Physical Properties of Nylon Textured Yarn according to False Twist Texturing Parameters (II) - Effect of Disk/Yarn and Temperature - (가연조건에 따른 나일론 섬유의 물성 (II) - Disk/Yarn과 온도의 영향 -)

  • Hu, Jong-Tea
    • Textile Coloration and Finishing
    • /
    • v.20 no.1
    • /
    • pp.36-43
    • /
    • 2008
  • False twist texturing uses the thermoplastic property of synthetic yarn and produces a bulk and a stretch by giving the filament a permanent crimp. This study investigated the effects of false twist texturing parameters, disk/yarn(D/Y) and heater temperature, on the physical properties of nylon textured yarn. D/Y was a primary determinant of twist numbers of filaments and was proportionally increased with the twist numbers of filaments, resulting in an increase of crimp rigidity of the textured yarn. Heater temperature, a determinant of the heat setting of transformed filaments, was proportionally increased with the increase of crimp rigidity. Nylon 6 was partially melted at $190^{\circ}C$. This study consequently suggested the optimal parameters of nylon 6 85d/68f full-dull POY.

Physical Properties of Nylon Textured Yarn according to False Twist Texturing Parameters (I) - Effect of Speed and Draw Ratio - (가연조건에 따른 나일론 섬유의 물성 (I) - 가연속도와 연신비의 영향 -)

  • Hu, Jong-Tea
    • Textile Coloration and Finishing
    • /
    • v.20 no.1
    • /
    • pp.28-35
    • /
    • 2008
  • Texturing is the process of including a characteristic of a natural fiber in a synthetic fiber. The most common method of it the false twist texturing. Nylon textured yarn is primarily manufactured by the disk type. The major process parameters or the disk type false twist machine ratio, disk/yarn, and heater temperature. This study therefore investigated the effects of false twist texturing, especially speed and draw ratio, on the physical properties of nylon textured yarn. The increase of speed was proportional to the increase of unwinding tension, which could reduce the production efficiency by elevating the tension affecting to fiber during the process. In addition, the increase of speed was inversely proportional to the increase of crimp rigidity of nylon textured yarn. Draw ratio was proportionally increased with the increase of tenacity and the reductions of fineness and elongation, showing the influence or draw ratio to the ultimate physical properties of textured yarn.

A Study on the Physical Properties of DTY Composite Yarns Manufactured by Pin, Disk and Belt Texturing Systems (핀ㆍ디스크ㆍ벨트 가연 시스템에서 제조된 DTY 복합사의 물성에 관한 연구)

  • 김승진;이종걸;박경순
    • Textile Coloration and Finishing
    • /
    • v.16 no.3
    • /
    • pp.39-46
    • /
    • 2004
  • This study surveys the physical properties of DTY composite yarns manufactured by pin, disk and belt texturing systems. For this purpose, 208d/36f POY PET and 40d/12f high shrinkable PET filaments are prepared for specimens. The composite yarns are manufactured with this texturized POY and high shrinkable PET filament using the pin, disk and belt type texturing machines. While the processing conditions of the pin and disk types texturing machines were fixed, those of a belt type texturing machine were varied with over feed to compare and analyze with the yarn physical properties of pin and disk type composite yarns.

Dyeing Properties of Nylon Textured Yarn according to False Twist Texturing Parameters(I) - Effect of Draw Ratio - (가연조건에 따른 나일론 섬유의 염색특성 (I) - 연신비의 영향 -)

  • Hu, Jong-Tea
    • Textile Coloration and Finishing
    • /
    • v.20 no.2
    • /
    • pp.47-52
    • /
    • 2008
  • Nylon textured yarn is usually manufactured by disk type false twist texturing. Dyeing properties of nylon textured yam have not been studied yet. In this study, dyeing properties of nylon textured yam according to draw ratio out of process parameters were investigated. The fact that microstructure of nylon textured yarn in amorphous region particularly is transformed by draw ratio was confirmed indirectly by measurement of dyeing rate because dyeing rate was affected by the structure of amorphous region. Dyeing rate at draw ratio 1.29 was the lowest because the higher draw ratio increase amorphous orientation and disturb dye diffusion into amorphous region. The microstructure according draw ratio was indirectly confirmed by 5% strength, tenacity, elongation. But difference in K/S value and fastness was insignificant.

The Effect of PET Filament Yarn and Properties and False Twist Processing Conditions on the Physical Properties of DTY (PET 원사와 가연공정 특성이 DTY의 물성에 미치는 영향)

  • 박경순;김승진;정기진;강지만
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2003.04a
    • /
    • pp.122-125
    • /
    • 2003
  • Easy-care성을 장점으로 하여 천연섬유 대체용으로 점차 차별화가 진행되며 개발된 PET 섬유는 범용적인 섬유특성으로 인해 의류ㆍ비의류용 분야에서 광범위한 소재로 많이 사용되고 있다. 고부가가치의 직물을 생산하기 위해서는 원사의 특성뿐만 아니라 원사 이후의 공정 특히 사가공공정에서의 각공정에 따른 絲의 물성을 파악하는 것이 중요하다. 원사를 가연하는 공정 중 최근 disk spindle과 큰축을 이루고 있는 belt 가연기구는 높은 생산속도와 균일한 가공사를 생산할 수 있어 많이 사용하고 있다. (중략)

  • PDF

A study on Optimum Design of Beating Cam Meachanism for Shuttleless Loom (무북직기용 Beating Cam 기구의 최적설계에 관한 연구)

  • Kim, Jong-Su;Sin, Jung-Ho
    • 연구논문집
    • /
    • s.22
    • /
    • pp.75-83
    • /
    • 1992
  • The beating motion of a high speed shuttleless loom is driven by cams. Two cams become one system and their shaft laid across each other. Moreover, the shape of the cams is very complex and requires high precision for successful weft insertion and good interlacing with warp yarn. The iterative contact method is developed for use in design and analysis of the driving mechanism of a disk type cam with oscillating roller follower. The optimum design is performed by utilizing a CAD program, DISKCAM. The 8th order polynomial is selected to interpolate the desired shape trajectory of the cam, the optimal shape of the cams is defined based on the demension of the follower. The kinematic motion of the beating cam mechanism is investigated. The phase angle is determined to achive harmonious cam motions

  • PDF