate Kinds on Fundamental Properties of Cement Mortar)

  • 김성환;배장춘;송승헌;차천수;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.85-88
    • /
    • 2006
  • This study investigated influence of fine aggregate types on fundamental properties of cement mortar. Test showed that concrete using lime stone crushed fine aggregate(L) exhibited the most favorable fluidity due to grain shape and particle distribution, and next was blending aggregate miting L and G, blending aggregate mixing L and N, granite crushed fine aggregate(G), natural fine aggregate(N) in an order. Concrete using N had the highest air content and L was the smallest value because of the effective filling performance by continuos particle distribution. Compressive, tensile and flexural strength of all concrete using L had the highest value due to the smallest value of air content. It is also found that concrete using L resulted in decrease of drying shrinkage length change ratio.

  • PDF

시멘트 페이스트에서 유동성과 입도분포와의 관계 (The Relationship between Rheology Properties and Particle size distribution in Cement paste)

  • 황해정;이승헌;이원준;김원기
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.721-724
    • /
    • 2006
  • In this study, particle size distribution of cement powder system were adjusted using the blast furnace slag powder, Blaine $2250cm^2/g\;and\;8300cm^2/g$, which easy to adjust particle size distribution to examine how particle size distribution of the binder has an effect on rheological properties of the cement paste. In addition, the relationship between n-value of Rosin-Rammler function and plastic viscosity were discussed. All measured flow curves represented thixotropy behavior and the hysteresis area was smaller for the more added coarse particle. When the combination was based on a ratio of $20{\sim}25vol%$ fine particles, $30{\sim}40vol%$ OPC and $40{\sim}45vol%$ coarse particles of the total volume, a high fluidity and low yield strength was achieved.

  • PDF

다중 낙하 분급기를 이용한 초미립자 시멘트의 제조 및 물리적 기초 특성 분석 (Manufacturing and Basic Physical Properties of Ultra Fine Cement with a Multi Air-Classifier of The Dry-Type)

  • 박원춘;문경주;소승영;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.757-760
    • /
    • 2006
  • This study aims to manufacture ultra fine cement(UFC) with a multi air-classifier of the dry-type. The classifier employed and devised for materials refining was a cyclone type fitted with an air suction device. This study also investigates the basic physical properties and quality of UFC and evaluates its utilizable possibility as a construction material. The basic properties of the UFC containing granulated blast furnace slag were analyzed and examined through recovery ratio, particle size distribution, scanning electron microscopy and compressive strength. Results obtained from the analysis of ultra fine cement have shown that there are possibilities for manufacturing UFC, which could compensate the weak properties of ordinary Portland cement.

  • PDF

A Study on the Mix Design and Quality Factors of the Combined High Flowing Concrete Using High Belite Cement

  • Kwon, Yeong-Ho
    • KCI Concrete Journal
    • /
    • 제14권3호
    • /
    • pp.121-129
    • /
    • 2002
  • This study investigates experimentally into the design factors and quality variations having an effect on the properties of the combined high flowing concrete to be poured in the slurry wall of Inchon LNG in-ground receiving terminal. Especially, high belite cement and lime stone powder as cementitious materials and viscosity agent in order to improve self-compaction and hydration heat are used in this study. Water-cement ratio(W/C), fine aggregate volume ratio(Sr) and coarse aggregate volume ratio(Gv) as design factors of the combined high flowing concrete are applied to determine the optimum mix design proportion. Also quality variations for sensitivity test are selected items as followings. (1)Surface moisture(5cases) and (2)Fineness modulus of fine aggregate(5cases), (3)Concrete temperature(3cases), (4)Specific surface(3cases) and particle size of lime stone powder. As experimental results, water-cement ratio, fine and coarse aggregate volume ratio are shown as the optimum range 51%, 43% and 53% separately considering site condition of slurry wall. Also quality factors by sensitivity test should be controlled in the following ranges. (1) Surface moisture :to.67% and (2)Fineness modulus 2.6$\pm$0.2 of fine aggregate, (3)Concrete temperature l0-20t, (4) Specific surface 6,000$\textrm{cm}^2$/g and particle size 9.7$\pm$1.0${\mu}{\textrm}{m}$ of lime stone powder. Based on the results of this study, the optimum mix design proportion of the combined high flowing concrete are selected and poured successfully in the slurry wall of LNG in-ground tank.

  • PDF

페로니켈슬래그를 잔골재로 사용한 비소성 시멘트 모르타르의 강도 특성 (Strength Characteristics of Non-Sintered Cement Mortar Utilizing Ferro-Nickel Slag as Fine Aggregate)

  • 류지수;장경수;나형원;형원길
    • 한국건축시공학회지
    • /
    • 제23권4호
    • /
    • pp.359-367
    • /
    • 2023
  • 본 실험에서는 포틀랜드 시멘트와 모래를 비소성 시멘트와 페로니켈슬래그로 대체 사용하여 친환경 시멘트 모르타르를 제작하였다. 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 강도 특성을 파악하기 위해 골재 종류와 양생방법을 구분하였다. 휨 및 압축강도 시험 결과, 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 강도는 Plain과 증기양생을 실시한 비소성 시멘트 모르타르의 강도보다 높았다. 이는 페로니켈슬래그의 입도, 밀도 및 흡수율 특성에 따른 강도 향상 효과로 판단된다. 모르타르의 XRD 분석 결과, 페로니켈슬래그에 포함된 MgO 성분이 복합 산화물 형태로 존재하며, 이를 통해 페로니켈슬래그가 적용된 비소성 시멘트 모르타르의 안정적인 강도 발현을 확인하였다.