Prediction of shear strength and drift capacity of corroded reinforced concrete structural shear walls

  • Yang, Zhihong;Li, Bing
    • Structural Engineering and Mechanics
    • /
    • 제83권2호
    • /
    • pp.245-257
    • /
    • 2022
  • As the main lateral load resisting system in high-rise reinforced concrete structures, the mechanical performance of shear wall has a significant impact on the structure, especially for high-rise buildings. Steel corrosion has been recognized as an important factor affecting the mechanical performance and durability of the reinforced concrete structures. To investigate the effect on the seismic behaviour of corroded reinforced concrete shear wall induced by corrosion, analytical investigations and simulations were done to observe the effect of corrosion on the ultimate seismic capacity and drift capacity of shear walls. To ensure the accuracy of the simulation software, several validations were made using both non-corroded and corroded reinforced concrete shear walls based on some test results in previous literature. Thereafter, a parametric study, including 200 FE models, was done to study the influence of some critical parameters on corroded structural shear walls with boundary element. These parameters include corrosion levels, axial force ratio, aspect ratio, and concrete compressive strength. The results obtained would then be used to propose equations to predict the seismic resistance and drift capacity of shear walls with various corrosion levels.

Flexural performance of RC beams incorporating Zinc-rich and epoxy bonding coating layers exposed to fire

  • Tobbala, Dina E.;Rashed, Ahmed S.;Tayeh, Bassam A.
    • Structural Engineering and Mechanics
    • /
    • 제82권2호
    • /
    • pp.163-172
    • /
    • 2022
  • Zinc-rich epoxy (ZRE) is used to overcome corrosion problems in reinforced concrete (RC) beams and coat steel rebars to protect them from humidity and chlorides. An extra coating layer of Sikadur-31 epoxy (SDE) is utilised to increase bond strength because the use of ZRE reduces the bond strength between concrete and steel rebars. However, the low melting point of SDE indicates that concrete specimens are vulnerable to fire. An experimental investigation on flexural performance of RC beams incorporating ZRE-SDE coating of steel rebars that were destroyed by fire is performed in this study. Twenty beams of five concrete mixes with different cementitious contents were tested to compare fire exposure for coated and uncoated rebars of the same beams at room temperature and determine the optimal cementitious content. Scanning electron microscopy (SEM) was also applied to investigate characteristics of fired mixture samples. Results showed that the use of SDE-ZRE at room temperature improves flexural strengths of the five mixes compared with uncoated rebars with percentages ranging from 8.5% to 12.3%. All beams with SDE-ZRE lost approximately 50% of their flexural strength due to firing. Moreover, the mix incorporating SF (silica fume) of 15% and cement content of 400 kg/m3 introduces optimum behaviour compared with other mixes. All results were supported and verified by the SEM analysis and compressive strength of cubic specimens of the same mixes.

Structural performance of concrete containing fly ash based lightweight angular aggregates

  • Pati, Pritam K.;Sahu, Shishir K.
    • Advances in concrete construction
    • /
    • 제13권4호
    • /
    • pp.291-305
    • /
    • 2022
  • The present investigation deals with the production of the innovative lightweight fly ash angular aggregates (FAA) first time in India using local class 'F' fly ash, its characterization, and exploring the potential for its utilization as alternative coarse aggregates in structural concrete applications. Two types of aggregates are manufactured using two different kinds of binders. The manufacturing process involves mixing fly ash, binder, and water, followed by the briquetting process, sintering and crushing them into suitable size aggregates. Tests are conducted on fly ash angular aggregates to measure their physical properties such as crushing value, impact value, specific gravity, water absorption, bulk density, and percentage of voids. Study shows that the physical parameters are significantly enhanced as compared to commercially available fly ash pellets (FAP). The developed FAA are used in concrete vis-à-vis conventional granite aggregates and FAP to determine their compressive, split tensile and flexural strengths. Although being lightweight, the strength parameters for concrete containing FAA are well compared with conventional concrete. This might be due to the high pozzolanic reaction between fly ash angular aggregates and cement paste. Also, RCC beams are cast and the load-deflection behaviour and ultimate load carrying capacity signify that FAA can be suitably used for RCC construction. Hence, the utilization of fly ash as angular aggregates can reduce the dead load of the structure and at the same time serves as a solution for fly ash disposal and mineral depletion problem.

