• 제목/요약/키워드: delamination buckling

검색결과 38건 처리시간 0.022초

Carbon/Phenolic 내열 복합재료의 기계적 특성 (Mechanical Properties of Carbon/Phenolic Ablative Composites)

  • 김평완;홍순형;김연철;예병한;정발
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 1999년도 추계학술발표대회 논문집
    • /
    • pp.160-163
    • /
    • 1999
  • The mechanical properties and failure behaviour of carbon/phenolic composites were inverstigated by tension and compression. Carbon/phenolic composites were fabricated by infiltration of matrix into 8 harness satin woven fabric of PAN-based carbon fibers. The tensile and compressive tests were performed at 25℃ under air atmosphere and, at 400℃ and 700℃ under N₂ atmosphere. The tensile strengths of carbon/phenolic composites in with-laminar/0° warp direction were about 10 times higher than those in with-laminar/45° warp direction, which was analyzed due to a change of fracture mode from fiber pull-out by shear to tensile fracture of fibers. The fracture of carbon/phenolic composites in with-laminar/45° direction was analyzed due to delamination by buckling. Tensile and compressive strength of carbon/phenolic composites decreased to about 50% at 400℃, and to about 10% at 700℃ compared to that at room temperature. The main reason for the decrease of tensile or compressive strength with increasing temperature was analyzed due to a reduction of bond strength between fibers and matrix resulting from thermal degradation of phenolic resin.

  • PDF

Postbuckling response and failure of symmetric laminated plates with rectangular cutouts under uniaxial compression

  • Singh, S.B.;Kumar, Dinesh
    • Structural Engineering and Mechanics
    • /
    • 제29권4호
    • /
    • pp.455-467
    • /
    • 2008
  • This paper deals with the buckling and postbuckling responses and the progressive failure of square symmetric laminates with rectangular cutouts under uniaxial compression. A detailed investigation is made to show the effects of cutout size and cutout aspect ratio on prebuckling and postbuckling responses, failure loads and failure characteristics of $(+45/-45/0/90)_{2s}$, $(+45/-45)_{4s}$ and $(0/90)_{4s}$ laminates. The 3-D Tsai-Hill criterion is used to predict the failure of a lamina while the onset of delamination is predicted by the interlaminar failure criterion. In addition, the effects of boundary conditions on buckling load, failure loads, failure modes and maximum transverse deflection for a $(+45/-45/0/90)_{2s}$ laminate with and without cutout have also been presented. It is concluded that square laminates with small square cutouts have more postbuckling strength than without cutout, irrespective of boundary conditions.

Curvilinear free-edge form effect on stability of perforated laminated composite plates

  • Zerin, Zihni;Basoglu, Muhammed Fatih;Turan, Ferruh
    • Structural Engineering and Mechanics
    • /
    • 제61권2호
    • /
    • pp.255-266
    • /
    • 2017
  • In this study, self-supporting roofing elements especially convenient for large-span structures such as stadium, airport terminal, mall, coliseum, etc. were examined with respect to critical buckling load. These elements were assumed as laminated composite plates and, variation of free-edge forms, cutout types and lamination configurations were used as design parameters. Based on the architectural feature and structural requirements, the effects of curvilinear free-edge form on critical buckling load were focused on in this research. Within this scope, 14 types of lamination configuration were specified according to various orientation angle, number and thickness of plies with a constant value of total plate thickness. Besides that, 6 different types of cutout and 3 different free-edge forms were determined. By combining all these parameters 294 different critical buckling load analyses were performed by using ANSYS Mechanical software based on finite element method. Effects of those parameters on critical buckling load were evaluated referring to the obtained results. According to the results presented here, it may be concluded that lamination conditions have more significant influence on the critical buckling load values than the other parameters. On the other hand, it is perceived that curvilinear free-edge forms explicitly undergo changings depending on lamination conditions. For future work, existence of delamination might be considered and progression of the defect could be investigated by using non-linear analysis.

