  • In this research, experimental and numerical simulations were adopted to investigate the effects of ligament angle on compressive strength and failure mode of rock-like material specimens containing two non-coplanar filled fissures under uniaxial compression. The experimental results show that with the increase of ligament angle, the compressive strength decreases to a nadir at the ligament angle of $60^{\circ}$, before increasing to the maximum at the ligament angle of $120^{\circ}$, while the elastic modulus is not obviously related to the ligament angle. The shear coalescence type easily occurred when ${\alpha}$ < ${\beta}$, although having the same degree difference between the angle of ligament and fissure. Numerical simulations using $PFC^{2D}$ were performed for flawed specimens under uniaxial compression, and the results are in good consistency with the experimental results. By analyzing the crack evolution process and parallel bond force field of rock-like material specimen containing two non-coplanar filled fissures, we can conclude that the coalescence and propagation of crack are mainly derived from parallel bond force, and the crack initiation and propagation also affect the distribution of parallel bond force. Finally, the displacement vectors in ligament region were used to identify the type of coalescence, and the results coincided with that obtained by analyzing parallel bond force field. These experimental and numerical results are expected to improve the understanding of the mechanism of flawed rock engineering structures.

접착제 미 사용시 치면열구전색제로서의 유동성 복합레진 평가 (EVALUATION OF THREE FLOWABLE COMPOSITES AS PIT AND FISSURE SEALANTS WITHOUT USING BONDING AGENTS)

  • 권호범;김명진;신철환;김지연;박기태
    • 대한소아치과학회지
    • /
    • 제33권2호
    • /
    • pp.244-252
    • /
    • 2006
  • 본 연구의 목적은 유동성 복합레진을 치면열구전색제로 사용할 수 있는지 여부를 평가하는 것이다. 세 종류의 유동성 복합레진(Filtek Flow, Tetric Flow, Charmfil Flow)과 한 종류의 filled sealant(Ultraseal XT plus)가 사용되었다 주사전자 현미경을 이용하여 세 종류의 유동성 복합레진 및 filled sealant의 resin tag형성 양상을 비교하였다. 미세누출 평가를 위해 발거된 사람의 소구치 54개를 각각 18개씩 무작위로 세 군으로 배분하였다. 각 군마다 통상의 filled sealant와 한 가지씩의 유동성 복합레진을 교합면 열구에 도포하였다. 치아들을 thermocycling($5^{\circ}{\pm}2^{\circ}C$$55^{\circ}{\pm}2^{\circ}C$ 사이에서 30초씩 1200회 시행) 후 48시간 동안 1% methylene blue 용액에 보관하였다. 각각의 치아를 절단하여 미세누출 정도를 관찰하였다. 세 종류의 유동성 복합레진 및 filled sealant는 유사한 resin tag 형성양상을 보였다 세 종류의 유동성 복합레진은 각각 filled sealant보다 현저히 더 많은 미세누출을 보였다. 세 종류의 유동성 복합레진 간의 미세누출 정도는 유사하였다. 유동성 복합레진은 통상의 filled sealant와 비교해볼 때 보다 많은 미세누출을 야기할 수 있으므로 치면열구전색제로 적절하지 않다.

  • PDF

치면열구전색제 도포 후 광중합 할 때까지의 경과시간이 전색제 침투에 미치는 영향 (EFFECT OF TIME ELAPSED FROM APPLICATION TO CURING ON THE PENETRATION OF SEALANT)

  • 최선아;이창섭;이상호;이난영
    • 대한소아치과학회지
    • /
    • 제32권3호
    • /
    • pp.491-498
    • /
    • 2005
  • 치면열구전색제 도포 후 시간에 따른 열구 내 침투율을 알아보고자 발치된 소구치 192개를 이용하여 전색제 도포 후 광중합 할 때까지 경과시간 3초, 5초, 10초, 20초별로 침투율을 비교 분석하였다. 여기에 추가적으로 상악과 하악, filled sealant와 unfilled sealant군으로 나누어 시간대별로 침투율에 차이가 있는지도 비교분석하였다. 그 결과 시간이 경과할수록, filled sealant군보다 unfilled sealant군에서, 상악보다는 하악에서 전색제의 침투율이 증가하였다. 이상의 결과에서 임상에서 치면열구전색을 시행할 때 이 결과를 임상적 지침으로 적용하면 유용하리라고 여겨진다.

