• Title/Summary/Keyword: duplex stainless steel

Search Result 183, Processing Time 0.028 seconds

Effect of and R Phase on the Pitting Corrosion in Super Duplex Stainless Steel (슈퍼 2상 스테인리스강의 공식에 미치는 R상의 영향)

  • Lee, Byung-Chan;Oh, Eun-Ji;Kang, Chang-Yong
    • Korean Journal of Materials Research
    • /
    • v.24 no.11
    • /
    • pp.610-616
    • /
    • 2014
  • In this study, we investigated the precipitation behavior of the R-phase precipitated at the initial stage of aging and its effect on the pitting corrosion of 25%Cr-7%Ni-4%Mo super duplex stainless steel. The R-phase in super duplex stainless steel was mainly precipitated at the interface of ferrite/austenite phases and inside of the ferrite phase during the initial stage of aging, and it was transformed into the ${\sigma}$-phase with an increase in aging time. The ferrite phase was decomposed into a new austenite phase and ${\sigma}$-phase. The R phase was an intermetallic compound, which represented a lower Ni and higher Mo than the matrix, and also had a higher Mo and Cr concentration than the ${\sigma}$ phase. With an increasing aging time, the pitting potential $E_p$ was increased slowly by the precipitation of the R-phase, and it was then steeply decreased by the precipitation of the ${\sigma}$-phase. The R-phase was decreased the pitting potential, but its effect was smaller than effect of ${\sigma}$-phase.

Study of Corrosion Resistance in Super-Duplex, Tungsten-Containing Stainless Steel (텅스텐이 첨가된 슈퍼 2상 스테인리스강의 내부식성에 관한 연구)

  • Choi, Han-Gul;Park, Hyung-Gyun;Jung, Byung-Ho;Han, Hyun-Sung;Bae, Dong-Su;Kang, Chang-Yong
    • Journal of Ocean Engineering and Technology
    • /
    • v.24 no.5
    • /
    • pp.55-59
    • /
    • 2010
  • The effect of aging on the precipitation of the $\sigma$ phase and corrosion resistance in W-substituted, super-duplex stainless steel was investigated. The volume fraction of the $\sigma$ phase and the current density increased as the aging temperature increased up to $750^{\circ}C$, and, then, they decreased. As aging time increased, the volume fraction of the $\sigma$ phase and the current density also increased. The $\sigma$ phase considerably influenced to corrosion resistance. When Mo was substituted for W in super-duplex stainless steel, the volume fraction of the $\sigma$ phase and the current density both decreased markedly.

Characteristic Evaluation Based on the Heat Treatment Conditions of Super Duplex Stainless Steel with 0.2% N as an Additive - Part 1: Mechanical Properties and Microstructure (0.2% N을 첨가한 수퍼 2상 스테인리스강의 열처리 조건에 따른 특성 평가 - 제1보: 기계적 특성 및 미세조직)

  • Ahn, Seok-Hwan;Kang, Heung-Joo;Nam, Ki-Woo
    • Journal of Ocean Engineering and Technology
    • /
    • v.22 no.4
    • /
    • pp.46-50
    • /
    • 2008
  • Super duplex stainless steel has along life in severe environments because of its strength and corrosion resistance. If 0.2$\sim$0.3% Nitrogen in aninterstitial solid solution is added, the austenite structure is reinforced. This improves the solid solution hardening and the anticorrosionability. In this study, the mechanical properties and structures of the super duplex stainless steel with the 0.2% N additive were investigated to determine the effect of various volume fractions on the austenite phase. The various volume fractions and distributions of the austenite structure in the applied test specimens were obtained by changing the heat treatment temperature and cycle. The characteristics by amounts of the $\sigma$ phase obtained from the precipitation heat treatment were alsoinvestigated. From the results, when the austenite volume fraction increases, the tensile strength decreases and elongation increases. And the $\sigma$ phase was rapidly increased by increasing the heat treatment time. When the volume fraction of the $\sigma$ phase increased, tensile strength increased.

