• 제목/요약/키워드: compression wood

검색결과 132건 처리시간 0.028초

Physical and Mechanical Properties of Light Red Meranti Treated with Boron Preservatives

  • Man Djun LEE;Ridge Wei Cheong TANG;Zeno MICHAEL;Miqdad KHAIRULMAINI;Azmi ROSLAN;Ahmad Faidzal KHODORI;Hazim SHARUDIN;Pui San LEE
    • Journal of the Korean Wood Science and Technology
    • /
    • 제52권2호
    • /
    • pp.157-174
    • /
    • 2024
  • This study investigates the influence of varying concentrations of boric acid (BA) preservative on the physical and mechanical properties of light red meranti (LRM) found in Sarawak. LRM or Shorea leprosula samples were treated with various concentrations of BA via the dip diffusion method using American Society for Testing and Materials (ASTM) standards. The physical property, particularly the retention rate and mechanical properties, bending strength, modulus of elasticity (MOE), tensile and compression strength parallel to grain of impregnated and control samples were tested to determine the effects of BA preservative. The retention rate was found to increase with increasing BA concentration and higher surface area to volume ratio. The mechanical properties in terms of the MOE and tensile strength parallel to grain were found to be greater than those of the control samples, whereas the bending strength and tensile strength parallel to grain were lower. Amongst the results, only the retention rate and MOE showed significant interaction effects at 5% level of significance between all factors tested (samples size and BA concentration for retention rate and BA concentration for MOE).

함수율과 섬유경사각이 목재의 압축강도 및 초음파 전달속도에 미치는 영향 (Effects of Moisture Content and Slope of Grain on Ultrasonic Transmission Speed of Wood)

  • 장상식
    • Journal of the Korean Wood Science and Technology
    • /
    • 제28권2호
    • /
    • pp.10-18
    • /
    • 2000
  • 초음파를 이용한 목재의 비파괴시험은 등급구분 수분 및 결점 탐지, 썩은 정도 평가 등의 용도에 적용되고 있다. 이와 같은 기술을 실제로 적용하기 위해서는 목재 내의 초음파 전달과 목재의 성질 사이의 관계에 대한 기본적인 연구가 선행되어야 한다. 이 연구에서는 함수율과 섬유경사각이 초음파 전달 속도에 미치는 영향을 분석하기 위하여 낙엽송과 소나무를 대상으로 초음파 비파괴시험을 실시하였다. 함수율에 대한 시험을 위한 시험편은 생재상태, 30%, 20%, 10% 및 전건상태의 함수율을 갖도록 준비하였고 섬유경사각에 대한 시험을 위해서는 접선방향으로 0, 15, 30, 45, 60, 75 및 90도의 섬유경사각을 갖는 시험편을 준비하였다. 초음파 전달 속도는 섬유포화점에 근사한 30% 이하의 낮은 함수율 범위에서는 함수율에 반비례하였으며 이보다 높은 함수율 범위에서는 함수율에 관계없이 일정한 경향을 나타내었다. 목재의 압축강도와 함수율 사이의 관계에서도 이와 유사한 경향이 관찰되었다. 목재의 섬유경사각도 초음파 전달 속도 및 압축강도와 반비례하는 경향을 나타내었다. 압축강도와 초음파 전달 속도 사이의 관계는 정비례하는 관계로서 하나의 직선식으로 나타낼 수 있었다.