  • PDF

35번 고속도로 고성 교차로 지역 공룡발자국의 보존을 위한 응용광물학적 연구 (Applied Mineralogy for the Conservation of Dinosaur Tracks in the Goseong Interchange Area)

  • 정기영;김수진
    • 한국광물학회지
    • /
    • 제17권3호
    • /
    • pp.189-199
    • /
    • 2004
  • 대전-통영간 35번 고속도로 고성교차로 건설공사현장에서 발견된 공룡발자국화석의 보존 및 전시를 위한 응용광물학적 연구를 실시하였다 백악기 공룡발자국 퇴적암은 흑색점토층과 암회색 실트층의 호층으로 구성되어 있으며, 수평 또는 수직 열극에는 방해석맥이나 표성기원의 산화철 또는 산화망간 침전물이 충전되어 있다. 강물조성은 전반적으로 석영, 앨바이트, K장석, 방해석, 녹니석 일라이트 백운모, 흑운모와 미량의 인회석, 금홍석으로 구성되어 있으며, 방해석과 앨바이드는 실트층, 그리고 석영, 일라이트,녹니석은 점토층에 부화되어 있다. 주원소인 Al, Fe, Mg, K, Ti, P는 절토층, Ca Na Mn은 실트층, 그리고 미랑원소인 V, Cr, Co, Ni, Cs, Zr, REE, Th, U 등은 점토층에 부화되어 있다. 탄소의 경우, 무기탄소는 실트층에 방해석의 형태로 농집되어 있으며, 유기탄소는 흑색점토층에 부화되어 있다. 흑색점토층은 열극을 따라 부분적으로 유기탄소가 이차적으로 산화제거되어 연황색 점토층으로 변질되었다. 점토광물이 풍부한 흑색 및 연황색 점토의 층리를 따른 선택적 박리현상, 실트층의 기질 또는 수직절리의 주요 충전물인 방해석의 용해성과 낮은 강도는 발자국 화석 표본의 향후 물리적, 화학적 훼손을 촉진할 수 있는 잠재적 요소로 평가되었다.

예방적 레진수복의 미세누출에 관한 연구 (A STUDY ON MICROLEAKAGE OF PREVENTIVE RESIN RESTORATION)

