Growth and Optical Properties of PbSnSe Epilayers Grown on BaF2(111) (PbSnSe 단결정 박막의 성장과 광학적 특성)

  • Lee, Il-Hoon
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.9 no.1
    • /
    • pp.35-41
    • /
    • 2004
  • This study investigated the crystal growth, crystalline structure and the basic optical properties of $PbSnSe/BaF_2$ epilayers. The PbSnSe epilayer was grown on $BaF_2$(111) insulating substrates using a hot wall epitaxy (HWE) technique. It was found from the analysis of X-ray diffraction patterns that $PbSnSe/BaF_2$ epilayer was grown single crystal with a rock-salt structure oriented along [111] the growth direction. Using Rutherford back scattering, the atomic ratios of the PbSnSe was found to be proper stoichiometric. The best values for the full width at half maximum (FWHM) of the DCXRD was 162 arcsec for PbSnSe epilayer. The epilayer-thickness dependence of the FWHM of the DCXRD shows that the quality of the $PbSnSe/BaF_2$ is as expected. The dielectric function ${\varepsilon}(E)$ of a semiconductor is closely related to its electronic energy band structure and such relation can be drawn from features around the critical points(CPs) in the optical spectra. The real and imaginary parts(${\varepsilon}1$ and ${\varepsilon}2$) of the dielectric function ${\varepsilon}$ of PbSe were measured, and the observed spectra reveal distinct structures at energies of the E1, E2 and E3 CPs. These data are analyzed using a theoretical model known as the model dielectric function (MDF). The optical constants related to dielectric function such as the complex refractive index ($n^*=n+ik$), absorption coefficient (${\alpha}$) and normal-incidence reflectivity (R) are also presented for $PbSnSe/BaF_2$.

  • PDF

Physicochemical Properties of Cross-linked Rice Starches (가교화 쌀 전분의 이화학적 특성)

  • Choi, Hyun-Wook;Chung, Koo-Min;Kim, Chung-Ho;Moon, Tae-Hwa;Park, Cheon-Seok;Baik, Moo-Yeol
    • Applied Biological Chemistry
    • /
    • v.49 no.1
    • /
    • pp.49-54
    • /
    • 2006
  • Physicochemical properties of cross-linked rice starches were investigated. Swelling power of cross-linked rice starch increased at relatively lower temperature $(60^{\circ}C)$ than native rice starch $(70^{\circ}C)$. Cross-linked rice starch showed lower solubility $(1.7{\sim}6.1%)$ than native rice starch $(2.2{\sim}13.8%)$ and solubility is not significantly different with the amount of phosphorus oxychloride. Pasting temperature $(69.2{\sim}70.6^{\circ}C)$ and peak viscosity $(2,874{\sim}3,175\;cp)$ of cross-linked rice starch were lower than native starch $(71.6^{\circ}C,\;3,976\;cp)$, but holding strength $(2,177{\sim}2,708\;cp)$ and final viscosity $(3,424{\sim}3,826 \;cp)$ of cross-linked rice starch were higher than native starch (1,000 cp, 2,312 cp). DSC thermal transitions of cross-linked rice starches were shifted to a lower temperature than native rice starch but there was no significant difference in gelatinization enthalpy between native and cross-linked rice starches. X-ray diffraction pattern of both native and cross-linked rice starches showed typical A-type crystal indicating that cross-linking had not affected the crystalline region of starch.

Surface Characteristics and Antifouling Performance of Inorganic MnOx-WO3-TiO2 Nanopowder for Self-polishing Copolymer Paint Applications (무기계 MnOx-WO3-TiO2 나노분말의 표면특성 및 자기마모형 수지 적용성 평가)

  • Shin, Byeongkil;Park, Hyun
    • Journal of the Korean Society of Marine Environment & Safety
    • /
    • v.22 no.2
    • /
    • pp.253-258
    • /
    • 2016
  • The $MnO_x-WO_3-TiO_2$ nanoscale powders were synthesized by sol-gel method in order to prevent the biological fouling on the ships and offshore structures. Powder characteristics and antifouling performance were investigated with respect to the crystalline, microstructure and surface property for application in self-polishing copolymer resins. The high antifouling activity of $TiO_2$-system biocide was attributed to its redox potential and soluble metal ions originating from tungsten oxides according to the improvements in the powder characteristics. Based on their physio-chemical characterizations, the specific surface areas of powders were about $90m^2/g$ and the grain size was in the region 100 ~ 150 nm. Powder characteristics and surface properties were improved by the addition of $WO_3$. Antifouling performance were analyzed according to their surface properties and static immersion tests to determine the effects of the $TiO_2$-system compounds. The surface of 2 wt. % added sample was clean for 5 month. This may be attributed to the ability of $MnO_x-WO_3-TiO_2$ powders to act as a promoter in antifouling agents.

