The paper deals with a non-linear finite element analysis of the thermomechanical distortions of an elastomeric O-ring seal including a temperature gradient. Axial compression of O-ring seals, as well as the influence of the temperature gradients and various O-ring seal models, are investigated based on the axisymmetric analysis. The highest temperature occurs near the interface of the O-ring between the dovetail groove bottom and the O-ring seal. The calculated FEM results indicate that the composite O-ring with the diametral ratio, 0.8 shows very stable and recommendable compared with other seal models far elevated temperatures and corrosive environments.
The purpose of this study was to evaluate the influences of incorporation of zirconium-silicate on diametral tensile strength, shear bond strength to the enamel, and depth of cure of 7 experimental composites. One group contained no filler(group 1 or control group), and the other 6 composites contain 75% filler in which zirconium-silicate(Zr-Si) were 0%, 2%, 4%, 6%, 8%, 10% with reduced contents of silica filler, respectively. Both of fillers were treated with 1% silane (${\gamma}$-methacryloxypropyltrimethoxy silane). Light curable monomers were prepared by mixing Bis-GMA and TEGDMA with 3:1 ratio and adding camphoroquinone(CQ) 0.6% with tertiary amine 0.3%. Diametral tensile strengths of specimens with $3mm{\times}6mm$ were measured with Instron (No.4467, USA) with 1mm/min crosshead speed. Shear bond strengths of composites which bonded to bovine enamel etched with 37% phosphoric acid were measured at Instron Testing Machine with as same speed as in diametral tensile strengths. Depth of cure were measured by a method that composite was filled in cylinder mold, illuminated at one side. and uncured composite was removed with acetone, and the residual thickness of composite was measured. Following results were obtained ; 1. Composites containing 0%, 2%, or 4% zirconium-silicate filler(group 2, 3 and 4) showed the statistically higher diametral tensile strength than the others. (p<0.05) 2. Increase of zirconium-silicate filler contents reduced the diametral tensile strength of experimental composites. ($r^2$=0.8721, p=0.0002) 3. Increase of zirconium-silicate filler contents did not affect the shear bond strength of experimental composites. ($r^2$=0.2815, p=0.4067) 4. Increase of zirconium-silicate filler contents reduced significantly the depth of cure of experimental composites. ($r^2$=0.9700, p<0.0001) These results mean that the mechanical properties of composites could not be improved by incorporation of small amount of zirconium-silicate filler. Also, the increased contents of zirconium-silicates fillers was found to reduce the diametral tensile strength and depth of cure.
The purpose of this study was to search the optimal silane concentrations for filler- silanization of seven experimental composites. Silica filer was a 25micron crushed type. 0.0%, 0.5%, 1.0%, 1.5%, 2.0%, 2.5%, and 3.0% silane($\gamma$-methacrylooxypropyltrimethoxysilane)were added into silica-filler with weight percentage (wt%). Mixtures(silica filler/silane)were reacted at 6$0^{\circ}C$ for 72hours, and crushed into fine particles those were used as fillers for 7 experimental composites. Monomer was a 3 : 1 mixture of Bis-GMA and TEGDMA containing 0.2% tertiary amine and 0.4% camphoroquinone for light curability. A ratio for mixing the monomer and filler was 75% and 25% respectively. Seven experimental composites was classified with the concentration of silane treated, and the specimen number for each test was 10. Specimens with 6mm diameter and 3mm height dimension for measuring the diametral tensile strength were destroyed with 1mm/min cross-head speed on Instron universal testing machine (No. 4467, USA). Shear bond strength was measured on the specimens bonded to bovine enamel etched with 37% phosphoric acid solution for 1 minute Fractured surfaces were observed by SEM (Hitachi S-3200, Japan) among that of the highest values measured from each groups. Following results were obtained: 1. Experimental composites containing silanized filter showed the significantly higher diametral tensile strength and shear bond strength than the composites containing un-silanized fillers(Group1) (p<0.05). 2. In silanized filler composite resins(Group 2~7), Diametral tensile strength of Group 3 showed the significantly higher than that of Group 2 and Group 6(p<0.05). 3. Shear bond strength was higher in Group 3 than that of Group 7 (p<0.05)in silanized fillers composite resins. 4. Fracture surface was formed in resin matrixes on the specimens from composites containing the fillers treated with 0.5% 1.0%, and 1.5% silane. These results mean that the optimal silane concentrations are exist for each fillet with its size and surface area, and that 1.0% is a optimal value for concentration to coat the 25$\mu\textrm{m}$ filler with silane.
Park, S. J.;Kim, S. M.;Kim, M. H.;Kim, C. S.;Lee, C. H.
