• 제목/요약/키워드: concrete fracture toughness

검색결과 117건 처리시간 0.026초

섬유의 종류, 형상 및 치환율에 따른 HPFRCC의 공학적 특성에 관한 실험적 연구 (An Experimental Study on the Engineering Properties of HPFRCC According to Kinds, Shapes and Volume Fraction of Fibers)

  • 김영덕;조봉석;김재환;김규용;최경렬;김무한
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2003년도 학술.기술논문발표회
    • /
    • pp.59-62
    • /
    • 2003
  • Kinds, shapes and fraction ratios of fibers have influence on properties of HPFRCC(High-Performance Fiver Reinforced Cementitious Concrete ) like bending strength, strain capacity and fracture toughness. For example, hydrophilic fibers have different chemical bond strength from hydrophobic fibers, fiber shapes influence on fiber pull-out and rupture, and fiber volume fraction influence on bending strength. In this study, to estimate influences of kinds, shapes and fraction ratios of fibers, we make HFRCC with 3 kind of fiber in various volume fraction of fiber and compare cracking, bending strength and fracture toughness. As the results, bending strength of HPFRCC was increased as fiber volume fraction was Increase and fiber tensile strength was increase, and strain capacity and fracture toughness of HFRCC was higher in fiber pull-out fracture than in fiber rupture fracture. And HFRCC showing pseudo strain hardening has higher fiber reinforce efficiency than others.

  • PDF

Fracture toughness of high performance concrete subjected to elevated temperatures Part 2 The effects of heating rate, exposure time and cooling rate

  • Zhang, Binsheng;Cullen, Martin;Kilpatrick, Tony
    • Advances in concrete construction
    • /
    • 제5권5호
    • /
    • pp.513-537
    • /
    • 2017
  • In this study, the fracture toughness $K_{IC}$ of high performance concrete (HPC) was investigated by conducting three-point bending tests on a total of 240 notched beams of $500mm{\times}100mm{\times}100mm$ subjected to heating temperatures up to $450^{\circ}C$ with exposure times up to 16 hours and various heating and cooling rates. For a heating rate of $3^{\circ}C/min$, $K_{IC}$ for the hot concrete sustained a monotonic decrease trend with the increasing heating temperature and exposure time, from $1.389MN/m^{1.5}$ at room temperature to $0.942MN/m^{1.5}$ at $450^{\circ}C$ for 4-hour exposure time, $0.906MN/m^{1.5}$ for 8-hour exposure time and $0.866MN/m^{1.5}$ for 16-hour exposure time. For the cold concrete, $K_{IC}$ sustained a two-stage decrease trend, dropping slowly with the heating temperature up to $150^{\circ}C$ and then rapidly down to $0.869MN/m^{1.5}$ at $450^{\circ}C$ for 4-hour exposure time, $0.812MN/m^{1.5}$ for 8-hour exposure time and $0.771MN/m^{1.5}$ for 16-hour exposure time. In general, the $K_{IC}$ values for the hot concrete up to $200^{\circ}C$ were larger than those for the cold concrete, and an inverse trend was observed thereafter. The increase in heating rate slightly decreased $K_{IC}$, and at $450^{\circ}C$ $K_{IC}$ decreased from $0.893MN/m^{1.5}$ for $1^{\circ}C/min$ to $0.839MN/m^{1.5}$ for $10^{\circ}C/min$ for the hot concrete and from $0.792MN/m^{1.5}$ for $1^{\circ}C/min$ to $0.743MN/m^{1.5}$ for $10^{\circ}C/min$ for the cold concrete after an exposure time of 16 hours. The increase in cooling rate also slightly decreased $K_{IC}$, and at $450^{\circ}C$ $K_{IC}$ decreased from $0.771MN/m^{1.5}$ for slow cooling to $0.739MN/m^{1.5}$ for fast cooling after an exposure time of 16 hours. The fracture energy-based fracture toughness $K_{IC}$' was also assessed, and similar decrease trends with the heating temperature and exposure time existed for both hot and cold concretes. The relationships of two fracture toughness parameters with the weight loss and the modulus of rapture were also evaluated.