High Strength Nanostructured Metastable Alloys

  • Eckert, Jurgen;Bartusch, Birgit;Schurack, Frank;He, Guo;Schultz, Ludwig
    • Journal of Powder Materials
    • /
    • v.9 no.6
    • /
    • pp.394-408
    • /
    • 2002
  • Nanostructured high strength metastable Al-, Mg- and Ti-based alloys containing different amorphous, quasicrystalline and nanocrystalline phases are synthesized by non-equilibrium processing techniques. Such alloys can be prepared by quenching from the melt or by powder metallurgy techniques. This paper focuses on one hand on mechanically alloyed and ball milled powders containing different volume fractions of amorphous or nano-(quasi)crystalline phases, consolidated bulk specimens and, on the other hand. on cast specimens containing different constituent phases with different length-scale. As one example. $Mg_{55}Y_{15}Cu_{30}$- based metallic glass matrix composites are produced by mechanical alloying of elemental powder mixtures containing up to 30 vol.% $Y_2O_3$ particles. The comparison with the particle-free metallic glass reveals that the nanosized second phase oxide particles do not significantly affect the glass-forming ability upon mechanical alloying despite some limited particle dissolution. A supercooled liquid region with an extension of about 50 K can be maintained in the presence of the oxides. The distinct viscosity decrease in the supercooled liquid regime allows to consolidate the powders into bulk samples by uniaxial hot pressing. The $Y_2O_3$ additions increase the mechanical strength of the composites compared to the $Mg_{55}Y_{15}Cu_{30}$ metallic glass. The second example deals with Al-Mn-Ce and Al-Cu-Fe composites with quasicrystalline particles as reinforcements, which are prepared by quenching from the melt and by powder metallurgy. $Al_{98-x}Mn_xCe_2$ (x =5,6,7) melt-spun ribbons containing a major quasicrystalline phase coexisting with an Al-matrix on a nanometer scale are pulverized by ball milling. The powders are consolidated by hot extrusion. Grain growth during consolidation causes the formation of a micrometer-scale microstructure. Mechanical alloying of $Al_{63}Cu_{25}Fe_{12}$ leads to single-phase quasicrystalline powders. which are blended with different volume fractions of pure Al-powder and hot extruded forming $Al_{100-x}$$(Al_{0.63}Cu_{0.25}Fe_{0.12})_x$ (x = 40,50,60,80) micrometer-scale composites. Compression test data reveal a high yield strength of ${\sigma}_y{\geq}$700 MPa and a ductility of ${\varepsilon}_{pl}{\geq}$5% for than the Al-Mn-Ce bulk samples. The strength level of the Al-Cu-Fe alloys is ${\sigma}_y{\leq}$550 MPa significantly lower. By the addition of different amounts of aluminum, the mechanical properties can be tuned to a wide range. Finally, a bulk metallic glass-forming Ti-Cu-Ni-Sn alloy with in situ formed composite microstructure prepared by both centrifugal and injection casting presents more than 6% plastic strain under compressive stress at room temperature. The in situ formed composite contains dendritic hcp Ti solid solution precipitates and a few $Ti_3Sn,\;{\beta}$-(Cu, Sn) grains dispersed in a glassy matrix. The composite micro- structure can avoid the development of the highly localized shear bands typical for the room temperature defor-mation of monolithic glasses. Instead, widely developed shear bands with evident protuberance are observed. resulting in significant yielding and homogeneous plastic deformation over the entire sample.

Morphological Structure of Poly(trimethylene terephthalate) Fibers Annealed by Passing on the Plate Heater (연속 평판열처리에 의한 폴리(트리메틸렌 테레프탈레이트) 섬유의 미세구조 변화)

  • Hong, Seong-Hag;Kim, Ryong;Choi, Chang-Nam;Choi, Hee;Lee, Woong-Eui;Cho, Sung-Yong
    • Polymer(Korea)
    • /
    • v.27 no.2
    • /
    • pp.106-112
    • /
    • 2003
  • Poly(trimethylene terephthalate)(PTT) fibers were treated by passing on the plate heater to study the annealing effect on the change of morphological structure and physical properties. In the X-ray diffraction curves of PTT annealed, a sharp peak at 2$\theta$=15.6$^{\circ}$ appeared and the peak intensity became stronger with the increase of annealing temperature and time. This peak was based on the (010) plane of PTT crystals. The crystallinity determined by density measurement was also increased by annealing. With the increases of temperature and time, the dynamic viscoelastic behaviors were shown to be a large reduction in T(tan $\delta$$_{max}$). The birefringence and $T_g$ were also reduced, but the melting temperature was the same. These results mean that the molecular chains in armorphous region are transfered into the crystalline legion, making the remained chains relaxed during annealing at tensionless state.

