• 제목/요약/키워드: color-$X^2$

검색결과 648건 처리시간 0.033초

Properties of $Y_{2-x}SiO_{5}:Ce_{x}^{3+}$ Phosphor Powder Prepared by Sol-gel Process (Sol-gel법에 의한 $Y_{2-x}SiO_{5}:Ce_{x}^{3+}$ 형광체 제조와 그 특성)

  • Kim, Sang-Mun;Kang, Kyoung-Tae;Kim, Tae-Ok
    • Journal of the Korean Ceramic Society
    • /
    • 제38권9호
    • /
    • pp.794-798
    • /
    • 2001
  • $Y_{2-x}SiO_5:Ce_x^{3+}$(x=0.002∼0.04) phosphors were prepared by sol-gel process, amorphous crystal phase was observed in calcining dry gel at 800$^{\circ}$C, but pure $X_2$ type of type $Y_2SiO_5$ phase appeared from heat treatment above 1000$^{\circ}$C. Light absorption of tye $Y_2SiO_5$ host lattice occurred at 230∼360nm, and light absorption of the $Y_{2-x}SiO_5:Ce_x^{3+}$ phosphors was observed at 300∼400nm in adding $Ce^{3+}$. $Y_{2-x}SiO_5:Ce_x^{3+}$ phosphors showed maximum emission shoulder at 436nm. Maximum CL intensities of $Y_{2-x}SiO_5:Ce_x^{3+}$ were observed in adding 0.025 $Ce^{3+}$ and the phosphor showed x=0.161, y=0.124 in color coordinate of CIE1931.

  • PDF

Synthesis and Formation Mechanism of Cobalt Doped Willemite Blue Pigments (Co-Doped Willemite 파란색 안료의 합성과 생성기구)

  • Hwang, Dong-Ha;Han, Kyong-Sop;Lee, Byung-Ha
    • Journal of the Korean Ceramic Society
    • /
    • 제47권6호
    • /
    • pp.603-607
    • /
    • 2010
  • Turquoise blue pigment of Vanadium-zircon blue (DCMA number 14-42-2), which was already commercialized, was stable to be reproduced but insufficient to give strong blue. However, it possible to obtain more intense blue by partially substituting cobalt ions into the willemite($Zn_2SiO_4$) lattice classified into DCMA number 7-10-2 for blue ceramic pigment. By the composition of willemite $Co_xZn_{2-x}SiO_4$(X=0.01, 0.03, 0.05, 0.07, 0.09 mole), this study used reagent grade zinc oxide, cobalt oxide and silicon dioxide as starting materials, carrying out the synthesis with solid reaction method by adding $H_3BO_3$ as a mineralizer. The firing temperature was between $1200^{\circ}C$ and $1400^{\circ}C$. The characteristics of synthesized pigment were analyzed by X-ray diffraction, Raman spectroscopy and SEM and the characteristics of color tones were analyzed by UV-Vis spectroscopy and CIE-$L^*a^*b^*$ measurement. As a result, the optimal composition was $Zn_{1.95}Co_{0.05}$ with 1wt% of $H_3BO_3$ as a mineralizer and firing condition was $1350^{\circ}C$/3 h. $L^*a^*b^*$ value was 29.25, 41.03, -59.93 for on glaze pigment and 37.03, 36.41, -60.03 for under glaze pigment.

Preference for Color and Fabric Motifs in Men's Clothing Design - In the area of men by age, physical type and job - (추동용 정장양복과 콤비양복의 색채 및 직물무늬에 관한 연구 - 성인남성의 연령별, 신체적 조건 및 직업에 따른 선호를 중심으로 -)

  • 조진숙
    • Journal of the Korean Home Economics Association
    • /
    • 제31권1호
    • /
    • pp.193-210
    • /
    • 1993
  • The purpose of this study was to investigate the effect of age, physical type and job on preference for color and fabric motifs in men's clothing design. Color preference measures consisted of clothing styles painted in CAD. Preference for fabric motifs was assesed by stripe fabrics in size, width and strength. All of the preference measures were devised specifically for this study. Furthermore, items on Hight and Weight for physical type, age and job of subjects were included I the questionnaire. Data were obtained by self-administered questionnaires form 243 men (25-54 years old) in Seoul. Analysis was by chi-square (X2), frequency, and percentage. The results obtained in this study were as follows : 1. Color preference was not affected by age and physical type, Job was related to coordinate color of men's clothing. 2. Preference for width of striped motifs was affected by age and job. 3. Preference for strength of fabric motifs in men's jacket was affected by physical type.

