Development of Metallic Bipolar Plate Material with W-addition in Austenitic Stainless Steel for PEMFC Environment

  • Kim, Kwang Min;Koh, Sung Ung;Kim, Kyoo Young
    • Corrosion Science and Technology
    • /
    • v.5 no.5
    • /
    • pp.153-159
    • /
    • 2006
  • Austenitic stainless steels with addition of various amounts of Mo and W were evaluated in terms of corrosion and contact resistance to determine optimum alloy composition of metallic bipolar plate for PEMFC. The corrosion property was evaluated by both acid fume exposure test at $130^{\circ}C$ and by electrochemical polarization tests in $H_3PO_4$ solution at $80^{\circ}C$. Austenitic stainless steel with proper amount of Mo and W demonstrated not only good corrosion resistance but also low contact resistance. Analyses on the passive film show that partial substitution of Mo by W enhances passive film stability and repassivation property. Test results suggest that austenitic stainless steel with 2 wt%Mo and 4 wt%W has optimum composition for metallic bipolar plate used in PEMFC.

Study on Corrosion Properties of Additive Manufactured 316L Stainless Steel and Alloy 625 in Seawater

  • Jung, Geun-Su;Park, Yong-Ha;Kim, Dae-Jung;Lim, Chae-Seon
    • Corrosion Science and Technology
    • /
    • v.18 no.6
    • /
    • pp.258-266
    • /
    • 2019
  • The objective of this study was to evaluate corrosion resistance of additive manufactured 316L stainless steel and alloy 625 powders widely used in corrosion resistance alloys of marine industry in comparison with cast alloys. Directed Energy Deposition (DED) method was used in this work for sample production. DED parameter adjustment was also studied for optimum manufacturing and for minimizing the influence of defects on corrosion property. Additive manufactured alloys showed lower corrosion resistance in seawater compared to cast alloys. The reason for the degradation of anti-corrosion property was speculated to be due to loss of microstructural integrity intrinsic to the additive manufacturing process. Application of heat treatment with various conditions after DED was attempted. The effect of heat treatments was analyzed with a microstructure study. It was found that 316L and alloy 625 produced by the DED process could recover their expected corrosion resistance when heat treated at 1200 ℃.

The study on the property of material for the shim of stone cultural properties (석조문화재 받침용 쐐기 재질의 물성 실험 연구)

  • Eom, Doo-Sung;Hong, Jung-Ki;Kim, Sa-Dug;Kang, Dai-Il;Lee, Myong-Hee
    • 보존과학연구
    • /
    • s.21
    • /
    • pp.101-118
    • /
    • 2000
  • Stone cultural properties(pagoda, Buddhist statue etc.) is moved in original place for many reasons and restored after taking to pieces for structural safety. With the movement and restoration after taking to pieces, the cast iron is used for the sake of a fixation and horizontality. The stone cultural properties are spoiled the beauty and accelerated the weathering because of the corrosion product of cast iron. So we need to substitute for the improved property in all aspects. We are executed the corrosion test and inquired the property of material on the usable material for the shim of stone cultural properties. That is the Cast iron, Stainless steel, Titanium and Fiber Reinforced Plastics. In the result of the physical property and strength, the Stainless steel and Titanium was superior to the Cast iron. And the Stainless steel and Titanium was slower than the Cast iron in the corrosion velocity for the acid, salt and rain. If the shim is substitute the Stainless steel or Titanium for the Cast iron, the stone cultural properties are able to reduce the pollution of stone cultural properties by corrosion product and should not happen in the matter of stone pagoda.

  • PDF

An Electrochemical Evaluation of the Corrosion Property on the Welded Zone of Sea Water Pipe by each Welding Materials (용접 재료 별 해수 배관 용접부위의 부식 특성에 관한 전기화학적 평가)

  • Kim, Jin-Gyeong;Won, Chang-Uk;Moon, Kyung-Man
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2006.11a
    • /
    • pp.185-188
    • /
    • 2006
  • The sea water pipe of engine room in all kinds of ships is being surrounded with severe corrosive environment. Therefore it's leakage part due to corrosion is inevitably prevented by various welding method. In this case corrosion property of welded zone may be considerably different by each welding materials. In this study corrosion resistance of the welded zone of sea water pipe with some welding materials such as shielded metal arc welding materials, inert gas arc welding materials was investigated with electrochemical method.

  • PDF

Effects of Sealing Solution for Anodized Mg-Al Alloys and Its Corrosion Resistance Property (양극산화한 Mg-Al합금에 대한 봉공처리액 조성의 효과와 그 내식성)

  • 장석기;김정일;김성종
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.28 no.5
    • /
    • pp.782-792
    • /
    • 2004
  • The effects of sealing solution for anodized Mg-Al alloys and their corrosion resistance property were investigated. focusing on the effects of anodizing potentials aluminum contents and sealing solutions. All of the anodized specimens showed better corrosion resistance than that of non-anodized specimens, regardless of applied potentials. It was found that the anodic film formed at 4 V had the best corrosion resistance. The sealing effects were improved by increasing the temperature of distilled water. the pH of solution and the relative intensity ratio of $Mg(OH)_2$.