  • 구현정;이상훈;한세현
    • 대한소아치과학회지
    • /
    • 제28권3호
    • /
    • pp.504-511
    • /
    • 2001
  • 예방적 레진수복은 교합면 열구전색의 개념을 확대하여 초기우식에만 국한한 와동을 형성하여 복합레진으로 충전한 후 나머지 건전한 부위의 소와열구를 치면열구전색재로 도포하는 것이다. 충전제가 첨가된 치면열구전색재로서 작은 와동의 수복도 가능하다는 새로운 방법은 소아환자의 치료시 술자와 환자 모두에게 도움을 줄 수 있을 것이다. 그러나 예방적 레진수복을 시행하여 비교한 연구가 아직까지는 부족한 실정이다. 이에 저자들은 4가지 방법의 예방적 레진수복시의 미세누출을 비교해보고자 하였으며 레진수복만을 한 경우도 함께 비교하여 보았다. 55개의 상, 하악 소구치를 준비하여 I급와동을 교합면에 형성하고 다음과 같이 수복하였다. 제1군 : 와동을 복합레진(Z-100)으로 수복 제2군 : 와동을 복합레진(Z-100)으로 수복 중합후, 비충전 전색재인 Teethmate F-1으로 소와열구도포 제3군 : 와동을 복합레진(Z-100)으로 수복 중합후, 충전 전색재인 Ultraseal XT-plus로 소와열구도포 제4군 : 와동과 소와열구를 한 번에 Ultraseal XT-plus로 수복 제5군 : 와동과 소와열구를 나누어 Ultraseal XT-plus로 수복 위와 같이 처리한 치아를 $5^{\circ}C$$55^{\circ}C$의 수조에 번갈아 30초씩 500회의 열순환을 실시하고 1% methylene blue용액에 24시간 담근 후 수세하고 투명레진에 매몰하였다. 매몰된 치아를 협설측으로 치아장축방향으로 평행하게 절단한 후 입체현미경으로 염색용액의 침투정도를 관찰하여 다음의 결과를 얻었다. 1. 평균 미세누출은 4군에서 가장 높았고, 3군에서 가장 낮았다. 평균 미세누출은 4>1>5>2>3군의 순으로 감소하였다. 2. 군간의 미세누출 비교에서 1군은 5군과는 통계학적으로 유의한 차이가 없었으나 2군, 3군보다 유의하게 높은 미세누출을 보였고(p<0.05), 4군보다는 유의하게 낮은 미세누출을 보였다(p<0.05). 3. 2군은 3군과는 통계학적으로 유의한 차이가 없었으나 4군, 5군보다는 유의하게 낮은 미세누출을 보였다(p<0.05). 4. 3군은 4, 5군보다 통계학적으로 유의하게 낮은 미세누출을 보였다(p<0.05). 5. 5군은 4군보다 통계학적으로 유의하게 낮은 미세누출을 보였다(p<0.05).

  • PDF

동화-황학산광산의 동광화작용 (Copper Mineralization of the Donghwa and Hwanghagsan Mine)

  • 이현구;김상중;김문영
    • 자원환경지질
    • /
    • 제31권1호
    • /
    • pp.1-10
    • /
    • 1998
  • Copper mineralization of the Donghwa and Hwanghagsan mines was deposited in hydrothermal quartz veins which filled fissures in Cretacous sedimentary rocks. Ore minerals are pyrite, sphalerite, chalcopyrite, bornite, galena, wittichenite and unidentified Cu-Bi-Pb-Sb-S mineral. On the basis of salinities and homogenization temperatures for fluid inclusions, the Donghwa deposit was deposited from $300^{\circ}C$ to $220^{\circ}C$ with 2.5 to 0.2 wt.% eq. NaCl, and the Hwanghagsan deposits was deposited from $300^{\circ}C$ to $160^{\circ}C$ with 4.0 to 0.0 wt.% eq. NaCl. Evidence of boiling suggests pressure of 170 to 60 bar, these pressures correspond to 1700 m to 600 m. The ${\delta}^{34}S_{H_2S}$ values of the Donghwa deposit (4.8~7.4%) are higher than those of the Hwanghagsan deposit (3.5~4.5%), sulfur isotope compositions indicate that ore fluids partially reacted with meteoric water and wall-rock. Equilibrium thermodynamic interpretation indicates that the temperature versus $fs_2$ of the Donghwa deposit (> $420^{\circ}C$, $10^{-3.2}atm$) is higher condition than that of the Hwanghagsan deposit (> $290^{\circ}C$, $10^{-7.0}atm$). K-Ar ages for biotite granite and quartz porphyry in the study area are 64.7 Ma, and 60.9 Ma, reapectively. Mineralization age using sericite in the Donghwa deposits is 59.8 Ma. Therfore, Copper mineralization in the study area was associated with acidic igneous activity such as biotite granite or quartz porphyry.