  • PDF

Luminescence Characteristics of Blue Phosphor and Fabrication of a UV-based White LED (UV 기반 백색 LED용 청색 형광체의 발광특성 및 백색 LED 제조)

  • Jung, Hyungsik;Park, Seongwoo;Kim, Taehoon;Kim, Jongsu
    • Korean Journal of Optics and Photonics
    • /
    • 제25권4호
    • /
    • pp.216-220
    • /
    • 2014
  • We have synthesized a $CaMgSi_2O_6:Eu^{2+}$ blue phosphor via a solid-state reaction method. The $CaMgSi_2O_6:Eu^{2+}$ phosphor has monoclinic structure with a space group of C2/c (15), and an emission band peaking at 450 nm (blue) due to the $4f^7-4f^65d$ transition of the $Eu^{2+}ion$. The emission intensity at $100^{\circ}C$ is 54% of the value at room temperature. A white LED was fabricated by integrating a UV LED (400 nm) with our blue phosphor plus two commercial green and red phosphors. The white LED shows a color temperature of 3500 K with a color rendering index of 87 (x = 0.3936, y = 0.3605), and a luminous efficiency of 18 lm/W. The white LED shows a luminance maintenance of 97% after operation at 350 mA for 400 hours at $85^{\circ}C$.

Effects of Eu3+ Concentration on the Photoluminescence Properties of Red-orange Phosphor Gd1-xPO4:Eux3+ (Eu3+ 농도가 적주황색 형광체 Gd1-xPO4:Eux3+의 발광 특성에 미치는 영향)

  • Cho, Seon-Woog
    • Korean Journal of Materials Research
    • /
    • 제21권11호
    • /
    • pp.611-616
    • /
    • 2011
  • Red-orange phosphors $Gd_{1-x}PO_4:{Eu_x}^{3+}$ (x = 0, 0.05, 0.10, 0.15, 0.20) were synthesized with changing the concentration of $Eu^{3+}$ ions using a solid-state reaction method. The crystal structures, surface morphology, and optical properties of the ceramic phosphors were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM), and photoluminescence (PL) spectrophotometry. The XRD results were in accordance with JCPDS (32-0386), and the crystal structures of all the red-orange phosphors were found to be a monoclinic system. The SEM results showed that the size of grains increases and then decreases as the concentration of $Eu^{3+}$ ionincreases. As for the PL properties, all of the ceramic phosphors, irrespective of $Eu^{3+}$ ion concentration, had orange and red emissions peaks at 594 nm and 613 nm, respectively. The maximum excitation and emission spectra were observed at 0.10 mol of $Eu^{3+}$ ion concentration, just like the grain size. An orange color stronger than the red means that $^5D_0{\rightarrow}^7F_1$ (magnetic dipole transition) is dominant over the $^5D_0{\rightarrow}^7F_2$ (electric dipole transition), and $Eu^{3+}$ is located at the center of the inversion symmetry. These properties contrasted with those of a red phosphor $Y_{1-x}PO_4:{Eu_x}^{3+}$, which has a tetragonal system. Therefore, we confirm that the crystal structure of the host material has a major effect on the resulting color.

Quality Characteristics of Hot-air Dried Radish (Raphanus sativus L.) Leaves (열풍 건조 무청의 품질특성)

  • Ku, Kyung-Hyung;Lee, Kyung-A;Kim, Young-Lim;Lee, Yong-Whan
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • 제35권6호
    • /
    • pp.780-785
    • /
    • 2006
  • The composition analysis of various radish (Rapharnus sativus L.) leaves and the effects of drying condition on the quality characteristics of hot-air dried radish leaves were carried out by a response surface methodology. Independent variables put in drying temperature $(X_1)$ and drying time $(X_2)$, dependent variables put in color, calcium, iron, vitamin, etc. In the proximate composition of radish leaves by varieties, there were no significant differences in the ash, protein, lipid, calcium and iron content of samples, but there were significant differences in the vitamins, chlorophyll and color value of samples. The quality characteristics on dried radish leaves by central composite design, it was significant value on the moisture content, chlorophyll and color value according to drying temperature and drying times. But there were no significant differences in the contents of calcium $(31.41{\sim}35.80\;mg/g,\;dry\;base)$ and iron $(0.21{\sim}0.29\;mg/g\;dry\;base)$. The multiplex regression coefficients analysis were calculated with independent variables $(X_1,\;X_2)$ and dependent variables (moisture, chlorophyll, color value). The calculated coefficient correlations for the each samples were $R^2>0.97$. The effects of drying temperature were greater than drying time in the total chlorophyll content changes of radish leaves. Based on the present study, the optimum drying condition for the lowest color changes and effective reduction of moisture of radish leaves were expected to be $5{\sim}6$ hours at $70^{\circ}C$.

