• 제목/요약/키워드: chromium oxidation

검색결과 107건 처리시간 0.027초

TiO2에 담지된 금속 산화물 촉매상에서 TCE 산화분해반응 (Oxidative Decomposition of TCE over TiO2-Supported Metal Oxide Catalysts)

  • 양원호;김문현
    • 한국환경과학회지
    • /
    • 제15권3호
    • /
    • pp.221-227
    • /
    • 2006
  • Oxidative TCE decomposition over $TiO_2$-supported single and complex metal oxide catalysts has been conducted using a continuous flow type fixed-bed reactor system. Different types of commercial $TiO_2$ were used for obtaining the supported catalysts via an incipient wetness technique. Among a variety of titanias and metal oxides used, a DT51D $TiO_2\;and\;CrO_x$ would be the respective promising support and active ingredient for the oxidative TCE decomposition. The $TiO_2-based\;CrO_x$ catalyst gave a significant dependence of the catalytic activity in TCE oxidation reaction on the metal loadings. The use of high $CrO_x$ contents for preparing $CrO_x/TiO_2$ catalysts might produce $Cr_2O_3$ crystallites on the surface of $TiO_2$, thereby decreasing catalytic performance in the oxidative decomposition at low reaction temperatures. Supported $CrO_x$-based bimetallic oxide systems offered a very useful approach to lower the $CrO_x$ amounts without any loss in their catalytic activity for the catalytic TCE oxidation and to minimize the formation of Cl-containing organic products in the course of the catalytic reaction.

Determination of Chemical Compositions and Oxidation States for Corrosion Products in LiCl Molten Salts

  • Park, Yong-Joon;Pyo, Hyung-Ryul;Kim, Do-Yang;Jee, Kwang-Yong;Kim, Won-Ho
    • Nuclear Engineering and Technology
    • /
    • 제32권5호
    • /
    • pp.514-520
    • /
    • 2000
  • The mechanism of corrosion behavior has to be understood clearly to select an optimum material for handling molten salts to be used in the oxide reduction process of PWR spent fuel. In this study, the oxidation states of corrosion products on the surface of Inconel 600 and 800H as well as their chemical compositions and structural informations were determined by using XPS, ICP-AES, AAS, EPMA and XRD after the corrosion experiment with lithium molten salts at 75$0^{\circ}C$ for 25 hours. Nickel and oxygen were detected from the corrosion products on the surface of Inconel plates and chromium was found to be dissolved out into lithium molten salts leaving cracks on the surface. The corrosion products were identified as metal oxides such as Fe$_2$O$_3$, Cr$_2$O$_3$, NiO, NiFe$_2$O$_4$and MnO by using XPS and XRD.

  • PDF

철에 의한 버네사이트의 결정도 및 화학적 활성의 변화 (Crystallinity and Chemical Reactivity of Bimessite(δ-MnO2) Influenced by Iron)

  • 김재곤
    • 한국토양비료학회지
    • /
    • 제32권4호
    • /
    • pp.327-332
    • /
    • 1999
  • 산화망간이 영양소물질과 오염물질과의 반응 및 망간이 식물의 필수 미량원소 등으로 인해 토양학에서 산화망간은 중요한 연구의 대상이 되어왔다. 토양 내에서 가장 흔한 산화망간 광물중의 하나인 버네사이트를 철의 존재 하에서 합성하였다. 토양 내에서 흔한 원소의 하나인 철이 버네사이트의 결정도, 형태 및 화학적 활성에 미치는 영향을 X-선회절, 전지현미경, 양이온 교환능력 및 크롬 산화력을 이용하여 연구하였다. 침전용액내의 철의 함량이 증가할수록 버네사이트의 결정도와 입자의 크기는 감소하였다. 침전된 버네사이트는 낮은 철의 농도에서 육각 판상형이 우세하였으나 농도가 증가 할 수록 미세입자로된 입단이 증가하였다. 그리고 크롬 산화능력은 철의 농도가 증가함에 따라 증가하였다. 양이온 치환능력은 철의 농도와 상관관계가 없었다. 침전용액속의 철은 버네사이트의 결정핵의 형성을 증가시켰고 표면흡착에 의해 결정의 성장을 방해하였다. 철은 토양 망간단과 내에서 산화철과 산화망간의 공존으로 미루어 보아 토양내의 버네사이트의 작은 입자, 낮은 결정도 및 높은 화학적 활성에 기여한 것으로 사료된다. 본 연구에서 입증된 버네사이트의 높은 양이온 교환 능력과 산화력은 버네사이트를 환경과 농업에 활용 가능성이 있음을 제시해준다.