  • PDF

볼트 간격에 따른 낙엽송 집성재 이중 볼트접합부의 전단강도 (Lateral Strength of Double-Bolt Joints to the Larix Glulam according to Bolt Spacing)

  • 김건호;홍순일
    • Journal of the Korean Wood Science and Technology
    • /
    • 제36권3호
    • /
    • pp.1-8
    • /
    • 2008
  • 볼트 간격에 따른 국내산 낙엽송 집성재 이중 볼트접합부의 내력성능을 검토하기 위하여 휨 type 전단강도실험을 실시하였다. 전단시편은 강판삽입형 볼트접합부 시편으로서 볼트구멍은 볼트직경(12 mm, 16 mm), 볼트 개수(단일 볼트 : Control, 이중 볼트), 볼트 열 방향(섬유평행 : Type-A, 섬유직교 : Type-B) 그리고 볼트 간격(Type-A : 4 d, 7 d, Type-B : 3 d, 5 d)을 달리하여 제작하였다. 조건에 따른 볼트접합부의 강도성능과 파괴형상을 비교, 검토하였다. 설계표준(KBCS, 2000)시 볼트간격이 감소된 기준허용전단내력에 대한 저감계수를 산출하였다. 본 연구의 결과는 다음과 같다. 1) 단일 볼트접합부와 Type-A의 이중 볼트접합부의 볼트 한 개당 지압응력은 볼트의 직경, 볼트 간격과 비례 관계를 보여주었다. Type-B의 지압응력은 볼트의 직경이 증가할 때 감소하였고, 볼트 간격이 증가할 때 2~10% 정도 감소하였다. 2) 단일 볼트접합부와 Type-A의 이중 볼트접합부의 파괴형상은 연단거리 방향으로 할렬파단이 일어났다. Type-B의 경우 볼트간격이 3 d일 때 인장부위 볼트가 압축부위 볼트보다 더 굴곡되었고 인장부위볼트에서 할렬파단이 시작되었다. 5 d 시편의 경우 인장부위와 압축부위 볼트의 굴곡은 비슷하게 나타났으며, 압축부위볼트에서 할렬파단이 시작되었다. 3) 설계표준시 기준볼트 간격(Type A : 7 d, Type B : 5 d)에 따른 항복하중을 무차원화시켜 저감계수를 산출하였다. 12 mm 볼트접합부의 경우 Type-A인 볼트 간격 4d와 단일 볼트접합부의 저감계수는 각각 0.87, 0.55였고 Type-B인 볼트 간격 3 d와 단일 볼트접합부의 저감계수는 0.91, 0.55였다. 16 mm 볼트접합부의 경우 Type-A인 볼트 간격 4 d와 단일 볼트접합부의 저감계수는 0.96, 0.76이었고 Type-B인 볼트 간격 3 d, 단일 볼트접합부의 저감계수는 0.91, 0.77이었다.

Application of silk composite to decorative laminate

  • Kimura, Teruo;Aoki, Shinpei
    • Advanced Composite Materials
    • /
    • 제16권4호
    • /
    • pp.349-360
    • /
    • 2007
  • Recently, natural fiber reinforced composite is attracting attention and considered as an environmentally friendly material. Usually cellulosic fibers are used to reinforce the composites, but some protein fibers such as silk and wool serve the same purpose. In this paper, we proposed a method of producing artistic composite from artistic fabric by using silk fiber reinforced biodegradable plastic, which is designated as 'silk composite', for reinforcement. In order to expand applications of the silk composite, we performed the compression molding of decorative laminates with woody material, which was selected as a core material, and examined the properties of molded decorative laminates with various content of the silk composite. Since plywood and medium-density fiberboard (MDF) are widely used for decorative laminates, we selected them as core materials. As a result, flexible decorative laminates with high flexural strength were obtained by compounding the silk composite with wood materials.

리기다소나무(Pinus rigida Miller)의 목재해부학적(木材解剖學的) 및 물리학적성질(物理學的性質)에 관(關)한 연구(硏究) - 간(幹), 지(枝), 근(根), 초두목(梢頭木)의 특성(特性)을 중심(中心)으로 - (Anatomical and Physical Properties of Pitch Pine (Pinus rigida Miller) - The Characteristics of Stem, Branch, Root and Topwood -)