Gemological Comparison between Gwangdong Tektite and Baikdusan Obsidian (텍타이트와 흑요석의 보석학적 특징비교 - 중국 광동 텍타이트와 백두산 흑요석을 중심으로 -)

  • Kim, Won-Sa
    • Journal of the Mineralogical Society of Korea
    • /
    • v.20 no.3
    • /
    • pp.181-191
    • /
    • 2007
  • The gemological charateristics of Gwangdong tektites and Baikdusan obsidians were investigated, using microscopy, density and refractive index measurements, X-ray fluorescence spectrometry, Inductively Coupled Plasma Mass spectrometry, X-ray powder diffraction, and electron microprobe analysis. The Gwangdong tektites and Baikdusan obsidians are both black in colour and slightly trans-lucent with various shades of brown when cut into a few mm thick. Both the materials yield conchoidal fracture on broken surface. The tektites occur as tear-drop shapes, ranging from 4 to 10 cm long, and in spheres, from 3 to 5 cm in diameter. On the surface numerous shallow pits up to 3 mm in diameter are present. Mohs' hardness and specific gravity are 5 to 5.5 and 2.66, respectively. The tektites are singly refractive, with an refractive index of 1.51. Numerous spherical air bubbles are randomly scattered throughout the tektites, and silica-rich glass inclusions are occasionally seen. X-ray powder diffraction analysis verifies that they are non-crystalline. The Baikdusan obsidians show very similar properties to those of the Gwangdong tektites, especially in hardness, amorphous nature and fracture. Nevertheless, the Baikdusan obsidian can readily be distinguished from the Gwangdong tektites by refractive index ($1.49{\sim}1.50$), specific gravity (2.67 to 2.68), and inclusions (absence of bubbles and presence of sanidine and magnetite crystals).

Magnetic Properties of Nanocrystalline $Fe_{76-x}Cu_1Mo_xSi_{14}B_9$(x=2,3) Alloys ($Fe_{76-x} Cu_1Mo_xSi_14B_9(x=2, 3)$ 초미세 결정합금의 자기적 특성)

  • Pi, W.K.;Noh, T.H.;Kim, H.J.;Kang, I.K.
    • Journal of the Korean Magnetics Society
    • /
    • v.1 no.1
    • /
    • pp.12-16
    • /
    • 1991
  • The effect of annealing on the magnetic properties and the microstructures of the amorphous $Fe_{76-x}Cu_1Mo_xSi_{14}B_9$(x=2,3) alloys were investigated. When annealed at 500${^{\circ}C}$ for 1hr, $8{\sim}9{\times}10^3$ of the effective permeability and 3~4 A/m of the coercive force were achieved upon crystallization to $\alpha$-Fe phase. And the average diameter of the $\alpha$-Fe grains was about 20nm. For the nanovrystalline ferromagnets. the fine grain size is the important requirement to obtain a good soft magnetic property. In this work, in order to get the finer grain size of $\alpha$-Fe phase, two-step annealing treatment was given. That is, following the low-temperature at $400{^{\circ}C}$ for 1~3hr, the high-temperature annealing at $500{^{\circ}C}$ for 1hr was carried out. As the low-temperature annealing time increased, the effective permeability increased to $1.2{\sim}1.7{\times}10^4$ and the coercive force decreased to about 2 A/m. And the grain size was observed to be smaller than 10nm. The increased permeability and the decreased coercive force were attributed to the reduced average crystalline anisotropy by the refinement of $\alpha$-Fe(Si) grains.