Proceedings of the Korean Society for Agricultural Machinery Conference
/
2000.11b
/
pp.388-395
/
2000
This study was performed to examine the effects of infrared (IR)/heated-air combination drying on some quality attributes of Korean white ginsengs. Ginseng roots were dried in a dryer where both the far infrared ray and heated-air are available as drying energy sources. Diametral shrinkage, external color, total saponin content, and ginsenosides and free sugar composition of the IR/heated-air combination dried ginsengs were measured and compared with those of commercial white ginseng products. The external color became lower in lightness and higher in saturation as the IR radiating plate temperature increased. IR/heated-air combination dried white ginsengs at IR plate temperature of 100$^{\circ}C$ was comparable to the commercial white ginseng products in color characteristics. Diametral shrinkage ratios ranged from 20 to 36% and appeared to be independent on the different drying methods. No definite evidence could be found whether the IR/heated-air combination drying and the conventional. hot-air drying practice resulted in white ginsengs having different ginsenoside contents and compositions. No conclusion could be made on whether the various drying treatments used in the study had effects on the free sugar contents and compositions of white ginsengs.
Kim, Dong-Ae;Kim, Gyu-Ri;Jun, Soo-Kyung;Lee, Jung-Hwan;Lee, Hae-Hyoung
Korean Journal of Dental Materials
/
v.44
no.1
/
pp.69-77
/
2017
The aim of this study was to investigate the effects of chitosan powder addition on the strengthening of conventional glass ionomer cement. Two types of chitosan powders with different molecular weight were mixed with conventional glass ionomer cement (GIC): low-molecular weight chitosan (CL; 50~190 kDa), high-molecular weight chitosan (CH; 310~375 kDa). The chitosan powders (CL and CH) were separately added into the GIC liquid (0.25-0.5 wt%) under magnetic stirring, or mixed with the GIC powder by ball-milling for 24 h using zirconia balls. The mixing ratio of prepared cement was 2:1 for powder to liquid. Net setting time of cements was measured by ISO 9917-1. The specimens for the compressive strength (CS; $4{\times}6mm$), diametral tensile strength (DTS; $6{\times}4mm$), three-point flexure (FS; $2{\times}2{\times}25mm$) with flexure modulus (FM) were obtained from cements at 1, 7, and 14 days after storing in distilled water at $(37{\pm}1)^{\circ}C$. All mechanical strength tests were conducted with a cross-head speed of 1 mm/min. Data were statistically analyzed by one-way ANOVA and Tukey HSD post-hoc test. The mechanical properties of conventional glass ionomer cement was significantly enhanced by addition of 0.5 wt% CL to cement liquid (CS, DTS), or by addition of 10 wt% CH (FS) to cement powder. The CL particles incorporated into the set cement were firmly bonded to the GIC matrix (SEM). Within the limitation of this study, the results indicated that chitosan powders can be successfully added to enhance the mechanical properties of conventional GIC.
The experimental study was carried out to evaluate the characteristics of the point load index and the uniaxial compressive strength of inherently anisotropic shale in the laboratory. In the testing program the effects of size and the shape on the point load index were investigated both in the axial and diametral direction. In general, the point load index of the shale was constant when the length/diameter (L/D) ratio of the specimen is greater than 1.0 in the diametral direction. The point load index in axial direction shows slight decrease as the L/D ratio is increased and the corner breakage was observed when L/D ratio is greater than unity. The minimum point load index was observed in the bedding angle of $\beta=15^{\circ}{\sim}30^{\circ}$ in the axial point load tests and of $\beta=30^{\circ}$ in the uniaxial compression tests. The relationship between the point load index and the uniaxial compressive strength was linear to ${\sigma}_c=25.0 I_{s(50)}$ for the specimen with the bedding plane angle, $\beta$ at the range of $0^{\circ}{\sim}90^{\circ}$. On the other hand, this relationship was appeared linear to ${\sigma}_c=14.4 I_{s(50)}$ when the bedding angle, $\beta$ is fixed to 90${^{\circ}}$ and this correlation is much different from ${\sigma}c=22 I_{s(50)}, which is generally applied to the rock specimen with no bedding plane in ISRM (1985). The anisotropic strength with different $\beta$ angle shows the shoulder type and this can be suitably modelled by the corrected Ramamurthy'(1993)s equation with the index value of 'n' equal to 3.0.