Novel approach to improve nano green mortar behaviour using nano-paper waste with nano-metakaolin

  • Radwa Defalla Abdel, Hafez;Bassam A., Tayeh;Raghda Osama Abd-Al, Ftah;Khaled, Abdelsamie
    • Advances in concrete construction
    • /
    • 제14권5호
    • /
    • pp.341-354
    • /
    • 2022
  • Treatment of solid waste building materials is a crucial method of disposal and an area of ongoing research. New standards for the treatment of solid waste building materials are necessary due to multisource features, huge quantities, and complicated compositions of solid waste. In this research, sustainable nanomaterial mixtures containing nano-paper waste (NPW) and nano-metakaolin (NMK) were used as a substitute for Portland cement. Portland cement was replaced with different ratios of NPW and NMK (0%, 4%, 8%, and 12% by weight of cement) while the cement-to-water ratio remained constant at 0.4 in all mortar mixtures. The fresh properties had a positive effect on them, and with the increase in the percentage of replacement, the fresh properties decreased. The results of compressive strength at 7 and 28 days and flexural strength at 28 days show that the nanomaterials improved the strength, but the results of NMK were better than those of NPW. The best replacement rate was 8%, followed by 4%, and finally 12% for both materials. The combination of NMK and NPW as a replacement (12% NMK + 12% NPW) showed less shrinkage than the others because of the high pozzolanic reactivity of the nanomaterials. The combination of NMK and NPW improved the microstructure by increasing the hydration volume and lowering the water in the cement matrix, as clearly observed in the C-S-H decomposition.

횡하중을 고려한 선체보강판넬의 압축 붕괴거동에 관한 연구 (Axial Collapse Behaviour of Ship's Stiffened Panels considering Lateral Pressure Load)

  • 고재용;박주신
    • 한국항해항만학회지
    • /
    • 제31권3호
    • /
    • pp.235-245
    • /
    • 2007
  • 선체의 갑판부와 선저부 그리고 해양구조물의 기본적인 구조는 보강판이다. 보강판넬은 한쪽방향으로 위치한 보강재 혹은 종/횡 방향으로 복잡하게 위치한 구조를 이루고 있으며, 후자의 모델을 그릴리지 구조라고 부른다 선체구조설계 단계에서 선박의 종강도 평가는 가장 중요한 항목이다. 일반적으로, 극심한 해상상태에 놓인 선박의 선저부에는 호깅조건에 의해 발생되는 횡모멘트에 기인하여 압축하중이 작용하게 되며, 이와 동시에 수압하중 작용으로 인한 국부휭모멘트가 작용된다. 본 논문에서는, 구조해석 결과의 검증을 위해서 여러 가지 해석프로그램 및 현재 사용되고 있는 선급룰과의 비교를 하여 횡하중의 영향에 따른 압축최종강도에 대해 분석하고, 여러 가지 설계변수를 변화하여, 각각의 영향을 검토하고, 최종적으로 조합하중 조건에서의 횡하중의 영향에 대해서 분석하였다. 본 연구에서 얻어진 결과들은 최종한계상태설계법에 기반을 두고, 조합하중이 작용하는 선체보강판의 구조강도 거동에 대해서 하중성분에 대한 관계를 고찰하였다.

포스트 텐션 플랫 플레이트 외부 접합부의 내진 거동 (Seismic Behaviour of Exterior Joints in Post-Tensioned Flat Plate Systems)

  • 한상환;기성훈;강현구;조종;이리형
    • 콘크리트학회논문집
    • /
    • 제18권5호
    • /
    • pp.595-602
    • /
    • 2006
  • 본 연구의 목적은 중력 하중에 저항하도록 설계된 플랫 플레이트 외부 접합부의 이력 거동을 평가하는 데 있다. 이러한 목적을 위하여 2/3의 크기가 조정된 PT 슬래브-기둥 외부 접합부 2개와 RC 슬래브-기둥 외부 접합부 1개를 대상으로 실험적 연구를 수행하였다. 여기서 각각의 PT 실험체는 서로 다른 강선 배치 형태를 띄고 있다. 중력 하중은 동일하게 설정하였고, 지속적인 정적 하중 하에서 유사 정적 횡하중을 적용하였다. 한편 모든 실험체는 ACI 318-05과 ACI 352.1R-89에 근거하여 기둥 폭 내에 하부 철근을 배근 하였다. 또한 PT 외부 접합부의 이력 거동에 대한 일반적인 결론을 얻기 위하여 기존 연구자들의 실험 결과와 함께 비교하였다. 이번 연구를 통하여 강선의 배치는 PT 접합부의 이력 거동을 결정하는 중요한 변수임을 확인하였다. 즉 횡변형 성능, 에너지 소산 능력, 파괴 메커니즘, 그리고 연성 능력이 강선의 배치에 따라 다르게 나타났다. 또한 ACI 352.1R-89에서 구조적 일체성을 위해 제공된 하부 철근의 양은 모멘트 역전에 의해 발생된 정모멘트를 저항하는데 있어서도 적절하다는 것이 밝혀졌다. 또한 실험체의 전단 강도는 강선의 포스트 텐션에 의한 평균 콘크리트 압축 응력($f_{pc}$)의 효과가 고려된 식이 그렇지 않은 식보다 전단 강도를 정확히 예측하는 것으로 나타났다.

