본 연구의 목적은 2가지 임시 수지 (Bis-acryl resin composite 및 polymethyl methacrylate (PMMA))의 굴곡 강도 및 미세 경도에 대한 경화 순서 및 중합 온도의 영향을 조사하는 것에 있다. 중합은 대기 중 $25^{\circ}C$ (대조) 및 온수 (40, 50, 60, 70 그리고 $80^{\circ}C$)에서 다양한 조건하에 수행되었다. 굴곡 강도 시험은 ISO-4049에 따라 수행되었다. 또한, 누프 경도를 측정 하였다. Bis-acryl resin의 경우, $50^{\circ}C$까지의 온도는 굴곡 강도와 bis-acryl resin composite의 경도를 증가시키지 않았지만 (p> 0.05), 온도가 높을수록 강도가 증가 하였다. PMMA 수지의 경우 굴곡 강도는 최대 $70^{\circ}C$의 온도에서 증가하고 약간 감소합니다. Bis-acryl resin은 PMMA 수지보다 기계적 특성이 더 컸다. 열의 영향은 Bis-acryl resin에서 PMMA 수지보다 더 두드러졌다(p <0.05).
Rocha Maia, Rodrigo;Oliveira, Dayane;D'Antonio, Tracy;Qian, Fang;Skif, Frederick
Restorative Dentistry and Endodontics
/
제43권2호
/
pp.22.1-22.9
/
2018
Objectives: To evaluate and compare light-transmittance in dental tissues and dental composite restorations using the incremental double-layer technique with varying layer thickness. Materials and Methods: B1-colored natural teeth slabs were compared to dental restoration build-ups with A2D and B1E-colored nanofilled, supra-nanofilled, microfilled, and microhybrid composites. The enamel layer varied from 0.3, 0.5, or 1.2 mm thick, and the dentin layer was varied to provide a standardized 3.7 mm overall sample thickness (n = 10). All increments were light-cured to $16J/cm^2$ with a multi-wave LED (Valo, Ultradent). Using a spectrophotometer, the samples were irradiated by an RGB laser beam. A voltmeter recorded the light output signal to calculate the light-transmittance through the specimens. The data were analyzed using 1-way analysis of variance followed by the post hoc Tukey's test (p = 0.05). Results: Mean light-transmittance observed at thicker final layers of enamel were significantly lower than those observed at thinner final layers. Within 1.2 mm final enamel resin layer (FERL) thickness, all composites were similar to the dental tissues, with exception of the nanofilled composite. However, within 0.5 mm FERL thickness, only the suprananofilled composite showed no difference from the dental tissues. Within 0.3 mm FERL thickness, none of the composites were similar to the dental tissues. Conclusions: The supra-nanofilled composite had the most similar light-transmittance pattern when compared to the natural teeth. However, for other composites, thicker FERL have a greater chance to match the light-transmittance of natural dental tissues.
PURPOSE. The aim of this study was to evaluate the effects of additional acid etching and curing mechanism (light-curing or self-curing) of a composite resin on the dentin bond strength and compatibility of one-step self-etching adhesives. MATERIALS AND METHODS. Sixteen human permanent molars were randomly divided into eight groups according to the adhesives used (All-Bond Universal: ABU, Clearfil S3 Bond: CS3), additional acid etching (additional acid etching performed: EO, no additional acid etching performed: EX), and composite resins (Filtek Z-250: Z250, Clearfil FII New Bond: CFNB). Group 1: ABU-EO-Z250, Group 2: ABU-EO-CFNB, Group 3: ABU-EX-Z250, Group 4: ABU-EX-CFNB, Group 5: CS3-EO-Z250, Group 6: CS3-EO-CFNB, Group 7: CS3-EX-Z250, Group 8: CS3-EX-CFNB. After bonding procedures, composite resins were built up on dentin surfaces. After 24-hour water storage, the teeth were sectioned to make 10 specimens for each group. The microtensile bond strength test was performed using a microtensile testing machine. The failure mode of the fractured specimens was examined by means of an optical microscope at ${\times}20$ magnification. The data was analyzed using a one-way ANOVA and Scheffe's post-hoc test (${\alpha}$=.05). RESULTS. Additional etching groups showed significantly higher values than the no additional etching group when using All-Bond Universal. The light-cured composite resin groups showed significantly higher values than the self-cured composite resin groups in the Clearfil S3 Bond. CONCLUSION. The additional acid etching is beneficial for the dentin bond strength when using low acidic one-step self-etch adhesives, and low acidic one-step self-etch adhesives are compatible with self-cured composite resin. The acidity of the one-step self-etch adhesives is an influencing factor in terms of the dentin bonding strength and incompatibility with a self-cured composite resin.