  • 이필우
    • 한국산림과학회지
    • /
    • 제16권1호
    • /
    • pp.33-62
    • /
    • 1972
  • 리기다소나무는 미국(美國)으로부터 우리나라에 도입(導入)하여 온지 60여년(餘年)의 세월이 흐르는 동안 오늘날에는 중요(重要)한 조림수종(造林樹種)으로 발전(發展)하였고 이미 국내(國內)에서는 상당량(相當量)의 목재생산(木材生産)이 이루지고 있기 때문에 합리적(合理的)인 목재이용(木材利用)을 위(爲)해서는 그 기본적(基本的)인 성질연구(性質硏究)가 필연적(必然的)으로 요청(要請)되고 있다. 따라서 본연구(本硏究)에서는 리기다소나무의 목재해부학적(木材解剖學的), 물리학적(物理學的), 기계학적성질(機械學的性質)을 구명(究明)키로 한 것이다. 본연구(本硏究)에서 사용(使用)한 공시목(供試木)은 서울대학교(大學校) 농과대학(農科大學) 부속수원연습림내(附屬水原演習林內)에 위치(位置)하고 있는 46~52년생(年生)의 리기다소나무임분(林分)에서 정상적(正常的)으로 생장(生長)한 15개림목(個林木)을 선정(選定)하였는데 5개림목(個林木)은 해부학적(解剖學的) 연구(硏究)를 위(爲)해서 1967년(年) 2월(月)에 대채(代採)하였다. 이들 시험목(試驗木)은 간(幹), 지(枝), 근(根), 초두목(梢頭木)의 성질연구(性質硏究)를 위(爲)해서 수목(樹木)의 모든 재부분(材部分)을 채취(採取)하였다. 이 연구(硏究)의 해부학적성질(解剖學的性質)에 있어서는 연륜(年輪), 수지구(樹脂溝), 방사조직(放射組織), 가도관(假導管), 방사가도관(放射假導管), 방사유세포(放射柔細胞) 및 막공등(膜孔等)의 육안적(肉眼的) 현미경적특징(顯微鏡的特徵)이 재부분(材部分)(간(幹), 지(枝), 근(根), 초두목(梢頭木))별(別)로 관찰(觀察)하고 측정(測定)하였다. 물리적(物理的) 그리고 기계적성질(機械的性質)에 있어서는 생재함수율(生材含水率), 목재비중(木材比重), 수축율(收縮率), 섬유평행방향(纖維平行方向)의 압축강도(壓縮强度), 섬유평행(纖維平行) 및 직각방향(直角方向)의 인장강도(引張强度), 경단(徑斷) 및 촉단방향(觸斷方向)의 전단강도(剪斷强度), 곡강도(曲强度), 할렬강도(割裂强度) 및 경도(硬度)에 관해서 연구(硏究)하였는데 본연구(本硏究)에서 얻은 결론(結論)은 다음과 같다. 1. 목재(木材)의 육안적성질(肉眼的性質)에 있어서 재부분간(材部分間)에 비교(比較)할수 있는 특성(特性)은 연륜(年輪)의 판명도(判明度), 연륜폭(年輪幅), 춘추재간(春秋材間)의 이행(移行), 재색등(材色等)이 가장 중요(重要)한 것이었다. 또 현미경적성질(顯微鏡的性質)에 있어서는 목재구성요소(木材構成要素)의 크기가 재부분간(材部分間)을 비교(比較)할수 있는 특징(特徵)이 되는데 가도관(假導管)의 장(長), 폭(幅), 막후(膜厚), 수지구(樹脂溝), 방사조직등(放射組織等)이 중요(重要)한 것이었다. 2. 