Characteristic Evaluation according to Heat Treatment Conditions of Super Duplex Stainless Steel with Additive 0.2% N - Part 2: Fatigue Crack Propagation Behavior (0.2% N을 첨가한 수퍼 2상 스테인리스강의 열처리 조건에 따른 특성 평가 - 제2보: 피로균열진전 거동)

  • Ahn, Seok-Hwan;Kang, Heung-Joo;Seo, Hyun-Soo;Nam, Ki-Woo;Lee, Kun-Chan
    • Journal of Ocean Engineering and Technology
    • /
    • v.23 no.5
    • /
    • pp.79-84
    • /
    • 2009
  • Super duplex stainless steel has long life in severe environments by showing the enough strength and corrosion resistance. Therefore, the fracture mechanics approach needs to support the structural strength integrity for the used material. In this study, fatigue crack propagation behavior was investigated to super duplex stainless steel with 0.2% nitrogen. The various volume fraction and distribution of austenite structure for applied specimen in test were obtained by changing the heat treatment temperature and cycle. From test results, fatigue crack propagation rate showed two kinds of tendency between da/dN and ${\Delta}K$ according to distribution of austenite structure and structure anisotropy.

Improvement of Surface Hardness of 2205 Duplex Stainless Steel by Laser Shock Peening and Observations of Surface Changes (레이저 쇼크 피닝에 의한 2205 듀플렉스 스테인리스강의 표면 경도 향상과 표면 변화 관찰)

  • Lim, H.T.;Jeong, H.M.;Kim, P.K.;Jeong, Sung-Ho
    • Laser Solutions
    • /
    • v.14 no.1
    • /
    • pp.19-24
    • /
    • 2011
  • This work reports the results for laser shock peening of duplex stainless steel (22% Chromium - 5% Nickel) using a pulsed Nd:YAG laser (wavelength = 532nm, pulse width = 8ns). for the application to high-capacity pumps for seawater desalination plants. By properly selecting the process parameters such as laser intensity of 10GW/$cm^2$, laser pulse density of 75pulse/$mm^2$, and $100{\mu}m$ thick aluminum foil as an absorbent coating layer, the surface hardness of duplex stainless steel could be enhanced by 26%, from 256HV to 323HV with little changes in surface morphology and roughness. The depth of laser shock peened layer was measured to be around 2mm. The large enhancement of surface hardness is considered to have high practical importance in minimizing abrasive and corrosive deterioration of pump parts.

  • PDF

Influence of Gadolinium Addition on Mechanical and Corrosion Properties of 2205 Duplex Stainless Steel (가돌리늄 첨가에 따른 2205 듀플렉스 스테인레스 강의 기계적 및 부식 특성 변화)

  • Lim, Jae-han;Ahn, Ji-Ho;Moon, Byung-Moon;Kim, Young-Jig
    • Journal of Korea Foundry Society
    • /
    • v.35 no.6
    • /
    • pp.163-169
    • /
    • 2015
  • This study reports the influence of gadolinium (Gd) addition on mechanical and corrosion properties of 2205 duplex stainless steel. In all alloys produced, regardless of the initial Gd content, Gd-based inclusions were well distributed in the duplex stainless steel matrix. As the Gd content increased from 0 wt% to 0.19 wt%, the ultimate tensile strength and hardness of the alloy increased from 630 MPa to 977 MPa and from 57 to 61, respectively, while elastic modulus, tensile elongation and impact energy of the alloy decreased. The critical crevice temperatures of Alloy1, Alloy2 and Alloy3 were $20^{\circ}C$, $20^{\circ}C$ and $15^{\circ}C$, respectively.

The Applications of the Duplex Stainless Steel as Hyperthermia Materials

  • Kim, Young-Kon
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2009.05a
    • /
    • pp.7.1-7.1
    • /
    • 2009
  • The use of Duplex stainless steel as a thermo-implant categorizes into two clinical applications: hyperthermia and thermal ablation or destruction. The goal of hyperthermia is to destroy the heat-sensitive abnormal cells and minimize normal cell death maintaining heat between $42^{\circ}C$ and $46^{\circ}C$. Thermal ablation takes place when the local tissue temperature increases greater than $46^{\circ}C$. This elevated temperature denatures protein irreversibly resulting cellular death. The author introduced several thermo-implants such as thermo-rod, thermo-stent, thermo-coil and thermoacupuncture-needle. Those thermo-implants are made of duplex stainless steel which can produce regulated heat by itself within an induction magnetic field. Thermal ablation characteristics of the thermo-rod on tumor hyperthermia depend on configurations of the thermo-rods and the magnitude of the induction magnetic strength. The exothermic properties of the thermo-implants can be characterized using the calorimetric test and the heat affected zone(HAZ) analyses in vitro. Thermal radiation studies using thermo-coils and thermo-stents show the capability of the occlusion of animal blood vessels and inhibiting the proliferation of the abnormal smooth muscle cell growth and inflammatory cell reactions maintaining the heat between $42^{\circ}C$ and $46^{\circ}C$ minimizing a normal cell death in the study on external iliac artery of the New Zealand White (NZW) rabbit. Thermal stimulation study using thermo-acupuncture needles suggests the potential applications of the automated acupunctural therapies.