유한요소법에 의한 콘크리트의 진행성 파괴해석 (Progressive Fracture Analyses of Concrete by Finite Element Methods)

  • 송하원
    • 콘크리트학회지
    • /
    • 제8권1호
    • /
    • pp.145-153
    • /
    • 1996
  • 콘크리트의 파괴진행영역은 콘크리트의 균열선단의 브리징영역과 미세균열영역으로 구성되는 비선형영역으로서 콘크리트의 파기거동을 지배한다. 파괴진행영역을 고려한 파괴역학은 콘크리트에 유용하게 적용될 수 있으며 파괴진행영역 모델의 개발은 콘크리트의 파괴현상을 규명하는데 매우 중요하다. 본 논문에서는 콘크리트의 균열진행을 해석하기 위하여 선형 인장 연화곡선을 사용한 Dugdale-Barenblatt형 모델로 콘크리트의 브리징영역을 모델링하였고 이를 이산균열방법을 사용하여 단지 요소경계면에 파괴진행영역을 발생시켜 유한요소 해석하는 방법과 요소내의 불연속 균열면을 도입한 균열요소를 사용함으로써 이산균열방법의 결점을 보완한 해석방법을 제시하였다. 또한 해석 예를 통해 균열진행해석에 사용된 유한요소모델을 검증하였다.

An efficient algorithm for scaling problem of notched beam specimens with various notch to depth ratios

  • Karamloo, Mohammad;Mazloom, Moosa
    • Computers and Concrete
    • /
    • 제22권1호
    • /
    • pp.39-51
    • /
    • 2018
  • This study introduces a new algorithm to determine size independent values of fracture energy, fracture toughness, and fracture process zone length in three-point bending specimens with shallow to deep notches. By using the exact beam theory, a concept of equivalent notch length is introduced for specimens with no notches in order to predict the peak loads with acceptable precisions. Moreover, the method considers the variations of fracture process zone length and effects of higher order terms of stress field in each specimen size. In this paper, it was demonstrated that the use of some recently developed size effect laws raises some concerns due to the use of nonlinear regression analysis. By using a comprehensive fracture test data, provided by Hoover and Bazant, the algorithm has been assessed. It could be concluded that the proposed algorithm can facilitate a powerful tool for size effect study of three-point bending specimens with different notch lengths.

Direct and indirect methods for determination of mode I fracture toughness using PFC2D

  • Sarfarazi, Vahab;Haeri, Hadi;Shemirani, Alireza Bagher
    • Computers and Concrete
    • /
    • 제20권1호
    • /
    • pp.39-47
    • /
    • 2017
  • In this paper, mode I fracture toughness of rock was determined by direct and indirect methods using Particle Flow Code simulation. Direct methods are compaction tension (CT) test and hollow centre cracked quadratic sample (HCCQS). Indirect methods are notched Brazilian disk (NBD) specimen, the semi-circular bend (SCB) specimen, hollow centre cracked disc (HCCD), the single edge-notched round bar in bending (SENRBB) specimen and edge notched disk (END). It was determined that which one of indirect fracture toughness values is close to direct one. For this purpose, initially calibration of PFC was undertaken with respect to data obtained from Brazilian laboratory tests to ensure the conformity of the simulated numerical models response. Furthermore, the simulated models in five introduced indirect tests were cross checked with the results from direct tests. By using numerical testing, the failure process was visually observed. Discrete element simulations demonstrated that the macro fractures in models are caused by microscopic tensile breakages on large numbers of bonded discs. Mode I fracture toughness of rock in direct test was less than other tests results. Fracture toughness resulted from semi-circular bend specimen test was close to direct test results. Therefore semi-circular bend specimen can be a proper test for determination of Mode I fracture toughness of rock in absence of direct test.

불포화 폴리에스테르 모르터의 인성강화에 관한 실험 연구 (An Experimental Study on Toughening of Unsaturated Polyester Mortar)

  • 김화중;박준철;윤명덕;윤요현;최영준
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회 논문집(II)
    • /
    • pp.1115-1120
    • /
    • 2000
  • The purpose of this study is to investigate toughening of unsaturated polyester resin by addition of liquid rubber. In general, unsaturated polyester liquid has strong brittleness in spite of if high strength Therefore; it is difficult use polyurethane liquid rubber for the place where impact resistance is demanded. In this study, it was evaluated strength, impact resistance and fracture toughness by adding to polyurethane liquid rubber(0~25%). As a result, it was found that a tendency to be increase bearing impact and fracture toughness as polyurethane liquid rubber increased but strength was decreased.

