Coagulant bath medium effect towards polylactic acid membranes structure and methylene blue dye removal

  • Amira M. Nasib;Stephen Simon;Syahmie M. Rasidi;Siti Kartini E. Ab. Rahim;Hoo Peng Yong;Ng Qi Hwa;Khairiraihanna Johari
    • Advances in materials Research
    • /
    • v.13 no.3
    • /
    • pp.243-251
    • /
    • 2024
  • The asymmetric polylactic acid (PLA) membrane was prepared via phase inversion method using non-solvent induced separation (NIPS) technique. This study aims to synthesized as well as to characterize the PLA membrane and evaluating the membrane performance on water flux and permeability. In addition, this research also studied the removal performance of methylene blue dye. The polymer solution has been prepared using 12 wt.% of PLA and dissolved in 88 wt.% of Dimethylacetamide (DMAc) as a solvent. Then, the cast film was immersed in different ratio of coagulant bath medium (distilled water: methanol: ethanol) ranging from 100:0:0, 75:25:0, 75:0:25 and 75:12.5:12.5, respectively). Several characterizations were performed which include, membrane contact angle and membrane porosity. Performance PLA membranes were determined in terms of water flux and permeability at 1 bar transmembrane pressure using dead-end permeation cell. Finally, methylene blue (MB) removal efficiency was tested at the same transmembrane pressure. The findings revealed that the increase of alcohol concentration in coagulant bath resulted in higher porosity and lower contact angle. In short, MB dye rejection efficiency is also closely related to the amount of alcohol ratio used in coagulant baths. Increases in concentration of methanol and ethanol in coagulant bath medium increases the membrane porosity thus increased in efficiency of methylene blue rejection.

The Effect of Coagulant and Molecular Weight on the Wet Spinnability of Regenerated Silk Fibroin solution

  • Yoo, Young-Jin;Kim, Ung-Jin;Um, In-Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.21 no.1
    • /
    • pp.145-150
    • /
    • 2010
  • The regenerated silk fibroin with various molecular weights (MW) was prepared by different dissolution condition and the effect of coagulant on the wet spinnability of the various MW silk fibroin solutions dissolved in formic acid was investigated by the observation of wet spun filament in coagulant and the measurement of maximum draw ratio. The observation on the wet spun filament in coagulation bath revealed that good fibers without bead were formed in a high MW and a very high MW silk fibroin samples. In contrast, beads were observed in the silk fibroin sample with medium MW. The maximum draw ratio of wet spun silk fibroin filament decreased with MW reduction. The decrease of maximum draw ratio in isopropanol, acetone, DMF and THF was remarkably higher than that in methanol and ethanol, indicating that the coagulant type strongly influenced the wet spinnability. The two simple evaluation methods used in this study showed complementary information for wet spinnability: (a) The observation of filament in coagulant was effective to check a continuous fiber formation and a bead formation, and (b) the maximum draw ratio measurement was useful to examine the post drawing ability related to molecular orientation.

Rheological Analysis in a Spinning Process of a hollow fiber membrane

  • Jang, Moon-Seog
    • Proceedings of the Membrane Society of Korea Conference
    • /
    • 1995.10a
    • /
    • pp.5-9
    • /
    • 1995
  • In the dry-jet-wet-spinning process of a hollow fiber membrane, the polymer solution is pumped into a coaxial tube, jet spinneret. The threadline emerging from the spinneret is stabilized by an internal coagulating medium(liquid or gas) as it emerges from the jet orifice. The nascent hollow thread is further stabilized in a quench bath as shown in Fig. 1. In this scheme, three mechanism of formatiota(temperature gradient, solvent evaporation, and solvent-nonsotvent exchange) can be combined. The changes which promote stabilization often play a dominant role in determining the ultimate fiber wall structure as well. Hence, in pratice, hollow fiber stabilization and development of membrane structure are commonly inseparable. However, fiber dimension(the inside diameter and wall thickness of the hollow fiber) is mainly a rheological problem and is determined by dope pumping rate, spinneret diatance from the coagulation bath, inner coagulant flow rate, and fiber draw-rate. Besides rheological phenomena play a prominent part in the final properties of the hollow fiber.

  • PDF

Phase Behavior and Morphological Studies of Polysulfone Membranes; The Effect of Alcohols Used as a Non-solvent Coagulant (비용매 알코올 응고조를 이용한 폴리술폰 막의 상전이 거동 및 모폴로지 특성 연구)

  • Park Byung Gil;Kong Sung-Ho;Nam Sang Yong
    • Membrane Journal
    • /
    • v.15 no.4
    • /
    • pp.272-280
    • /
    • 2005
  • In this study, asymmetric polysulfone membranes were prepared by the phase inversion method and the casting solutions were containing N-methyl-2-pyrrolidone (NMP) as a solvent. Deionized water and various alcohols(methanol, ethanol, and propanol) were used as a coagulation medium in preparing asymmetric polysulfone membranes. This study investigates the effect of alcohol coagulants having different solubility parameters as a pore-former on the construction of porous structures and their pure water permeation properties. Asymmetric polysulfone membranes immersed in the pure alcohol coagulation bath solution showed the typical sponge-like structures and the reduced water permeability as compared with those of polysulfone membranes precipitated in the pure water coagulation bath solution. In the water/alcohol mixtures, asymmetric polysulfone membranes showed the finger-like structures with the sponge-like structures. Therefore, the sponge-like structure of polysulfone membrane was formed under the delayed demixing systems while the porosity of membrane was decreased significantly. The water permeability of polysulfone membrane precipitated in the pure water coagulant showed 164 [$L/m^2hr$] at 14.7 psi. In case of polysulfone membranes prepared in the pure methanol and ethanol coagulant, they showed the water permeability of 56 and 30 [$L/m^2hr$], respectively.