• 제목/요약/키워드: electrodes thickness

검색결과 406건 처리시간 0.04초

광전극 두께와 표면적 변형에 따른 DSSC의 효율 특성 (DSSCs Efficiencies of Photo Electrode Thickness and Modified Photo Electrode Surface Area)

  • 권성열;양욱;주택원
    • 한국전기전자재료학회논문지
    • /
    • 제27권2호
    • /
    • pp.115-120
    • /
    • 2014
  • Photo electrode is an important component for DSSC. DSSCs electrical characteristics and efficiencies fabricated with different $TiO_2$ photo electrodes thickness and modified phoro electrode surface area were studied. $11{\mu}m$ $TiO_2$ photo electrode shows a 4.956% efficiency. The highest short circuit current density was a $9.949mA/cm^2$. Efficiencies and short circuit current density increased as tape casting thickness decreased. Modified surface area of the photo electrode by needle stamp processing were studied. 200 times needle stamp processing on photo electrodes shows a highest 5.168% efficiency. Also the short circuit current density was a $10.261mA/cm^2$.

ESD 전극을 이용한 분무코팅 균일도 개선에 관한 연구 (Improvement of Spray Coating Uniformity using ESD Electrodes)

  • 당현우;양성욱;도양회;최경현
    • 한국기계가공학회지
    • /
    • 제15권2호
    • /
    • pp.118-124
    • /
    • 2016
  • In this study, experiments are conducted to improve spray coating uniformity by using second and third electrodes based on the electrospray atomization mechanism. The uniformity of fabricated thin films can be improved by adjusting the design of the second electrode. The implementation of the second electrode with an elongated hole and a bending angle of $90^{\circ}$ results in highly uniform films. In addition, induced area to substrate is increased by lowering the applied voltage using the third electrode with a round rod shape. A linear correlation between applied voltage and induced area is confirmed. Thin film thickness and surface roughness are measured after the fabrication of thin films through the electrospray process. It is confirmed that a thin film is formed having an average thickness of 273.44 nm, a thickness uniformity of less than 10%, and a surface roughness of 3 nm.

심박 모니터링을 위한 전도성 소재의 전도성 및 물성 비교 연구 (A Comparative Study on the Conductivity and Physical Properties of Conductive Materials for Heart Rate Monitoring)

  • 김지민;김종준
    • 패션비즈니스
    • /
    • 제22권4호
    • /
    • pp.118-129
    • /
    • 2018
  • The purpose of this study is to develop ECG electrode materials for the heart rate monitoring smart band, a smart device used for ECG and heart rate measurement. The purpose of the evaluation is to assess properties and conductivity of electrodes of the existing heart rate monitoring smart band, and to determine suitability through a representative conductive sample. Because level of thickness does not differ significantly from value of conductive specimen from thickness of the smart band, it can be used as a conductive electrode. Surface conductivity of conductive samples and smart bands, is expected to be available as electrodes except for conductive film. Also, since the knit have conductivity only in the metal processing layer, it is necessary to use electrodes on the part of the metal processing layer that is conductive when applying the knit. Tensile strength and electrical conductivity of the tensile were generally revealed to have a tendency. Thickness of the specimen that can be used as an electrode for the smart band is suitable for all samples, electrical resistance, conductive woven, conductive knit, and conductive cord. In the case of conductive cord, however, the electrode attached to the human body will not conform to the flat shape of the electrode attached to the human body. Therefore, the conductive woven and the conductive knit will be available as an electrode.

전극 홈 형상에 따른 스캐닝 미러의 구동 특성 (Driving Characteristics of the Scanning Mirrors to the Different width and Number of the Grooves on the Electrodes)

