• Title/Summary/Keyword: crack evaluation

검색결과 1,260건 처리시간 0.093초

5083-0 알루미늄合金의 疲勞균열進展 擧動과 균열닫힘에 관한 硏究 (A study of Fatigue Crack Growth Behavior and Crack Closure in 5083-O Aluminum Alloy)

  • 박영조;김정규;김일현
    • 대한기계학회논문집
    • /
    • 제10권2호
    • /
    • pp.208-214
    • /
    • 1986
  • 본 연구에서는 균열 닫힘에 관한 연구의 일환으로 5083-O 알루미늄합금을 사용하고 소규모강복조건하에서 일정진폭하중피로시험을 시행하여 이 재료의 피로균열 진전속도와 균열닫힘에 관하여 검토하였다.

열화상기술을 이용한 모멘트 변화에 따른 피로균열진전 연구 (A Study of the Fatigue Crack Propagation Behavior According to the Moment Change using Infrared Thermography)

  • 김경석;정현철;박찬주;정덕운;장호섭
    • 한국생산제조학회지
    • /
    • 제19권3호
    • /
    • pp.359-364
    • /
    • 2010
  • The objective of this study is to propose an effective method for measurement and analysis of fatigue crack. A technique that can measure the statue of fatigue crack propagation fast and correctly for enhancing safety of constructions and securing reliability is necessary. Moreover, the crack propagation behavior characteristics evaluation technique has to be developed using this technique. In this paper, fatigue crack was caused via the fatigue experiment with repeated load on the CT specimen that is made up of STS304. Fatigue crack propagation was measured by tracing the position of the maximum temperature according to the cycles using infrared thermography. The crack growth characteristics was evaluated by applying the moment values on the measuring area to the measured value. As a result of this study, the possibility that the infrared thermography could be applied to measure the fatigue crack was identified. Moreover, it was identified that fatigue crack propagation have a relationship with the moment value of construction.

AC2B 알루미늄 주조합금의 응고균열 강도에 미치는 금형 예열온도의 영향 (Effect of Mold Preheat Temperature on Solidification Crack Strength of AC2B Aluminum Alloy)

  • 김헌주
    • 한국주조공학회지
    • /
    • 제34권5호
    • /
    • pp.162-169
    • /
    • 2014
  • The effect of the mold preheat temperature on the solidification crack strength was investigated in AC2B aluminum alloy. A tension type apparatus as part of a solidification crack test which could measure the stress-strain relationship quantitatively was utilized. The evaluation of the solidification crack strength with varying mold preheat temperatures was performed by the test procedure established in this research. When the mold preheat temperatures were $250^{\circ}C$, $150^{\circ}C$ and $50^{\circ}C$, the solidification crack strengths were found to be $7.8Kgf/cm^2$, $12.9Kgf/cm^2$ and $28.6Kgf/cm^2$, respectively. In the same way, when the mold preheat temperatures were $250^{\circ}C$, $150^{\circ}C$ and $50^{\circ}C$, the corresponding temperatures of the failure sites were $610^{\circ}C$, $600^{\circ}C$ and $571^{\circ}C$, and the calculated solid fractions were 14.0%, 29.3% and 50.8% when the specimens failed, respectively. The solidification crack strength increased in proportion to the solid fraction of the failure site. The solidification crack strength obtained in this test is assumed to reflect the effects of metallurgical factors on the thermo-plastic characteristics of a solidifying alloy such as the grain size of the solid, the grain morphology, and the distribution of solid grain.