  • PDF

산화성 크롬의 배양세포에서의 독성작용 (Toxic Activities of the Oxidant Chromate in Culture Cells)

  • 박형숙
    • Environmental Analysis Health and Toxicology
    • /
    • 제13권1_2호
    • /
    • pp.1-9
    • /
    • 1998
  • The ROS-producing potency of chromium compounds of several oxidation states were determined in the H4 cells. $K_2Cr_2O_7$ as Cr (VI), synthetic Cr (V) compounds and Cr (III) as TPP produced high level of ROS. However, ROS values of Cr-picolinate as Cr (III), CrCl$_2$, CrCI$_2$, were almost equal to the control. The effects of physiological antioxidants compounds which react with free radicals were examined for their effects on chromate-induced production of reactive oxygen species (ROS) in A549 cells after the addition of $K_2Cr_2O_7$. The compounds used were vitamin C (ascorbate), vitamin E ($\alpha$-tocopherol), superoxide dismutase (SOD) and catalase. The preincubation of ascorbate (200uM) with A549 cells for 20hr resulted in a significant reduction of hexavalent chromate(100uM) induced ROS. However, there is no effects of preincubation of the cells with vitamin E succinate (10 and 20uM, 20hr) on the ROS production. Also, the effects of Cr (VI) on the cell cycle of A549 cells was measured by adding the DNA intercalating agent, propidium iodide. S phase of the cell cycle was increased by the chromium (VI) compounds up to 20uM indicating toxicity or possible mitogenic action of the cell. The shoulder in Go/G1 phase at 20uM Cr (VI) with 24 hr treatment indicates apoptosis.

  • PDF

폐산화철촉매에 의한 도금폐수중 크롬이온 회수에 관한 기초연구 (A study on the recovery of chromium from metal-plating wastewater with spent catalyst)

  • 이효숙;오영순;이우철
    • 자원리싸이클링
    • /
    • 제13권2호
    • /
    • pp.9-15
    • /
    • 2004
  • 석유화학공정으로부터 폐기되는 폐산화철촉매를 이용하여 도금합성폐수중 크롬회수에 관한 연구를 회분식과 연속식으로 실시하였다. 도금합성제수 중 $CrO _{4}^{-2}$ 형태의 음이온으로 존재하는 6가 크롬은 폐산화철촉매의 등전점(pH 3.0)이하에서 폐촉매와 물리적 흡착을 한다. 한편, 6가 크롬은 pH 3.0 이상에서도 폐촉매의 수산화철과 산화환원반응에 의해 일부 환원되어 $Cr(OH)_3$로 침전한다. 컬럼을 이용한 크롬 연속회수실험에서 크롬합성폐수의 pH가 0.5∼2.0일 때 폐촉매의 크롬흡착량은 2.0∼2.3g/L이며, pH가 3.0에서는 1.5g/L이었다. 폐수 중 크롬농도가 50∼500mg/L로 높아질수록 폐촉매에 흡착한 크롬누적량은 1.29∼8.56g/L로 증가하지만, 유속이 30∼80 ml/mm으로 증가하여도 크롬 흡착누적량은 2.21∼2.49 mg/L로 거의 유사하였다.

전기화학적 산소요구량 측정용 이산화납 전극 센서의 유효성 (Effectiveness of the Sensor using Lead Dioxide Electrodes for the Electrochemical Oxygen Demand)

  • 김홍원;정남용
    • 한국생산제조학회지
    • /
    • 제21권4호
    • /
    • pp.575-581
    • /
    • 2012
  • The electrochemical oxygen demand (ECOD) is an additional sum parameter, which has not yet found the attention it deserves. It is defined as the oxygen equivalent of the charge consumed during an electrochemical oxidation of the solution. Only one company has yet developed an instrument to determine the ECOD. This instrument uses $PbO_2$-electrodes for the oxidation and has been successfully implemented in an automatic on-line monitor. A general problem of the ECOD determination is the high overpotential of electrochemical oxidations of most organic compounds at conventional electrodes. Here we present a new approach for the ECOD determination, which is based on the use of a solid composite electrodes with highly efficient electro-catalysts for the oxidation of a broad spectrum of different organic compounds. Lead dioxide as an anode material has found commercial application in processes such as the manufacture of sodium per chlorate and chromium regeneration where adsorbed hydroxyl radicals from the electro-oxidation of water are believed to serve as the oxidizing agent. The ECOD sensors based on the Au/$PbO_2$ electrode were operated at an optimized applied potential, +1.6 V vs. Ag/AgCl/sat. KCl, in 0.01 M $Na_2SO_4$ solution, and reduced the effect of interference ($Cl^-$ and $Fe^{2-}$) and an expended lifetime (more than 6 months). The ECOD sensors were installed in on-line auto-analyzers, and used to analyze real samples.

2,2'-Bipyridinium Chlorochromate에 의한 치환 벤질 알코올류의 산화반응과 메카니즘에 관한 연구 (A Study for Mechanism and Oxidation Reaction of Substituted Benzyl Alcohols by 2,2'-Bipyridinium Chlorochromate)