숏크리트 및 콘크리트 라이닝의 역학적 거동에 관한 실험 및 수치해석적 연구 (A study on the structural behaviour of shotcrete and concrete lining by experimental and numerical analyses)

  • 김재순;김영근
    • 터널과지하공간
    • /
    • 제8권4호
    • /
    • pp.307-320
    • /
    • 1998
  • 터널 라이닝은 터널의 최종 지보수단이며, 지반응력과 터널 지보재 사이의 상호작 용의 결과가 총체적으로 드러나는 면이다. 최근 콘크리트 라이닝에 발생하는 많은 균열로 인해 터널의 유지, 관리 측면에서 큰 어려움이 따르고 있어 이에 대한 해석이 요구되고 있 다. 본 연구에서는 실험과 수치해석을 통해 터널 라이닝의 역학적 거동 특성을 규명하였다. 특히 숏크리트오 콘크리트 라이닝을 모두 포함하는 복층 라이닝에대해 실험과 수치해석을 실시하여 두 라이닝 사이의 상호작용을 규명하였다. 실험은 터널 라이닝 모형 시험체에 대 해 하중, 측압, 라이닝 두께, 복층 라이닝, 복층 라이닝의 배면공동, 지반 모델 타설 등에 다양한 조건에 대해 실시하였다. 측압의 영향으로 라이닝 전반에 걸쳐 압축력이 분포하여 내하력을 증가시켰다. 라이닝의 두께가 50% 증가함에 Efkk 균열하중은 2배 정도 증가하였 다. 복층 라이닝의 배면공동으로 이해 라이닝의 내하력은 콘크리트 라이닝 두께 감소량고 k 같은 수준으로 감소하였다. 라이닝의 측벽부에 지반 모델을 타설한 경우 라이닝라이닝 어깨 부분의 밀림을 억제하여 균열하중 및 파괴하중이 크게 증가하였다. 수치해석에서는 인터페 이스 요소를 도입하여 복층 라이닝을 해석할 수 있는 수치해석 프로그램을 개발하여 실험 결과와 비교 해석을 실시하였다.

  • PDF

견고한 점토층에서 실시된 터널근접시공으로 인한 단독말뚝의 거동에 대한 연구 (A Study on the Behaviour of Single Piles to Adjacent Tunnelling in Stiff Clay)

  • 전영진;이철주
    • 한국지반환경공학회 논문집
    • /
    • 제16권6호
    • /
    • pp.13-22
    • /
    • 2015
  • 본 연구에서는 3차원 유한요소 해석을 수행하여 터널굴착에 의한 말뚝의 거동변화를 지배하는 말뚝선단에 대한 터널의 상대 위치를 고려하여 분석하였다. 수치해석 결과를 순수하게 터널굴착으로 발생한(Tunnelling-induced) 말뚝두부의 침하, 상대변위, 체적손실률(Volume loss), 말뚝의 축력, 전단응력 그리고 겉보기안전율 등을 분석하였다. 터널과 말뚝선단의 상대위치를 고려했을 때 말뚝선단이 터널굴착으로 인한 지반침하 영향권 내부에 존재하는 경우 Tunnelling-induced 말뚝두부의 침하는 지표면의 침하보다 크게 나타났으며, 이는 말뚝에 Tunnelling-induced 인장력을 발생시켰다. 반대로 말뚝선단이 터널굴착으로 인한 지반침하 영향권 외부에 존재할 경우, 말뚝상부에서 유발된 하향의 전단응력으로 인해 말뚝에는 Tunnelling-induced 압축력이 작용하였다. 수치해석을 통해 분석된 하중-변위 관계를 이용하여 겉보기안전율을 분석한 결과 말뚝선단이 터널굴착으로 인한 지반침하 영향권 내부에 존재할 경우 말뚝의 겉보기안전율은 평균 약 36% 감소하는 것으로 나타났다. 터널의 상대위치에 따른 전단응력전이 매커니즘을 Tunnelling-induced 말뚝축력, 전단응력과 말뚝의 겉보기안전율을 고려하여 심도 있게 고찰하였다.

