With the increasing attention to environmental pollution caused by particulate matter globally, the automotive industry has also become increasingly interested in particulate matter, especially particulate matter generated by automobile brake systems. Here, we designed a coating composition and analyzed its mechanical properties to reduce particulate matter generated by brake systems during braking of vehicles. We designed a composition to check the mechanical properties change by adding Cr3C2 and YSZ to the WC-Ni-Cr composite composition. Based on the designed composition, coating samples were manufactured, and the coating properties were analyzed by Vickers hardness and ball-on-disk tests. As a result of the experiments, we found that the hardness and friction coefficient of the coating increased as the amount of Cr3C2 added decreased. Furthermore, we found that the hardness of the coating layer decreased when YSZ was added at 20vol%, but the friction coefficient was higher than the composition with Cr3C2 addition.
주차장 바닥재로 많이 사용되는 A사 에폭시 코팅제와 B사 바닥코팅제(A, B type)에 대하여 GC/MS(Gaschromatography/Mass spectrometer)를 이용하여 제품별로 함유하고 있는 휘발성유기화합물(VOCs)의 종류와 함량을 측정해보고, 휘발성유기화합물(VOCs)중 작업자나 입주자들에게 유해한 폼알데하이드(Formaldehyde), 톨루엔(Toluene), 크실렌(Xylene)을 외부 환경에 따른 오차를 줄이고자 가장 안 좋은(밀폐) 환경을 가정하고 가스검지관을 이용하여 가스배출량을 측정해 보았다. 그 결과 A사 에폭시코팅제가 제품 자체에도 휘발성유기화합물(VOCs)을 가장 많은 양 함유하고 있고, A사 에폭시코팅제에 비하여 B사 바닥코팅제 A type은 약 79%, B type은 약 96% 이상의 적은 양을 나타냈다. 또한, 밀폐된 환경 조건에서 1시간과 8시간 경과 후 가스검지관을 이용하여 폼알데하이드(Formaldehyde), 톨루엔(Toluene), 크실렌(Xylene)에 대한 가스배출량을 측정하고 TWA값으로 환산한 결과에서도 A사 에폭시코팅제가 가장 높게 측정되었다. A사 에폭시코팅제보다 B사 바닥코팅제 A type은 약 42.3%이상의 적은 측정값을 나타냈으며, B type의 경우 밀폐된 환경 조건에서도 시간가중평균노출기준(TWA)을 모두 만족하였다.
We investigated the effects of Al and Mg on the microstructure and hardness of the coating layer of galvanized steel sheets, by thermodynamic calculations, X-ray diffraction, scanning electron microscopy, and Vickers hardness tests of Zn-0.2Al, Zn-6Al-2Mg, and Zn-10Al-5Mg coating layers. Regardless of the alloy composition of the galvanizing bath, a Fe-Al layer was observed between the coating layer and steel sheet. The Zn-0.2Al coating layer consists of major h.c.p. Zn phase and minor f.c.c. Al phase. The fraction of f.c.c. Al phase (containing a significant amount of Zn) of the coating layer increases with increasing the chemical composition of Al of the galvanizing bath. The h.c.p. MgZn2 phase was formed in the Al/Mg-containing Zn-6Al-2Mg and Zn-10Al-5Mg coating layers, forming Zn-Al-MgZn2 eutectic microstructure. The primary MgZn2 phase was additionally formed in the Zn-10Al-5Mg coating layers containing high concentrations of Al and Mg. The Vickers hardness values of Zn-0.2Al, Zn-6Al-2Mg, and Zn-10Al-5Mg coating layers were 59.1 ± 1.2 HV, 161.2 ± 5.7 HV, and 215.5 ± 40.3 HV, respectively. The addition of Al and Mg increased the hardness of the coating layer by increasing the fraction of the Al phase (containing Zn) and MgZn2 intermetallic compound, which were harder than the Zn phase.
Metal transfer behavior of three shielded metal arc welding electrodes, AWS El1018, E6013 and E6010, were investigated through the characterization of size distribution of droplets and measurement of arc voltage signals. Of the three electrodes, Ell018 electrode showed the largest droplet size with the smallest amount of spatter, while E6010 electrode showed the smallest droplet size with the largest amount of spatter. Even though Ell0l8 electrode showed a good agreement between the frequencies of voltage drop in FFT processed voltage signals and the transfer rate of droplets, E6013 and E6010 electrodes showed weaker correlation because of their dominant explosive transfer behavior. The type of cathode used and electrode baking time also influenced the metal transfer behavior. Compared to bead-on-plate welding using steel plate as a cathode, welding on a water-cooled copper pipe showed less short-circuiting and higher melting rate in all electrodes because of higher arc potential and/or anode drop. When baked for a long time, E6010 electrode showed much more stable arc with less short-circuiting and explosion due to the loss of gas formation ingredients.