  • 박근우;김용권
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제50권11호
    • /
    • pp.575-580
    • /
    • 2001
  • In this paper, using $500\mum-thickness\; (100)\; silicon\; wafer,\; flat\; 65\mum-thickness$ silicon mirror plates were fabricated through dry etching and wet etching, and $45\mum-depth$ grooved driving electrodes were fabricated through UV-LIGA process. Four shapes of the driving electrode were fabricated: twenty four grooves of the $50\mum-width$, twelve grooves of the $100\mum-width$, six grooves of the $200\mum-width$, and no grooves on the driving electrode. Fabricated mirror plate size and spring size are $2400\times2400\times65\mum3\; and \;500\times10\times65\mum3,$ respectively. Mirror plate parts and driving electrodes were assembled into the scanning mirrors. Measured natural resonance frequencies were about 600Hz which have error within $\pm 2%$ to calculated value. Due to the squeeze effect in the narrow gap between the mirror plate and the driving electrode, measured resonance frequencies were reduced as raising the amplitude of the mirror plate. In a case of driving electrode without grooves, the resonance frequency was reduced largely, compared with a case of driving electrode with grooves. According to the experimental results, squeeze effect was smaller in the driving electrode with smaller-width and many grooves. Therefore, the driving electrode with smaller-width and many grooves was effective in low voltage and high speed operation.

  • PDF

Comparison of characteristics of IZO-Ag-IZO and IZO-Au-IZO multilayer electrodes for organic photovoltaics

  • Jeong, Jin-A;Choi, Kwang-Hyuk;Park, Yong-Seok;Park, Ho-Kyun;Kim, Han-Ki
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.131-131
    • /
    • 2010
  • We compared the electrical, optical, structural, and interface properties of indium zinc oxide (IZO)-Ag-IZO and IZO-Au-IZO multilayer electrodes deposited by linear facing target sputtering system at room temperature for organic photovoltaics. The IZO-Ag-IZO and IZO-Au-IZO multilayer electrodes show a significant reduction in their sheet resistance (4.15 and 5.49 Ohm/square) and resistivity ($3.9{\times}10^{-5}$ and $5.5{\times}10^{-5}$Ohm-cm) with increasing thickness of the Ag and Au layers, respectively. In spite of its similar electrical properties, the optical transmittance of the IZO-Ag-IZO electrode is much higher than that of the IZO-Au-IZO electrode, due to the more effective antireflection effect of Ag than Au in the visible region. In addition, the Auger electron spectroscopy depth profile results for the IZO/Ag/IZO and IZO/Au/IZO multilayer electrodes showed no interfacial reaction between the IZO layer and Ag or Au layer, due to the low preparation temperature. To investigate in detail the Ag and Au structures on the bottom IZO electrode with increasing thickness, a synchrotron x-ray scattering examination was employed. Moreover, the OSC fabricated on the IZO-Ag-IZO electrode shows a higher power conversion efficiency (3.05%) than the OSC prepared on the IZO-Au-IZO electrode (2.66%), due to its high optical transmittance in the wavelength range of 400-600 nm, which is the absorption wavelength of the P3HT:PCBM active layer.

  • PDF

저항 용접을 이용한 금속 샌드위치 판재 접합에 관한 연구 : Part 1 - 공정변수의 선정 (A Study on the Resistance Welding of Metallic Sandwich Panel : Part 1 - Determination of Process Parameters)

  • 이상민;김진범;나석주
    • Journal of Welding and Joining
    • /
    • 제23권6호
    • /
    • pp.49-54
    • /
    • 2005
  • Inner Structured and Bonded(ISB) panel, a kind of metallic sandwich panel, consists of two thin skin plates bonded to a micro-patterned inner structure. Its overall thickness is $1\~3mm$and it has attractive properties such as ultra-lightweight, high efficiency in stiffness-to-weight and strength-to-weight ratio. In many previous studies, resistance welding, brazing and adhesive bonding are studied for joining the panel. However these methods did not consider productivity, but focused on structural characteristics of joined panels, so that the joining process is very complicated and expensive. In this paper, a new joining process with resistance welding is developed. Curved surface electrodes are used to consider the productivity and the stopper is used between electrodes during welding time to maintain the shape of inner structure. Welding time, gap of electrodes and distance between welding points are selected as the process parameters. By measuring the tensile load with respect to the variation of welding time and gap of electrodes, proper welding conditions are studied. Welding time is proper between 1.5-2.5cycle. If welding time is too long, then inner structures are damaged by overheating. Gap of electrode should be shorter than threshold value fur joint strength, when total thickness of inner structure and skin plate is 3.3mm, the threshold distance is 3.0mm.