Semantic crack-image identification framework for steel structures using atrous convolution-based Deeplabv3+ Network

  • Ta, Quoc-Bao;Dang, Ngoc-Loi;Kim, Yoon-Chul;Kam, Hyeon-Dong;Kim, Jeong-Tae
    • Smart Structures and Systems
    • /
    • 제30권1호
    • /
    • pp.17-34
    • /
    • 2022
  • For steel structures, fatigue cracks are critical damage induced by long-term cycle loading and distortion effects. Vision-based crack detection can be a solution to ensure structural integrity and performance by continuous monitoring and non-destructive assessment. A critical issue is to distinguish cracks from other features in captured images which possibly consist of complex backgrounds such as handwritings and marks, which were made to record crack patterns and lengths during periodic visual inspections. This study presents a parametric study on image-based crack identification for orthotropic steel bridge decks using captured images with complicated backgrounds. Firstly, a framework for vision-based crack segmentation using the atrous convolution-based Deeplapv3+ network (ACDN) is designed. Secondly, features on crack images are labeled to build three databanks by consideration of objects in the backgrounds. Thirdly, evaluation metrics computed from the trained ACDN models are utilized to evaluate the effects of obstacles on crack detection results. Finally, various training parameters, including image sizes, hyper-parameters, and the number of training images, are optimized for the ACDN model of crack detection. The result demonstrated that fatigue cracks could be identified by the trained ACDN models, and the accuracy of the crack-detection result was improved by optimizing the training parameters. It enables the applicability of the vision-based technique for early detecting tiny fatigue cracks in steel structures.

집중유도형 교류전위차법에 의한 강자성체 및 상자성체의 2차원 표면결함의 비파괴평가 (Nondestructive Evaluation of 2-Dimensional Surface Crack in Ferromagnetic Metal and Paramagnetic Metal by ICFPD Technique)

  • 김훈;장자철웅;정세희
    • 대한기계학회논문집
    • /
    • 제19권5호
    • /
    • pp.1202-1210
    • /
    • 1995
  • Aiming at nondestructive evaluation of defect with high accuracy and resolution, ICFPD(Induced Current Focusing Potential Drop) technique was newly developed. This technique can be applied for locating and sizing of defects in components with not only simple shape such as plain surface but also more complex shape and geometry such as curved surface and dissimilar joing. This paper describes the principle of ICFPD technique and also the results of 2-dimensional surface crack in ferromagnetic metal(A508 Cl. III steel) and paramagnetic metal (pure aluminum and stainless 304 steel) measured by this technique. Results are that surface defects in each specimen are detected with the difference of potential drop, and potential drops are distributed a similar shape for each metal and each depth. The normalized potential drop ( $V_{\delta}$2/$^{t}$ / $V_{{\delta} 2}$$^{-1}$) max. in the vicinity of defect is varied with the depth of defect. Therefore, ICFPD technique can be used for the evaluation of defect not only in ferromagnetic metal but also in paramagnetic steel..

실링 테이프 적용에 따른 시공조인트 균열 저항성 평가 (Evaluation of Crack Resistance of Cold Joint as Usage of Sealing Tape)

  • 이재준;이선행;김두병;이진욱
    • 한국도로학회논문집
    • /
    • 제20권3호
    • /
    • pp.1-9
    • /
    • 2018
  • PURPOSES : In order to evaluate a crack resistance at cold joint, sealing tape was adopted to apply at cold joint instead of typical tack coat material(RSC-4). The sealing tape was made by hot sealing material. The crack resistance as function of environmental and traffic loading was measured with visual observation. METHODS : In this study, the crack resistance was evaluated as function of environmental and traffic loading. The freeze-thaw method was adopted for environmental loading of asphalt pavement. condition. The damage of cold joint under freeze-thaw action is initiated by ice expansion load and accelerated by the interfacial damage between new and old asphalt pavement. The traffic loading was applied with wheel tracking machine on the cold joint area of the asphalt pavement for 3 hours at $25^{\circ}C$. The evaluation of crack resistance was measured with visual observation. The freeze-thaw results shows that the sealing tape was significantly increased the crack resistance based on. RESULTS : To estimate the crack resistance at cold joint area due to the environmental loading, the Freeze-thaw test was conducted by exposing the product to freezing temperature(approximately $-18^{\circ}C$) for 24 hours, and then allowing it to thaw at $60^{\circ}C$ for 24 hours. The tack coat material(RSC-4) was debonded after 21 cycles of the Freeze-thaw test. The first crack was observed after 14 freeze-thaw cycle with RSC-4 material. But, the sealing tape was not debonded after 24 cycle test. Also, the sealing tape shows the better performance of the crack resistance under the traffic loading with wheel track test. The crack was generated the under traffic loading with RSC-4(tack coating), however, the crack was not shown with sealing tape. It indicates that the sealing tape has a strong resistance of tensile stress due to traffic loading. CONCLUSIONS :Based on limited laboratory test result, a performance of crack resistance using the sealing tape is better than that of general tack coat material(RSC-4). It means that the sealing tape is possible to extend a pavement service life because the crack, one of the main pavement distresses, will be delayed.