굽힘 하중을 받는 하니컴 샌드위치 복합재료의 변형 및 파괴 해석 (Deformation and Fracture Analysis of Honeycomb Sandwich Composites under Bending Loading)

  • 김형구;최낙삼
    • Composites Research
    • /
    • 제18권1호
    • /
    • pp.30-37
    • /
    • 2005
  • 본 연구에서는 3점 굽힘 실험과 코어의 실제 형상을 모델링한 유한요소 시뮬레이션을 병행하여 외피층의 항복, 층간분리 코어의 전단 및 국부적 좌굴과 같은 다양한 파손모드를 고려한 하니컴 샌드위치 복합재료의 강도 특성과 변형거동을 검토하였다. 외피층과 하니컴 코어층 사이를 완전 접착한 시험편과 부분 층간분리 시험편을 대상으로 하니컴 코어의 셀 크기와 외피층 두께를 변화시켜 시험편의 굽힘 강성, 굽힘 강도. 굽힘 응력, 변형 및 파손 거동을 해석하였다. 결론적으로 하니컴 코어의 셀 크기와 외피층의 두께가 하니컴 샌드위치 복합재료의 굽힘 강성과 강도, 변형/파괴 거동에 주된 영향을 미쳤으며 코어의 셀 크기가 크고 외피층의 두께가 얇은 경우 굽힘 강도는 $30\~68\%$ 정도까지 저하됨을 알 수 있었다.

다중 층간 분리부가 내재된 복합재 쉘 고차 지그재그 모델의 유한요소 해석 (A Finite Element Analysis based on Higher-Order Zig-Zag Shell Theory for Laminated Composites with Multiple Delamination)

  • 오진호;조맹효
    • 한국전산구조공학회:학술대회논문집
    • /
    • 한국전산구조공학회 2004년도 가을 학술발표회 논문집
    • /
    • pp.229-236
    • /
    • 2004
  • A new three-node triangular shell element based on higher order zig-zag theory is developed for laminated composite shells with multiple delaminations. The present higher order zig-zag shell theory is described in a general curvilinear coordinate system and in general tensor notation. All the complicated curvatures of surface including twisting curvatures can be described in an exact manner in the present shell element because this element is based on geometrically exact surface representation. The displacement field of the proposed finite element includes slope of deflection. which requires continuity between element interfaces. Thus the nonconforming shape function of Specht's three-node triangular plate bending element is employed to interpolate out-of-plane displacement. The present element passes the bending and twisting patch tests in flat surface configurations. The developed element is evaluated through the buckling problems of composite cylindrical shells with multiple delaminations. Through the numerical examples it is demonstrated that the proposed shell element is efficient because it has minimal degrees of freedom per node. The accuracy of the present element is demonstrated in the prediction of buckling loads and buckling modes of shells with multiple delaminations. The present shell element should serve as a powerful tool in the prediction of buckling loads and modes of multi-layered thick laminated shell structures with arbitrary-shaped multiple delaminations.

  • PDF

적층보의 박리좌굴에 관한 해석적 연구 (Analytical Study of Delamination Buckling in Laminated Beams)

  • 김영찬
    • 한국강구조학회 논문집
    • /
    • 제8권4호통권29호
    • /
    • pp.51-58
    • /
    • 1996
  • 연직하중을 받는 적층보에서 박리좌굴하중을 산정하는 방법을 제시하였다. 재료역학적 방법에 근거하여 박리된 보의 변위함수를 설정하였으며 힘과 변위의 적합조건을 이용하여 연직하중과 박리좌굴하중과의 관계식을 유도하였다. 또한 박리의 진전을 판단하기 위한 변형도에너지 방출율(release rate)을 산정하였다. FRP로 보강된 GLULAM보에 대한 실험과 비교한 이론해는 정확한 결과를 보여 주었으며 연직하중을 받는 적층보의 박리 진전현상은 축하중을 받는 보와는 다른 거동을 보였다.

  • PDF

Study the effect of machining process and Nano Sio2 on GFRP mechanical performances

  • Afzali, Mohammad;Rostamiyan, Yasser
    • Structural Engineering and Mechanics
    • /
    • 제76권2호
    • /
    • pp.175-191
    • /
    • 2020
  • In this study, the effect of Nano silica (SiO2) on the buckling strength of the glass fiber reinforced laminates containing the machining process causes holes were investigated. The tests have been applied on two status milled and non-milled. To promote the mechanical behavior of the fiber-reinforced glass epoxy-based composites, Nano sio2 was added to the matrix to improve and gradation. Nano sio2 is chosen because of flexibility and high mechanical features; the effect of Nanoparticles on surface serenity has been studied. Thus the effect of Nanoparticles on crack growth and machining process and delamination caused by machining has been studied. We can also imply that many machining factors are essential: feed rate, thrust force, and spindle speed. Also, feed rate and spindle speed were studied in constant values, that the thrust forces were studied as the main factor caused residual stress. Moreover, entrance forces were measured by local calibrated load cells on machining devices. The results showed that the buckling load of milled laminates had been increased by about 50% with adding 2 wt% of silica in comparison with the neat damaged laminates while adding more contents caused adverse effects. Also, with a comparison of two milling tools, the cylindrical radius-end tool had less destructive effects on specimens.