  • 김영식;박영조
    • 한국산학기술학회논문지
    • /
    • 제13권7호
    • /
    • pp.3252-3260
    • /
    • 2012
  • 6M HCl 용매 하에서 2,2'-bipyridine과 chromium(VI) trioxide의 반응을 통하여 2,2'-bipyridinium chlorochromate[$C_{10}H_8N_2HCrO_3Cl$]를 합성하여, 적외선분광광도법(IR), 유도결합 플라즈마(ICP) 등으로 구조를 확인하였다. 여러 가지 용매 하에서 2,2'-bipyridinium chlorochromate를 이용하여 벤질 알코올의 산화반응을 측정한 결과 유전상수(${\varepsilon}$) 값이 큰 용매 즉, 시클로헥센<클로로포름<아세톤$p-CH_3$, H, m-Br, $m-NO_2$)을 효과적으로 산화시켰다. 그리고 전자받개 그룹들은 반응속도가 감소한 반면에 전자주개 치환체들은 반 응속도를 증가시켰다. 또한 Hammett 반응상수(${\rho}$) 값은 -0.64(303K) 이었다. 이러한 알코올류의 산화반응성은 polysilsesquioxane과 같은 고분자물질을 용해시켜 코팅제로 활용할 때 열안정성과 같은 물성을 연구하는데 중요한 인자 가 될 수 있다. 그러므로 본 실험에서 알코올의 산화반응 과정은 속도결정단계에서 수소화 전이가 일어나는 메카니즘임 을 알 수 있었다.

High Temperature Corrosion in Carbon-Rich Gases

  • Young, D.J.
    • Corrosion Science and Technology
    • /
    • 제7권2호
    • /
    • pp.69-76
    • /
    • 2008
  • Common methods for large scale hydrogen production, such as steam reforming and coal gasification, also involve production of carbonaceous gases. It is therefore necessary to handle process gas streams involving various mixtures of hydrocarbons, $H_2$, $H_2O$, CO and $CO_2$ at moderate to high temperatures. These gases pose a variety of corrosion threats to the alloys used in plant construction. Carbon is a particularly aggressive corrodent, leading to carburisation and, at high carbon activities, to metal dusting. The behaviour of commercial heat resisting alloys 602CA and 800, together with that of 304 stainless steel, was studied during thermal cycling in $CO/CO_2$ at $650-750^{\circ}C$, and also in $CO/H_2/H_2O$ at $680^{\circ}C$. Thermal cycling caused repeated scale separation, which accelerated chromium depletion from the alloy subsurface regions. The $CO/H_2/H_2O$ gas, with $a_C=2.9$ and $p(O_2)=5\times10^{-23}$ atm, caused relatively rapid metal dusting, accompanied by some internal carburisation. In contrast, the $CO/CO_2$ gas, with $a_C=7$ and $p(O_2)=10^{-23}-10^{-24}$ atm caused internal precipitation in all three alloys, but no dusting. Inward diffusion of oxygen led to in situ oxidation of internal carbides. The very different reaction morphologies produced by the two gas mixtures are discussed in terms of competing gas-alloy reaction steps.

Cr (VI) 촉매에 의한 Tetraline 의 선택적 산화반응 (I) (A Selective Oxidation of Tetraline by Chromium (VI) Compounds (I))

  • 배선건;이상봉;박대철;이규완
    • 대한화학회지
    • /
    • 제33권1호
    • /
    • pp.106-112
    • /
    • 1989
  • Tetralin의 액상 공기 산화반응에 N,N-dialkylamide 용매하에서 Cr(Ⅵ)의 heterocyclic base염들과 CrO$_3$-N,N-dialkylamide complex계를 적용한 결과 CrO$_3$-N,N-dialkylamide complex의 경우, 반응온도 90$^{\circ}$C에서 tetralin의 전환율이 35.2%이었고, ${\alpha}$-tetralone의 선택율은 96.1%이었으며, ${\alpha}$-tetralol은 무시할만한 양으로 생성되었다.

  • PDF

X20CrMoV12.1 고크롬강의 고온산화거동 (The high temperature oxidation behavior of X20CrMoV12.1 high-chromium steel)

  • 정진성;김두수;김범수;김의현;하정수
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.46-46
    • /
    • 2003
  • 고크롬강은 산업용 발전설비의 효율적인 열교환을 위해 수천개의 튜브로 구성된 보일러에 적용되고 있다. 이러한 보일러 튜브는 고온에 노출되어 있으며, 튜브 내면에는 고온의 증기가 고압으로 존재하고 있다. 따라서 보일러 튜브는 장기간 고온의 환경에서 사용되기 때문에 고온강도와 고온내산화 및 내부식 특성이 요구된다. 보일러 튜브의 열화는 이세조직 변화에 따른 고온강도의 저하를 재료내부의 열화와 고온산화 및 부식 등 외부환경에 의 한 열화로 크게 두 가지로 대별된다. 이러한 보일러 튜브의 수명평가는 튜브의 수명을 미리 예측하여 적절한 시점에 교체함으로서 운전 중 손상에 따른 발전정지 등을 방지하여 막대한 비용을 절감할 수 있기 때문에 현장에서는 중요한 의미를 갖는다. 본 연구에서는 보일러 튜브의 여러 가지 수명평가 방법 중 현재 산업용 발전설비의 보일러에 적용되고 있는 X-20 고크롬강의 고온산화 거동을 조사하여 향후 보일러 튜브의 수명평가 방법 중 산화스케일을 이용한 방법에 활용하는데 있어 기초 자료로 이용하고자 한다.