역사이클하중하에서의 균열길이 측정법에 따른 파괴저항곡선의 평가 (J-R Curve Evaluation According to the Crack Length Measurement Techniques Under Reverse Cyclic Loading)

  • 원종일;우흥식;석창성
    • 한국안전학회지
    • /
    • 제13권4호
    • /
    • pp.96-101
    • /
    • 1998
  • J-R curve tests were performed on 1T compact specimens of SA516 Gr. 70 carbon steels under reverse cyclic loading. A Direct-Current Potential Drop (DCPD) method, one of the nondestructive techniques to detect flaw of structure, is being increasingly used for monitoring crack initiation and stable crack growth in typical fracture mechanics specimens for J-R testing. In many aspects this method is simpler than the unloading compliance method. The objective of this paper is to evaluate the J-R Curve according to the crack length measurement techniques under reverse cyclic loading. In order to prove the reliability and repeatability of the DCPD method, the crack length measured by using DCPD method was compared to one determined from unloading compliance. Consequently, this DCPD method correlated well with J-R curves and crack extension measurements determined from unloading compliance method.

  • PDF

균열 자기치유형 혼화재 적용 콘크리트의 수축균열 평가 (Evaluation on the shrinkage crack of concrete with crack self-healing agent)

  • 홍석범;유조형;김우재
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.82-83
    • /
    • 2014
  • Concrete with self-healing admixture can reduce the crack width by using a compound for chemical reaction with incoming water and carbon dioxide through the crack. Also, concrete with self-healing admixtures can reduce early-age shrinkage crack by using a inorganic expansive agent. In this research, we perform the basic workability test and compressive test. Also, We measure the drying shrinkage of concrete specimen. Finally, we make mock-up (3m X 3m X 0.23m) and monitor the crack width and length for 3 months.

  • PDF

평가 방법에 따른 피로균열 성장속도에 관한 연구 (A Study on Fatigue Crack Growth Rate for Evaluation Methods)

  • 국중민
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 1998년도 춘계학술대회 논문집
    • /
    • pp.251-257
    • /
    • 1998
  • The distribution of fatigue crack growth rate is subjected to the measuring interval and calculated method of growth rate. In this paper, in order to establish the method of determining the distribution of fatigue crack growth rate, which ignores those influences, a series of fatigue crack growth experiments and measuring intervals of crack length calculated reasonable are presented. The main conclusions obtained are summarized as follows: 1) As a result of the ΔP constant test and ΔK constant test, it is thought that an approximate measuring interval of 0.3~0.7mm is reasonable, which allows for few errors and is little subjected to the calculated method of crack growth rate.

  • PDF

Nonlinear Time Reversal Focusing and Detection of Fatigue Crack

  • Jeong, Hyun-Jo;Barnard, Dan
    • 비파괴검사학회지
    • /
    • 제32권4호
    • /
    • pp.355-361
    • /
    • 2012
  • This paper presents an experimental study on the detection and location of nonlinear scattering source due to the presence of fatigue crack in a laboratory specimen. The proposed technique is based on a combination of nonlinear elastic wave spectroscopy(NEWS) and time reversal(TR) focusing approach. In order to focus on the nonlinear scattering position due to the fatigue crack, we employed only one transmitting transducer and one receiving transducer, taking advantage of long duration of reception signal that includes multiple linear scattering such as mode conversion and boundary reflections. NEWS technique was then used as a pre-treatment of TR for spatial focusing of reemitted second harmonic signal. The robustness of this approach was demonstrated on a cracked specimen and the nonlinear TR focusing behavior is observed on the crack interface from which the second harmonic signal was originated.