• Title/Summary/Keyword: dry-cleaning

Search Result 335, Processing Time 0.028 seconds

A study on the properties of commercial nonwoven fabrics (시판 부직포의 물성에 관한 연구)

  • Soon Song Wha
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.11 no.1
    • /
    • pp.79-85
    • /
    • 1987
  • The purpose of this study was to help the consumer about the care of nonwoven fabrics by investigation of the properties such as launderability. shrinkage, color fastness and strenth. Materials used were two types, soft and stiff, of commercial nonwoven fabrics. Deter-gents used were neutral detergents, synthetic detergents and dry cleaning solutions(perch-toro-ethylene) The results of this study were summerized as follows; 1. Laundering of nonwoven fabrics in low temperature is more ideal as morphological changes by laundering in high temperature were more prominent than that in low temperature. 2. Ironing of nonwoven fabrics wants more attention on environmental temperature as the rate of shrinkage in high temperature was higher than that in low temperature. Neutral detergents are more desirable as the rate of shrinkage of nonwoven fabrics by laundering with synthetic detergents was more prominent than that with neutral deter-gents. The rate of shringkage of nonwoven fabrics was not affected by dry cleanining. 3. Special care is wanted in order to prevent color transfer from non woven fabrics to polyester or wool during dry cleaning or laundering as the color fastness test show that color changes of nonwoven fabrics were not affected, but that color stain was increased on polyester or wool. 4. The strength was affected by composition of fibers and types of nonwoven fabrics, soft or stiff.

  • PDF

Durable Water and Oil Repellent Finish of Wool Fabric(II) (양모직물의 내구성 발수 및 발유가공(II))

  • 나도춘;정순량;박병기;정경락
    • Textile Coloration and Finishing
    • /
    • v.10 no.4
    • /
    • pp.1-6
    • /
    • 1998
  • It is important in the durable water and oil repellent finishing for wool fabric what kinds of water-repellent agents will be used. Water repellent agents and its concentration were aleady chosen in the previous paper, one of the crosslinking agents which has less damages(harsh handle or yellowing) to the treated fabrics was a low molecular weight urethane-based resins(eg. Elastron BN-11). In repellent finishing, fabrics were padded in a bath which contained aqueous solution of water-repellent agents, and crosslinking agents, and wetting agents, followed by drying and curing. The most suitable treating condition for excellent repellency and durability to dry-cleaning was as follows : Fabrics are padded at liquor pick-up ratio of 50%, with aqueous solution which contained $30g/\ell$ of water-repellent agents, and $1g/\ell$ of crosslinking agents, and 40g/s of wetting agents. And the padded fabrics were dried at $110^\circ{C}$ for 1 minute, and cured at $160^\circ{C}$ for 1 minute. For the fabrics, water and oil repellencies and durability to repeated dry-cleanings were observed. For enhancing the durability to dry-cleaning, the role of crosslinking agents was important for they bonds water-repellent agents and fibers to 3-dimensional net structure. Therefore, the most suitable drying and curing conditions should be selected according to the kinds of crosslinking agents.

  • PDF

An Experimental Study on Explosion Hazard of Dry Cleaning Solvent Recovery Machine in Laundry (세탁소 유기용제 회수건조기의 폭발 위험성에 관한 실험적 연구)

  • Choi, Jung-Min;Son, Bong-Se;Kim, Dong-Suk
    • Fire Science and Engineering
    • /
    • v.27 no.1
    • /
    • pp.39-45
    • /
    • 2013
  • This study analyzes the explosion hazard of dry cleaning solvent recovery machine in laundry shop in two aspects, i.e. combustible and ignition source, and determines the explosive conditions of this machine by conducting mockup explosion tests repeatedly, varying conditions and using real dry cleaning solvent recovery machines. As to combustibles, two kinds of combustibles used widely in Korea have been selected and tested. The flash points, LEL's, and saturation vapor pressures of those combustibles have been measured, and their explosion specific curves have been drawn, based on the results of the measurements, so that the explosion risks of those materials may be determined, depending on the temperatures. Potential voltages generated from materials for laundry and foreign materials of metals have been assumed to be the ignition sources in this application, and their potential voltages have been measured, depending on temperature, humidity, and antistatic agent, by using real materials for laundry and a potential voltage measuring device. Tests have been conducted, varying the quantities, concentrations, and operating temperatures of materials for laundry. As a result, explosions have not been generated with potential voltages of materials for laundry, but explosions have been observed when applying artificial spark energy of 2.0 mJ.