Effect of shear-span/depth ratio on cohesive crack and double-K fracture parameters of concrete

  • Choubey, Rajendra Kumar;Kumar, Shailendra;Rao, M.C.
    • Advances in concrete construction
    • /
    • 제2권3호
    • /
    • pp.229-247
    • /
    • 2014
  • A numerical study of the influence of shear-span/depth ratio on the cohesive crack fracture parameters and double - K fracture parameters of concrete is carried out in this paper. For the study the standard bending specimen geometry loaded with four point bending test is used. For four point loading, the shear - span/depth ratio is varied as 0.4, 1 and 1.75 and the ao/D ratio is varied from 0.2, 0.3 and 0.4 for laboratory specimens having size range from 100 - 500 mm. The input parameters for determining the double - K fracture parameters are taken from the developed fictitious crack model. It is found that the cohesive crack fracture parameters are independent of shear-span/depth ratio. Further, the unstable fracture toughness of double-K fracture model is independent of shear-span/depth ratio whereas, the initial cracking toughness of the material is dependent on the shear-span/depth ratio.

재생골재를 이용한 폴리프로필렌 섬유보강콘크리트의 강도 및 휨인성 특성연구 (Characteristics of the Strength and Toughness of Polypropylene Fiber Reinforced Concrete using Recycled Aggregates.)

  • 류택은;박재성;조영래;오희보;구봉근
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.655-660
    • /
    • 2000
  • This study was performed to verify the properties of concrete used recycled aggregate(0, 30%, 50%). Also, to improve the brittle fracture, energy absorption and apparent ductility of concrete, we added polypropylene fibers(0, 0.1, 0.2, 0.5, 1.0% by volume of concrete). As the experimental results, adding 30% recycled aggregates and 0.5% polypropylene fibers to concrete mixes enhances the properties of both compressive strength and toughness.

  • PDF

강섬유 보강 콘크리트의 조기 재령에서의 휨 인성 발현에 관한 연구 (Investigation of Flexural Toughness Development of Steel Fiber Reinforced Concrete at Early Ages)

  • 이창준;신성우
    • 한국안전학회지
    • /
    • 제24권6호
    • /
    • pp.103-110
    • /
    • 2009
  • Since the mechanical properties of cement-based materials are time-dependent due to the prolonged cement hydration process, those of fiber reinforced concrete(FRC) may also be time-dependent. Toughness is one of important properties of FRC. Therefore, it should be investigated toughness development of FRCs with curing ages to fully understand the time-dependent characteristics of FRCs. To this end, the effect of curing ages on flexural toughness development of steel fiber reinforced concrete is studied. Three point bending test with notched beam specimen was adapted for this study. Hooked-end steel fiber(DRAMIX 40/30) was used as a fiber ingredient to investigate w/c ratio and fiber volume fraction effect on toughness development during curing. Three different water-cement ratios(0.44, 0.5 and 0.6) and fiber volume fractions(0%, 0.5% and 1%) were used as influence factors. Each mixture specimens were tested at five different ages, 0.5, 1, 3, 7 and 28 days. The study shows that flexure toughness development with age is quite different than other concrete material properties such as compressive strength. The study also shows that the toughness development trend correlates more closely to water/cement ratio than to fiber volume fraction.

Toughness and microscopic pore structure analysis of pasture fiber recycled concrete

  • Hailong Wang;Lei Wang;Hong Yang
    • Advances in concrete construction
    • /
    • 제16권3호
    • /
    • pp.141-153
    • /
    • 2023
  • In order to develop and take full advantage of pasture fiber and waste concrete, this article studied how different amounts of pasture fiber influenced the toughness and pore structure of concrete with different replacement rates of recycled fine aggregate. Pasture fiber recycled concrete constitutive equations were established under idealized stiffness and toughness damage rate, based on fracture energy and damage mechanics theories. The relationship between pore structure and toughness was studied utilizing nuclear magnetic resonance and fractal theory. The toughness of text groups (0% (JZ), 10% (ZS10), 20% (ZS20)) first increased and then decreased with increasing amounts of pasture fiber, based on the damage rate of toughness. The toughness of concrete samples with recycled fine aggregate and pasture fiber is negatively correlated to the fractal dimension of small and medium-sized pores with a pore size of 0-500 nm. At a replacement rate of 10% of the recycled fine aggregate, the fractal dimension of the air voids (r: 500-9000 nm, i.e., Lg(r) ∈ [2.7, 3.9]) shows a gradual decrease with the increase of grass fiber dosage, indicating that with such a replacement rate of the recycled fine aggregate, the increase of pasture fiber can reduce the complexity of the pore structure of the air voids (500-9000 nm).