유공보강판의 좌굴 및 극한강도 특성에 관한 연구 (Characteristic of Buckling and Ultimate Strength of the Perforated Stiffened Plate)

  • 박주신;고재용;오경근
    • 한국항해항만학회지
    • /
    • 제30권6호
    • /
    • pp.439-446
    • /
    • 2006
  • 선체는 기본적으로 판부재들의 조합으로 구성되어 있으며 상당수는 유공판(Perforated plate)으로 이루어져있다. 선체에 설치된 유공판으로서는 선체 상갑판 해치(하역시설로 사용), 선저부의 거더와 플로어(중량경감과 선박 건조 및 검사시 통로확보용), 다이어프램(중량경감 및 파이프 관통의 목적)등이 있다. 이들 유공판에 압축하중이 작용하면 좌굴과 극한강도 특성이 크게 변화할 뿐만 아니라 수반되는 면내응력도재 분포하게 되어 심각한 문제를 발생한다. 실적선에서는 유공주위에 스티프너 보강을 통하여 취약한 좌굴강도 보완하고 있으며, 유공을 고려한 실선에서 사용 중인 유공보강판 모델을 적용하여 좌굴강도 및 극한강도를 파악할 필요성이 있다. 이와 같은 측면에서 각 조선소에서는 각국 선급들이 제시하는 유공판의 좌굴설계식을 사용하여 강도계산을 하고 있으나 임의의 유공크기에 대한 좌굴강도 및 극한강도 평가법을 찾기란 매우 어려운 일이다. 본 연구에서는 실선에서 사용 중인 유공보강판의 모델을 조사하여 비선형 유한요소법(ANSYS)을 사용하여 면내 압축하중이 작용하는 경우에 대해서 유공비, 웹 치수, 두께 그리고 보강재 단면을 변화시켜가며, 극한강도 시리즈 해석을 수행하고 압축극한강도에 미치는 영향을 검토하였다.

순환 굵은골재의 혼입률에 따른 콘크리트와 이형철근의 부착 거동 (Effect of Recycled Coarse Aggregate (RCA) Replacement Level on the Bond Behaviour between RCA Concrete and Deformed Rebars)

  • 장용헌;최기선;유영찬;김긍환;윤현도
    • 콘크리트학회논문집
    • /
    • 제22권1호
    • /
    • pp.123-130
    • /
    • 2010
  • 순환골재 콘크리트와 철근의 부착 거동 규명은 철근콘크리트 구조물에 순환골재를 적용하기 위해서 매우 중요한 요소이다. 이에 따라 이 연구에서는 콘크리트와 철근 상호간의 부착 거동을 평가하기 압축인발 실험을 수행하였다. 실험에 사용된 변수는 설계압축강도(21, 27, 40 MPa), 순환 굵은골재 치환율(0, 30, 60, 100%) 및 철근의 배근방향 및 위치(상단근, 하단근)로 하였다. 이 연구를 통하여 얻어진 실험 결과를 종합해 보면, V형 시험체의 경우 순환골재 치환율에 관계없이 상호 유사한 값을 나타내고 있으며 H형 시험체의 경우는 철근의 배근 위치에 영향을 받는 것으로 나타났으나 일부 HT형 시험체를 제외하고는 대부분 CEB-FIP 및 ACI 408 기준식에 의한 계산 값을 상회하는 것으로 나타나 재생골재 사용에 따른 성능 저하는 크지 않은 것으로 판단된다. HT형 시험체의 경우 순환골재 치환율 증가에 따라 골재 침하 현상이 크게 발생되며 불리딩 및 레이턴스에 의한 부착면적의 감소로 최대 부착응력이 다른 시험체에 비하여 낮게 나타났다. 전술한 바에 의하면 현행 규준에서 정하는 상부철근의 높이인 300 mm 이하(높이 225 mm)에서도 부착강도의 저하가 발생하며 이에 따라 현재 규준에서 제안하는 철근 위치 보정계수 1.3의 값의 수정과 신뢰성 확보가 필요할 것으로 판단된다.