Journal of the Korean Society of Hazard Mitigation
/
v.10
no.3
/
pp.39-43
/
2010
The main objective of this research is to develop a mechanistic performance predictive model for fatigue cracking of asphalt-aggregate mixtures. Controlled-stress diametral fatigue tests were performed to characterize fatigue cracking of asphalt-aggregate mixtures. Performance prediction model for fatigue cracking was developed using the internal damage ratio (IDR) growth method. In the IDR growth method, the general concepts of the dissipated energy, the reference tensile strain, the threshold tensile strain, and the strain shift factor were introduced. The source of the dissipated energy in the fatigue test is from the intrinsic viscoelastic material property of an asphalt concrete mixture and the damage growth within the asphalt concrete specimen. In controlled-stress mode test, the dissipated energy is gradually increased with an increasing number of load applications.
Fabio Rocha Bohns;Vicente Castelo Branco Leitune;Isadora Martini Garcia;Bruna Genari;Nelio Bairros Dornelles Junior;Silvia Staniscuaski Guterres;Fabricio Aulo Ogliari;Mary Anne Sampaio de Melo;Fabricio Mezzomo Collares
Restorative Dentistry and Endodontics
/
v.45
no.4
/
pp.50.1-50.11
/
2020
Objectives: In this study, we investigated the potential of amoxicillin-loaded polymeric microspheres to be delivered to tooth root infection sites via a bioactive reparative cement. Materials and Methods: Amoxicillin-loaded microspheres were synthesized by a spray-dray method and incorporated at 2.5% and 5% into a mineral trioxide aggregate cement clinically used to induce a mineralized barrier at the root tip of young permanent teeth with incomplete root development and necrotic pulp. The formulations were modified in liquid:powder ratios and in composition by the microspheres. The optimized formulations were evaluated in vitro for physical and mechanical eligibility. The morphology of microspheres was observed under scanning electron microscopy. Results: The optimized cement formulation containing microspheres at 5% exhibited a delayed-release response and maintained its fundamental functional properties. When mixed with amoxicillin-loaded microspheres, the setting times of both test materials significantly increased. The diametral tensile strength of cement containing microspheres at 5% was similar to control. However, phytic acid had no effect on this outcome (p > 0.05). When mixed with modified liquid:powder ratio, the setting time was significantly longer than that original liquid:powder ratio (p < 0.05). Conclusions: Lack of optimal concentrations of antibiotics at anatomical sites of the dental tissues is a hallmark of recurrent endodontic infections. Therefore, targeting the controlled release of broad-spectrum antibiotics may improve the therapeutic outcomes of current treatments. Overall, these results indicate that the carry of amoxicillin by microspheres could provide an alternative strategy for the local delivery of antibiotics for the management of tooth infections.
Transactions of the Korean Society of Mechanical Engineers
/
v.18
no.3
/
pp.591-599
/
1994
A design system for power transmission bevel gears(straight, zerol, and spiral) is developed, in which the strength and durability of bevel gears can be estimated and the size of bevel gears can be minimized by introducing optimal techniques. The size of bevel gear pair as the object function to be minimized is the volume of equivalent spur gear pair at mean normal section, and the design variables to be determined are considered as the number of teeth, face width, diametral pitch, and spiral angle in spiral bevel gear. The strength(bending strength, pitting resistance) according to the AGMA standards, geometrical quantities, and operating characteristics(interference of pinion, contact ratio, etc.) are considered as the constraints in design optimization. The optimization with these constraints becomes nonlinear problem and that is solved with ALM(Augmented Lagrange Multiplier) method. The developed design method is applied to the example designs of straight, zerol, and spiral bevel gears. The design results are acceptable from the viewpoint of strength and durability within the design ranges of all other constraint, and the bevel gears are designed toward minimizing the size of gear pair. This design method is easily applicable to the design of bevel gears used as power transmitting devices in machineries, and is expected to be used for weight minimization of bevel gear unit.
In the ASTM and ISRM, an uniaxial compressive strength(${\sigma}_{c}$) has been estimated to be 23(ASTM) or $20{\sim}25$(ISRM) times of point load strength index using a diametral test regardless of the rock rating or geological conditions. This paper presents a relationship between $I_{s}$ and ${\sigma}_{c}$ of a weak sedimentary rocks on Ulsan of the Kyung-Sang Basin in Korea. In the results of 291 for ${\sigma}_{c}$ test and 2310 for $I_{s}$ test from 77 spots, the predicted errors of ${\sigma}_{c}$ determined by strength ratio of ${\sigma}_{c}/I_{s}$ have been relatively less than those determined by linear regression analysis. And in case of weak sedimentary rocks such as mudstones, shales and sandstones, ${\sigma}_{c}$ should be lower than those suggested by ISRM and ASTM.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.