Experimental Study on Carbon Corrosion of Gas Diffusion Layer in PEM Fuel Cell (고분자전해질형 연료전지 가스확산층의 탄소 부식에 관한 실험적 분석)

  • Ha, Taehun;Cho, Junhyun;Park, Jaeman;Min, Kyoungdoug;Lee, Eunsook;Jyoung, Jy-Young
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2010.11a
    • /
    • pp.76.1-76.1
    • /
    • 2010
  • Recently, many efforts to solve the durability problem of PEM fuel cell are carried on constantly. However, despite this attention, durability researches of gas diffusion layer (GDL) are not much reported yet. Generally, GDL of PEM fuel cell experiences three external attacks, which are dissolution of water, erosion of gas flow, corrosion of electric potential. In this study, among these degradation factors, carbon corrosion of electric potential was focused and investigated with accelerated carbon corrosion test. Through the test, it is confirmed that carbon corrosion occurred at GDL, and corroded GDL decreased a performance of operating fuel cell. The property changes of GDL were measured with various methods such as air permeability meter, pore distribution analyzer, thermo gravimetric analyzer, and tensile stress test to discover the effects of carbon corrosion. Carbon corrosion caused not only loss of weight and thickness, but also degradation of mechanical strength of GDL. In addition, to analysis the reason of GDL property changes, a surface and a cross section of GDL were observed with scanning electron microscope. After 100 hours test, the GDL showed serious damage in center of layer.

  • PDF

Comparison of Electrochemical Corrosion Properties of Permanent Mold Casting GZ21 Alloy and AZ91 Alloy (금형 주조한 GZ21 합금과 AZ91 합금의 부식특성 비교)

  • Kim, Dae Han;Kim, Byeong Ho;Park, Kyung Chul;Chang, In Ki
    • Journal of Korea Foundry Society
    • /
    • v.36 no.2
    • /
    • pp.60-66
    • /
    • 2016
  • In this study, comparison of corrosion properties of the Mg-1.5Ge-1Zn (GZ21) alloy and Mg-9Al-1Zn (AZ91) alloy were investigated. The studied alloys were fabricated by permanent mold casting method. And the potentiodynamic test, hydrogen evolution test, immersion test and A.C Impedance test were carried out in a 3.5% NaCl solution with pH7.2 at room temperature to measure the corrosion properties. The microstructure of GZ21 alloy was composed of ${\alpha}-Mg$ and $Mg_2Ge$ phases and AZ91 alloy was composed of ${\alpha}-Mg$ and $Mg_{17}Al_{12}$ phases. From the test results, the corrosion property was improved by adding Ge. It seemed that the corrosion mechanism was changed from galvanic corrosion (AZ91) to filiform corrosion (GZ21).

Surface Modification of Functional Titanium Oxide to Improve Corrosion Resistance (내식성 향상을 위한 기능성 타이타늄 표면 개질)

  • Park, Youngju;Jeong, Chanyoung
    • Corrosion Science and Technology
    • /
    • v.20 no.5
    • /
    • pp.256-265
    • /
    • 2021
  • Titanium is applied in various industries due to its valuable properties and abundant reserves. Generally, if a highly uniform oxide structure and a high-density oxide film is formed on the surface through anodization treatment, the utility value such as color appearance and corrosion inhibition efficiency is further increased. The objective of this study was to determine improvement of water-repellent property by controlling titanium oxide parameters such as pore size and inter-pore distance to improve corrosion resistance. Oxide film structures of different shapes were prepared by controlling the anodization processing time and voltage. These oxide structures were then analyzed using a Field Emission Scanning Electron Microscope (FE-SEM). Afterwards, a Self-Assembled Monolayer (SAM) coating was performed for the oxide structure. The contact angle was measured to determine the relationship between the shape of the oxide film and the water-repellency. The smaller the solid fraction of the surface, the higher the water-repellent effect. The surface with excellent hydrophobic properties showed improved corrosion resistance. Such water-repellent surface has various applications. It is not only useful for corrosion prevention, but also useful for self-cleaning. In addition, a hydrophobic titanium may open up a new world of biomaterials to remove bacteria from the surface.

Mechanical Property and Corrosion Resistance of Mg-Zn-Y Alloys Containing Icosahedral Phase (준결정상을 포함한 Mg-Zn-Y 합금의 기계적 특성 및 부식 저항성)

  • Kim, Do Hyung;Kim, Young Kyun;Kim, Won Tae;Kim, Do Hyang
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.2
    • /
    • pp.145-152
    • /
    • 2011
  • Mechanical and property corrosion resistance of Mg-Zn-Y alloys with an atomic ratio of Zn/Y of 6.8 are investigated using optical microscopy, scanning electron microscopy, transmission electron microscopy, uniaxial tensile test and corrosion test with immersion and dynamic potentiometric tests. The alloys showed an in-situ composite microstructure consisting of ${\alpha}$-Mg and icosahedral phase (I-phase) as a strengthening phase. As the volume fraction of the I-phase increases, the yield and tensile strengths of the alloys increase while maintaining large elongation (26~30%), indicating that I-phase is effective for strengthening and forms a stable interface with surrounding ${\alpha}$-Mg matrix. The presence of I-phase having higher corrosion potential than ${\alpha}$-Mg, decreased the corrosion rate of the cast alloy up to I-phase volume fraction of 3.7%. However further increase in the volume fraction of the I-phase deteriorates the corrosion resistance due to enhanced internal galvanic corrosion cell between ${\alpha}$-Mg and I-phase.

The Development of Repair System for RC Members with Damaged by Rebar Corrosion Using Inhibitor with High Nitrite Content (아초산계 방청제 도포에 의한 철근 부식 보수 시스템 공법 개발)

  • 이한승;나정일;박순만
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.359-364
    • /
    • 2001
  • The purpose of this study is to develop the repair system for RC members with damaged by rebar corrosion using new corrosion inhibitor which was high nitrite content. In the experiments, the acceleration corrosion test of rebar was conducted using the specimen which was applied by various repair system. As a result, it was confirmed that the new repair system without concrete patching had high anti-corrosion property compared with other repair systems and was very effective as a spray type corrosion inhibitor in concrete containing chloride (0.1% of NaCl).

  • PDF