  • PDF

의성지역(義城地域)의 금(金)-은(銀) 광화작용(鑛化作用) (Gold-Silver Mineralization of the Euiseong Area)

  • 지세정;최선규;도성재;고용권
    • 자원환경지질
    • /
    • 제24권2호
    • /
    • pp.151-165
    • /
    • 1991
  • The Au-Ag deposits of the Euiseong area occurred in quartz veins which filled fissures in Cretaceous sedimentary and volcanic rocks. These ore veins can be classified in two types of deposits based on metallic mineral assemblages as follow: a pyrite type gold-silver deposit (Hoedong mine), characterized by Cu sulfides with Au-Ag alloy, and a Sb-rich silver deposit (Keumdongdo mine), characterized by base metal with Ag-bearing sulfosalts. Mineralogic and fluid inclusion evidences suggest that the ore minerals of these deposits was deposited from initial high temperatures (near $350^{\circ}C$) to later lower temperatures ($200^{\circ}C$) with moderate salinity fluids ranging from 5.8 to 3.8 eq. wt. % NaCl. The gold-silver mineralization of the Hoedong mine occurred at temperatures between 300 and $200^{\circ}C$ from fluids with log $f_{s_2}$ of -10 ~ -16 atm. The antimony - silver mineralization of the Keumdongdo mine were deposited at the higher temperatures (350 to $250^{\circ}C$) and $f_{S_2}$ (-10 ~ -13 atm) than gold mineralization of the Hoedong mine. The calculated log f02 of fluids at $250^{\circ}C$ in two deposits are -32 to -34 atm and -36.5 to -38.5 atm, respectively. Boiling evidences indicate that the ore mineralization of the Hoedong mine occurred at more shallow depth (0.5km) than that (1km) of the Keumdongdo mine. The above differences of depositional environments between two deposits caused the compositional changes of ore minerals such as electrum and sphalerite.

  • PDF

무주 수왕광산에서 산출되는 섬아연석의 황동석 병변에 관한 연구 (Chalcopyrite Disease in Sphalerite: A Case of the Soowang Ore Deposits in Muju, Republic of Korea)

  • 윤석태
    • 한국지구과학회지
    • /
    • 제29권7호
    • /
    • pp.551-558
    • /
    • 2008
  • 수왕광상은 중생대 백악기 중기의 반상화강암이나 선캄브리아기의 소백산 편마암 복합체에 발달한 열극을 충진한 석영맥에서 산출된다. 광물 공생군에 대한 연구 결과 광화작용은 4차례에 걸쳐 일어났다. 섬아연석은 광화작용이 진행되는 동안 광화 I, II, III기에 각각 정출하였다. 현미경 관찰과 전자현미분석 결과 섬아연석에서 나타나는 황동석 점적과 황동석 병변은 광화 III기 초에 열수용액의 교대작용에 의하여 생성되었을 것으로 생각된다. 황동석 병변의 생성과정은 아래와 같다. (1) Fe가 풍부한 용액이 Fe가 결핍된 섬아연석의 가장자리나 틈을 통해 Fe부화 (2)광화 II기에 Fe가 결핍된 섬아연석에 황동석 점적을 형성하고 Cu를 함유한 용액에 의해 황동석 점적 주변의 섬아연석에 Fe 감소 (3)광화 III기 초에 황동석 병변을 형성하였다.

명봉광산의 광미 내 비소의 고정화 특성 연구 (Characterization of Arsenic Immobilization in the Myungbong Mine Tailing)