Cutout shape and size effects on response of quasi-isotropic composite laminate under uni-axial compression

  • Singh, S.B.;Kumar, Dinesh
    • Structural Engineering and Mechanics
    • /
    • 제35권3호
    • /
    • pp.335-348
    • /
    • 2010
  • Cutouts are often provided in structural and aircraft components for ventilation, for access, inspection, electric lines and fuel lines or sometimes to lighten the structure. This paper addresses the effects of cutout shape (i.e., circular, square, diamond, elliptical-vertical and elliptical-horizontal) and size on buckling and postbuckling response of quasi-isotropic (i.e., $(+45/-45/0/90)_{2s}$) composite laminate under uni-axial compression. The finite element method is used to carry out the investigation. The formulation is based on first order shear deformation theory and von Karman's assumptions are used to incorporate geometric nonlinearity. The 3-D Tsai-Hill criterion is used to predict the failure of a lamina while the onset of delamination is predicted by the interlaminar failure criterion. It is observed that for the smaller size cutout area there is no significant effect of cutout shape on load-deflection response of the laminate. It is also concluded that the cutout size has substantial influence on the buckling and postbuckling response of the laminate with elliptical-horizontal cutout, while this effect is observed to be the least in case of laminate with elliptical-vertical cutout.

Stereo-digital image correlation in the behavior investigation of CFRP-steel composite members

  • Dai, Yun-Tong;Wang, Hai-Tao;Ge, Tian-Yuan;Wu, Gang;Wan, Jian-Xiao;Cao, Shuang-Yin;Yang, Fu-Jun;He, Xiao-Yuan
    • Steel and Composite Structures
    • /
    • 제23권6호
    • /
    • pp.727-736
    • /
    • 2017
  • The application of carbon fiber reinforced polymer (CFRP) in steel structures primarily includes two categories, i.e., the bond-critical application and the contact-critical application. Debonding failure and buckling failure are the main failure modes for these two applications. Conventional electrometric techniques may not provide precise results because of the limitations associated with single-point contact measurements. A nondestructive full-field measurement technique is a valuable alternative to conventional methods. In this study, the digital image correlation (DIC) technique was adopted to investigate the bond behavior and buckling behavior of CFRP-steel composite members. The CFRP-to-steel bonded joint and the CFRP-strengthened square hollow section (SHS) steel column were tested to verify the suitability of the DIC technique. The stereo-DIC technique was utilized to measure continuous deformation. The bond-slip relationship of the CFRP-to-steel interface was derived using the DIC data. Additionally, a multi-camera DIC system consisting of four stereo-DIC subsystems was proposed and applied to the compressive test of CFRP-strengthened SHS steel column. The precise buckling location and CFRP delamination of the CFRP-strengthened SHS steel column were identified. The experimental results confirm that the stereo-DIC technique can provide effective measurements for investigating the behaviors of CFRP-steel composite members.

필라멘트 와인딩 공법 GFRP 원형 튜브의 에너지 흡수특성에 관한 연구 (A Study on the energy absorption characteristics of GFRP circular tubes fabricated by the filament winding method)

  • 김거영;구정서
    • Composites Research
    • /
    • 제22권4호
    • /
    • pp.1-12
    • /
    • 2009
  • 본 논문에서는 복합재 원형튜브의 에너지 흡수 특성을 평가하기 위해 준정적 압괴실험을 시행하였다. 사용된 시편은 필라멘트 와인딩 공법으로 제작된 GFRP(유리섬유/에폭시수지) 원형 튜브이다. 복합재 튜브의 에너지 흡수 특성 분석을 위한 파라미터로서 튜브의 트리거메커니즘, t/D, 섬유배향각 등을 고려하여 그 특성을 비교하였다. 튜브의 형상 측면에서 튜브 직경이 커짐에 따라 delamination에 의한 국부좌굴 발생빈도가 증가하게 되어 불안정한 압괴모드가 발생하는데 이러한 현상은 섬유 배향각을 조정하여 안정적인 압괴모드를 도출할 수 있었다.