재부분간(材部分間)에 비교(比較)된 현미경적특성(顯微鏡的特性)은 간재(幹材)와 초두목간(梢頭木間)에 비슷한 결과(結果)를 나타내었으나 근재(根材)는 촉단면상(觸斷面上)에서 다른 재부(材部)와 비교(比較)하여 일층(一層) 큰 방사조직(放射組織)이 관찰측정되었는데 단열방사조직최대(單列放射組織最大)의 것은 높이 27세포고(細胞高)($550{\mu}$)에 폭(幅)은 $35{\mu}$이었다. 그리고 방추상방사조직(紡錘狀放射組織)은 1~수개(數個)의 수평수지구(水平樹脂溝)를 내포(內包)하는 연합방사조직(連合放射組織)을 형성(形成)한다. 한편 지재(枝材)에 있어서 조직(組織)의 특징(特徵)은 간재(幹材)와 같았으나 구성요소(構成要素)의 측정치(測定値)가 다른 재부(材部)에 비(比)하여 일층(一層) 작었다. 3. 재부분간(材部分間)에 측정(測定)된 가도관(假導管)의 크기는 간재(幹材)에서 길이가 가장 길었고 지재(枝材)에서 가장 짧았다. 재부분가도관장간유의차(材部分假導管長間有意差)를 검정(檢定)한바 간재(幹材)와 근재간(根材間)에만 차이(差異)가 없었고 기타재부분간(基他材部分間)에는 모두 차이(差異)가 있었다. 가도관폭(假導管幅)은 근재부분(根材部分)이 가장 넓었고 지재부분(枝材部分)이 가장 좁았으나 재부분간(材部分間)에는 차이(差異)가 없었다. 막후(膜厚)는 근재(根材)가 가장 두꺼웠고 지재(枝材)가 가장 좁았는데 재부분간(材部分間)에는 근재(根材)와 초두목간(梢頭木間), 근재(根材)와 지재간(枝材間) 또 간재(幹材)와 지재간(枝材間)에는 차이(差異)가 있었으나 기타재부분간(基他材部分間)에는 차이(差異)가 없었다. 4. 입목(立木)의 생재함수율(生材含水率)은 초두목(梢頭木)이 가장 높았고 간재(幹材)의 심재부분(心材部分)이 가장 낮았다. 재부분별(材部分別) 함수량간유의차(含水量間有意差)를 검정(檢定)한바 초두목(梢頭木)과 기타재부분간(基他材部分間), 심재(心材)와 기타재부분간(基他材部分間)에 차이(差異)가 있었으나 근재(根材)와 지재간(枝材間) 그리고 근재(根材)와 변재간(邊材間)에는 차이(差異)가 없었다. 5. 목재(木材)의 비중(比重)은 간재(幹材)가 가장 높았고 다음은 근재(根材), 지재(枝材)의 순(順)이고 초두목(梢頭木)은 가장 낮았다. 재부분비중간유의차(材部分比重間有意差)를 검정(檢定)한바 간재(幹材)와 다른 재부분(材部分) 사이에는 뚜렷하게 차이(差異)가 있으며 근재(根材)와 지재(枝材)사이에는 차이(差異)가 없었고 초두목(梢頭木)은 제일작은 치(値)로서 유의차(有意差)가 인정(認定)된다. 6. 함수율(含水率) 14%때 재부분간(材部分間)의 섬유평행방향압축강도(纖維平行方向壓縮强度)를 비교(比較)하면 가장 높은 강도(强度)는 간재(幹材)에서 나타났고 다음은 지재(枝材), 근재(根材)의 순(順)이고 초두목(梢頭木)은 가장 낮은 강도(强度)를 나타내었다. 7. 함수율(含水率) 14%때 재부분간(材部分間)의 곡강도(曲强度)를 비교(比較)하면 지재(枝材)에서 뚜렷하게 높은 강도(强度)를 나타내었으며 다음은 간재(幹材), 지재(枝材), 근재(根材)의 순(順)이고 초두목(梢頭木)은 가장 낮은 강도(强度)를 나타내었다. 특(特)히 지재(枝材)는 간재(幹材)보다 낮은 비중(比重)을 갖이고 있었는데도 불구(不拘)하고 높은 곡강도(曲强度)를 나타내었다.