  • PDF

Phase Analysis and Magnetic Properties of $Fe_5Si_xB_{5-x}$ (x = 0, 1, 2, 3) Powders Prepared by Mechanical Alloying (기계적합금법으로 제조된 $Fe_5Si_xB_{5-x}$ (x = 0, 1, 2, 3) 분말의 상분석 및 자기적 특성)

  • Hwang, Yeon;Kim, Taek-Soo;Lee, Hyo-Sook
    • Journal of the Korean Magnetics Society
    • /
    • v.7 no.6
    • /
    • pp.293-298
    • /
    • 1997
  • $Fe_5Si_Xb_{5-x}$ (x=0, 1, 2, 3) powders were prepared by mechanical alloying, and their phases and magnetic properties were investigated by using XRD, TEM, Mossbauer spectroscopy and VSM. Starting elements are incorporated into $\alpha$-Fe in the early stage of mechanical alloying, and the stable phases are formed as the milling proceeds. After the annealing at 80$0^{\circ}C$ for 2 hours, it is found that the FeB and $Fe_2B$ phases coexist for the $Fe_5B_5$(x=0) composition. By substituting Si for B, the formation of $Fe_2B$ phase is restricted and the $Fe_5SiB_2$, $Fe_2Si_{0.4}B_{0.6}$ and paramagnetic phase begin to appear. The FeB phase has wide range of hyperfine magnetic field because it is not fully crystallized on the annealing at 800 $^{\circ}C$. On the contrary, others have good crystalline phases and show well-defined hyperfine magnetic field. Magnetic saturation is highest for the $Fe_5B_5$ composition where the amount of the $Fe_2B$ phase in large.

  • PDF

Partial purification and Properties of Alkaline Cellulase from Pseudomonas sp. AC-711 (Pseudomonas sp. AC-711이 생산하는 알칼리성 Cellulase의 부분정제 및 효소적 성질)

  • Yoon, Min-Ho;Lim, Sang-Ho;Choi, Woo-Young
    • Korean Journal of Agricultural Science
    • /
    • v.25 no.1
    • /
    • pp.131-137
    • /
    • 1998
  • The cellulase components were partially purified from the culture filtrate of the alkalophilic bacterium Pseudomonas sp. AC-711 and its enzymatic properties were characterized. The specific activity of the purified major enzyme component was 3.5 units/mg protein as carboxymethyl cellulase and the yield was 23% of the total activity of the culture broth. The molecular weight of the component was 46,000 and the Km and Vmax on CMC were determined as $15.4mg\;mL^{-1}$ and $4.17{\mu}moles\;mL^{-1}\;min^{-1}$, respectively. The enzyme was stable at the temperatures below $60^{\circ}C$ and at the pH range of 4.0~11.0, and the optimal temperature and pH were $60^{\circ}C$ and pH 8.0, respectively. The enzyme activity was not significantly affected by the common surfactants (concentration: 0.05%) such as ${\alpha}$-olefin sulfonate, linear alkylbenzene sulfonate, sodium dodecyl sulfonate, hexadecyltrimethylammonium bromide and Tween 80. The enzyme was activated by the metal ions such as $Ca^{2+}$, $Cu^{2+}$, $Co^{2+}$, whereas inhibited by $Hg^{2+}$ and $Zn^{2+}$. The enzyme exhibited relatively high activity toward amorphous CMC as compared with crystalline substrates such as filter paper and avicel.

  • PDF

A study on the preparation of $(Ba_{1-X}Sr_X)ZrO_3$ using oxalate method and its dielectric properties (수산염법에 의한 $(Ba_{1-X}Sr_X)ZrO_3$의 합성 및 그의 유전특성에 관한 연구)

  • Oh Seong Kweon;Nam Seok Baik;Byung Ha Lee
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.4 no.3
    • /
    • pp.252-261
    • /
    • 1994
  • The $(Ba_{1-X}Sr_X)ZrO_3$ powder showing chemically pure and fine particle size was attempted to be synthesized by the oxalate method. The objective of this study is to determine the optimum synthesis condition of stable $(Ba_{1-X}Sr_X)ZrO_3$ powder in terms of the temperatures coefficient of resonant frequency ${\tau}_f$ by examining the microstructure and dielectric properties of the synthesized powder. The six compounds (x=0, 0.2, 0.4, 0.6, 0.8, 1) of $(Ba_{1-X}Sr_X)ZrO_3$ were prepared by the oxalate method, and then calcined at $1000^{\circ}C$ to obtain the crystalline $(Ba_{1-X}Sr_X)ZrO_3$ powder. The synthesized powder showed the globular-shape and average particle size of less than $0.2 \mu\textrm{m}$. The composition of x=0.5, i.e., half of Ba was replaced by Sr, is experted to show the zero value of temperatures coefficient of capacitance ${\tau}_c$.