A Study on the Cleaning Resistance of Chrome-Tanned Garment Leathers. (II) - Effect on the Fading and Stiffening by DryCleaning Solvents - (의류용 크롬유혁의 내클리닝성에 관한 연구(II) -드라이클리닝 용제의 종류에 의한 변색과 경화를 중심으로-)

  • 조승식;심미숙;김운배
    • Textile Coloration and Finishing
    • /
    • v.2 no.1
    • /
    • pp.1-7
    • /
    • 1990
  • The cleaning resistance of tanned chrome garment leathers was investigated by using drycleaning solvents. Hydrocarbon, perchloroethylene and fluorocarbon (F-113) were used as solvent. Various test methods, such as color difference test, surface view by scanning electron microscope, mechanical properties measured by KES-FB System and their hand values and wearing abilities are carried out in this study. The results can be obtained as follows: 1. Fluorocarbon type (F-113) was demonstrated a suitable solvent for drycleaning of leather. 2. Perchloroethylene showed the worst in fading and stiffening among three different types of solvents.

  • PDF

Atmospheric Plasma application for dry cleaner, PR ashing & PI rework in the $5^{th}$ generation and beyond LCD production

  • Park, Young-Chun;Lee, Bong-Ju
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2003.07a
    • /
    • pp.421-424
    • /
    • 2003
  • An AP plasma technology has been developed for the application of dry cleaner, PR ashing and PI rework in the large glass size. The technology is cost effective, environment friendly, and best fits for coming generation LCD production since the design is easily scalable to bigger size glasses. Surface cleaning results based on the contact angle study has been presented for $5^{th}$ generation LCD bare glass. PR ashing results and various parametric studies have been also presented.

  • PDF

Removal of Nano-scaled Fluorescence Particles on Wafer by the Femtosecond Laser Shockwave (펨토초레이저 충격파에 의한 형광 나노입자 제거)

  • Park, Jung-Kyu;Cho, Sung-Hak;Kim, Jae-Gu;Chang, Won-Seok;Whang, Kyung-Hyun;Yoo, Byung-Heon;Kim, Kwang-Ryul
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.26 no.5
    • /
    • pp.150-156
    • /
    • 2009
  • The removal of tiny particles adhered to surfaces is one of the crucial prerequisite for a further increase in IC fabrication, large area displays and for the process in nanotechnology. Various cleaning techniques (wet chemical cleaning, scrubbing, pressurized jets and ultrasonic processes) currently used to clean critical surfaces are limited to removal of micrometer-sized particles. Therefore the removal of sub-micron sized particles from silicon wafers is of great interest. For this purpose various cleaning methods are currently under investigation. In this paper, we report on experiments on the cleaning effect of 100nm sized fluorescence particles on silicon wafer using the plasma shockwave occurred by femtosecond laser. The plasma shockwave is main effect of femtosecond laser cleaning to remove particles. The removal efficiency was dependent on the gap distance between laser focus and surface but in some case surface was damaged by excessive laser intensity. These experiments demonstrate the feasibility of femtosecond laser cleaning using 100nm size fluorescence particles on wafer.

Factors in Dry Period Associated with Intramammary Infection and Subsequent Clinical Mastitis in Early Postpartum Cows