  • PDF

수입(輸入)코르크와 국산(國産)코르크의 물리(物理)·기계적(機械的) 성질(性質)에 관(關)한 연구(硏究) (Studies on the Physical and Mechanical Properties of Imported and Domestic Corks)

  • 김병로
    • Journal of the Korean Wood Science and Technology
    • /
    • 제21권4호
    • /
    • pp.45-54
    • /
    • 1993
  • This study examines the differences in structures, physical and mechanical properties between domestic(Quercus variabilis Blume) and foreign(Quercus suber L.) corks. The results obtained are as follows: 1. The cork tissue consists of cork cells, lenticels, sclereids and dark-brown zone. There was a significant difference in ratio of cork cells between foreign cork(93 %) and domestic cork(87 %). The ring width and width of late cork of the foreign cork were wider than those of domestic cork. But the percentage of late cork of domestic cork was richer than that of foreign cork. The size of cork cell of foreign cork was larger by about two times than that of domestic cork. 2. The density was slightly higher in domestic cork(0.22 g/$cm^3$) than in foreign cork(0.19 g/$cm^3$). During first 24 hours, the amount of water absorption of the foreign cork was greater than that of domestic cork. However, after 24 hours, the tendency was reversed. The level of EMC was higher in domestic cork than in foreign cork. Total shrinkage in the radial and tangential directions was larger in domestic cork than tn foreign cork. In the longitudinal direction, the tendency was reversed. There was no difference in total swelling in three woody directions between the two corks. 3. The modulus of elasticity in compression in the logitudinal and tangential direction was higher in domestic cork than in foreign cork, but the tendency was reversed in the radial direction. Both corks showed 95% of recovery rate after 24 hours when they were compressed by 0.5. There were no differences in tension strength and Brinell,s hardness bet ween domestic and foreign corks.

  • PDF

구성형태(構成形態)에 따른 파티클과 파이버로 제조(製造)한 패널의 물리적 및 기계적 성질 (Physical and Mechanical Properties of Panels Fabricated with Particle and Fiber by Composition Types)

  • 윤형운;이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제20권2호
    • /
    • pp.9-22
    • /
    • 1992
  • The aim of this research was to investigate physical and mechanical properties of various composition panels, each fabricated with a ratio of fiber to particle of 2 to 10. Type A consisted of fiber-faces and particle-core in layered-mat system. Type B consisted of fiberboard-faces on particleboard-core. Type C consisted of fibers and particles in mixed-mat system. The results obtained from tests of bending strength, internal bond, screw holding strength and stability were as follows: 1. The bending strength and internal bonding of both the Type A panel and the Type B panel were higher than those of the Type C panel and three-layered particle board. 2. The mechanical properties of the Type C panel showed the lowest values of all composition methods. It seems that the different compression ratios of the particle and fiber interrupted the densification of the fibers when hot pressed. 3. The dimensional stability of layered-mat system panels consising of fiber-faces and particle-core was better the than control particleboard. 4. In composition methods of particle and fiber, layered-composition method was more resonable than mixed-composition. The Type B panel had the highest mechanical properties of all the composition types. 5. The Type A panel was considered the ideal composition method because of its resistance to delamination between the particle-layer and the fiber-layer and because of its lower adhesive content and more effective manufa cturing process.