Color Enhancement of Natural Sapphires by High Pressure High Temperature Process

  • Song, Jeongho;Noh, Yunyoung;Song, Ohsung
    • Journal of the Korean Ceramic Society
    • /
    • 제52권2호
    • /
    • pp.165-170
    • /
    • 2015
  • We employed the high-pressure high temperature (HPHT) process to enhance the colors of natural sapphires to obtain a vivid blue. First, we analyze the content of the coloring agent $Fe_2O_3$ using the wavelength dispersive X-ray fluorescence (WD-XRF) method. The HPHT procedure operates under 1 GPa at various temperatures of 1700, 1750, and $1800^{\circ}C$ for 5 minutes using a cubic press. We determine the color changes using the optical microscopic images, UV-VIS near-infrared (NIR) spectra, micro-Raman spectra, and Fourier transform-infrared (FT-IR) spectra for all sapphire samples before and after the treatment. The optical microscopic results indicate that the HPHT process can enhance the sapphire color to a vivid blue at temperatures above $1750^{\circ}C$. The UV-VIS-NIR spectra identify the color changes explicitly and quantitatively through providing the Lab color scales and color differences. Both results demonstrate that the colors of natural sapphires can be enhanced to a vivid blue using the HPHT process above $1750^{\circ}C$ under 1 GPa for 5 minutes.

Synthesis and Optical Characteristics of Green-Emitting (Mg,Zn)$Al_2O_4:Mn^{2+}$ Phosphor for 3D- PDP Applications

  • Han, Bo-Yong;Yoo, Jae-Soo;Heo, Eun-Gi;Yoo, Young-Gil
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2009년도 9th International Meeting on Information Display
    • /
    • pp.272-275
    • /
    • 2009
  • A new green phosphor, ($Mg_{1-x-yZnx)$)$Al_2O_4:Mn^{2+}{_y}$ (0 x 0.6, 0.001 y 0.01), was synthesized by a flux-assisted solid reaction and its vacuum ultraviolet (VUV) excitation and emission characteristics were examined in this study. The chromaticity and peak intensity of the $(Mg_{0.79}Zn_{0.2})Al_2O_4:Mn^{2+}{_{0.01}}$ (x = 0.177, y = 0.745) phosphor were found to be more desirable than that of $Zn_2SiO_4:Mn^{2+}$ (x = 0.216, y = 0.72) phosphor as a green primary color.

  • PDF

Effect of the Amount of Pigment on the Color of Silk Dyed with Fermented Indigo Powder Dye (발효쪽 분말염료로 염색한 견직물의 색소 함량이 직물의 색상에 미치는 영향)

  • Yoo, Wansong;Ahn, Cheunsoon
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • 제42권2호
    • /
    • pp.342-359
    • /
    • 2018
  • This research investigated the relationship between the amount of fixed pigment and the color of silk dyed with three types of fermented indigo powder dye under different temperatures and pH, by reduction or nonreduction method. Amount of fixed pigment was analyzed using the Ultimate 3000 HPLC-DAD instrument and the color of dyed silk was measured using the X-rite spectrocolorimeter. All silk samples dyed by reduction method showed PB color. The amount of indigotin fixation was dependent on the dyeing temperature and pH regardless of the indigotin composition in the dye. Indirubin was less dependent upon the dyeing condition in the reduction dyeing and its fixation was minimum level. Dyeing conditions which can maximize the indigotin fixation were $50^{\circ}C/pH$ 11 and $70^{\circ}C/pH$ 7 conditions in reduction dyeing. Color of silk showed more redness ($a^*$) thus higher PB color when the indigotin fixation was low and indirubin fixation was relatively high. Indirubin fixation was very low with slightly better fixation by nonreduction method. More reddish color was obtained by nonreduction dyeing, and by more alkaline dyebath.

Particle Size, Morphology and Color Characteristics of C.I. Pigment Red 57:1 : 2. Effect of Salt Milling Process

  • Seo, Hee Sung;Lee, Hyun Kyung;Yoo, Eui Sang
    • Textile Coloration and Finishing
    • /
    • 제27권4호
    • /
    • pp.245-260
    • /
    • 2015
  • The effect of salt milling process on the crystal size, morphology, and color characteristics of C.I. Pigment Red 57:1 was studied. The primitive morphology and color properties of the pigment after synthesis were studied in the former series work. The size and morphology of primary particles and the second aggregation features should be considered because they are very important to determine pigment quality. We compared the primary morphology of pigment particles before drying with the secondary aggregated morphology of pigment particles after drying and salt milling process. Morphological properties were investigated by particle size analysis, X-ray diffraction, and scanning electron microscopy and color measurement was carried out. Significant reduction in particle size as well as enhanced crystallite size after salt milling process was observed. This result might give a difference in color of the pigment, turning into brighter and more blue-toned red color. It was revealed that synthesis condition affect the morphology and color of the pigment even after milling. Increase in HCl concentration in the synthesis process enhanced crystal size and quality forming bluer-red pigments but an increase in $CaCl_2$ concentration resulted in more amorphous crystals forming darker-red pigments after salt milling.