  • Leelahapongsathon, Kansuda;Piroon, Tipapun;Chaisri, Wasana;Suriyasathaporn, Witaya
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.29 no.4
    • /
    • pp.580-585
    • /
    • 2016
  • The objective of this study was to determine cow characteristics and farm management factors during the dry period associated with early postparturient intramammary infection (IMI) and subsequent clinical mastitis (CM). Data were collected three times: before drying off (P1), during the dry period (P2), and 5 to 14 days after calving (P3), using questionnaires and farm investigation. Milk samples were aseptically collected for bacterial identification at P1 and P3. Factors associated with IMI and CM were analyzed using multiple logistic regression models. The final model showed that IMI in early postpartum was significantly associated with full insertion of dry cow antibiotic, dry cows in barns with a combination of tie and free stalls, body condition score (BCS) in dry period and after calving, and milk yield before drying off. For IMI cows, factors significantly associated with clinical expression of mastitis were having daily barn cleaning, teat disinfected with alcohol before administration of dry cow therapy, BCS before drying off, milk yield before drying off, and days in milk at drying off. In conclusion, both cow and farm management factors are associated with the IMI rate and subsequent expression of clinical signs of mastitis in early postpartum cows.

Review of Problems with Use of Halogenated Cleaning Solvents Revealed through Case Studies of Cleaning Solvent Poisoning and Analysis of Domestic and Overseas Regulations (세척제 용매 중독 사례와 국내·외 규제 검토를 통한 할로겐화 용매 세척제 사용의 문제점 고찰)

  • Naroo Lee;Hye Jin Lee;Sujin Jeong;Dohee Lee;Arom Shin
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.33 no.4
    • /
    • pp.517-527
    • /
    • 2023
  • Objectives: We examine cases of chemical poisoning that occurred in the cleaning of metal parts and the regulations on halogenated solvents in other countries and propose regulations necessary to prevent chemical poisoning from halogenated solvents. Methods: We collected cases of chemical poisoning through the website of the Korea Occupational Safety and Health Agency. A review of the literature was conducted focusing on regulations related to halogenated solvents in the United States and the European Union, particularly for cleaning metal parts. Among the Material Safety Data Sheets submitted to the government, MSDS containing eleven substances were extracted to confirm the composition and product use. We investigated cleaning methods for metal parts used in South Korea. For the hazard classification, the European Chemicals Agency or Japan's NITE's website was used. Results: In the case of poisoning, the cleaning methods involving trichloromethane were dipping and dry, which was not found in the literature. It was confirmed that many halogenated solvents and dimethyl carbonate were used for metal cleaning in South Korea. In vapor degreasing using TCE in the USA, even if the facility is strictly managed, such as by installing cooling coils in open cleaning facilities, the risk of exposure to TCE is considered to be not only carcinogenic but also a concern for acute and chronic effects. In comparison, exposure through Korean work methods such as dipping and drying operations is inevitably much higher. Conclusions: The transition to water-based cleaning with low-hazard chemicals should be a priority in the cleaning process. In the case of metal parts that require precise cleaning, if the use of a halogenated solvent is inevitable, a closed degreasing facility should be used to minimize exposure. The current regulations in the Occupational Safety and Health Act, the Chemical Substances Control Act, and the Air Environment Conservation Act do not require cleaning facilities to minimize emissions. To protect the health of workers using halogenated solvents to clean metal parts, regulations that require a fundamental reduction in exposure will be necessary.

Effect of Wet Cleaning on Shrinkage and Detergency of Wool and Rayon Fabrics (웨트클리닝이 양모, 레이온 직물의 치수 안정성과 세탁성능에 미치는 영향)

  • Chung, Seung-Eun;Yun, Chang-Sang;Park, Chung-Hee;Kim, Hyun-Sook
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.36 no.2
    • /
    • pp.127-137
    • /
    • 2012
  • This study focuses on the optimal washing conditions for dry cleaning recommended fabrics to minimize dimensional changes using wet cleaning. We suggest water-based alternatives to a perchloroethylene based cleaning process. Wool and rayon fabrics were laundered under various washing conditions and then air-dried for 24hrs. All specimens were extended after spinning and shrunk after drying. This is probably because the fibers were swollen and extended by wetting. The wool fabrics were shown to be acutely influenced by washing temperature and mechanical force. The optimal washing conditions for wool fabric to minimize the dimensional change implied a normal washing temperature and minimized mechanical force. For rayon specimens, dimensional change by a hand wash showed a remarkable decrease compared with a machine wash. Rayon fabric seemed to be influenced by the quantity of water contained in the fabric after spinning and washing time. Therefore, the desirable washing conditions for rayon fabric are to reduce the time required for washing and to increase the spin speed.