Objectives: This study evaluated the antibacterial effect and mechanical properties of composite resins ($L_{CR}$, $M_{CR}$, $H_{CR}$) incorporating chitosan with three different molecular weights (L, Low; M, Medium; H, High). Materials and Methods: Streptococcus (S). mutans 100 mL and each chitosan powder were inoculated in sterilized 10 mL Brain-Heart Infusion (BHI) solution, and was centrifuged for 12 hr. Absorbance of the supernatent was measured at $OD_{660}$ to estimate the antibacterial activities of chitosan. After S. mutans was inoculated in the disc shaped chitosan-containing composite resins, the disc was cleansed with BHI and diluted with serial dilution method. S. mutans was spread on Mitis-salivarius bacitracin agar. After then, colony forming unit (CFU) was measured to verify the inhibitory effect on S. mutans biofilm. To ascertain the effect on the mechanical properties of composite resin, 3-point bending and Vickers hardness tests were done after 1 and 3 wk water storage, respectively. Using 2-way analysis of variance (ANOVA) and Scheffe test, statistical analysis was done with 95% significance level. Results: All chitosan powder showed inhibition effect against S. mutans. CFU number in chitosan-containing composite resins was smaller than that of control resin without chitosan. The chitosan containing composite resins did not show any significant difference in flexural strength and Vickers hardness in comparison with the control resin. However, the composite resin, $M_{CR}$ showed a slightly decreased flexural strength and the maximum load than those of control and the other composite resins $H_{CR}$ and $L_{CR}$. Conclusions: $L_{CR}$ and $H_{CR}$ would be recommended as a feasible antibacterial restorative due to its antibacterial nature and mechanical properties.
Bond-Fill SB는 분말 / 액체로 만들어져 있으며, 브러시의 액량을 조절하여 유동성을 조절할 수 있습니다. TBB라고하는 강력한 촉매 덕분에 물과 산소가있는 상태에서도 중합이 가능하다는 장점이 있습니다. 또한 4-META를 함유하고있어 적절한 표면 처리로 금속 및 세라믹에 접착 할 수있는 장점이 있습니다. 이러한 장점을 충분히 이해하시면 기존의 복합 레진으로 처리하기 어려운 경우에 적극 활용할 수 있습니다.
치아의 수복에 사용되는 재료인 Methacrylate 기질 복합레진(Clearfil AP-X)과 Silorane 기질 복합레진(Filtek P90)을 대상으로 스트레인게이지법과 FEM 분석법으로 중합수축응력거동을 분석하였다. 또한 복합레진의 탄성계수와 수축변형률을 중합수축응력과 관계시켜 이론식을 제시하고 이 식의 계산결과와 FEM 분석법의 결과를 비교하였다. 스트레인 게이지법으로 측정한 결과, 중합수축응력의 최대값은 Clearfil AP-X가 Filtek P90 보다 약 2.8배 높게 나타났다. FEM 분석 결과, Von-Mises 응력은 복합레진 수복재와 PMMA 링사이의 계면부에서 최대로 되었으며 시편표면의 계면부가 내부보다 응력집중이 더 컸음을 알았다. 예측식을 통한 반경 방향의 수축응력은 평면응력상태의 FEM 분석법을 통한 값과 비교하여 오차 5% 이내로 정확했음을 확인하였다.
