• Title/Summary/Keyword: carbon dioxide curing

Search Result 41, Processing Time 0.03 seconds

Syntheses and Characterization of UV-curable Polyurethane Acrylates with Eco-friendly Polyols (친환경 폴리올을 이용한 광경화형 폴리우레탄 아크릴레이트의 합성)

  • Lee, Bong;Kim, Yeong Woo;Lee, Won-Ki
    • Journal of Adhesion and Interface
    • /
    • v.20 no.4
    • /
    • pp.140-145
    • /
    • 2019
  • In view of environmental considerations, the control of carbon dioxide (CO2) and volatile organic compounds (VOCs) is one of important issues in the film and coating industries. Therefore, UV-curable system has been developed due to minimize emissions of VOCs and reduce CO2 emission due to low energy consumption from fast curing. Also, biodegradable polymers economically are attractive because of environmental and economic concerns associated with huge waste plastics. In this study, UV-curable polyurethane acrylates with different compositions of biodegradable polylactide (PLA) diol and poly(ethylene glycol) as diols were synthesized and curing reaction of their end-capped acrylates was performed by UV exposure. Tensile strength, elongation, and Tg of the UV-cured polyurethane acrylates increased with PLA diol content in the diol while their hydrophilicity and thermal stability increased with the PEG content. These results indicated a property of UV-cured polyurethane acrylates could be controlled by environment-friendly diols.

Hydration and Carbonation Properties of Different Hydraulic Lime (수경성석회 종류에 따른 수황 및 탄산화 특성)

  • Moon, Ki-Yeon;Choi, Moon-Kwan;Cho, Kye-Hong;Cho, Jin-Sang;Ahn, Ji-Whan;Yeon, Kyu-Seok
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.2
    • /
    • pp.72-81
    • /
    • 2014
  • The main mineral phases of natural hydraulic lime (NHL) as a hydraulic lime binderare $Ca(OH)_2$, $C_2S$, $C_3S$, $C_3A$, and $SiO_2$ residues. Also, NHL has the characteristic of setting and hardening by a hydration reaction with water and by carbonation reactions with carbon dioxide from the air. In this study, in an effort to investigate changes of the mineral phases by NHL hydration and carbonation reactions, transitions of mineral phases and the microstructures of hardened pastes were analyzed by XRD, DSC, SEM, and by pore size distributions using domestic and foreign-sourced NHL pastes after curing at 1, 3, 7, and 28 days. On the basis of the analysis results, it was confirmed that domestic low-grade limestone can be used for the manufacturing of NHL. The main hydration mineral phases were $Ca(OH)_2$, $CaCO_3$, $C_2S$, and $SiO_2$ residues, while in the case of foreign-sourced NHL, a small amount of an aluminium hydration phase formed. Also, the $CaCO_3$ content after the carbonation reaction increased with an increase in the curing time. After hydration for 28 days, NHL containing considerable amounts of $C_2S$ and $C_3S$ showed higher carbonation ratios than others types.

Noncement-based Hydroball Evaluation of Permeable Block Strength Properties (무시멘트 기반 하이드로볼을 활용한 투수블록의 강도 특성)

  • Hwang, Woo-Jun;Lee, Chang-Woo;Lee, Sang-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2022.11a
    • /
    • pp.207-208
    • /
    • 2022
  • Since 1960, the green area has decreased due to rapid urbanization and the artificial surface has increased, and the repair and water function of the previous surface has decreased due to the decrease in rainwater absorption capacity. In addition, the risk of carbon dioxide and fine dust is emerging due to the use of fossil fuels due to urbanization. As a result, permeable blocks, an eco-friendly product, are in the spotlight. Therefore, this study was conducted to examine the strength properties of the permeable block using a hydroball. As a result of the experiment, the flexural strength and compressive strength tended to decrease as the hydroball replacement rate increased. It is judged that the hydroball absorbs a large amount of moisture during the mixing process and lacks moisture required for curing, resulting in a decrease in strength. According to KS F 4419, since the hydroball replacement rate is satisfied up to 20%, further research is needed to analyze the adsorption performance of air pollutants in the future and evaluate their utilization as a permeable block in the future.

  • PDF

Investigation of Early-Age Concrete Strength Development Using Hardening Accelerator (경화촉진제를 사용한 콘크리트의 초기강도 발현 특성 검토)

  • Kim, Gyu-Yong;Kim, Yong-Ro;Park, Jong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.28 no.3
    • /
    • pp.309-316
    • /
    • 2016
  • In this study, performance of hardening accelerator types which promote setting and hardening of cement has been reviewed in order to develop early age strength of concrete with compressive strength of 21~27 MPa after examination of strength development of the concrete at early age according to curing temperature and unit cement(binder) content. As results, soluble mineral salt showed better hardening acceleration effect than organic salt in the scope of this study. Also, hydration reaction accelerating effect of $C_3S$ by Soluble mineral salt is effective on development of early age compressive strength and it was shown that the Pt's hydration reaction accelerating effect was the best. Construction duration reduction can be expected by securing compressive strength for prevention of early aged freezing damage in 25hour-curing time under curing temperature at $15^{\circ}C$. Also, it was shown that compressive strength of specimen cured at $5^{\circ}C$ was similar with plain specimen cured at $10^{\circ}C$. Therefore, it is expected that fuel costs and carbon dioxide can be reduced when the same construction duration is considered.

