• Title/Summary/Keyword: early age damage

Search Result 125, Processing Time 0.031 seconds

The Properties of Temperature History of Concrete with Surface Insulating Material in Cold Weather Concreting (한중콘크리트 시공시 표면 단열재 변화에 따른 콘크리트의 온도이력 특성)

  • 문학용;신동안;김경민;김기철;오선교;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.05a
    • /
    • pp.7-11
    • /
    • 2003
  • This study investigate the hydration heat history with variation of surface insulating material in cold weather concreting. According to the results, the temperature of concrete lowers below zero in 24hours, so early frost damage occurs in the case of exposure and 1 fold bubble sheet, but the lowest temperature keeps above zero, so a adiabatic effect is very favorable in the case of double bubble sheet and 부직포. Compressive strength of core specimen at 7 and 28 days is highest In the case of double bubble sheet and 부직포. But, considering convenience of construction and economical efficiency, it is thought that the most effective surface insulating material is 1 fold bubble sheet +blanket.

  • PDF

Evaluation on Compressive Strength of Mortar and Concrete at Early Age Using Variable Cement and Self-heating Binder (시멘트 산지 및 자기발열분체 사용에 따른 모르타르 및 콘크리트의 저온에서의 압축강도성능 평가)

  • Hong, Seok-Beom;Kim, Woo-Jae;Yoo, Jo-Hyeong
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.152-153
    • /
    • 2016
  • In this research, we evaluate the performance for preventing frost damage at early age of mortar using variable cement and self-heating binder. Purpose of final research is preventing freezing and thawing by making the compressive strength 5MPa in 3days below zero temperature without heat curing. We compare the compressive strength of mortar and concrete using variable cements and self-heating binder in low temperature.

  • PDF

Investigation on the Method of Evaluating the Resistance to Freezing and Thawing of Concrete Subjected Initial Frost Damage (초기동해를 받은 콘크리트의 내동해성 평가법에 대한 검토)

  • 고경택;장일영
    • Journal of the Korea Concrete Institute
    • /
    • v.11 no.4
    • /
    • pp.117-127
    • /
    • 1999
  • In concrete incorporating high volume ground granulated blast-furnace slag that has frozen at early age, to evaluated the results of resistance to freezing and thawing is very difficult because the hydration of the concrete increases over the duration of rapid freezing and thawing test. Hence, the dynamic modulus of elasticity of specimens after freezing and thawing will be favorable results unless the hydration effect is taken into consideration. In this study, a method of evaluating to the resistance to freezing and thawing of concrete subjected freezing at early age, in which the effect of hydration is modified for its increase during rapid freezing and thawing test, is investigated.

Characteristics of Temperature History of Slab concrete by the Change of Hot wire Heat Capacity at -10℃ (-10℃ 조건에서의 열선 열용량 크기 변화에 따른 슬래브 콘크리트의 온도이력 특성)

  • Jung, Eun-Bong;Ahn, Sang-Ku;Jung, Sang-Hyun;Koh, Kyung-Taek;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.05a
    • /
    • pp.75-77
    • /
    • 2013
  • In this study, the characteristics of temperature history was evaluated for three hot wires with different capacity installed in slab concrete which are relatively thin. Results can be summarized as follows. First, for the case of material using 5W hot wire, all decreased to below zero at or around 24 hours. Similarly, the material using 20W hot wire decreased to 2℃ below zero at or around 80 hours but satisfied the accumulative temperature of 45° D·D at 7 days of material age. On the other hand, the case of 30W hot wire, the biggest capacity, showed the high temperature history of 5℃ in average at all areas except the corners. Thus, the target accumulative temperature was secured at or around the 3 days of material age. Considering the above, the initial damage by freezing can be prevented only if 20W or higher hot wires are used for the slabs at -10℃ of extremely low temperature environment.

  • PDF

Compressive Strength Properties of Concrete by the Form Material Change at 10 below Zero (양생온도 -10℃에서 거푸집 재료 변화에 따른 콘크리트의 압축강도 특성)

  • Choi, Si-Hyun;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.05a
    • /
    • pp.107-108
    • /
    • 2016
  • When the construction in a low temperature, the concrete performance is deteriorated by frost damage at early age. In this study, the form utilizing heating sheet and insulation is measured the performance to prevent frost damage at 10 below zero. It produced five types of the form and to measure the temperature history and compressive strength. At first, form attached heating sheet showed the highest temperature. But the form attached vacuum insulation showed the highest temperature ever since 12hours. In the case of compressive strength, the form attached heating sheet + isopink(polystyrene foam board) showed the highest compressive strength. It was followed by vacuum insulation. As a result, the form utilizing insulation and heating sheet helped to prevent frost damage.

  • PDF

Diagnosis of Crack Occurrence of Very-Early Strength Latex-Modified Concretes through Field Tests (현장실험을 통한 VES-LMC 균열발생 원인분석)

  • Choi, Pan-Gil;Lee, Bong-Hak
    • Journal of Industrial Technology
    • /
    • v.26 no.A
    • /
    • pp.139-146
    • /
    • 2006
  • Many concrete bridge decks develop transverse cracking shortly after construction. These cracks accelerate corrosion of reinforcing steel and lead to concrete deterioration, damage to components beneath the deck, unsightly appearance. These cracks shorten the service life and increase maintenance costs of bridge structures. In this study, VES-LMC overlay, which provides the same benefits as a conventional overlay, is designed to cure very quickly. Although the materials for VES overlays are more expensive, the cost is more than offset by the savings on traffic control and work zone safety measures. Otherwise, reaction of hydration occurs very rapidly in beginning step(concrete placing). As a results, thermal cracking can be occur by thermal stress in accordance with hydration-heat The purpose of this study was to estimate diagnosis of crack occurrence of VES-LMC through field tests at early-age.