  • PDF

Effect of Alloying Composition and Plastic Deformation on the Microstructure of 22Cr Micro-Duplex Stainless Steel (합금원소와 소성변형이 22Cr 마이크로 듀플렉스 스테인리스강의 미세조직에 미치는 영향)

  • Park, Jun-Young;Ahn, Yong-Sik
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.11
    • /
    • pp.793-800
    • /
    • 2012
  • The effect of cold rolling on the microstructural evolution in 22Cr-0.2N micro-duplex stainless steel was investigated. The 22Cr-xNi-yMn-0.2N duplex stainless steel plates with various Ni and Mn contents were fabricated. The steels were vacuum induction melted and hot rolled, followed by annealing treatment at the temperature range of $1000-1100^{\circ}C$, in which both the austenite and ferrite phases were stable. The volume fraction of the ferrite phase depending on the alloy compositions of Ni and Mn increased with an increase in the annealing temperature. Grain growth in the ferrite phase occurred markedly after cold rolling followed by annealing, while fine recrystallised grains were still found in the austenite phase. A large number of martensite laths was found in the microstructure of cold rolled steels, which should be formed by strain-induced martensite from the austenite phase. The intersections of stacking faults were revealed by TEM observation. The volume fraction of the martensite phase increased with an increase of the reduction ratio by cold rolling.

Effects of pH and Chloride Concentration on Corrosion Behavior of Duplex Stainless Steel and Titanium Alloys Ti 6Al 2Nb 1Ta 1Mo at Elevated Temperature for Pump Impeller Applications

  • Aymen A., Ahmed;Ammar Yaseen, Burjes;Ammar Yaseen, Burjes
    • Corrosion Science and Technology
    • /
    • v.21 no.6
    • /
    • pp.454-465
    • /
    • 2022
  • The objective of this study was to determine effects of temperatures and pH of sodium chloride solution with MgCl2 ions on corrosion resistance of duplex stainless-steel X2CrNiMoN22-5-3 (DSS) and Ti 6Al 2Nb1Ta1Mo (Ti). Effects of sodium chloride concentration on corrosion resistance were also studied. Corrosion behavior and pitting morphology of duplex stainless steel (DSS) and Ti alloys were evaluated through potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and scanning electron microscopy (SEM). It was found that a decrease in pH significantly reduced the corrosion resistance of both alloys. Changes in chloride concentration and temperature had more substantial impact on corrosion behavior of DSS than on Ti alloys. Pitting corrosion was formed on DSS samples under all conditions, whereas crevice corrosion was developed on Ti samples with the presence of magnesium chloride at 90 ℃. In conclusion, magnesium chloride ions in an exceedingly strong acidity solution appear to interact with re-passivation process at the surface of these alloys and influence the resulting surface topography.

Fatigue Crack Propagation Characteristics of Duplex Stainless Steel Weldments (I) (이상계 스테인리스강 용접부의 피로크랙 전파특성 (I))

  • 권종완;김상태;이택순
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.12 no.4
    • /
    • pp.738-746
    • /
    • 1988
  • Fatigue crack propagation of duplex stainless steel weldments was studied to develop further phenomenological understanding of the influences of welding heat cycle accompanying microstructural changes. Fatigue tests were carried out under constant amplitude of load in air at room temperature. The results showed that the crack propagation rate was different in base metal, heat affected zone and welding line. The crack propagation behavior in each part of duplex stainless steel was strongly dependent on phase ratio(.gamma../.alpha.) and several factors of microstructure also affected this propagation behavior. The fractographic feature in each part of steel were discussed on crack propagation behaviors.