Printed mottle of coated paper is one of the most common but the most difficult problem in offset printing. Printed mottle is caused by an uneven penetration of Ink into the paper, binder migration, etc. For a high quality printing, development of new paper coating technologies to prevent print mottle is required. So for, the study of solving printed mottle is coated paper absorption controlled by base paper sizing and coating layer binder migration control. As a results, printed mottle has improved in coated paper. But printing is worked by interaction of printing ink, coated paper and printing pressure, then we need to understand of interaction printing work and coated paper. This research focused on a way of improving printed mottle by investigating various printing conditions such as ink dispersion, nip condition and amount of ink transfer using IGT printability tester.
In this study, we conducted an impact assessment of the amount of volatile organic solvents addition on hybrid water-proofing system of urethane waterproof coating material and modified asphalt sheet. Also, we conducted a comparative assessment of whether modified asphalt sheet is dissolved or not and oil leakage by dissolution in order to perform a comparative analysis of characteristics of the impact on modified asphalt sheet according to the volatility of volatile organic solvents included in urethane waterproof coating material. The test was carried out by adding the same amount of organic solvents into each experimental group which is subject to volatility and non-volatility of organic solvents, respectively. The results of the test showed that in both experimental groups modified asphalt sheet was dissolved when adding over 10 percent of organic solvents regardless of volatility, and oil leakage observed only in the experimental group subject to volatility.
Song, Young Il;Lee, Jung Woo;Kim, Tae Yoo;Jung, Hwan Jung;Jung, Yong Chae;Suh, Su Jeung;Yang, Cheol-Min
Carbon letters
/
제14권4호
/
pp.255-258
/
2013
Flexible transparent conducting films (TCFs) were fabricated by dip-coating single-wall carbon nanotubes (SWCNTs) onto a flexible polyethylene terephthalate (PET) film. The amount of coated SWCNTs was controlled simply by dipping number. Because the performance of SWCNT-based TCFs is influenced by both electrical conductance and optical transmittance, we evaluated the film performance by introducing a film property factor using both the number of interconnected SWCNT bundles at intersection points, and the coverage of SWCNTs on the PET substrate, in field emission scanning electron microscopic images. The microscopic film property factor was in an excellent agreement with the macroscopic one determined from electrical conductance and optical transmittance measurements, especially for a small number of dippings. Therefore, the most crucial factor governing the performance of the SWCNT-based TCFs is a SWCNT-network structure with a large number of intersection points for a minimum amount of deposited SWCNTs.
This study has developed an organic/inorganic hybrid solution according to amount of $SiO_2$ polysilicate, and the amount of melamine is constant. The three types of cold rolled steel were evaluated a corrosion resistance properties by using these solutions. $US_3M_3$ and $US_{11}M_3$ solutions were generate a lot of corrosion. $US_7M_3$ solution was excellent in corrosion resistance, regardless of the steel type. The appearance of coating by $US_3M_3$ and $US_{11}M_3$ solutions were bumpy surface, and were a lot of fine defects. $US_7M_3$ solution was made a sophisticated molecular cross-linking structure inside the coating, it was a slick surface. Other characteristics are exhibited the excellent property for all solutions.
Objectives: A radon emission reducing agent was prepared using charcoal and zeolite, and the amount was measured after coating construction materials with the agent. The availability of the radon emission reducing agent was evaluated. Methods: Construction materials (red brick, cement brick, and gypsum board) coated with reducing agent were placed in a chamber to measure radon emissions. The construction materials were coated one through three times. The spread volume for brick and gypsum board was 50 mL and 75 mL per application, respectively. The amount of radon emitted was measured by RAD-7 after 48 hours. Results: The reduction ratio increased with the number of coatings, and the reduction ratios for red brick, cement brick, and gypsum board were 63.3, 73.6, and 58%, respectively, in the case of three coatings of RA-1. The reduction ratios for red brick, cement brick, and gypsum board were 42.8, 58.1, and 26.2%, respectively in the case of three coatings with RA-2. RA-1 was slightly better than RA-2 in radon emission reduction. Conclusions: Radon emissions from construction materials decreased according to the concentration of reducing agent coating, and it was more effective than existing methods.
The pearlesent pigment has received attention in a diversity of fields like cosmetics, inks, paints and so on. Ferric Ferrocyanide, one of the nano sized pearlescent pigment, is a kind of surface modification pigment that covers a metal oxidized substance or a coloring agent with uniform thickness. Characteristics of pearlescent pigment are various interference color, intense gloss effect and a three-dimensional effect. We synthesised the pearlesent pigment that ferric ferrocyanide can be deposited on the titania/mica surface by hydrothermal synthesis method. The process parameters are concentration of precursor, controlling pH and reaction temperature. The optimun conditions is that amount of iron(III) chloride hexahydrate is 3.1 wt% and amount of potassim ferrocynide trihydrate is 3.6 wt% in the started pH 4.5 at $70^{\circ}C$. The coating rate and coating efficiency of ferric ferrocyanide was about 1.47 % and 96.7 %, respectively. The synthesised pearlesent pigment was characterized by SEM, XRD, FT-IR and EDS.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.