  • PDF

Investigation of Early-Age Concrete Strength Development Using Hardening Accelerator (경화촉진제를 사용한 콘크리트의 초기강도 발현 특성 검토)

  • Kim, Gyu-Yong;Kim, Yong-Ro;Park, Jong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.28 no.3
    • /
    • pp.309-316
    • /
    • 2016
  • In this study, performance of hardening accelerator types which promote setting and hardening of cement has been reviewed in order to develop early age strength of concrete with compressive strength of 21~27 MPa after examination of strength development of the concrete at early age according to curing temperature and unit cement(binder) content. As results, soluble mineral salt showed better hardening acceleration effect than organic salt in the scope of this study. Also, hydration reaction accelerating effect of $C_3S$ by Soluble mineral salt is effective on development of early age compressive strength and it was shown that the Pt's hydration reaction accelerating effect was the best. Construction duration reduction can be expected by securing compressive strength for prevention of early aged freezing damage in 25hour-curing time under curing temperature at $15^{\circ}C$. Also, it was shown that compressive strength of specimen cured at $5^{\circ}C$ was similar with plain specimen cured at $10^{\circ}C$. Therefore, it is expected that fuel costs and carbon dioxide can be reduced when the same construction duration is considered.

International Test Mock-up of the Self-Heating of Cement Developed using a Reducing Slag (환원슬래그를 이용하여 개발된 자기발열 시멘트의 해외 Mock-up Test 관한 연구)

  • Min, Tae-Beom;Choi, Hyun-Kuk;Kim, Hyeong-Cheol;Kim, Jae-Young;An, Dong-Hee
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.05a
    • /
    • pp.228-229
    • /
    • 2017
  • MOCK-UP TEST was conducted in the extreme region of the cement which was researched and developed by using the reducing slag Experimental results show that the basic properties (air volume, slump) are improved compared with the specimens using Mongolian cement. The compressive strength achieved the target strength (target strength: age 3day: 7MPa, age 7day 14MPa) and the hydration heat was about 8 ℃ higher than that of Mongolian cement products. Therefore, it is considered that the cement powders developed by our company showed the strength of concrete due to high hydration heat even at extreme temperatures.

  • PDF

Which One Is Better to Reduce the Infection Rate, Early or Late Cranioplasty?

  • Oh, Jae-Sang;Lee, Kyeong-Seok;Shim, Jai-Joon;Yoon, Seok-Mann;Doh, Jae-Won;Bae, Hack-Gun
    • Journal of Korean Neurosurgical Society
    • /
    • v.59 no.5
    • /
    • pp.492-497
    • /
    • 2016
  • Objective : Decompressive craniectomy is an effective therapy to relieve high intracranial pressure after acute brain damage. However, the optimal timing for cranioplasty after decompression is still controversial. Many authors reported that early cranioplasty may contribute to improve the cerebral blood flow and brain metabolism. However, despite all the advantages, there always remains a concern that early cranioplasty may increase the chance of infection. The purpose of this retrospective study is to investigate whether the early cranioplasty increase the infection rate. We also evaluated the risk factors of infection following cranioplasty. Methods : We retrospectively examined the results of 131 patients who underwent cranioplasty in our institution between January 2008 and June 2015. We divided them into early (${\leq}90days$) and late (>90 days after craniectomy) groups. We examined the risk factors of infection after cranioplasty. We analyzed the infection rate between two groups. Results : There were more male patients (62%) than female (38%). The mean age was 49 years. Infection occurred in 17 patients (13%) after cranioplasty. The infection rate of early cranioplasty was lower than that of late cranioplasty (7% vs. 20%; p=0.02). Early cranioplasty, non-metal allograft materials, re-operation before cranioplasty and younger age were the significant factors in the infection rate after cranioplasty (p<0.05). Especially allograft was a significant risk factor of infection (odds ratio, 12.4; 95% confidence interval, 3.24-47.33; p<0.01). Younger age was also a significant risk factor of infection after cranioplasty by multivariable analysis (odds ratio, 0.96; 95% confidence interval, 0.96-0.99; p=0.02). Conclusion : Early cranioplasty did not increase the infection rate in this study. The use of non-metal allograft materials influenced a more important role in infection in cranioplasty. Actually, timing itself was not a significant risk factor in multivariate analysis. So the early cranioplasty may bring better outcomes in cognitive functions or wound without raising the infection rate.

Strength Development of Mock-up Concrete Structure subjected to Extremely Low Temperature Condition Due to Curing Methods (극저온 조건에서의 양생방법 변화에 따른 실구조체 콘크리트의 강도발현 특성)

  • Jung, Eun-Bong;Jung, Sang-Hyeon;Ahn, Sang-Ku;Ko, Gyeong-Taek;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2012.11a
    • /
    • pp.47-49
    • /
    • 2012
  • Under this study, the characteristics of concrete intensity condition following the curing method under the extremely low temperature environment have been contemplated, and as a result, in the event of insulation + heat cable curing, the intensity and accumulated temperature accomplishment period is required for two times of requiring initial frost damage prevention than the case of heating + heat insulation curing method due to the insufficient calories supplied in general.

  • PDF