실리콘 이종접합 태양전지의 버스바 전극 두께와 접합강도의 상관관계 (A Study on Correlation between Busbar Electrodes of Heterojunction Technology Solar Cells and the Peel Strength)

  • 전다영;문지연;박고등;오트곤게렐 줄만다크;남혜령;권오련;임현수;김성현
    • Current Photovoltaic Research
    • /
    • 제11권2호
    • /
    • pp.44-48
    • /
    • 2023
  • In heterojunction technology (HJT) solar cells, low-temperature curing paste is used because the passivation layer deteriorates at high temperatures of 200℃ or higher. However, manufacturing HJT photovoltaic (PV) modules is challenging due to the weak peel strength between busbar electrodes and cells after soldering process. For this issue, the electrode thicknesses of the busbars of the HJT solar cell were analyzed, and the peel strengths between electrodes and wires were measured after soldering using an infrared (IR) lamp. As a result, the electrodes printed by the screen printing method had a difference in thickness due to screen mask. Also, as the thickness of the electrode increased, the peel strength of the wire increased.

압전 수정진동자의 설계민감도 해석과 위상 최적설계 (Design Sensitivity Analysis and Topology Optimization of Piezoelectric Crystal Resonators)

  • 하윤도;조선호;정상섭
    • 한국전산구조공학회:학술대회논문집
    • /
    • 한국전산구조공학회 2005년도 춘계 학술발표회 논문집
    • /
    • pp.335-342
    • /
    • 2005
  • Using higher order Mindlin plates and piezoelectric materials, eigenvalue problems are considered. Since piezoelectric crystal resonators produce a proper amount of electric signal for a thickness-shear frequency, the objective is to decouple the thickness-shear mode from the others. Design variables are the bulk material densities corresponding to the mass of masking plates for electrodes. The design sensitivity expressions for the thickness-shear frequency and mode shape vector are derived using direct differentiation method(DDM). Using the developed design sensitivity analysis (DSA) method, we formulate a topology optimization problem whose objective function is to maximize the thickness-shear component of strain energy density at the thickness-shear mode. Constraints are the allowable volume and area of masking plate. Numerical examples show that the optimal design yields an improved mode shape and thickness-shear energy.

  • PDF

Synthesis and Electrochemical Characterization of Polypyrrole/Multi-walled Carbon Nanotube Composite Electrodes for Supercapacitor Applications

  • Paul, Santhosh;Lee, Yoon-Sung;Choi, Ji-Ae;Kang, Yun-Chan;Kim, Dong-Won
    • Bulletin of the Korean Chemical Society
    • /
    • 제31권5호
    • /
    • pp.1228-1232
    • /
    • 2010
  • The nanocomposites of polypyrrole (PPy) and multi-walled carbon nanotube (MWCNT) with different composition are synthesized by the chemical oxidative polymerization method. In these composites, the MWCNTs are uniformly coated by PPy with different thickness. The electrochemical properties of the composite electrodes are investigated by cyclic voltammetry, galvanostatic charge-discharge cycling and electrochemical impedance spectroscopy. The full cells assembled with the PPy/MWCNT composite electrodes deliver initial specific capacitances ranging from 146.3 to 167.2 F/g at 0.5 mA/$cm^2$ and exhibit stable cycling characteristics. The effect of content of MWCNT in the composite on cycling performance of the cells is also investigated.

PDP에서 방전전극상의 유전층의 절연내력과 투명도에 관한 연구 (A Study on the Dielectric Breakdown Strength and Transparency of Dielectric Layer on the Discharge Electrodes in PDP)

  • 이성현;김영기;지성원;조정수;박정후
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1997년도 추계학술대회 논문집 학회본부
    • /
    • pp.379-381
    • /
    • 1997
  • The dielectric layers in AC plasma display panel(AC PDP) are essential to the discharge cell structure, because they protect metal electrodes from sputtering by positive ion and from a sheath of wall charges which are essential to memory function of AC PDP. Furthermore, this layer should be transparent because the visible light must pass through the layer. In this paper, the dielectric breakdown strength and transparency of the dielectric layer on the discharge electrodes are studied. The variables in this test are the dielectric layer thickness, dielectric firing condition, gas pressure, species of gas and so on.

  • PDF