Catalytic Cracking of Waste Lubricant Oil over Solid Acid Catalysts (고체산 촉매를 이용한 폐윤활유의 촉매 분해)

  • Hwang, In Hye;Yang, Hyeon Sun;Lee, Jong-Jib;Choi, Ko-Yeol;Lee, Chang-Yong
    • Applied Chemistry for Engineering
    • /
    • v.23 no.3
    • /
    • pp.320-325
    • /
    • 2012
  • The catalytic cracking of waste lubricant oil was carried out on silica-alumina (SA), hydrogen-type mordenite (HM), and dealuminated mordenite (DM) with the silica/alumina ratio of 10.5, 10, and 12.5, respectively. Activity in the catalytic cracking was found to be in the order of SA > DM > HM. Carbon number distribution of the oil obtained over SA was similar to that of gasoline while that of the oil obtained over DM was similar to that of diesel. Carbon number distribution of the oil obtained over HM was similar to that between gasoline and diesel. Acid amounts of three kinds of catalysts were found to be in the order of $SA\;{\approx}\;HM$ > DM. Unlike HM and DM with pores of an uniform diameter below 10 A, SA had a pore size distribution within the range of 10 to 50 A. These results indicate that the acid amount and pore size of the catalysts may be related to the carbon number distribution of the cracked oil. The decrement of surface area by the accumulation of carbon and impurities on the surface of the catalyst was found to be in the order of SA > DM > HM.