  • 이우춘;정종옥;김주용;김순오
    • 자원환경지질
    • /
    • 제43권2호
    • /
    • pp.137-148
    • /
    • 2010
  • 백악기 불국사화강암 내 열극을 충진한 함금은석영맥으로 구성된 명보광산은 전남 보성군에 위치한 광산이다. 본 연구에서는 명봉광산의 광미를 채취하여 광미 내 황화광물 풍화와 이차 삼차 광물 생성 또는 변질 등의 다양한 과정들이 비소의 고정화에 어떠한 영향을 미치는지 살펴보았다. 광물학적 화학적 방법으로 나누어 연구를 수행하였으며, 광물학적 방법으로는 비중/자력 선별, 초음파 서}척, 기기분석(X-선 회절 분석기, 에너지 분산분광기, 전자탐침미세현미경) 등이 이용되었다. 그리고 왕수분해법을 적용하여 광미 내 원소함량을 알아보았다. 연구결과, 광미의 풍화로 형성된 철 (산)수산화물은 충진, 침전, 변질 등의 3가지 형태로 존재하는 것으로 확인되었다. 즉, 황철석의 가장자리와 균열부를 충진하는 형태, 맥석광물을 피복하여 침전된 형태 그리고 유코나이트로 변질된 형태 등이었다. 초기 다량의 산-발생 광물인 황철석과 유비철석의 풍화로 인해 산화반응이 빠르게 일어나면서 많은 철 (산)수산화물과 스코로다이트 등이 이차적으로 생성되는 것이 인지되었다. 이와 더불어 산화 환경에 대한 노출기간이 길어지고 산-발생 광물이 소모되면서 광미 내 pH 감소속도는 점차적으로 줄어들게 될 뿐만 아니라 주변 모암 내 함유된 방해석과의 중화반응이 더 크게 기여함으로써 광미의 pH는 증가한 것으로 생각된다. 이러한 광미 내 pH의 상승으로 인하여 이차적으로 생성된 스코로다이트의 안정도가 감소하면서 비소가 재용출 되어진다. 또한 방해석과 스코로다이트로부터 용출된 칼슘이온과 비소이온이 국부적으로 농집되면서 삼차적으로 유코나이트로 성장하게 되고, 이러한 비산염광물의 일종인 유코나이트는 비소의 함량이 높은 광물로서 비소를 고정화시키는데 크게 기여한 것으로 판단된다. 뿐만 아니라 광미의 주요한 일차광물인 황철석이 풍화되면서 생성된 다량의 철 (산)수산화물은 비소의 거동에 대하여 제어능력이 큰 것으로 인지되었다. 결론적으로 본 연구는 이러한 일련의 과정에 통하여 일차적으로 용출되거나 이차적으로 재용출된 비소는 흡착, 공침, 흡수 등과 같은 다양한 수착 반응들로 인해 고정화됨을 확인하였다.

무주 수왕광상의 금-은 광화작용 (Gold and Silver Mineralization of the Soowang Ore Deposits in Muju, Korea)

  • 박희인;윤석태
    • 한국지구과학회지
    • /
    • 제25권6호
    • /
    • pp.484-494
    • /
    • 2004
  • 수왕금은광상은 백악기 중기의 반상화강암이나 선캠브리아기의 소백산 편마암 복합체에 발달한 열극을 충진한 석역맥에서 산출된다. 광물공생군에 대한 연구결과 광화작용은 4시기에 걸쳐서 일어났다. 광화 띠는 주요황화광물과 소량의 에렉트럼, 광화 II기는 에렉트럼, 광화 III기는 함은황화염광물과 소량의 에렉트럼, 그리고 광화IV기는 광석광물정출과 무관한 시기이다. 광물학적 연구 및 유체포유물 연구결과 수왕광상의 광석광물은 초기에는 고온(300$^{\circ}C$)에서 정출하여 후기로 가면서 온도가 150$^{\circ}C$까지 하강하는 경향을 보이고, 염농도는 섬아연석의 10.4wt.%에서 중정석의3.1wt.%의 영역을 보여준다. 수왕광상의 금은 광화작용은 140${\sim}$250$^{\circ}C$의 온도와 황분압이 $10^{-12}{\sim}10^{-18}$ atm을 갖는 광화유체에서 일어났다. 유체포유물의 비등증거로부터 광화작용이 진행되는 동안의 압력 조건은 정암압 환경에서 약 210bars 정도로 추정되며, 이는 대략 약 800m의 심도에서 광화작용이 일어났음을 시사한다.