  • PDF

Analysis and design of metal-plate-connected joints subjected to buckling loads

  • Hussein, R.
    • Structural Engineering and Mechanics
    • /
    • 제9권5호
    • /
    • pp.417-432
    • /
    • 2000
  • A comprehensive analytic study has been conducted to investigate the instability problems of metal-plate-connected (MPC) joints in light frame trusses. The primary objective in this study is to determine the governing factors that constitute the buckling of the metal connectors and their effects on the structural response of joints. Another objective is to recommend design curves for the daily structural design of these joints. The numeric data presented in this paper has emerged from a broad base that was founded on over 350 advanced computer simulations, and was supported by available experimental results obtained by others. This basic-to-applied research includes practical engineering parameters such as size of gaps, shear lengths, gauge (plate thickness) of connectors, size of un-braced areas, failure modes, and progressive disintegration of joints. Square-end members have been emphasized though the results cover the custom-made fitted joints. The results indicate that chord shears cause and dominate the buckling of MPC joints, and the shear length has a more pronounced effect than the size of gaps. Further, large gauges and small un-braced areas improve the buckling response. Several practical recommendations have been suggested throughout the paper such as keeping the ratio of gap/shear length below 3/4 for improving the buckling strength. The study reveals that multi-area joints should not be simplified as single web-to-chord MPC joints such as keeping the ratio of gap/shear length below 3/4 for improving the buckling strength, even where one web is in tension and the other in compression. Finally, the results obtained from this study favorably agree with experimental data by others, and the classic buckling theories for other structural components.

목탄을 이용한 친환경 건축자재 이용기술(I) - 목탄으로 제조된 건축자재의 특성 평가 - (Utilization of Charcoal as an Environmentally Friendly Building Materials (I) - Characterization of Building Materials Prepared with Charcoal -)

  • 안병준;조태수;이성숙;백기현;김선익
    • Journal of the Korean Wood Science and Technology
    • /
    • 제37권6호
    • /
    • pp.537-545
    • /
    • 2009
  • 본 연구는 일반 페인트 및 건조시멘트에 목탄을 첨가하여 제조된 건축자재의 제반 물리 화학적 특성 조사를 바탕으로 하여 목탄의 친환경 건축자재 혼합제로서의 활용 가능성을 모색하기 위한 목적으로 수행되었다. 목탄을 포함한 액상몰탈의 물리 화학적 물성 시험결과, 목탄 20% 이상을 포함한 액상몰탈의 경우, 점도에 대한 저항치인 주도와 불휘발분이 품질기준에 적합하였다. 목탄 첨가량이 증가할수록 건조시간은 지연되었으나, 모든 처리구에서 품질기준인 60분 이내에서 건조가 완료되었다. 기타 제반 물성에서는 모든 처리구에서 품질기준을 충족하였다. 이 결과로 볼 때, 액상 몰탈에 대한 적정 목탄 함량은 25%로 판단된다. 건조 시멘트 몰탈에 대한 압축강도는 목탄 5% 첨가구에서 가장 우수하였으며, 20% 이상 첨가구에서는 KS 기준치에 비해 낮은 것으로 조사되었다. 또한 목탄 첨가량 증가로 보수성은 지속적으로 증가하며, 암모니아가스 탈취율의 경우 일반 시멘트 몰탈이 59.5%, 목탄 10% 첨가 시멘트 몰탈은 71.6%의 암모니아를 흡착하였다.

베개의 압축성에 대한 인간공학적 연구 (The Ergonomic Study on the Compressibility of the Pillow)

  • 이연순;남윤자
    • 한국의류학회지
    • /
    • 제13권3호
    • /
    • pp.187-196
    • /
    • 1989
  • The purpose of this study is to find at the basic data for the appropriate compressibility of the pillows for the Koreans as well as, for the appropriate conditions to establish the estimating criterion for the pillows on the market place. This paper also aim to grasp thr compressibility of the materials used to make the pillows for sale. The appropriate compressive rate of the pillows have been investigated by sensuous test. The compressive rate, recovery rate, and decreasing rate of compression and recovery have been investigated by means of ergonomic and physical experiments. The results were as follows; 1) By sensuous test, the compressive rate of the pillows for the most comfortable state turns up $45\%{\pm}5\%$ in men and women. 2) As for the compressive rate and recovery rate of the eight pillow materials on market, panya, duck feather two kinds of synthetic fiber are highest, wood is lowest. 3) The compressive rate of panya, duck feather, and two kinds of fiber is within the range of the comfort by sensuous test. 4) In the durability of the compressive rate and recovery rate against the repeated use of the pillows, duck feather is in the highest grade, panya is the lowest grade and the others are graded between two.

  • PDF