Indirect composite resins are used as an popular effective esthetic material in prosthetic dentistry, often with metallic substructure that provides support for restorations. Recently, new indirect composite resins as a substitute of ceramic have been developed. These resins provide good esthetics, with a wide range of hue and chroma. And the flexural strength of those is in the range of 120-150MPa, Which is higher than that of feldspathic Ceramic, and similar th that of Dicor. Although it has many merits, one of the major clinical problems of composite resins is the bond failure between metal and resin due to insufficient interfacial bond strength. The purpose of this study was to evaluate shear bond strength of the reinforced indirect composite resin to dental alloys. Three different composite resin systems($Artglass^{(R)},\;Sculpture^{(R)},\;Targis^{(R)}$) as test groups and ceramic($VMK\;68^{(R)}$) as control group were bonded to Ni-Cr-Be alloy($Rexillium\;III^{(R)}$) and gold alloy(Deva 4). All specimens were stored at $^37{\circ}C$ distilled water for 24 hours and the half of specimens were thermocycled 2000 times at temperature from $5^{\circ}C\;to\;60^{\circ}C$. The shear bond strengths of reinforced indirect composite resins to dental alloys were measured by using the universal testing machine, and modes of debonding were observed by stereoscope and scanning electron microscope. The results were as follows: 1 The shear bond strengths of reinforced indirect composite resins to dental alloys were approximately half those of ceramic to dental alloys(P<0.01). 2. There was no significant difference between the shear bond strength of several reinforced indirect composite resins to metal. 3. Alloy type did not affect on the shear bond strengths of resin to metal, but the shear bond strengths of ceramic to gold alloys were higher than those of ceramic to Ni-Cr alloys(P<0.05). 4. The shear bond strengths of Artglass and Targil to gold alloys were significantly decreased after thermocycling treatment(P<0.01). 5. Sculpture showed cohesive, adhesive, and mixed failure modes, but Artglass and Targis showed adhesive or mixed failures. And ceramic showed cohesive and mixed failures.
Fernandes, Renan Aparecido;Strazzi-Sahyon, Henrico Badaoui;Suzuki, Thais Yumi Umeda;Briso, Andre Luiz Fraga;Santos, Paulo Henrique dos
Restorative Dentistry and Endodontics
/
제45권1호
/
pp.12.1-12.8
/
2020
Objectives: The aim of this in vitro study was to evaluate the microhardness and surface roughness of composite resins before and after tooth bleaching procedures. Materials and Methods: Sixty specimens were prepared of each composite resin (Filtek Supreme XT and Opallis), and BisCover LV surface sealant was applied to half of the specimens. Thirty enamel samples were obtained from the buccal and lingual surfaces of human molars for use as the control group. The surface roughness and microhardness were measured before and after bleaching procedures with 35% hydrogen peroxide or 16% carbamide (n = 10). Data were analyzed using 1-way analysis of variance and the Fisher test (α = 0.05). Results: Neither hydrogen peroxide nor carbamide peroxide treatment significantly altered the hardness of the composite resins, regardless of surface sealant application; however, both treatments significantly decreased the hardness of the tooth samples (p < 0.05). The bleaching did not cause any change in surface roughness, with the exception of the unsealed Opallis composite resin and dental enamel, both of which displayed an increase in surface roughness after bleaching with carbamide peroxide (p < 0.05). Conclusions: The microhardness and surface roughness of enamel and Opallis composite resin were influenced by bleaching procedures.
자이오머는 불소를 유리하는 최근 개발된 광중합 레진 제재이다. 본 실험에서는 복합레진, 자이오머, 컴포머를 이용하여 $5^{\circ}C$와 $55^{\circ}C$에서 5000번 열순환 후 압축강도와 미세경도 변화를 비교 평가하였다. 1. 열순환 전.후 모두 압축강도는 복합레진이 가장 높았으며, 자이오머, 컴포머 순으로 낮아졌다. 복합레진은 자이오머, 컴포머와 통계학적으로 유의차를 보였고(p<0.05), 자이오머와 컴포머 사이에는 유의차가 없었다. 2. 열순환 전.후 미세경도는 복합 레진, 자이오머, 컴포머 순으로 낮아졌으며, 각각 통계학적으로 유의차를 보였다(p<0.05). 3. 복합레진, 자이오머, 컴포머는 열순환 후 통계학적으로 유의하게 미세경도가 감소하였다(p<0.05). 이상의 결과를 종합해보면, 자이오머는 컴포머보다 높은 미세경도를 보이지만, 복합레진보다 낮은 압축강도와 미세경도를 보인다. 열순환 후 미세경도가 감소하므로 임상적 사용시 물리적 성질에 대한 충분한 고찰이 필요할 것으로 사료된다.
There is a difficulty for many practioner in anterior direct restroation with composit resin. Because its result is various according to patient, a practioner have a fear about that unpromisable result. Moreover in esthetic region, there is difference in satisfaction by patient character. That is one of difficulty in this practice. But if we make a manual for parctice it will be easier. So I will summarize the process and things to note in direct anterior composite resin restoration.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.