Properties of Non-Sintered Hwangtoh Mortar Using Eco-Friendly Inorganic Binding Material (친환경 무기결합재를 이용한 비소성 황토모르타르의 특성)

  • Heo, Jun-Oh;Lee, Jae-Kyu;Hyung, Won-Gil
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.4
    • /
    • pp.499-506
    • /
    • 2014
  • A number of studies on eco-friendly and healthy building materials are being conducted as modern people are becoming more conscious about health and the environment they live in. Among those materials, studies on Hwangtoh are the most prevalent but due to its strength, crack coming from drying shrinkage, and susceptibility to water, the usage of Hwangtoh is incomplete and limited to be used as a common building material. Cement concrete, considered as one of the most widely used building materials, is extensively used in construction because it is economical, easily accessible and moldable and has proper compressive strength. Due to carbon dioxide created in the process of making cement concrete, it is recognized as pollution. Accordingly, there are a lot of studies on reduction of carbon dioxide in cement concrete industry. There are increasing numbers of researches as well as developments on Hwangtoh or traditional construction materials used in South Korea to reduce the environmental problems. Therefore, this study suggests the basic features of the construction material that can replace cement concrete in the future with the non-sindtered cement mixed with non-sintering hwangtoh which is made with the furnace slag and multiple stimulants.

Characteristics of Solidification/Carbonation in the Heavy-Metal-Contaminated Sediment Treated by MgO-Based Binder (MgO 기반 고화제를 이용하여 처리한 중금속 오염 준설토의 고형화/탄산염화 특성)

  • Hwang, Kyung-Yup;Seo, Jeong-Yun;Phan, Hoang Quang Huy;Ahn, Jun-Young;Hwang, Inseong
    • Journal of Soil and Groundwater Environment
    • /
    • v.18 no.1
    • /
    • pp.102-111
    • /
    • 2013
  • A novel MgO-based binder was developed and applied to treat the anoxic sediment that was collected from Seonakdong river, Korea and was contaminated with heavy metals. The treated sediment was evaluated by measuring compressive strength, expansion, leaching of heavy metals and storage characteristics for $CO_2$. Initially, an optimal blending ratio of lime (L)/fly ash (FA)/blast furnace slag (BFS) that was to be mixed with MgO was screened to be $L_{0.3}-FA_{0.1}-BFS_{0.6}$. Long-term strengths of the sediments that were treated by various mixtures of MgO and $L_{0.3}-FA_{0.1}-BFS_{0.6}$ were then evaluated and the blending ratios between 4 : 6 and 6 : 4 were found optimal, which yielded a compressive strength of 4.09 MPa. On this basis, the optimal MgO-based binder was selected to be a 5 : 5 mixture of MgO and $L_{0.3}-FA_{0.1}-BFS_{0.6}$. The good performance of the MgO-based binder was believed to be due to the formation of Mg $(OH)_2$, which filled the micropores and also increased the density of the solidified matrices. The MgO-based binder exhibited an average stabilizing capacities for heavy metals of 92.9%, which was similar to or higher than that of Portland cement. It was found that 69.1 kg of carbon dioxide could be sequestrated after 365 days of curing when treating a ton of anoxic sediments.

Characterizations and Quantitative Estimation of Alkali-Activated Binder Paste from Microstructures

  • Kar, Arkamitra;Ray, Indrajit;Halabe, Udaya B.;Unnikrishnan, Avinash;Dawson-Andoh, Ben
    • International Journal of Concrete Structures and Materials
    • /
    • v.8 no.3
    • /
    • pp.213-228
    • /
    • 2014
  • Alkali-activated binder (AAB) is recently being considered as a sustainable alternative to portland cement (PC) due to its low carbon dioxide emission and diversion of industrial wastes and by-products such as fly ash and slag from landfills. In order to comprehend the behavior of AAB, detailed knowledge on relations between microstructure and mechanical properties are important. To address the issue, a new approach to characterize hardened pastes of AAB containing fly ash as well as those containing fly ash and slag was adopted using scanning electron microscopy (SEM) and energy dispersive X-ray spectra microanalyses. The volume stoichiometries of the alkali activation reactions were used to estimate the quantities of the sodium aluminosilicate (N-A-S-H) and calcium silicate hydrate (CSH) produced by these reactions. The 3D plots of Si/Al, Na/Al and Ca/Si atom ratios given by the microanalyses were compared with the estimated quantities of CSH(S) to successfully determine the unique chemical compositions of the N-A-S-H and CSH(S) for ten different AAB at three different curing temperatures using a constrained nonlinear least squares optimization formulation by general algebraic modeling system. The results show that the theoretical and experimental quantities of N-A-S-H and CSH(S) were in close agreement with each other. The $R^2$ values were 0.99 for both alkali-activated fly ash and alkali-activated slag binders.

Application of Precast Concrete Products of Non-Sintered Cement Mortar based on Industrial by-Products (산업부산물을 이용한 비소성 시멘트 모르타르의 프리캐스트콘크리트 제품 적용성 평가)

  • Na, Hyeong-Won;Moon, Kyoung-Ju;Hyung, Won-Gil
    • Journal of the Korea Institute of Building Construction
    • /
    • v.20 no.1
    • /
    • pp.19-26
    • /
    • 2020
  • This study aimed to develop non-sintered cement that could replace portland cement which emits large amount of carbon dioxide during firing process. For this purpose, ground granulated blast furnace slag, type c fly ash and slaked lime were used. In addition, through the experimental results, the characteristics of the non-sintered cement binders according to the mixing ratios will be identified, and the utilization plans for the precast concrete products will be presented. In this experiment, non-sintered cement binders using industrial by-products were prepared to compare the flexural strength and compressive strength of each of the 3, 7 and 28 days. As a result, the results satisfy the KS of the target product proposed in this study. Therefore, this study presents the possibility of using precast concrete products by developing non-sintered cement binders using industrial by-products.

Strength and Carbonation Characteristics in OPC Concrete under Long-Term Exposure Conditions in Various Sea Environments (다양한 해양환경에 장기 노출된 OPC 콘크리트의 강도 및 탄산화 특성 )

  • Hyeon-Woo Lee;Geum-Chae Shin;Seung-Jun Kwon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.28 no.1
    • /
    • pp.53-60
    • /
    • 2024
  • Compressive strength in concrete has many affecting parameters and varies with exposure conditions. Although the concrete has same mix proportions, its properties are different with exposure conditions, and sea-environment can be classified into three groups such as tidal, atmospheric, and sea submerged region particularly. In this study, compressive strength was evaluated on 7-year-cured concrete and the results from previous equations (KDS, ACI, CEB, and JSCE) were compared with them. Furthermore the strength and carbonation progress were evaluated on concrete cured for 7 years exposed to three different sea environment. Three levels of w/c (water to cement) ratio (0.37, 0.42, and 0.47) and three different exposure conditions (tidal, atmospheric, and submerged) were considered. The results from wet-cured condition are all higher than those from the previously proposed equations, and the results from different sea exposure conditions (tidal, atmospheric, and submerged region) were lower than those from wet-cured condition. A reduction of strength was evaluated with increasing w/c ratio and the minimum strength was evaluated in the sea-submerged conditions. Several experimental constants applicable to the previous equations were obtained from regression analysis since the strength change with w/c ratios were not considered in those equations. Regarding carbonation depth with different exposure conditions, higher carbonation depth clearly was observed with increasing w/c ratios, and evaluated in the order of atmospheric, submerged, and tidal region. Considerable carbonation depth was observed in submerged and tidal region due to sulfate ion and dissloved carbon dioxide as well.

Mineralogical Analysis of Calcium Silicate Cement according to the Mixing Rate of Waste Concrete Powder (폐콘크리트 미분말 치환율에 따른 이산화탄소 반응경화 시멘트의 광물상 분석)

  • Lee, Hyang-Sun;Song, Hun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.24 no.2
    • /
    • pp.181-191
    • /
    • 2024
  • In the realm of cement manufacturing, concerted efforts are underway to mitigate the emission of greenhouse gases. A significant portion, approximately 60%, of these emissions during the cement clinker sintering process is attributed to the decarbonation of limestone, which serves as a fundamental ingredient in cement production. Prompted by these environmental concerns, there is an active pursuit of alternative technologies and admixtures for cement that can substitute for limestone. Concurrently, initiatives are being explored to harness technology within the cement industry for the capture of carbon dioxide from industrial emissions, facilitating its conversion into carbonate minerals via chemical processes. Parallel to these technological advances, economic growth has precipitated a surge in construction activities, culminating in a steady escalation of construction waste, notably waste concrete. This study is anchored in the innovative production of calcium silicate cement clinkers, utilizing finely powdered waste concrete, followed by a thorough analysis of their mineral phases. Through X-ray diffraction(XRD) analysis, it was observed that increasing the substitution level of waste concrete powder and the molar ratio of SiO2 to (CaO+SiO2) leads to a decrease in Belite and γ-Belite, whereas minerals associated with carbonation, such as wollastonite and rankinite, exhibited an upsurge. Furthermore, the formation of gehlenite in cement clinkers, especially at higher substitution levels of waste concrete powder and the aforementioned molar ratio, is attributed to a synthetic reaction with Al2O3 present in the waste concrete powder. Analysis of free-CaO content revealed a decrement with increasing substitution rate of waste concrete powder and the molar ratio of SiO2/(CaO+SiO2). The outcomes of this study substantiate the viability of fabricating calcium silicate cement clinkers employing waste concrete powder.